IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 310 documents. Displaying 25 entries per page.


A new approach to wood protection: Potential of biologically synthesised CuO and ZnO nanoparticle formulation as a wood preservative
2022 - IRG/WP 22-30758
Even though metal nanoparticles are effective in protecting wood, they are less preferred, as they are synthesised using methods which are expensive and are not environmentally friendly. Biological synthesis of nanoparticles using plants, fungi, yeast, bacteria and viruses, has been accepted as an alternative approach and is referred to as green synthesis. Utilization of biologically synthesised n...
Shiny K S, R Sundararaj, N Mamatha


Properties of Iron (II) Sulphate treated Norway Spruce
2022 - IRG/WP 22-30765
Exterior wood is exposed to various environmental factors that cause weathering. Weathering is important primarily from an aesthetic standpoint. However, not all parts of the building are equally susceptible to weathering. Parts exposed to moisture will discolour faster than protected parts, such as wood under roof overhangs. To achieve fast and uniform artificial greying, a surface treatment with...
B Lesar, M Humar, M Škamlec


Environmentally Friendly Wood Modification based on Tannin-Furfuryl alcohol - Effect on stabilisation, mechanical properties and decay durability
2022 - IRG/WP 22-40929
Furfurylation is a well-known wood modification technology. This paper studied the effect of tannin addition on the wood furfurylation. Three kinds of dicarboxylic acids, adipic acid, succinic acid, and tartaric acid, as well as glyoxal as a comparing agent, were used to catalyse the polymerisation of furanic or tannin-furanic solutions during wood modification. Impregnation of furanic or tannin-f...
M Mubarok, E Azadeh, F O Akong, S Dumarçay, A Pizzi, C Charbonnier-Gérardin, P Gérardin


Optimisation of accelerated weathering procedure as an alternative to natural weathering
2023 - IRG/WP 23-20693
Comprehensive tests need to be performed to obtain the most accurate data possible on the durability of wood. The most reliable performance tests are field tests. However, since this is very time-consuming, we frequently rely on laboratory tests. To increase the reliability of the laboratory tests, samples are preconditioned with natural or artificially accelerated weathering methods that simulate...
E Keržič, M Humar, V Vek


Optimization of furfurylic alcohol/tannin ratio to improve the performance of biosourced thermoset resins for wood protection
2023 - IRG/WP 23-40994
This study concerns the chemical modification of wood with different ratios of tannin and furfuryl alcohol (FA) in the presence of maleic acid as catalyst. Tannins were used not only as cross-linking agents, but also as co-monomers to improve wood durability, while reducing the amount of FA used. Different aqueous formulations were prepared containing decreasing amount of FA (from 45.45% to 0%) an...
E Azadeh, A Pizzi, P Gérardin, C Gérardin-Charbonnier


Exposure tests on railroad ties treated with DOT
2024 - IRG/WP 24-20705
Keruing railroad ties were treated with disodium octaborate tetrahydrate (DOT) to retentions of 0.7 to 1.7% boric acid equivalent (BAE) and selected borate treated ties were subsequently over treated with creosote/diesel fuel mixture. The treated ties were exposed in a simulated railway track test bed in Malaysia. The leaching of borate was measured over 5 years. BAE in the ties after 5 years of e...
L Arthur, J-W Kim


Comparison of copper leaching from alkaline copper quat and copper compound nanosol-based wood preservative treated wood
2024 - IRG/WP 24-20726
To improve the leaching resistance of copper ion-based wood preservatives, copper compound nanosol-based wood preservatives were developed and its copper leaching characteristics were evaluated. Three types of preservatives (DC1, DC2, DC3) were prepared with different crystallinity and dispersant types of copper compound nanosol, and the copper concentration was adjusted to be the same as that of ...
Y-S Choi, S-M Yoon, J O Kim, J-G Kang, J-G Park


Leaching and chemical redistribution of CCA components in refractory heartwood of E. nitens
2024 - IRG/WP 24-41011
Chromated Copper Arsenate (CCA) is a wood preservative widely used to protect against fungal and insect attack. The fixation mechanism of CCA involves complex chemical reactions, including the reduction of chromium (VI) to chromium (III) and the formation of insoluble complexes. Despite fixation efforts, a portion of CCA components tends to leach from treated wood, influenced by factors like wood ...
J R Vargas, L Yermán, K C Wood, T Singh


Copper migration from preservative-treated Douglas-fir decking: models vs laboratory leaching data
2024 - IRG/WP 24-50390
The ability of a model to predict copper migration from Douglas-fir treated with organic metallic substances into a freshwater slough was evaluated against data generated through simulated overhead leaching. The model predicted very high loadings of ammoniacal copper zinc arsenate, alkaline copper quaternary or copper azole that had the potential to impact water quality while data from the exper...
M J Konkler, G Presley, J J Morrell, T Singh


Quantifying metal migration from a deck constructed with copper-azole-treated lumber
2024 - IRG/WP 24-50391
Soluble copper or micronized copper wood preservatives are the most common available wood preservative systems for residential applications in the United States. Copper containing wood preservatives have been scrutinized for their potential negative impacts on the environment, across many jurisdictions. Concerns arise from the potential for preservatives to migrate out of treated wood upon water e...
G Presley, M Konkler


Previous Page