Chemical mediated depolymerization of cotton cellulose for the understanding of non-enzymatic fungal decay
2010 - IRG/WP 10-10731
Small, low molecular weight non-enzymatic compounds have been linked to the early stages of brown rot decay as the enzymes involved with holocellulose degradation are found to be too large to penetrate the S3 layer of intact wood cells. The most pronounced of these which were analyzed in this study are hydrogen peroxide, iron, and oxalic. The compounds related to the Fenton reaction: the combinati...
A C Steenkjær Hastrup, B Jensen, F Green III


Use of Internal Remedial Treatment to Extend Wood Life at the Fort Vancouver National Historic Site
2010 - IRG/WP 10-30525
The condition of wood in a reconstructed fur trading fort was assessed over a 30 year period. Poor initial treatment had resulted in the development of extensive early decay. While supplemental treatment with chloropicrin and methylisothiocyanate had arrested the attack, the results suggested that remedial treatments were unable to completely overcome the initial problems associated with treatmen...
C S Love, C Freitag, J J Morrell


Assessment of Boracol 200RH (FrameSaver) as a remedial treatment to control decay in pre-decayed model timber frame units
2010 - IRG/WP 10-30529
Model timber frame units constructed from untreated radiata pine were pre-wetted to approximately 40% moisture content and inoculated with Coniophora puteana and Oligoporus placenta. Units were transferred to a controlled environment room maintained at 25°C and 95% RH for 7 and 10 weeks to allow two levels of decay to become established in units. Following pre-decay, units were disassembled, clea...
Mick Hedley, Dave Page, Jackie van der Waals


Mobility of Copper from MCQ in Shell-Treated Wood Exposed Above Ground
2010 - IRG/WP 10-30534
Most Canadian treated decking in service has been given just a thin shell of preservative treatment but it has still performed very well. This is because copper migrated into checks and prevented germination of basidiospores on the freshly exposed untreated wood. Unlike soluble copper systems, MCQ has its copper primarily in the form of small basic copper carbonate particles. For MCQ to be effecti...
R Stirling, P I Morris


Treatment of Scots pine wood with oil in water and water in oil emulsion systems: Effects on boron leaching and water absorption
2010 - IRG/WP 10-30535
The aim of this study was to investigate the water absorption and water repellent efficiency of oils and oil water emulsions [oil-in-water (O/W) and water-in-oil (W/O)] and possibilities of reducing the amount of boron leaching from treated wood. Scots pine wood samples treated with waste or sunflower oil and water formulations contained 3%BA. The level of water absorption and water repellent effi...
E D Tomak, Ü C Yildiz, A Can


The Effects of Natural Weathering on the Properties of Heat Treated Alder Wood
2010 - IRG/WP 10-40484
Heat treatment is an effective method to improve the dimensional stability and biological durability of wood. The heat treatment technology and the heat treated wood products were recently introduced to Turkey. However, only a few studies have been reported on the effect of natural weathering on the properties of heat treated wood in both Turkey and the world. In this study, heat treated alder (Al...
S Yildiz, Ü C Yildiz, E D Tomak


Chemical protection of historic timber structures: Results and future needs
2010 - IRG/WP 10-40487
The paper concentrates on the analysis of the effectiveness of chemical protection for timber structures in the Russian State Museums “Kizhi” (Karelia) and “Vitoslavlitsy” (Novgorod). The condition of historic timber was tested at the monuments treated with PCP, borax, potassium carbonate, boric acid, Pinotex chemicals in the 1970-80. Long-term analysis revealed that in many cases the...
M Kisternaya, V Kozlov


Study on the thickness swelling of mould-resistant chemical treated bamboo strand woven outdoor flooring
2010 - IRG/WP 10-40489
To prevent bamboo strand woven flooring from mould, several preservatives were chosen to treat bamboo strand before dipping into adhesives and pressing. The thickness swelling and mould resistant effect of the finished board were studied. Results showed that different preservatives had different influences on the thickness swelling of BSWF, and in order to reduce the thickness swelling of the fini...
Fangli Sun, Binfu Bao, Shenyuan Fu, Anliang Chen


Development of markers to predict decay durability of heat treated wood
2010 - IRG/WP 10-40496
Effect of heat treatment temperature on elemental composition of Scots pine sapwood (Pinus sylvestris) has been investigated in the range of temperatures between 220 and 250°C. Results revealed an important increase of carbon content, while oxygen content significantly decreases. Independently of the heat treatment temperature, elemental composition is strongly correlated with the mass losses due...
Ž Šušteršic, A Mohareb, M Chaouch, M Pétrissans, M Petric, P Gérardin


TMT–Interlab–Test to establish suitable quality control techniques - Structure and first results
2010 - IRG/WP 10-40503
As a result of growing quality demands from manufacturers and end-consumers of thermally modified timber (TMT) recent scientific research activities are increasingly focussed on modification mechanisms and by this on the development of suitable quality control methods. To deepen the knowledge in modification mechanisms and to obtain a larger variety of scientific data for TMT depending on the trea...
C R Welzbacher


Durability of heat treated Malaysian bamboo Gigantochloa scortechinii strips
2010 - IRG/WP 10-40514
Bamboo is one of the fastest growing plants and can be used for various products. In tropical countries such as Malaysia bamboo is abundantly available at reasonable prices, therefore it is used for numerous purposes. However, bamboo (as a lignocellulosic material) is susceptible to fungal and insect attack and it is difficult to protect by preservative treatment. Heat treatment is an option to im...
N Kamarudin, K Sugiyanto


Effect of borax-boric acid Treatment of simul (Bombax ceiba) Veneers on Glue-Bond Quality of Plywood
2010 - IRG/WP 10-40525
The glue-bond quality of plywood made of treated simul (Bombax ceiba) veneers was investigated. The veneers were treated with cold and hot water solution of borax-boric acid (BB) of different concentrations and treatment durations. The plywoods were made at three different pressures in hot press using urea formaldehyde glue. The glue-bond strength of untreated plywood in dry shear-test was found t...
K Akhter, Md Abul Hashem, S Akhter


Preservative Treatment of simul (Bombax ceiba) Veneers with Hot and Cold Water Solution of borax-boric acid by Soaking Process
2010 - IRG/WP 10-40528
Veneers of simul (Bombax ceiba) were treated with different concentrations of water- borne preservatives borax-boric acid (BB) by soaking process for different time periods. In the case of hot water treatment, it was found that the average retention of preservative chemicals increased gradually with the increasing treatment period from 20 minutes to 60 minutes. Similar trend was observed in the ca...
K Akhter, Md Abul Hashem, S Akhter


Effect of Nano-Silver Treatment on Densified Wood Properties. Part One: Swelling, Recovery Set, Bending Strength
2010 - IRG/WP 10-40533
In this research the effect of Nano-Silver treatment on compressed wood properties, was studied. Wood specimens were cut from Popolus alba (poplar) and impregnated with Nano-Silver and water. Then the saturated samples were compressed through radial direction in a hot press under pressure of 6 MPa, for 1 and 4 hours. The temperatures of press were 150°C and 175°C. Swelling (24h), recovery set ...
G Rassam, H Reza Taghiyari, B Jamnani, M Ali Khaje


Deterioration of wooden heritage in outdoor exposure in Romania
2010 - IRG/WP 10-40535
The paper contains a study of the deterioration of wooden heritage in Romania, in outdoor exposure. Romania belongs to the few countries having a rich heritage of this kind. A quantitative image of this heritage reveals the 1,350 objectives transferred and reconstructed in 16 open-air museums, over 1,500 wooden churches, more than 4,000 buildings and technical facilities, historical monuments ...
L Bucşa, C Bucşa


Comparative Study of Heat Treatment of Beech Wood in Hot Water and Steam Medium
2010 - IRG/WP 10-40536
Heat treatment of wood is an effective method to improve the dimensional stability and durability against biodegradation. Heat treatments of beech wood in 2 different mediums (hot water and steam) in 180ºC were compared in physical, mechanical and anatomical properties. Mass loss in hydrothermally treated wood was higher than hygrothermally treated samples. Mechanical properties (MOR, MOE and CS)...
A Talaei, K Yaghoobi, A N Karimi


Combined Effect of Boric Acid and Waste Oil Treatment on Boron Leaching
2010 - IRG/WP 10-50268
In this study it was aimed to investigate the boron leaching amounts in Scots pine wood samples treated with boric acid (BA) and waste oil (WO) alone or by dual treatment. The level of water absorption and water repellent efficiency were determined with cyclical wetting tests, total of 336 hours. Wood samples that have both covered and uncovered transversal section were impregnated with 3% boric a...
Ü C Yildiz, E Dizman


Chapter 11 - Preservation of talla bamboo
2007 - IRG/WP 07-10635-11
Researches revealed that the talla bamboo (Bambusa tulda Roxb.)) in Bangladesh could be full-cell pressure treated with CCA in green and dry conditions. The dry bamboo gives higher loading absorptions than green one when impregnated at same treating conditions. Also higher absorptions are obtained at nodes rather than internodes. Adequate penetration and retention results for ground and wate...
A K Lahiry


Chapter 12 - Treatment Groups of Bamboo
2007 - IRG/WP 07-10635-12
Study on distribution of CCA in three major bamboo species in Bangladesh, full-cell pressure treated at green and dry conditions revealed two treatment groups and some treating principles. Higher adequate treatment for ground and water contact use is only possible by treating problematic bamboo species pre-kiln dried up to half of its FSP and non-problematic species pre-dried up to FSP (20% ...
A K Lahiry


Multilayer hot-press drying and chemical modifying of poplar wood with urea-formaldehyde prepolymer
2011 - IRG/WP 10-40539
The objective of this study was to determine the technology of chemical modifying and multilayer hot-press drying on poplar wood. The chemicals were impregnated into cell lumen space by pulse-dipping machine to improve the dimension stability and mechanical property of timber. The timbers were compressed and dried by the multilayer hot-press drying to increase the density of timber. Results indica...
Guofeng Wu, Yifei Jiang, Sheng Yao, Junwen


Comparative investigations between thermal and microwave assisted digestion as a novel tool for the chemical analysis of inorganic wood preservative components
2011 - IRG/WP 11-20461
The correct chemical impregnation of wood requires an internal as well as external quality control of the treated wood. The active is located in a solid matrix, therefore it is often difficult to analyse such material since most analytical procedures are based on liquid systems. Because of this quite a number of methods – like extraction or thermal digestion - were developed in order to transfer...
H Ahl, J Fromm, E Melcher


Methods of field data evaluation - time versus reliability
2011 - IRG/WP 11-20466
Field testing of wood and wood-based products is so far the most reliable way to get information on performance with respect to durability and expected service life. However, field trials are extremely time and cost consuming. The main objective of the present study was to investigate possible correlations between early stages of decay, preferably during the first 5 years, and the actual service l...
P Larsson Brelid, C Brischke, A O Rapp, M Hansson, M Westin, J Jermer, A Pilgård


A comparative study and evaluation of methodologies used for determining wood preservative penetration
2011 - IRG/WP 11-20475
A series of methods for determining penetration of wood preservatives into the wood structure have been developed for either quality control (QC) or research and development purposes. QC methods range from monitoring the solution uptake, applying colour indicators or sampling specific wood samples followed by wood acid digestion/atomic absorption spectroscopy (AAS) or solvent extraction/chromatogr...
R Craciun, R Moeller, J Wittenzellner, T Jakob, J Habicht


Slice - Cut and Analyze Laser Microdissection (LMD): A method to produce sample material from modified wood for chemical quality analysis
2011 - IRG/WP 11-20478
Wood modification with its various systems is an established way to enhance a wood products’ service life in outdoor applications. Per definition, selected material properties are enhanced by means of modification without producing toxic substances or residues during service life and combustion afterwards. The systems of impregnation modification include a physical and often chemical alteration ...
K Zimmer, E Larnøy, A Treu, M Fongen


LOSP for glulam, when should the treatment be applied?
2011 - IRG/WP 11-30555
Treatment options for outdoor above-ground (H3) exposed glulam of Pinus radiata and P. elliottii were examined. Beams were treated with azole LOSP (containing a zinc tracer) aiming for retentions of 35-40 l/m3 or 70-80 l/m3. Treatment was conducted either before or after gluing. TBTN LOSP and CCA were included as comparative treatments. Test specimens for exposure were cut after treatment, while w...
L J Cookson