Field-testing of Norway Spruce Claddings with Monitoring of Moisture Content, Material Temperature and Microclimate
2012 - IRG/WP 12-20502
The physical function of a cladding is to protect the interior construction. Under normal circumstances the performance requirements can be met for a very long time, meaning that the technical service life of a wooden cladding can be very long. Since the cladding is a major part of the facade, it also has visual requirements that may define the aesthetic service life, and often it is much shorter ...
G I Vestøl, L Ross Gobakken


Mould growth on wood-based materials – a simulated in-service study
2012 - IRG/WP 12-20503
Ten different wood-based materials including preservative-treated wood, fire retardant-treated wood, modified wood, WPCs and untreated references of pine sapwood and spruce were placed in three different environments (an attic and two crawl spaces) for a period of 26 months. Mould growth was analysed at five to seven month intervals in an effort to map the growth development. The relative humidit...
G Bok, P Johansson, J Jermer


Triazole – based ionic liquids to protect of lignocellulosic materials against fungi
2012 - IRG/WP 12-30601
In presented paper we examined on biotic properties of novel structure of tebuconazole derivatieves: tebuconazole hydrochloride, allyltebuconazole chloride, methyltebuconazole iodide, tebuconazole dihydrocitrate. Our investigation against wood-degrading fungi were contained also the didecyldimethylammonium 3-aminotriazolate as well as didecyldime-thylammonium nitrate(V) with tebuconazole or wit...
J Zabielska-Matejuk, J Pernak, I Frąckowiak, A Stangierska, W Przybylska, M Kot


Protective nanoparticle coating reducing water absorption of wood species
2012 - IRG/WP 12-40614
Nanoparticle coatings were deposited onto different tropical wood samples for controlling the surface hydrophobicity. The styrene(maleimide) nanoparticles were synthesized in aqueous dispersions under pure conditions or in combination with 70 wt.-% palm oil. A first evaluation of the non-coated wood surfaces indicates a high dependence between the water contact angles, the average surface roughnes...
P Samyn, A Paredes, G Becker, H Van den Abbeele, L Vonck, D Stanssens


Detection of Aureobasidium as the dominant fungus on coated wood
2013 - IRG/WP 13-10796
Wood is often covered with a coating in order to protect the surface. Unwanted dark mold growth on paint covered surfaces in external conditions is a familiar phenomenon. Simple microbial techniques have commonly been used to determine the dominant fungal species present in the discoloured area, for example morphological analysis of microscopic preparations of fungal pieces sticking to an adhesive...
E J Van Nieuwenhuijzen, M F Sailer, R A Samson, O C G Adan


Communities of mold fungi on flooded building materials
2013 - IRG/WP 13-10799
A small building built to residential code was flooded using farmland pond water to a depth of two feet at Tuskegee University. The building was drained and left enclosed for an additional three weeks. A total of 168 material samples were removed either immediately after opening (wet) or seven months after flooding (dry). Wall materials sampled included fiberglass batt insulation, gypsum wallboard...
F Skrobot III, H Aglan, S V Diehl


Inhibitory extractives or nutrients? Mould growth on coated heartwood and sapwood of Pinus sylvestris and Gleditsia triacanthos
2013 - IRG/WP 13-10806
Sometimes mould fungi grow over weathered coated sapwood, whereas the coated heartwood is not colonised. Two factors may be responsible for these differences: Either the larger content of nutrients in the sapwood, or the content of biocidal extractives in the heartwood. In this study the factors for the difference in mould growth on coated heartwood and sapwood of Pinus sylvestris (Scots Pine) and...
D Lukowsky, N Buddruhs


Focus on the European standardization - Towards a revision of the EN 350 natural durability standard: a different approach to the inherent resistance and performance of wood and wood-based materials
2013 - IRG 13-10811
The European standard EN 350 “Natural durability of solid wood”, Parts 1 and 2, is one of the fundamental standards developed by the CEN/TC 38 “Durability of wood and wood-based products”. This standard is widely used by wood industries as the reference document which provides information on the resistance of wood species used in mainly the construction sector against decay fungi, wood-bor...
M Kutnik


Method for determining the critical moisture level for mould growth on building materials
2013 - IRG/WP 13-20530
The natural conditions of relative humidity (RH) and temperature (T) in different parts of a building is rarely constant over time. Instead, RH and T often vary cyclically and may pose a risk of mould growth as these conditions are the two key environmental parameters that controls mould growth. Consideration to both humidity and temperature conditions and the susceptibility to mould in a material...
A Ekstrand-Tobin, P Johansson, G Bok


Copper Coating on Wood: a New Way of Protecting Wood
2013 - IRG/WP 13-30617
Thermal spray metal coating technology was used to apply a thin layer of copper on the surfaces of a number of wood species. The adhesion of metal coating to mahogany, oak, soft maple, spruce, white pine and medium density fibreboard (MDF) was evaluated by pull off adhesion test. The resistance of copper coated wood samples to mildew were assessed in the lab. Also, the decay resitance and water re...
M Nejad, R Shafaghi, L Pershin, J Mostaghimi, P Cooper


Study of UV resistance and natural weathering of coatings on chemically modified wood
2013 - IRG/WP 13-40629
In this study, UV resistance and weathering performance of rubberwood (Hevea brasiliensis) and radiata pine (Pinus radiata) modified with benzoyl chloride and acetic anhydride was studied. Performance of polyurethane based wood coatings on modified wood was also evaluated. Unmodified and chemically modified specimens were exposed to accelerated and natural weathering. Modified and unmodified woo...
K K Pandey, K Srinivas


Protective effectiveness of antifouling coatings for wooden boats in the Northern Adriatic Sea
2013 - IRG/WP 13-40634
There are various conventional biocide containing antifouling coatings and some more environmentally friendly paints for boats on the market. However, the question of their performance in accordance with the manufacturers’ statements or guaranties arises. The aim of our preliminary investigation was to state which type of antifouling coating exhibits better effectiveness against fouling organism...
M Petrič, M Humar, J Adamek, B Kričej


Influence of coatings on water uptake of wood surfaces before and after natural and artificial weathering
2013 - IRG/WP 13-40641
Liquid water absorption of wood surfaces with and without coating, before and after exposure to artificial and natural weathering has been studied. Spruce, oak and sapele samples have been exposed to the cycle of EN 927-6, to the cycle of the Gardner wheel and to natural weathering. Five coatings were tested including solventborne and waterborne, semi-transparent and opaque products. Exposure to w...
L Podgorski, S Collignan, J-D Lanvin


Using hyperspectral imaging to detect and quantify mould and blue stain on coated and uncoated wood
2014 - IRG/WP 14-10822
Hyperspectral imaging has been applied on the surface of samples of coated and uncoated Norway spruce (Picea abies) as a new technique to detect and quantify growth of mould and blue stain fungi. Principal Component Analysis of the hyperspectral images resulted in a clear visualization of the fungi and the amount of mould coverage could be estimated. This indicates that NIR hyperspectral imaging c...
L Ross Gobakken, I Burud, A Flø, K Kvaal, T K Thiis


Communities of mold fungi in moisture damaged building materials
2014 - IRG/WP 14-20542
The critical conditions needed for the development of mould and decay fungi have been modelled for different building materials. However, current knowledge of indoor microbes growing on building materials relies on culture-based methods and more advanced molecular biological techniques should be employed to study the complex microbial communities in building materials. In this paper molecular biol...
E Sohlberg, H Viitanen


Field performance of wood-based decking materials in the Western United States
2014 - IRG/WP 14-30645
While wood has long been used for the construction of decks and other outdoor features, a variety of wood-plastic composite (WPC) decking products have emerged over the past decade with claims of exceptional durability and low maintenance. There are relatively few long term comparative tests on these products. The performance of selected WPC decking products was compared with naturally durable we...
S Lipeh, C S Love, J J Morrell


Effect of polyurea coatings on performance of Douglas-fir in tropical above ground exposures
2014 - IRG/WP 14-40665
The potential for using polyurea barriers to limit fungal and termite attack was investigated on Douglas-fir lumber and timbers. Termites were capable of penetrating the barrier to attack non-treated wood as well as wood dip-treated with disodium octaborate. The coatings were also exposed above ground for 48 months in Hilo Hawaii. Samples were dissected to detect internal decay. Coated non-trea...
S Uysal, J J Morrell


Lignin Modification to Produce Sustainable Polyurethane Resin for Wood Coatings
2014 - IRG/WP 14-40682
The use of lignin as the most abundant aromatic natural polymer has been evaluated for use in the production of lignin-based polyurethane resin for coating applications. Coatings are made of resins (ca. 50%), which today are mainly derived from petroleum-based polymers. This study is focused on the development of an environmentally friendly method of modifying lignin to be used as source of natura...
M Nejad, M Arefmanesh, S Chandra, J Mostaghimi, E Master


Applicability of wood durability testing methods to bio-based building materials
2015 - IRG/WP 15-20561
It is well known that organic materials may be susceptible to attack from a range of fungal organisms and any bio-based material used in locations where there is the possibility of microbiological activity must be expected to be able to withstand or prevent such attack. There are a wide range of test methods and standards in place to test susceptibility although most of these test individual compo...
S F Curling, B K Stefanowski, E Mansour, G A Ormondroyd


Development of a rapid screening method to determine the susceptibility to mould growth of novel construction and insulation products
2015 - IRG/WP 15-20562
Wood-based materials are commonly used in building construction/insulation as a replacement for solid timber. However, these materials are susceptible to microbiological growth and different environmental conditions influence the vulnerability of wood-based materials. Moulds are a common problem found within homes and cause aesthetic damage, health problems and can increase material vulnerability ...
B K Stefanowski, S F Curling, E Mansour, G A Ormondroyd


Acceptance levels of surface disfigurement - tolerance to defects of coated wood
2015 - IRG/WP 15-20564
Service life planning (PSL) has become an important issue in performance based building and substantial progress has been made in recent years. The role of predicting the aesthetical service life of wooden building components has been underestimated for quite long time but is recently attracting more and more notice. It is influenced by numerous factors such as discoloration, fading, flaking, crac...
C Brischke, P Kaudewitz


Colonization of treated and untreated decking materials by bacteria, fungi and algae quantified by qPCR
2015 - IRG/WP 15-20568
The use of durable wood species for wood decking in outdoor applications, e.g. garden terrace (use class 3) is gaining more and more interest on the part of consumers and architects. To get detailed information on the practical use of deckings, a project was started in 2010. In total 71 different decking materials (0.03 m²) were installed and evaluated over 30 months. Beside other parameters, the...
E Stoyanova, B Schmöllerl, A Steitz, N Pfabigan, R Gründlinger


Performance of bio-based building materials – viewpoints from the first year of COST Action FP1303
2015 - IRG/WP 15-20572
Maintaining and expanding the market potential for bio-based building products in indoor and outdoor construction uses remains a key activity for industries in the forestry and biotechnological sector, particularly in Europe. Whilst there are ongoing activities within IRG for collecting and populating a database on performance on wood, the performance data for many other (i.e. non-wood) "environme...
D Jones


Indentation and pendulum hardness tests: two convenient assessment methods of the performance of exterior wood coatings
2015 - IRG/WP 15-40689
Developing formulations of exterior wood coatings with long service life is a big challenge. For many years in Europe the performances have been mainly evaluated through weathering tests (within the EN 927 series) followed by visual assessment (blistering, flaking, mould growth, chalking and cracking), colour and gloss measurements, and adhesion tests. Very recently the importance of the mechanica...
L Malassenet, L Podgorski, M Truskaller, G Grüll


Application of nanoparticles of silver and nanoparticles of titanium dioxide in reinforcement of wood and coating for wood in Costa Rica
2015 - IRG/WP 15-40698
Wood is one of the most widely used materials in last 20 years by society in many applications, with a considerable proportion of this material coming from forest plantations. Plantations usually produce timber with reduced strength properties and low natural durability. On the other hand, nanotechnology applications have the potential to increase wood properties. Likewise, nanotechnology cannot o...