Your search resulted in 903 documents. Displaying 25 entries per page.
Preservative properties of boron-treated paulownia wood
2024 - IRG/WP 24-20729
This research was performed to investigate the preservative retention properties of paulownia wood treated using boric acid/borax at mass ratio of 1:1.8. Different portion of paulownia wood (top, middle, bottom) were used as a sample throughout of this study. In the treatment process, the paulownia wood was dipped in the 1% boric acid/borax solution for 1, 24, 72, 120 and 240 hours to achieve requ...
T Khadiran, M A M Abdullah, S Lipeh
Physical, durability and chemical characterization of Gmelina arborea (Roxb.) wood treated with lactic acid
2024 - IRG/WP 24-30803
The increase in demand for durable wood has drawn attention to the use of fast-grown plantation species across the globe. Chemical modification was used to treat Gmelina arborea wood with lactic acid for property enhancement. The treated samples were obtained from two different ages of 15 and 10 years and sawn into (20 x 20 x 60) mm and (20 x 20 x 20) mm for physical, durability and chemical chara...
T O Akinwamide, J M Owoyemib, E A Iyiolac
Citric acid and sorbitol treatment: A comparative study of Canadian and Norwegian species
2024 - IRG/WP 24-30806
Dimensional instability can reduce the competitiveness of wood in exterior applications such as cladding and decking. The objective of this work was to evaluate the dimensional stability of permeable and refractory softwoods from Europe and North America modified via a sorbitol and citric acid treatment. White spruce and Norwegian spruce, refractory species, and jack pine and Scots pine, relativel...
D Schorr, Erik Larnøy, R Stirling, G Boivin
A novel treatment for increasing UV stabuility of wood based on citric acid and urea
2024 - IRG/WP 24-30811
Wood, a fundamental material in the Built Environment, faces challenges related to durability and weathering, notably UV degradation leading to colour changes. This study explored a novel treatment method utilising citric acid and urea to enhance the UV stability of wood. The reaction between these compounds forms fluorescent species and insoluble nanoparticles upon thermal treatment. Two treatmen...
S Jué, A Scharf, C-F Lin, R Moutou Pitti, D Sandberg, D Jones
Evaluation of the water exclusion ability and inherent bioactivity of heartwood against decay in Japanese and European wood species via above-ground exposure and water absorption tests
2024 - IRG/WP 24-40998
The natural durability of wood has been thought to mainly depend on bioactive extractives and the water exclusion ability. To clarify the contribution of each factor to wood durability, above-ground exposure tests were conducted on Japanese and European wood species. A double-layer test was carried out using heartwood specimens of four wood species, i.e., Japanese cedar, Japanese cypress, Scots pi...
T Osawa, R Noda, K Yamamoto
Outdoor termite resistance performance of zinc borate (Borogard® ZB) treated parallel strand lumber (PSL) – 15 years field test results
2024 - IRG/WP 24-40999
This report discloses the outdoor termite resistance performance of PSL samples treated with zinc borate at a dosage of 0.85% BAE and 1.72% BAE in Wuxi, China. The outdoor field trial lasted for 15 years and observations were made after 6 months, 3 years, 5 years 1 month, 6 years 6 months and 15 years. The retaining rates of B2O3 and ZnO in the final samples were also tested, and the hypothesis wa...
S Shi, E Laval, K Lung, F Ascherl, R Williams, W Li, X Li
Evaluation of vacuum borate treated spruce or pine CLT in an above ground protected test in southern Mississippi
2024 - IRG/WP 24-41001
Cross laminated timber (CLT) has become a popular wood composite in large building applications that were previously limited to concrete and steel. To extend service and prevent biological attack, chemical protectants are often applied to wood. Cross laminated timber panels are not typically treated, in part due to a lack of data on efficient and effective methods for treating large panels. Ther...
M E Mankowski, A Taylor, G T Kirker
Modelling the service life of wood in ground contact – Verification of remotely sensed soil data from the reanalysis dataset ERA5-Land using in-situ measurements at a test site of utility poles in Eastern Norway
2024 - IRG/WP 24-41003
This study compared soil moisture and temperature estimates from the 5th European reanalysis (ERA5-Land) dataset with in-situ measurements to assess the accuracy and applicability of ERA5-Land data for modelling the service life of wood in ground contact. The ERA5-Land soil temperature estimates showed a moderate correlation with the in-situ temperature measurements (Spearman’s ρ of 0.73) and a...
U Hundhausen, P B van Niekerk, B Marais
Performance of Douglas-fir cross laminated timber (CLT) subjected to elevated humidity in a ground proximity field test for 6 years
2024 - IRG/WP 24-41010
The ability of insecticidal soil drenches or spray-on insecticide/fungicide treatments to protect mass timber elements exposed in a high moisture environment but out of direct soil contact was assessed using a modified AWPA ground proximity test established in 2017. Three-ply Douglas-fir CLT pieces measuring 305 x 355 x 105 mm (L x H x W) were installed at the Harrison Experimental Forest (HEF) (S...
M E Mankowski, J J Morrell, T G Shelton, G T Kirker
Field test method for wood in above ground situation - The full CEN/TC 38 guideline for the Sandwich method. Part 1 - Determining the relative protective effectiveness of a wood preservative
2024 - IRG/WP 24-41013
The attached draft CEN Technical Specification (i.e. pre-EN standard) has been drafted in order to become an alternative to the Lap-Joint test method (EN 12037:23) for testing of wood in above ground situation and the draft CEN/TS Part 1 is specifically intended for determining the relative protective effectiveness of a wood preservative. The new draft CEN/TS is based on a test method developed by...
M Westin, R Ringman, A Christof, F Friese
Structural health assessment of wood - A comparison of methods for determining the spatial spread of fungal infestation in beams and rafters
2025 - IRG/WP 25-11051
Wood decay in buildings can cause severe economic losses, require comprehensive refurbishment, and removal of decayed wooden elements from the building. The latter aims at restoring the structural integrity of the component or the entire building through replacement, and at preventing the infestation from spreading further. In practice, components are cut out of the structure to such an extent tha...
C Brischke, N Sommerfeld, E Flohr, A K Mayer, S Bollmus
A comparison of methods – how to achieve a robust and conclusive durability classification of wood
2025 - IRG/WP 25-11063
The biological durability of wood is a relative and unitless size, and therefore wood species and wood-based materials are assigned to durability classes (DC). In Europe, such classes are based on a variety of measures, which can be absolute or relative to a non-durable reference species. The aim of efforts to develop and standardise methods for determining biological durability should be to ensur...
C Brischke
Investigation of oxalic acid production in brown-rot fungi
2025 - IRG/WP 25-11074
Brown-rot fungi play a crucial role as wood decomposers in forests and are also known as the main cause of biodeterioration of wooden buildings in Japan. Therefore, understanding their decomposition mechanisms is important for the maintenance and preservation of wooden structures. While white-rot fungi generally use enzyme-system for degradation, many brown-rot fungi lack cellobiohydrolases which ...
S Matsumoto, R Tsukida, T Ito, M Iritani, M Yoshida
Enhancing the Fire Resistance of Spruce Wood through Treatment and Additive Application: Small Flame Test Method
2025 - IRG/WP 25-20737
Spruce panels treated by spraying with Burnblock® spray, were tested using “Small flame test method” according to EN ISO 11925-2:2011. The fire retardant product from Burnblock ApS is reported by the Danish company to be bioderived and non-toxic. The results for the untreated planed spruce showed moderate flammability whereas the Burn Block treated panels exhibited exceptional fire resistance...
E S Mujanic, R Hasanagic, E Kerzic, L Fathi, M Humar
Securing Flame Retardancy in Wood: Durability After Artificial and Natural Weathering Test
2025 - IRG/WP 25-20738
The outdoor use of wood is often limited by challenges such as dimensional instability, vulnerability to fungal decay, and high flammability. Traditional flame retardant treatments improve fire resistance but suffer from significant leaching under environmental exposure, reducing their long-term effectiveness. This study introduces an innovative solution by integrating flame retardants with DMDHEU...
M Wu, L Martin, H Militz
Citric acid/urea derivatives as an anti-discolouration treatment for wood surfaces
2025 - IRG/WP 25-20741
The exterior-use wood faces raining and sunlight exposure, which can cause property changes of the wood, such as the discolouration, dimensional instability, and biological attack. This article explores the use of citric acid and urea as surface protection of wood. The heating of citric acid and urea can result in the fluorescent carbon dots. These carbon dots can absorb UV light with the emission...
C-F Lin, O Myronycheva, D Jones, O Karlsson
Are we barking up the right tree? - the use of bark residues in wood protection
2025 - IRG/WP 25-20742
Tree bark, a lignocellulosic side-stream, is typically underutilised, often combusted or landfilled, thus contributing to greenhouse gas emissions. This communication paper explores the potential of bark residues, particularly suberinic acid, tannins and other polyphenols, in wood protection applications, including coatings, adhesives, and fire retardants. Several European projects have been initi...
A Treu, M Altgen, M Sipponen, M Borrega
Durability Analysis of Bio-based Phenol-Formaldehyde Resin-Treated Wood
2025 - IRG/WP 25-20753
The aim of this study is to explore the application of bio-based materials in outdoor construction. Enhancing the durability of wood products effectively extends their carbon storage lifespan, making it essential to investigate their long-term durability. The study used commercial resin (CPF) and laboratory-synthesised petro-based phenolic resin (LPF) as control groups. Japanese cedar specimens we...
T-H Lin, P-Y Kuo
Enhancing the Effectiveness of Penflufen by using a Plant Booster
2025 - IRG/WP 25-20759
Penflufen (Preventol® A 800) is a modern pyrazole fungicide which has been approved by the US EPA for the use in wood protection in 2018. Penflufen is an inhibitor of the succinate dehydrogenase (SDHI). It is highly efficient against wood decaying basidiomycetes fungi. In the European standard efficacy test EN 113/ EN 84, penflufen is controlling both brown rot and white rot fungi at the low rete...
D Messaoudi, A Robert, P Meckler, T Jaetsch
Unlocking the Potential of Dairy Coproducts in Wood Modification
2025 - IRG/WP 25-30822
The production of dairy coproducts, such as whey (sweet or acid) and whey ultrafiltration permeate, has significantly increased in response to the rising global cheese consumption. Proteins found in by-products are purified for human nutrition. However, upcycling lactose, which is the major compound of cheese by-products, is more challenging due to the high cost of upcycling processes. Furthermore...
A Keralta, J Karthäuser, J Winninger, J Chamberland, M-J Dumont, V Landry, H Militz
Performance Verification of Water-Based Outdoor Wood Protection Coatings Based on Weather Resistance Evaluation
2025 - IRG/WP 25-41015
Recent trends in wood protective coatings: Concerns over volatile organic compound (VOC) emissions and the need to reduce maintenance costs have increased demand for environmentally friendly and highly durable coatings. While conventional solvent-based paints are superior in durability, they have been associated with problems such as environmental impact and odour during application. As an alterna...
N Ikemoto
Evaluation of moisture exclusion ability of wood using double-layer outdoor exposure tests
2025 - IRG/WP 25-41021
The material resistance of wood to decay must be due to the combined effects of heartwood extractives and the moisture content state. Evaluating the moisture exclusion ability of wood is important for assessing its durability in outdoor use. We conducted previously double-layer outdoor exposure tests and investigated the relationship between moisture content over time and the progress of decay usi...
T Osawa, R Noda, K Yamamoto
AI Models for Accelerating Wood Protection Testing: Development of Predictive Tools Based on Long-Term Field Test Data
2025 - IRG/WP 25-41023
In this study, we present the development of DecAI, an artificial intelligence (AI) model designed to optimise and accelerate performance evaluations of wood protection products in the European EN 330:2014 "Field test: L-joint method." The Danish Technological Institute (DTI) compiled a dataset of over 100,000 data points from approx.10,000 L-joint samples collected over +15 years at field sites i...
J Stenbaek, B Noufel, L Glade, P Bisgaard
Optimising properties of citric acid-sorbitol bonded particleboards with added ammonium dihydrogen phosphate as fire retardant
2025 - IRG/WP 25-41033
Due to the adverse health effects of formaldehyde-based adhesives and their fossil origin, there is an ongoing search for appropriate bio-based adhesives for particleboards. Although there are some possible solutions, their use in construction is limited partly due to their low moisture resistance and flammability. The latter can be improved by adding various fire retardants. A particleboard with ...
L Kopač, S Medved, B Lesar, M Humar
Durability evaluation of outdoor-exposed CLT treated with various wood presevatives using CT scans
2025 - IRG/WP 25-41035
Methods for wood preservation treatment of large materials such as Cross Laminated Timber (CLT) are limited. It is unclear which wood preservation treatment methods can effectively protect CLT from rot risk. In this study, accelerated rot tests (fungus cellar test) of CLT treated with the solvent-borne wood preservative by non-pressure treatment, named ‘deep penetration treatment’, were conduc...
Y Sakurai, T Shigeyama, Y Sugai