IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3435 documents. Displaying 25 entries per page.


How to Document the Performance of Super-Critical Treated Wood in above Ground Situations?
2005 - IRG/WP 05-20316
The paper presents practical experiences from the preparation of a new preservative treated wood product for introduction to the market. The product in question is Superwood™, which is treated with organic biocides using CO2 in a supercritical state as a solvent. The question is how to evaluate the performance of a new product such as Superwood™ in order to get an acceptance on the market a...
N Morsing, A H H Wong, F Imsgard, O Henriksen


Organic solvent preservatives. Essays on the ecotoxicology of new formulations
1991 - IRG/WP 3642
The knowledge on the ecotoxicological profile of wood preservatives become more and more important. The acute toxicity against aquatic organisms was examined for oil-borne preservatives, based on combinations of new fungicides (Tebuconazole, Propiconazole, Dichlofluanid) and insecticides (Permethrin, Cyfluthrin). These tests were conducted with fish, daphnia and algae. In principle the different f...
H-W Wegen


Co-operative studies on determining toxic values against wood-destroying Basidiomycetes: Progress report to May 1989
1989 - IRG/WP 2339
This document reports progress on the co-operative study between nine laboratories set up following the proposals contained in Document IRG/WP/2316. Results have been received from two laboratories. Toxic values data have been established successfully using the test fungus Coniophora puteana but problems have been encountered with the other test fungi....
A F Bravery, J K Carey


Health aspects concerning the use of bifluorides in wood
1981 - IRG/WP 3173
An attempt has been made to find a correlation between the quantities F¯ and HF present among other ions in an 'Improsol' solution consisting of NH4F.HF and KF.HF, the quantity absorbed by the wood from this after immersion and the toxicological effects of this treated wood when it is used in rooms destined for the residence of people or animals or for the storage of foodstuffs....
H F M Nijman


Monographic cards for wood-destroying fungi. [Fiches monographiques pour les champignons lignivores]
1970 - IRG/WP I 5B
C Jacquiot


Thermal treatment of wood: European Processes and their background
2002 - IRG/WP 02-40241
Recent efforts on thermal treatment of wood lead to the development of several processes introduced to the European market during the last few years. The total production capacity of heat treated wood in 2001 is estimated as approx. 165.000 m3. In the paper the different heat processes are presented. The general technology as well as scientific data on the chemical transformation of the cell wall ...
H Militz


The evaluation of permethrin for wood preservation
1977 - IRG/WP 3107
The toxicity of the synthetic pyrethroid permethrin (NRDC 143) to a range of wood destroying insects has been investigated. In tests using Hylotrupes bajulus, Anobium punctatum, Lyctus brunneus and Reticulitermes santonensis permethrin showed a similar order of toxicity to that of gamma-BHC. Although the toxicity of permethrin to adult Anobium punctatum was of the same order as that of gamma-BHC, ...
R W Berry


Developments in the protection of wood and wood-based products
1980 - IRG/WP 340
Technology is playing an increasingly important role in the field of wood protection. This current review highlights how modern techniques have provided greater insight into the biological and physical processes affecting the durability of wood and wood-based products. Emphasis is also given to developments in preservative testing methodology and to the encouraging changes towards both the correct...
J M Baker


Low temperature drying conditions of Pinus radiata wood for avoiding internal stain
1989 - IRG/WP 3507
It has been observed that, if in little sawmills, timber is dried with a low temperature schedule, it arrives at destination with internal sapstain besides of superficial mould. In this study, the lowest drying temperature at which wood should be exposed for sterilization, which results to be 52°C, is searched. It is not possible to avoid entrainment of pentachlorophenol, even though a waiting pe...
M C Rose


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. 2nd Interim Report
1981 - IRG/WP 477
Three reference wood species - Alstonia scholaris, Fagus sylvatica and Pinus sylvestris, untreated and treated with 3%, 6% and 10% CCA and CCB solutions were supplied to all participants for submergence at local sites. Regular examination of samples is being carried out - 6 months, 12 months and then annually for 7 years....
R A Eaton


Types of decay observed in CCA-treated pine posts in horticultural situations in New Zealand
1984 - IRG/WP 1226
The few reported failures of 11-12-year-old horticultural posts in New Zealand in 1982 were caused by brown-rot. A subsequent survey of CCA-treated posts in all the major horticultural areas has revealed decay of many posts. A microscopic examination of these posts has shown decay by brown-rot, white-rot, soft-rot and bacteria. Several types of bacterial decay have been observed....
J A Drysdale, M E Hedley


Results of chemical analyses in the field of wood preservation in the Bundesanstalt für Materialprüfung
1973 - IRG/WP 321
The results of qualitative and quantitative chemical analyses of wood preservatives are often the basis for evaluating the various works in the field of wood preservation. In the past 10 to 15 years a number of such works was carried out in the Bundesanstalt fur Materialprüfung, Berlin-Dahlem, dealing with the identification and effectiveness of wood preservatives and with methods of wood preserv...
H J Petrowitz


The decay resistance of chemically modified aspen composites to the white rot fungus Coriolus versicolor (L.) Quelet
1998 - IRG/WP 98-40122
Chemical modification of Aspen wood (Populus tremula L.) in the form of solid wood, veneers and sawdust was undertaken by a two step procedure consisting of esterification with maleic anhydride (MA) and subsequent oligoesterification with MA and glycidyl methacrylate (GMA) or allyl glycidyl ether (AGE). Modified wood was thermoplastic and was thermally formed by hot-pressing to produce veneer or s...
M C Timar, A J Pitman, M D Mihai


Wood preservation in Lithuania
2004 - IRG/WP 04-30363
This article is intended to give basic information on wood preservation activities in Lithuania and the main actors in wood preservations practice and research. Currently the main actors in practical Lithuanian wood preservation activity are enterprises of wood preservation industry united by the Lithuanian Wood Preservation Association. The most intensive activity in wood preservation practice an...
J Saladis


A summary of current information on actinomycetes and wood
1978 - IRG/WP 177
B King, R A Eaton, A A W Baecker


Improved equipment and technique for high pressure sap displacement impregnation of natural round wood
1972 - IRG/WP 309
Hitherto the main problem in the practical application of high pressure sap displacement impregnation (HPSD) has been in devising a satisfactory cap. Such a cap must be easily fitted to different size log ends to give a leak proof seal. The present contribution describes a new type of cap and sealing system designed to meet these requirements....
C G W Mason, F B Shorland


The Third Annual Report of the International Research Group on Wood Preservation 1971-1972
1972 - IRG/WP 511
IRG Secretariat


The Fourteenth Report of the Internatinal Research Group on Wood Preservation 1984-1985
1985 - IRG/WP 5218
R Cockcroft


Leaching of the new boron based biocide from coated wood
2001 - IRG/WP 01-30267
We investigated leachability of the new boron based biocide - a complex of an amine and boric acid - from vacuum impregnated spruce wood samples. It was determined by the standard ENV 1250-2 procedure that the new biocide is susceptible to leaching so from the water borne as well as from the ethanol borne boron containing preservative treated wood. Leaching may be retarded by application of surfac...
M Petric, M Pavlic, F Cadez


Fungicidal activity of some organic solvents, copper carboxylates and their complexes with 2-aminoethanol
1997 - IRG/WP 97-30136
We evaluated the activity of eight organic solvents against wood - rotting fungus Trametes versicolor in order to choose the most appropriate one for rapid screening tests of some copper(II) carboxylates and their adducts with 2-aminoethanol. Their activity against the selected fungus was classified in the following order: chloroform > N,N-dimethylformamide > acetonitrile > methanol > ...
M Petric, F Pohleven


Possible regulatory status of treated wood waste and implications
1998 - IRG/WP 98-50101-07
In relation to the European Community or the French regulations, treated wood waste can get two different regulatory status: <<recycled product or fuel>> or <<waste>>. Then, into the waste status, two categories are possible for these residues: <<domestic waste and assimilated>> or <<hazardous waste>>. These different status and categories are import...
G Deroubaix


Comparison of Different Methods for Assessing the Performance of Preservatives in the BAM Fungus Cellar Test
1998 - IRG/WP 98-20149
The fungus cellar test is a common means to get reliable data on the long term performance of treated wood in soil contact. A constantly high humidity and a suitable of water holding capacity for a range of micro-organisms provide high decay rates in untreated wood and produce intensive microbial pressures on wood treated with biocides. Presently a range of biocides are under test in the BAM fungu...
I Stephan, M Grinda, D Rudolph


Insects in dry wood (other than termites)
1977 - IRG/WP 153
S Cymorek


The Seventh Annual Report of the International Research Group on Wood Preservation 1975-1976
1976 - IRG/WP 551
IRG Secretariat


Programme section 3, Wood protecting chemicals
1997 - IRG/WP 97-30159
IRG Secretariat


Previous Page | Next Page