The biological durability approach for wood product performance and service life prediction
2010 - IRG/WP 10-20457
The performance of wood-based products under conditions that enable biodegradation are of concern to all who envisage sustainable use of forest based products. This concern is also the basis of classification of wood species on the basis of their biological durability. Engineers are looking for options to transfer such classification into practical service life values for constructions and related...
J Van Acker, J Van den Bulcke, L De Boever


Biological performance of wood treated with tar-oil recovered during slow pyrolysis of macadamia nut shells
2010 - IRG/WP 10-30523
This study evaluated decay and termite resistance of wood treated with tar oil obtained from a commercial pyrolysis process of macadamia nut shells. Vacuum-treated pine wood specimens were subjected to various brown and white rot fungi based on the soil-block test method specified by the American Wood Protection Association (AWPA) after leaching process. Treated specimens were also subjected to th...
S Nami Kartal, E Terzi, C Kose, J Hofmeyr, Y Imamura


A Comparison of the Performance of Related Copper Based Preservatives against Soft Rot
2010 - IRG/WP 10-30540
The performance of pine and beech wood treated with either a soluble copper + quat (ACQ type D) preservative system or a particulate copper + quat system was evaluated in unsterile soil using the European standard ENV 807 soft rot decay test procedure. In addition, to compare soft rot performance of soluble and particulate copper directly without the influence of co-biocides, beech and pine test...
M Ray, D Dickinson, K Archer


Accelerated L-joint performance testing of organosilicon treated wood
2010 - IRG/WP 10-30551
In this research Scots pine sapwood L-joints were treated with organosilicons and organosilicons in combination with biocides. These L-joints were prepared and exposed according to the accelerated L-joint method. They were inspected each season for fungal discolouration and removed from the rack after three years outdoor exposure. Subsequently the moisture content, mass loss and decaline uptake we...
L De Vetter, J Van Acker


Effect of 4 Preservatives on Physical, Mechanical and Mold-Resistant Properties of Bamboo Oriented Strand Boards
2010 - IRG/WP 10-40483
This study investigated the effects of 4 preservative systems on physical, mechanical and mold-resistant properties of bamboo oriented strand board (OSB) panels bonded with urea formaldehyde resin. Preservative A (Zinc Borate), B (IPBC), C (AAC+Borate) and D (carbendazim + prochloraz) were incorporated with strands during blending at three loading levels. The results showed that the mechanical and...
Juwan Jin, Daochun Qin, Wanshu Wei, Kuan Fan


Comparison of colour change in wood clear-coating systems including inorganic and organic UV absorbers for exterior use
2010 - IRG/WP 10-40499
The aim of this work is to compare the performance of inorganic and organic UV absorbers used in a wood coating application against weathering. Our study has investigated the colour changes of selected UV absorbers; hombitec 402 RM from the Sachtleben Company as an inorganic UV absorber, tinuvin 477 DW from the Ciba Company as an organic UV absorber. The study was carried out on two wood species; ...
Ö Özgenç, B Forsthuber, A Teischinger, C Hansmann


Performance of selected types of coated and uncoated modified wood in artificial and natural weathering
2010 - IRG/WP 10-40510
The objective of the present work was to investigate the influence of commercial wood modification methods on weathering behaviour and coating performance. It was aimed to compare modification methods and to set up maps of weathering behaviour for these methods with and without a semi-transparent wood stain. Artificial and natural weathering trials were carried out with a selection of different ty...
G Grüll, L Podgorski, M Truskaller, I Spitaler, V Georges, S Bollmus, A Steitz


Wet and dry adhesion of coatings on modified and unmodified wood: comparison of the pull-off test and the cross-cut test
2010 - IRG/WP 10-40524
The objective of this paper is to study the influence of several types of modification (acetylation, furfurylation, thermal modification) on coatings adhesion and to compare two methods of assessing the adhesion: the cross-cut test and the pull-off test both tested in dry and wet conditions. The study also investigates the effect of other parameters of the wood substrates on adhesion like the ring...
L Podgorski, G Grüll, M Truskaller, J D Lanvin, V Georges, S Bollmus


Effect of Coatings on the Durability of Birch and Spruce Plywood. Part 1: Weathering Performance
2010 - IRG/WP 10-40526
Several different coated birch and spruce plywood types were investigated in Finland using outdoor weathering. The weather performance of the tested coated birch plywood was good compared with uncoated birch and spruce plywood. The paint base film coated and painted birch plywood performed well in outdoor testing at VTT's test site. Phenol film coated plywood was sensitive to UV light, but on...
A Nurmi, H Viitanen


Effects of intumescent formulation of vinyl acetate-based coating on flame-retardancy of thin painted red lauan (Parashorea spp.) plywood
2011 - IRG/WP 10-40537
Using intumescent coatings on wood-based materials is an effective method for fire safety. The intumescent coatings consist of four major components: (1) binder resin (BR), (2) carbonizing substance (CS), (3) foam producing substance (FPS) and (4) dehydrating agent (DA). Previous studies have demonstrated that the formulation of the four components strongly influences the performance of coatings. ...
Chih-Shen Chuang, Kuang-Chung Tsai, Te-Hsin Yang, Ming-Kuang Wang, Chun-Han Ko


Decay hazard mapping for Europe
2011 - IRG/WP 11-20463
In this study, two different dose-response models for above-ground decay as well as a model transferring macro climate data to wood climate data are presented. The models base on data from field trials, which had been conducted at 28 European test sites, and were used to calculate the relative risk for decay caused by climate variability in Europe. The two dose-response models give coherent result...
C Brischke, E Frühwald Hansson, D Kavurmaci, S Thelandersson


Service life prediction of wooden components - Part 3: Approaching a comprehensive test methodology
2011 - IRG/WP 11-20464
This paper is the third in a series on 'service life prediction' of wooden components and should be considered as a discussion paper. The authors tried to analyze the topic with a look from a distance and comment sometimes with a smile on the current controversial discussion about SLP issues. Nevertheless, the viewpoints of different groups, such as natural scientists, engineers, approva...
C Brischke, C R Welzbacher, L Meyer, T Bornemann, P Larsson Brelid, A Pilgård, E Frühwald-Hansson, M Westin, A O Rapp, S Thelandersson, J Jermer


Improving our understanding of moisture and other durability-related properties of wood in building envelope performance prediction
2011 - IRG/WP 11-20468
Building science has become an increasingly important field in recent years with rapid changes in construction methods, building materials and consumer expectations. The field has also been brought to prominence by a few large-scale premature building envelope failures in a few regions across the world. Considerable effort has been put into developing hygrothermal models to simulate heat, air, vap...
Jieying Wang, P Morris


Aesthetic service life of coated and uncoated wooden cladding - influencing factors and modelling
2011 - IRG/WP 11-20470
Mould growth on exterior coated cladding façades is an undesirable element and will often shorten the aesthetical service life. Mould growth on painted surfaces is influenced by type and concentration of film fungicides, the paint formulation and the wood substrate itself, and wooden cladding may experience exponential fungal deterioration caused by variation in the climatic factors, often within...
L Ross Gobakken, O A Høibø


Wet and dry adhesion of coatings on modified and unmodified wood: influence of 18 months of natural weathering on the pull-off test and cross-cut test results
2011 - IRG/WP 11-40569
The objective of this paper is to study the influence of several types of modification (acetylation, furfurylation, heat treatment) on coatings adhesion after 18 months of natural weathering according to EN 927-3 in Vienna (Austria). The paper compares two methods for assessing the adhesion: the cross-cut test (EN ISO 2409) which is the conventional method used and recommended in EN 927-3 and th...
L Podgorski, G Grüll, M Truskaller, J D Lanvin, S Bollmus


Performance of Zinc Borate-Treated Oriented Structural Straw Board against Mold Fungi, Decay Fungi and Termites–A Preliminary Trial
2011 - IRG/WP 11-40571
The performance of zinc borate (ZB)-treated oriented structural straw board (OSSB) against mold fungi, decay fungi and termites was examined in standard laboratory evaluations. OSSB was fabricated with split wheat straw and diphenylmethane diisocyante (pMDI) resin. The ZB was added during panel manufacture to achieve preservative levels (wt.%) of 1.0%, 1.5%, 2.0%, and 3.0%. Untreated (0.0% ZB) OSS...
Guangping Han, M Manning, Wanli Cheng, E Pierre, W Wasylciw


Performance of Creosote/Chlorothalonil Preservatives
2011 - IRG/WP 11-30580
The addition of chlorothalonil to P2 creosote was found to increase the durability of southern pine in a series of ground contact stake tests. At retentions lower than those specified in the AWPA Standards, performance was increased when the creosote was amended with chlorothalonil. This indicates that lower creosote retentions may be required for as good or better ground contact when the amende...
H M Barnes, M G Sanders, G B Lindsey, T L Amburgey


Preliminary laboratory and field evaluation on the performance of Rubbermite as a graded physical barrier against subterranean termite species in Australia
2012 - IRG/WP 12-10766
This paper describes the performance of Rubbermite as a potential graded particle barrier against two subterranean termite species of Coptotermes in laboratory and field test. The results of these bioassays suggest that Rubbermite is a viable control option against Coptotermes species in Australia, particularly against Coptotermes acinaciformis (Froggatt) and Coptotermes lacteus (Froggatt). Rubber...
B M Ahmed (Shiday), J R J French


Comparative studies on the moisture performance and durability of wooden facades
2012 - IRG/WP 12-20492
Wooden claddings are traditionally used in many parts of the world. Also modern structures are frequently made from timber and timber engineering panel products. However, wood has to compete with other cladding materials and its durability needs to assure sufficient functional and aesthetic service life. Besides many other factors the durability of a wooden facade is dominated by its moisture perf...
T Bornemann, C Brischke, J-M Lück


Moisture performance based wood durability testing
2012 - IRG/WP 12-20495
In the frame of a scientific cooperation within the Swedish research program ‘WoodBuild’ comparative field and laboratory durability studies have been carried out by the Technical Research Institute of Sweden SP and Leibniz University Hannover. One objective was to improve test methods as well as evaluation systems in order to facilitate the use of (field) testing for service life prediction. ...
L Meyer, C Brischke, A Pilgård


Performance of Wood Protection Systems at Multiple Field Test Sites Using the Ground Proximity Test Method
2012 - IRG/WP 12-20499
A series of preservative systems were used to treat southern pine ground proximity test samples which were then exposed at a range of test sites located throughout the world. The sites were chosen on the basis of having vastly different Scheffer Climate decay indices. After almost 14 years exposure, distinct differences are apparent in how different preservative systems perform at the different ...
A Zahora, A Preston, L Jin


Testing service life for use class 3: accelerated L-joint performance of commodities
2012 - IRG/WP 12-20500
Above ground testing is considered important for the assessment of treated wood intended for use class 3. Laboratory testing of efficacy of biocides as well as of natural durability focussing on such applications has to be linked to performance and service life. An accelerated L-joint test was some 15 years ago developed at the Ghent University to allow worst case assessment under semi-controlled ...
J Van Acker, J Van den Bulcke, I De Windt, L De Vetter


Performance of boron diffused wood products used indoors for 144 months in Bangladesh
2012 - IRG/WP 12-30581
In this service performance study of boron diffused hardwoods, boron in the form of boric acid (H3BO3) was applied separately through paste and through wet cloth. The born diffused woods were kept indoors for 144-months in Bangladesh to ascertain the performance of treated wood against wood destroying insects. The new easy application processes of cost effectual boric acid have been found effectiv...
A K Lahiry, T Lahiry


Performance superiority of CCA-C treated wooden jetty poles and piles used for 30 years in Bangladesh against marine borers
2012 - IRG/WP 12-30582
Observational study along with previous investigation and records revealed that chromated copper arsenate type C (CCA-C) impregnated southern pine poles and piles of jetty constructed in most vulnerable brackish water in Bangladesh are stable and resistant to attack of all types of marine borers after 30 years of use. It is evident from the service records of other construction materials that CCA-...
A K Lahiry


Performance of wood treated with linseed and tung oil against wood decay fungi and wetting
2012 - IRG/WP 12-30598
Most of the European wood species does not have durable wood. In order to use it in outdoor conditions nondurable material has to be protected. Nowadays, non-biocidal solutions for wood protection are attracting a lot of attention, particularly in use class 2 and 3 applications. One of the non-biocidal techniques is treatment of wood with water repellents like wax emulsions and oils. Linseed oil a...
M Humar, B Lesar