A comparison between the effects of ACC & CFK on the durability of beech, hornbeam and cottonwood by using Dipping & Bethel methods in the North of Iran
1997 - IRG/WP 97-40089
From the economical point of view, increasing the lumber durability by the application of preservative treatments is very important. In this study, samples were randomly selected from Fagus orientalis Lipsky., Carpinus betulus L. and Populus deltoides Bartr. in two forms (Board & Squared cross-section) and have been treated with ACC & CFK by using Dipping & Bethel methods. The matched ...
D Parsapajouh, V Etemad, K Pourtahmasebi


Microwave conditioning of Pinus radiata D. Don for preservative treatment
2000 - IRG/WP 00-40182
This paper reviews the effect of pressure steam conditioning on the permeability and treatability of green radiata pine heartwood and the potential for substituting microwave conditioning for steaming. The penetration of liquids into radiata pine occurs mainly in the radial tissue. The permeability of green radiata pine improves following steam conditioning by blowing out the soft radial tissue. T...
P Vinden, G Torgovnikov, J Romero


Occurrence of marine wood borers at three ports in Andhra Pradesh, India
2004 - IRG/WP 04-10509
Marine wood borers are a specialised group of organisms which destroy the wooden structures and cause huge monetary losses. They are site specific and their distribution depends on the water quality of a particular area. Seven species of wood borers such as Martesia striata, Teredo furcifera, T. parksi, Lyrodus pedicellatus, L. bipartita, Bankia campanellata and B. carinata have been identifi...
B Tarakanadha, M.Balaji, R Ramamurthi, K S Rao


Anatomical Characteristics to the Distribution of Water-borne Copper Wood Preservatives in Wood
2004 - IRG/WP 04-40277
The objective of this study was to understand the micro-distribution of a copper-based preservative in wood in connection with anatomical morphology and to consider the fixation of copper in wood. Bulk specimens and semi-ultra thin sections (0.5µm) obtained from Japanese cedar were treated with a CuAz preservative solution. After fixation, SEM-EDXA was used to investigate the micro-distribution...
H Matsunaga, J Matsumura, K Oda


Moisture condition in treated wood exposed outdoors. A progress report
1989 - IRG/WP 3533
Wood treated with water-borne preservatives, mainly CCA (copper/chromium/arsenic), CCB (copper/chrome/boron) or CC (copper/chrome) is often said among users in Sweden to absorb more water than untreated wood. In laboratory tests this statement has not been confirmed but no field tests have been carried out in Sweden to study this phenomenon. In 1986 a project was started to compare water absorptio...
M-L Edlund, C E Sundman


Evaluation of chlorpyrifos as an insecticidal component of a wood preservative
1984 - IRG/WP 3301
After two years of laboratory and field testing, chlorpyrifos is showing excellent potential as an insecticidal treatment to wood. In laboratory termite tests, retentions as low as 1-2 parts-per-million or approximately 0.0008 kg/m³ (0.00005 lbs/ft³) are effective against the Coptotermes formosanus. Laboratory leaching tests have shown no significant effect on the concentration of the retained c...
K Rose, J Kozuma, P Sparrow


An investigation of organotin compounds in treated wood using Mössbauer spectroscopy
1983 - IRG/WP 3249
The influence of sample preparation on the 119mSn Mössbauer spectrum of tributyltin chloride in ponderosa pine was investigated. Initial studies with sawdust and compressed discs concluded that the latter were clearly superior. Further studies showed that compressed discs prepared from 0.4 g of treated wood and 0.1 g of cellulose were robust and gave excellent Mössbauer spectra. The possibility ...
J N R Ruddick, J K Ingram


Leaching Characteristics of Copper in Copper Treated Wood
2003 - IRG/WP 03-30316
The leaching characteristics of copper in copper treated bamboo and other wood species such as slash pine and poplar has been conducted in this paper according to AWPA M11-87 standard, the result indicates that: --Copper fixation rate of salts from organic acids such as citrate and oxalate and malate is less than other non-organic acid formulations. --Copper fixation rate of oven-dried bamboo sa...
Mingliang Jiang, Junliang Liu, Daochun Qin, Yamei Wang, Zehui Jiang


Xenon simulation of natural weathering of external joinery preserving - Finishing systems
1992 - IRG/WP 92-2412
Semitransparent wood stains ('lazures') for external joinery have developed by means of product combination towards complete wood finishing systems that are easy to applicate, have a good weathering resistance and low maintenance cost. The search for enhanced formulations and the possibilities to standardize these products or treatment systems are always facing long periods of we...
J Van Acker, M Stevens, M Nys


Evaluation of some polyurethanes as protective marine coatings for wood
1985 - IRG/WP 4115
Several polyurethane formulations were evaluated in the marine environment as possible replacements for Irish felt used on U.S. Navy minesweepers as a marine borer barrier between the main wooden hull and an outer, wooden sheathing which covers it. Pine panels coated with the candidate materials were tightly juxtaposed with untreated pine baitwood to simulate the hull/sheathing configuration, the ...
J D Bultman, J E Pinto


Effect of media composition on the antagonistic properties of Trichoderma spp. against wood decay fung
1992 - IRG/WP 92-1538
Most screening of potential biocontrol agents of wood decay fungi has previously been undertaken using artificial media. Similarly experiments designed to evaluate the mechanisms involved in antagonism between biological control agents and target fungi, have largely been carried out in conditions which do not accurately reflect the nutrient status of wood. This paper examines the influence of nutr...
U Srinivasan, A Bruce, H J Staines


Durability of surface preserved wood particle boards submitted to atmospherical influence
1995 - IRG/WP 95-40039
The worldwide problem of the continuously growing deficit of high quality natural wood material has caused the attempts of many research workers to find effective composites such as wood particle boards (WPBs) for replacing the massive wood for constructive purposes, depending on where the boards are exploited - in the open or under a shed, they are submitted to various climatic factors such as he...
L Valcheva


Resistance of painted wood to mould fungi. Part 2. The effect of wood substrate and acrylate paint systems on mould growth
1997 - IRG/WP 97-10234
Resistance of acrylate paint systems on different types of pine and spruce sapwood to mould fungi was studied. Dipping into the preservative prior to painting, a primer with and without a fungicide (propiconazole + IPBC 0.50 + 0.2%) and a topcoat with and without a fungicide (propiconazole + IPBC 0.25 + 0.12%) were combinations of the treatments studied. The efficacy of the treatment systems varie...
H Viitanen, P Ahola


Determination of fixation properties by bioassays - A proposal for the assessment of safety indexes in wood protection
1990 - IRG/WP 3566
In the determination of environmental effects of chemicals tests with fishes, daphnia and algae have proved to be practicable. With respect to wood protection such bioassays are suitable to control effects of treated timber against aquatic organisms. By using the fish-acute-toxicity-test the development of a laboratory test method is described for the checking of the fixation rate of a copper-chro...
H-W Wegen


Risk reduction from curative treatments, restoration and maintenance of building and individual housing - simple precautions that make the difference
2005 - IRG/WP 05-50224-15
This document explores the potentialities of risk reduction, from activities of remediation in construction, developped at small scale by professionals or individuals on targets like moulds, rots, termites and other wood destroying insects, with products distributed for professional or do-it-yourself purposes. At the first stage, an inventory of the type / interest of products / processes is carri...
G Ozanne


Efficacy of linear chain carboxylic acid anhydrides as wood protection chemicals
2002 - IRG/WP 02-30295
This paper presents an assessment of the effectiveness of linear chain carboxylic acid anhydrides namely, acetic, propionic, butyric, valeric and hexanoic anhydride, in improving the decay resistance of Corsican pine (Pinus nigra Schneid) sapwood. Wood-anhydride bond formation was verified by the increase in sample weight and volume. A brown rot fungus [Coniophora puteana (Schum.:Fr)] was selec...
A N Papadopoulos, M D C Hale, C A S Hill


Optimum growth conditions for the metal-tolerant wood decay fungus, Meruliporia incrassata TFFH 294
1999 - IRG/WP 99-50142
There is a worldwide need for alternative methods for the treatment and disposal of CCA-treated waste wood. Illman and Highley (IRG/WP 96-10163) reported the isolation of a unique strain of Meruliporia incrassata (TFFH 294) with tolerance to CCA. The strain is capable of degrading CCA treated waste wood, giving a 40% weight loss in the ASTM soil block test. The strain is an ideal candidate for deg...
V W Yang, B Illman


Accelerated laboratory soil contact decay test using soil amended with composted wood
2004 - IRG/WP 04-20284
The effect of amending soil with wood compost on the decay rate of wood wafers in contact with the unsterile soil, as measured by radial compression strength loss, was explored. It was found that the addition of composted wood to the soil significantly increased the wood decay rate. The reason for this acceleration in wood decay is not entirely clear, but appears to be at least partially associate...
D D Nicholas, H Borazjani, T Schultz


Leaching and fixation characteristics of chrome-copper-fluoride-zinc (CCFZ) treated wood
1996 - IRG/WP 96-30096
The leaching characteristics of radiata pine sapwood blocks treated with CCFZ were evaluated by the AWPA standard leaching test. The rate of fixation of the preservative components in CCFZ treated radiata pine were also evaluated by quantitative analysis of solution expressed from the treated wood. Both leaching and fixation characteristics of CCFZ were compared with CCA-Type C treated wood sample...
Gyu-Hyeok Kim, Jong-Bum Ra


Wood protection processes in the Asean countries
1994 - IRG/WP 94-40034
This paper presents the wood processing practices in the Asean countries composing Indonesia, Malaysia, Philippines, Singapore, and Thailand except Brunei. The development of wood preservation industry in these countries started as early as 1922 to 1960. As in other industrial countries, treatment pressure with creosote of utility poles, railway sleepers, and marine pilings are the prime commoditi...
F R Siriban


Inhibition of termite damage by N'N-napthaloylhydroxyamine (NHA): Reticulotermes flavipes (Kollar) vs. Coptotermes formosanus Shiraki
2000 - IRG/WP 00-10354
The calcium precipitating agent NHA has been shown to protect southern yellow pine (SYP) from wood decay and termite damage comparable to CCA in field tests (Gulfport, MS) for two years (Crawford and Green, 1999). In a collaborative study, SYP wood blocks were vacuum treated with three concentrations of aqueous NHA and exposed in a no-choice test to Eastern subterranean termites (FPL, USA) and For...
F Green III, S T Lebow, T Yoshimura


Treatment of wood with formaldehyde. Acid catalysis of the reaction between formaldehyde and wood
1980 - IRG/WP 3146
Formaldehyde reacts with the free OH-groups in wood forming cross-linking bonds. The reaction can be brought about without any catalyst but in that case the activation energy is very high and high temperatures and long reaction times are needed. Normally, the reaction is catalysed by different acids. Acid catalysts, however, tend to degrade the cellulose and the wood matrix causing reduction in th...
T Vihavainen, K Piispanen, P Mansikkamäki


Practical consequences of the clarification of the chemical mechanism of CCA fixation to wood
1983 - IRG/WP 3220
Practical consequences derived from the chemical investigation of the mechanism of fixation of CCA to the wood constituents are discussed. Among these, formulas for the calculation of the time of hexavalent chrome fixation are presented. Furthermore, three parameters are shown to be important to the long-term effectiveness of CCA-treated timber: (i) the temperature of treatment, (ii) the initial p...
A Pizzi


Environmental situation on wood preservation industries in Bangladesh
2000 - IRG/WP 00-50148
The hazard that wood preservative chemicals pose to people and the environment is serious. The lack of information, legislation and awareness create an unfavorable situation on wood preservation industries. In this regard, three wood preservation industries have been visited to collect the information about pollution. It was observed that different steps have been taken to minimize the contaminati...
K Akhter


SEM investigation of the production of extracellular mucilaginous material (ECM) by some wood inhabiting and wood decay fungi when grown in wood
1997 - IRG/WP 97-10193
Previous reports have illustrated the involvement of extracellular mucilage (ECM) in wood decay by Basidiomycetes. Its production is investigated in a range of stain, mould and soft rot fungi in Corsican pine, Scots pine and European beech. Fungi examined were: Chaetomium globosum, Ceratocystis coerulescens, Trichoderma harzianum, Ophiostoma piceae, Mucor sp. and Penicillium. sp. The samples were ...
A R Abu, D J Dickinson, R J Murphy