IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1150 documents. Displaying 25 entries per page.


Changes of EPR spectra of wood, impregnated with copper based preservatives, during exposure to Antrodia vaillantii
2000 - IRG/WP 00-10355
Spruce wood (Picea abies) samples were impregnated with two different aqueous solutions: copper(II) octanoate with ethanolamine or copper(II) sulfate (cCu = 1,0 x 10-2 mol/l). Impregnated and unimpregnated test pieces were exposed to wood rotting fungus Antrodia vaillantii. Some strains of this fungus are known as copper tolerant. After four weeks of exposure to A. vaillantii, we could not detect ...
M Humar, M Petric, F Pohleven, M Šentjurc


The development of a new boron-based wood preservative
1995 - IRG/WP 95-30085
The paper describes a new boron based wood preservative for the treatment of green timber. The product offers many benefits over conventional boron diffusion treatment including: 1. high viscosity, high concentration formulation; 2. permits dip treatment of a wide range of sawn board and pole sizes at ambient temperatures; 3. permits full cross section diffusion of borates without block stacking a...
P Turner, D Conradie


The examination of preservative-treated radiata pine using electron spin resonance spectroscopy
1987 - IRG/WP 3423
Electron spin resonance spectroscopy (ESR) may be used to characterise the molecular environment of chemical species containing unpaired electrons. These species include free radicals, bi-radicals, point defects in solids, localised crystal imperfections and many transition metal ions. ESR has previously been applied to the examination of wood weathering or wood pyrolysis and now FRI and Massey Un...
D V Plackett, E W Ainscough, A M Brodie


A comparison of analytical and visual techniques used for assessment of weathering properties of chromium and copper azole treated timber
1994 - IRG/WP 94-20023
The weathering properties of preservative treated timber were studied by measuring surface lignin loss and by microscopic examination after weathering, and results were related to qualitative assessments of visual appearance after weathering. Measurement of relative rates of delignification of untreated and preservative treated timber obtained by FTIR analysis, and weight loss determined on thin v...
J A Cornfield, M D C Hale, G Fettis


Performance of Copper-Chrome-Arsenic (CCA) and Copper-Chrome-Boric (CCB) treated panels of Bombax ceiba and Paraserianthus falcataria against bio-deterioration at Krishnapatnam harbour, east coast of India
2003 - IRG/WP 03-30310
Results of investigations on the durability of light weight timber species (Specific gravity below 0.4) i.e., Bombax ceiba and Paraserianthus falcataria in treated and untreated condition conducted at Krishnapatnam harbour (Lat 13o28’ to 13o59’ N; Long: 80o10’ to 80o16’E) along the east coast of India are reported in the paper. Exposure trails were conducted with panels (Size: 30 x 3.8 x...
B Tarakanadha, N R Raveendra Prasad, K S Rao


The use of low cost X-ray fluorescence instruments in the determination of copper chromium and arsenic in preservative treated wood
1987 - IRG/WP 2278
Internal quality control in timber treatment plants can be pursued by analysis of preservative treatment solutions and treated timber. Treaters must proceed with costly and lengthy analyses through analytical laboratories. An alternative approach for the timber treater, is to use low cost analysers (L.C.A.'s) based upon x-ray fluorescence. Detailed comparisons have been made between stand...
J Norton, L E Leightley


Preservative leaching from copper-chrome-arsenic treated timber: Towards an international standard for environmental monitoring
1996 - IRG/WP 96-50076
A review of standards and legislative requirements around the world relating to environmental contamination from copper-chrome-arsenic wood preservative indicates a plethora of methodologies for expressing and determining contamination levels. The imposition of arbitrary quarantine periods for treated timber, or special fixation processes, appear to be applied without a rational analysis of what l...
S Walley, P R S Cobham, P Vinden


Leaching Characteristics of Alder Wood Treated with Copper Based Wood Preservatives
2005 - IRG/WP 05-50225
In this study, it was designed for determining leaching characteristics of CCA and alternatives wood preservatives. Alder wood blocks were treated with CCA (1 % and 2 %), ACQ-1900 (2 % and 3 %), ACQ-2200 (1 % and 2 %), Tanalith E 3491 (2 % and 2.8 %), Wolmanit CX-8 (% 1 and 2 %). Leaching studies were conducted according to AWPA E11-97. Copper analyses of leachate were determined Atomic absorption...
A Temiz, Ü C Yildiz, E D Gezer, S Yildiz, E Dizman


Application of paint primers after light organic solvent preservative treatment
1986 - IRG/WP 3381
The application of three alternative paint primers is investigated, including a slow-drying oil-based primer, a fast-drying oil-based primer, and a fast-drying water-based primer. The treatment schedules employed, in particular the evacuation period after treatment, have a marked effect on subsequent paintability. Priming can potentially be carried out immediately after treatment with approved Tim...
P Vinden


CCA removal from treated wood by chemical, mechanical and microbial processing
1998 - IRG/WP 98-50101-26
Most preservative-treated wood produced and consumed in the U.S. is treated with toxic inorganic compounds containing copper, chromium, and arsenic. Because chromated copper arsenate (CCA) is fixed to the wood, treated wood has not been considered toxic or hazardous and is currently landfilled. Increasing public concern about environmental contamination from treated wood combined with increasing q...
C A Clausen, R L Smith


Effect of soil chemistry and physical properties on wood preservative leaching
1998 - IRG/WP 98-50111
When treated wood is placed in contact with soil, complicated mass transfer and chemical reactions occur which causes the preservative components to leach from the wood. There are several factors that are known to affect the amount of chemical leached from wood. These are properties of the preservative and carrier, preservative retention, degree of fixation, exposure time, grain orientation, surfa...
Joan-Hao Wang, D D Nicholas, L S Sites, D E Pettry


Ecotoxicological effects of exposed CCA preservative treated wood in environments
2001 - IRG/WP 01-50173
For the evaluation of environmental effect of CCA treated wood exposd in the field, the simulated soil pot system of the laboratory was used. The effective components of preservatives were leached and determined after artificially conditioning a soil pot of CCA treated wood with more than 500mm water, the average monthly precipitation. As the water passed through the soil, As, Cr and Cu in the soi...
Dong-heub Lee, Dong-won Son


The influence of UV and IR radiation on leaching of copper and chromium from preservative-treated pine and spruce
1992 - IRG/WP 92-3687
The influence of artifical UV- and IR-radiation on the leaching of copper and chromium components of a CCB-preservative from freshly treated pine and spruce was evaluated. On small pinewood samples it could be shown, that the leaching of copper and chromium can considerabely be reduced by UV-radiation. A Philips HPA lamp type reduced the leaching most effective. IR-radiation lead to higher leachin...
H Militz


Fungal degradation of wood treated with metal-based preservatives. Part 1: Fungal tolerance
1996 - IRG/WP 96-10163
In recent years, concerns have arisen about the leaching of heavy metals from wood treated with chromated copper arsenate (CCA), particularly because of the large amount of CCA treated wood that will be discarded in the coming years. The long term objectives of this work are to determine the fate of copper, chromium and arsenic with the aging and potential decay of CCA-treated wood, and to develop...
B Illman, T L Highley


Chromated copper arsenate preservative treatment of hardwoods. Part 1: CCA fixation performance of seven North american hardwoods
1997 - IRG/WP 97-30131
There has been an increased interest in utilisation of hardwoods from eastern North America for exterior applications which require protection with preservatives such as CCA. We have examined CCA fixation at two selected temperatures of seven common North American species: red maple (Acer rubrum L.,), white birch (Betula papyrifera ), yellow poplar (Liriodendron tulipifera L.), trembling aspen (Po...
T Stevanovic-Janezic, P A Cooper, Y T Ung


The role of oxalic acid in tolerance to N’N-naphthaloylhydroxylamine in Tyromyces palustris
2006 - IRG/WP 06-10584
Certain wood decay fungi exhibit tolerance to one or more wood preservatives. Copper tolerance of brown-rot fungi has been studied in our laboratory for the past six years. We have observed some degree of tolerance to N’N-naphthaloylhydroxamine (NHA), a recently patented termite bait, by the brown-rot fungus Tyromyces palustris TYP-6137. In an effort to try and confirm this tolerance in other is...
R A Arango, C A Clausen, F Green III


Is Field Test Data from 20 x 20mm Stakes Reliable? Effects of Decay Hazard, Decay Type and Preservative Depletion Hazard
2006 - IRG/WP 06-20327
Effects of decay hazard, decay type and preservative depletion hazard on the performance of variously preservative treated 20 x 20 x 500 mm Radiata pine and Fagus sylvatica test stakes across 13 field test sites in New Zealand and Queensland Australia were determined. Radiata pine treated with an ammoniacal copper quaternary preservative (ACQ) (1.56% m/m a.i.) and copper chrome arsenate (CCA) (...
R Wakeling


The Use of Modulus of Elasticity and Modulus of Rupture to Assess Wood Decay in Laboratory Soil-Bed Test
2006 - IRG/WP 06-20338
The efficacy of wood preservatives were determined in a soil-bed test. Samples of alder wood sapwood (Alnus glutinosa subsp. barbata) (5x10x100 mm) were treated with Solutions of CCA (1 % and 2 %), ACQ-1900 (2 % and 3 %), ACQ-2200 (1 % and 2 %), Tanalith E 3491 (2 % and 2.8 %), Wolmanit CX-8 (% 1 and 2 %). Modulus of Elasticity, modulus of rupture, mass loss and decay rate according to AWPA E7 wer...
A Temiz, Ü C Yildiz


Measuring Soil Respiration as a New Approach to Describe the Interaction Between Wood (Treated and Untreated) and Microbiologically Active Soil
2006 - IRG/WP 06-20344
Soil respirometry was employed to examine the relationship between both the performance of copper organic preservatives in contact with and the amount of carbon dioxide evolved from soil and the effect of wood treated with preservatives on carbon turnover in soil. Wood was treated with a range of copper organic preservatives intended for use in ground contact as well as an organic preservative in...
I Stephan, W Mierke


Preliminary screening of a boron based wood preservative for biological efficacy (fungicidal) in treated timber
2006 - IRG/WP 06-30396
The resistance of Pinus radiata D.Don sapwood blocks, treated with a boron based preservative, to attack by five wood destroying fungi (Fomitopsis lilacino-gilva, Coniophora olivacea, Gloeophyllum abietinum (boron resistant), Serpula lacrymans and Perenniporia tephropora) was investigated. A phenyl pyrazole termiticide (fipronil) was also incorporated into the formulation to examine if its presen...
S R Przewloka, J A Hann, P Vinden


Above and Below-Ground Depletion of Copper, Chromium and Arsenic from Pinus radiata and Fagus sylvatica at Thirteen Test Sites in New Zealand and Australia
2006 - IRG/WP 06-30402
The objective was to determine the significance of site and wood species on preservative depletion for a copper chrome arsenate preservative (CCA) from 20 x 20 x 500 mm field test stakes after 5.5 and 4.5 years for pine and beech respectively. At least 5 sacrificial stakes were used to produce site means. Site and wood species had a major effect on copper, chromium and arsenic loss from CCA treate...
R Wakeling


Addition of boron compounds and octanoic acid for improvement of biocidal properties and copper fixation at copper-ethanolamine based wood preservatives
2006 - IRG/WP 06-30408
Copper-ethanolamine based wood preservatives became important active substance (formulation) for wood protection, novelty. As copper itself can not ensure sufficient protection against wood destroying organisms and fixation in wood we combine it with other biocides like ethanolamine, boron and octanoic acid. This investigates were performance on spruce wood impregnated with different combination o...
F Pohleven, M Humar


The Development of a novel method to preserve reeds using an environmentally friendly timber preservative and a unique engineering design.
2006 - IRG/WP 06-40335
Reeds are used in the construction of bush lodges in Northern Kwa- Zulu Natal, South Africa. Fungal, insect and ultra-violet damage to these reeds is posing a severe problem. Within a space of two years, the reeds are attacked and have to be subsequently replaced; a time consuming and costly exercise. A novel method has been used to successfully preserve these reeds with an environmentally friendl...
K Govender, K G Moodley


CCB Preservative treatment of split muli (Melocanna baccifera ) bamboo by soaking process
2006 - IRG/WP 06-40336
This study was carried out in order to investigate the retention of chemicals inside the split muli ( Melocanna baccifera ) bamboo after preservative treatment by soaking process. Treatment with 10% aqueous solution of CCB (copper-chrome-boron) was applied in split bamboo of two sizes (1/4 part and 1/8 part) at three different moisture contents and five time periods (24, 48, 72, 96, 120 hours). It...
K Akhter, M H Chowdhury


Non-pressure preservation technique of five less durable timber species – Kadam (Anthocephalus cadamba), Shimul (Bombax ceiba), Pithalu (Trewia nudiflora), Am (Mangifera indica) and Boroi (Ziziphus jujube) of Bangladesh
2006 - IRG/WP 06-40322
Wood is a versatile renewable resource, which has been extensively used as a reliable construction material as well in furniture ever since the beginning of civilization. The Major disadvantage of wood is its susceptibility to biodeterioration by fungi, insects and bacteria. In tropical countries like Bangladesh, fungi is the most significant of these biodeterioration agents. Kadam (Anthocephalus...
G N M Ilias, A H Kabir, F Begum, M F Alam


Previous Page | Next Page