Glued laminated poles - Progress report after 43 years of testing
2023 - IRG/WP 23-20692
In 1979, a number of glued laminated poles treated with CCA and creosote were placed in a greenhouse in Uppsala, in the Simlångsdalen test field in south-western Sweden and in a power lane in Vuollerim in northern Sweden, in order to study their resistance against biological degradation. The test poles were treated in a two-step process. All laminations of Scots pine (Pinus sylvestris) were first...
J Jermer, M Westin, N Terziev


Field durability testing of wood above ground - Part 1: 15 years’ experience with the Bundle method
2023 - IRG/WP 23-20695
A ‘jack of all trades’ method for above-ground wood durability testing has been sought for decades, but until now no method has found its way into standardization. The method of choice shall be applicable for untreated and treated wood – ideally also for wood composites. It shall be reproducible, objective, fast, easy, and inexpensive. Finally, it shall provide high predictive power. This s...
C Brischke, G Alfredsen, L Emmerich, M Humar, L Meyer-Veltrup


Field durability testing of wood above ground - Part 2: The full guideline of the Bundle method
2023 - IRG/WP 23-20696
To determine the biological durability of wood above ground, numerous approaches for test methods have been pursued and tried out in the field in the past. So far, no method has managed to find its way into a European standard. During the last 15 years, experience with the Bundle method has been gained. As described in Part 1 of this paper, the method is recommended as a suitable tool for determin...
C Brischke, G Alfredsen, L Emmerich, M Humar, L Meyer-Veltrup


Laboratory durability testing of preservative treated wood products – first attempts and observations
2023 - IRG/WP 23-20697
In the past, durability classes (DC) had been assigned to wood species, sometimes also to homogenously modified wood-based materials such as thermally modified wood. More recently, some standards allow for classifying the biological durability of chemically modified wood, preservative treated wood and wood composites. Even treated products may be subject to durability classification, but necessary...
C Brischke, M Sievert, M Schilling, S Bollmus


Virtual Reality of Wood Protection
2023 - IRG/WP 23-20698
Virtual reality (VR) is a technology that allows people to explore and interact with computer generated environments using devices that stimulate different senses (sight, sound and touch). VR is mainly used for education, training and entertainment, but it also has the potential to provide new insights into scientific phenomena. In this paper we describe the evolution of VR and its many uses, focu...
D Feng, Y Liu, M Turner, A Limaye, P D Evans


Accelerated surface mould testing for exterior wood treatment in Temperate, Tropical and Laboratory environments
2023 - IRG/WP 23-20699
Mould attack is a very common cause of discoloration on wooden surfaces and can subsequently promote development of wood decay by other organisms. Prevention of mould growth is relevant for both pigmented wood paints as well as more transparent systems with a high or low amount of binder. The use of commercial biocides has led to effective microbiological inhibition in many contexts, but the incre...
A Nazeri, J Stenbaek, T R Laursen, A H H Wong, B M Hasnul


Simulations of microclimates for wood-decaying fungi in the built environment using environmental analysis
2023 - IRG/WP 23-20703
Simulations of fungal decay risk were run on two similar building geometries exposed to typical annual climate conditions of two different geographical locations, Brunswick (Germany) and Cairns (Australia). The simulations were conducted to capture the effect of wind-driven rain and solar irradiation exposure over nodes of the common building geometry. The moisture content and temperature variatio...
P B van Niekerk, J Niklewski, S H Hosseini, B N Marais, I Frimannslund, T Kringlebotn Thiis, C Brischke


Moisture performance of wooden shingles tested on the Golobar cable yarding
2023 - IRG/WP 23-20704
Wood is a traditional roofing material in Europe and other parts of the world. In the 17th century, wooden roofing was generally used on more important buildings, but today it is mainly used on huts and houses in the Alpine regions. As wooden roofing is expensive, we investigated the possibility of extending the service life of the roofing through material selection and details. The roof of the Go...
M Humar, B Lesar, D Kržišnik


Geopolymer as a fixation method for tannin-based wood preservatives
2023 - IRG/WP 23-30774
This study aims to test if a second step impregnation with a geopolymer solution can fix Colatan GT10, a commercial extract rich in tannins, to wood, reducing their leaching and improving their performance as wood preservatives. Scots pine sapwood specimens of 40×10×5 mm3 were impregnated with Colatan GT10 tannin mix, geopolymer, and as combined treatment Colatan GT10 with subsequent geopolymer ...
Y M López-Gómez, A Barbero-López, A Haapala


Performance of a noise barrier with different wood materials – results from a service trial after 25 years of exposure
2023 - IRG/WP 23-30776
In connection with the construction of the railway connection between Stockholm Arlanda airport and Stockholm city, an 11 km long noise barrier made of untreated European larch was built along the railway line. This provided an opportunity to implement a full-scale study comparing different untreated wood species and preservative treatments. Thus, in March 1996 ten test sections including untreate...
J Jermer, M Westin


Improvement of durability of Scots pine against termites by impregnation with citric acid and glycerol followed by in situ polyesterification
2023 - IRG/WP 23-30777
Scots pine (Pinus sylvestris) sapwood samples were impregnated with solution containing citric acid (CA) and glycerol (Gly) followed by heating 140 °C according to already described procedure (L'hostis et al. 2018). The resulting modified woods were then used to evaluate the effect of chemical modification on the durability against termites. Two kinds of experiments were conducted for this purpos...
M Mubarok, J Damay, E Masson, E Fredon, Y S Hadi, I W Darmawan, P Gerardin


Suitability of boron preservative treatment of minor species as framing in New Zealand buildings
2023 - IRG/WP 23-30778
The inclusion of alternative species to radiata pine, predominantly exotic species, in the building code (NZS 3602) raises questions as to whether they require preservative treatment and, if so, whether they can be adequately treated using current industry processes. Early research with boron indicated that the dip/diffusion method for green timber would give adequate preservative retention in sa...
D Page, I Simpson, T Singh


Establishing the minimum effective penetration of wood preservatives in the refractory heartwood of E. nitens
2023 - IRG/WP 23-30780
Conventional pressure treatment of many Australian hardwoods results in little to no penetration of heartwood and a non-uniform envelope treatment of <5 mm surrounding a mostly untreated core. This is a major issue for many of the low durability plantation hardwood timbers that are grown in Tasmania, which contain high percentages of heartwood. Long term studies on softwoods such as spruce decking...
J R Vargas, J J Morrell, L Yermán, K C Wood


Field performance of MCA-treated wood in ground contact
2023 - IRG/WP 23-30782
Micronized Copper Azole (MCA) was evaluated for its ability to resist biodegradation at two Canadian test sites using Pacific silver fir and white spruce stakes, and lodgepole pine and red pine roundwood posts. After 12 years of exposure the treated stakes exhibited low to moderate levels of decay while the untreated controls had failed. When stakes were moved to an active termite site, the untrea...
C Wilson, J Zhang, R Stirling


Recent studies into improved fire retardancy of wood undertaken at Luleå University of Technology
2023 - IRG/WP 23-30784
Modern construction is moving more towards engineered wood products, such as glulam and cross-laminated timber (CLT). This increase is driven by the aspiration to deliver high-rise buildings with enhanced environmental profiles and human well-being. This desire to use wood in construction is pushing the need for fire treatments capable of meeting a products service life. However, the use of wood ...
D Jones, C-F Lin, I Kim, E Garskaite, O Karlsson, D Sandberg


Reuse of discarded wood and alternative wood species to replace spruce in the development of wooden windows for complete disassembly – REWINNUSE
2023 - IRG/WP 23-30785
The REWINNUSE project focuses on the reuse of discarded wood and alternative wood species and on the development of wooden windows that can be easily disassembled into their basic components. In cooperation with the project partners (M Sora, the University of Ljubljana Biotechnical Faculty (BF), the Norwegian Institute of Bioeconomy - NIBIO and the Slovenian Forestry Institute (GIS)), the project ...
B Lesar, M Humar, J Levanič, A Treu, A Ugovšek, L Kramarič, B Štrakel, L Križnar, B Šubic, J Gričar


Influence of weathering of wood surfaces before and after treatment with iron(II) sulphate
2023 - IRG/WP 23-30786
Outdoor wood is exposed to various factors that cause the wood to grey or age. The ageing processes can vary greatly depending on the exposure. Parts of the wood that are not exposed to external factors, e.g. under the eaves, are less exposed and the ageing process is therefore slower. This can be accelerated by solutions based on iron ions. In this way, the wood greys quickly and evenly. However,...
B Lesar, M Humar, F Osvald


Tall oil in combination with eugenol for wood protection
2023 - IRG/WP 23-30787
The aim of this study was to investigate the possibility to use tall oil in combination with eugenol for wood protection. The idea was that the eugenol would increase the decay resistance of the tall oil while the tall oil would decrease the leaching of the eugenol. The results show that an impregnation liquid of 31,5% tall oil, 3% eugenol and 65,5% methanol increased decay resistance of pine sa...
R Ringman, M Westin


How the biochemical activities of polyphenols may be effective for the protection of wood deterioration by termites?
2023 - IRG/WP 23-30789
In spite of the remarkable mechanical characteristics of wood for building construction and furniture industry, this material is prone to biodeterioration by xylophagous organisms. This compromises its durability and performances during storage and services, and results in considerable economical losses estimated by the billions. Protection against fungi, termites and other wood biodegrading organ...
J-P Joseleau, D Messaoudi, K Ruel


Tree bark as a renewable source of wood protection materials for building applications (BarkBuild)
2023 - IRG/WP 23-30792
The BarkBuild project aims to address climate change mitigation by developing new, sustainable, and long-lasting wood building materials with low environmental impact. The project focuses on developing bark-based wood protection and building formulations that demonstrate technical performance, safety, and sustainability in both outdoor and indoor applications. The research objectives of the projec...
A Treu, M Sipponen


A novel wood preservative with vegetal extracts-cypermethrin mixture protects H2-weathered envelope-treated tropical hardwood kempas against Coptotermes termites
2023 - IRG/WP 23-30794
In accordance with sustainability development initiatives by commercial wood protection to conceive of cost-effective, environmentally acceptable wood treatment solutions replacing traditional biocides, this paper reports an aboveground subterranean termite test of termite-susceptible heartwood blocks of the tropical (Malaysian) structural hardwood kempas (Koompassia malaccensis) envelope-treated ...
D Messaoudi, A H H Wong


Envelope wood protection against subterranean termites under H2-hazard class tropical environment by a new generation wood preservative with vegetal extracts-cypermethrin mixtures
2023 - IRG/WP 23-30795
Wood protection industries in progressive economies globally are compelled to develop cost-effective, environmentally acceptable wood treatment solutions for long term carbon storage in wood materials/products while appealing to consumer demands for low environmental impact treated wood. A new generation wood preservative, based in part on 2% vegetal extracts and 0.16% cypermethrin components, has...
D Messaoudi, A H H Wong


Identifying compatible waterborne timber preservatives and fire retardants for use in a VPI system: a practical approach
2023 - IRG/WP 23-30796
To enhance the use and suitability of timber in all applications in both exterior and interior settings, timber typically needs to be treated with a preservative and/or a fire retardant chemical. Combining fire retardants with preservatives into a single treatment process has been a long-term aim of researchers in the timber preservative industry because of the significant logistic and economic ad...
R Robinson, S Meldrum


Emerging wood nanotechnologies towards sustainable application and preservation
2023 - IRG/WP 23-40959
Wood is one of the most abundant biomaterials on earth and has been used for construction historically. Although existing wood composites are commercially successful, materials development has not targeted nano-structural control of the wood cell wall, which could extend the property range. The high porosity and permeability of wood scaffold provide excellent opportunities for material infiltratio...
Q Fu, T Singh, D Elustondo, M Sorieul


Biological durability and wood-water interactions of sorbitol and citric acid modified wood – Effects on the expected service life
2023 - IRG/WP 23-40960
A high level of research activities on sorbitol and citric acid (SorCA) modified wood has been recognized in Europe over the last few years. As this treatment is close to entering an industrial-scale production, it is of interest to investigate how such treated wood performs upon long-term outdoor exposure. Hence, in this study Scots pine (Pinus sylvestris L.) sapwood was modified with aqueous sol...
K Kurkowiak, L Emmerich, H Militz