Above Ground Field Testing – Influence of test method and location on the relative performance of various preservative systems
2008 - IRG/WP 08-20393
Standardized above ground tests such as the lap-joint or test deck methods can be very slow in producing useful information on the relative performance of wood preservative systems. It often requires many years for decay to develop in wood treated to sub-optimal concentrations of standardized preservatives, making relative comparisons of performance between new systems and established preservativ...
A Zahora


Effectiveness of MOQ® OX 50 (CCB-Oxide) wood preservative – Part 2: Field tests
2008 - IRG/WP 08-30483
MOQ® OX 50 is a chromated copper borate preservative known around the world as CCB. In Brazil, this product is the only CCB-oxide type preservative with fungicide and insecticide properties registered at the Brazilian Institute for the Environment and Renewable Resources (IBAMA) that complies with the requirements of the Brazilian and European markets for preserved wood. For over five decades, s...
A Gandolfi Jr, C Salvela, D R Macedo, J M Vidal


Multifactorial Antimicrobial Wood Protectants
2008 - IRG/WP 08-30484
It is unlikely that a single antimicrobial compound, whether synthetic or natural, will provide the ‘magic bullet’ for eliminating multiple biological agents affecting wood products. Development of synergistic combinations of selected compounds, especially those derived from natural sources, is recognized as a promising approach to improved wood protection. Recent adoption of effective fungici...
R D Coleman, C A Clausen


Biological Performance of micronized copper wood preservative formulations in field and laboratory tests
2008 - IRG/WP 08-30488
Micronized Copper wood preservative formulations with different co-biocides were exposed to brown rot fungi in an 8-week AWPA E10 soil block decay test and two AWPA E7 ground-contact decay tests in Hawaii. The micronized copper formulations performed well against decay at or above the AWPA UC3 and UC4 retentions stipulated by the ICC-ES. Micronized copper preservatives performed comparably to a ...
G M Larkin, J Zhang, D L Richter, R J Ziobro, P E Laks


Performance of dip and pressure treated wood in termite ground proximity exposures in Hilo, HI, and Colombia
2008 - IRG/WP 08-30491
A number of preservative systems were evaluated for their ability to control termite attack when applied as both dip and pressure treatments. With dip treatments, better performance was observed with southern pine than spruce-pine-fir using the same solution strength treatment, probably as a result of the about 50% greater uptake with southern pine and associated deeper preservative penetration. B...
P Walcheski, A Zahora


Laboratory and field exposures of FRT plywood: Part 1. Physical test data
2008 - IRG/WP 08-40426
Our understanding of the laboratory induced degradation with fire retardant systems is currently limited since we are unable to correlate laboratory steady-state experiments with actual in-service field degradation. Current model studies have generally been limited to isothermal rate studies with selected model FR chemicals. Other factors also play a major role in the degradation of FR-treated woo...
H M Barnes, J E Winandy, C R McIntyre


Impact of decay and blue stain causing fungi on the structural integrity of wood
2009 - IRG/WP 09-10699
The potential influence of diverse decay patterns caused by different brown rot provoking basidiomycetes on the structural integrity of wood was investigated. Additionally the potential impact of blue stain on the structural integrity was examined. Therefore decayed Norway spruce (Picea abies Karst.) specimens representing a wide range of mass loss, caused by four different brown-rot fungi and one...
C Brischke, C Welzbacher, T Huckfeldt, F Schuh


Natural Durability Variations of Malaysian Timbers from Sarawak after 26 Years Exposure by Stake Test
2009 - IRG/WP 09-10704
An extensive graveyard stake test site was established in 1977 in Sibu, Sarawak, Malaysia, to evaluate the in-ground durability of 132 Sarawak wood species, mainly hardwoods. Test samples were planted at 100 x 50 cm spacing. Authenticated wood specimens from 3 trees of each of 132 species were processed into 20 replicated outer heartwood (or else undifferentiated heartwood) stakes of 19 x 19 x 457...
A H H Wong, Ling Wang Choon


Degradation of wood veneers by Fenton’s reagents: effects of low molecular weight phenolic compounds on hydrogen peroxide decay and tensile strength loss
2009 - IRG/WP 09-20400
Pine wood (Pinus sylvestris) veneers strips were incubated in acetate buffer containing hydrogen peroxide and iron to mimic mechanisms of brown rot decay and assess the degradation of cellulose through analysis of the tensile properties of the decayed wood. The tensile properties of thin wood strips treated with Fenton system reagents or precursors were determined and correlated to weight loss as ...
Yanjun Xie, R Well, Zefang Xiao, B Goodell, J Jellison, H Militz, C Mai


Effectiveness of sol-gel treatments coupled with copper and boron against subterranean termites
2009 - IRG/WP 09-30493
Wood modification by sol-gel treatments shows many positive features, like antimicrobial properties. Wood was also successfully modified with alkoxysilanes enhancing its resistance against soil micro-organisms. Silver, copper, zinc compounds, boric acid or organic biocides such as alkylammonium compounds may be added to the sol-gel to enhance its biocidal properties. Nevertheless, if some of these...
E Feci, L Nunes, S Palanti, S Duarte, G Predieri, F Vignali


Resistance to decay fungi of ammonium borate oleate treated wood
2009 - IRG/WP 09-30505
Ammonium borate oleate molecule (ABO) produced from reaction between boric acid, ammonia and oleic acid was tested as wood preservative treatment against brown and white rot fungi according to European standards. This compound was prepared according to a previous study which has proved existence of synthesis reaction and effectiveness against termites (Lyon et al. 2007b). Four solutions of ABO in ...
F Lyon, M-F Thevenon, A Pizzi, J Gril


Laboratory test of some formulations against stain and mould fungi isolated from bamboo wood
2009 - IRG/WP 09-30508
To screen the effective anti-mould formulations, fungicides such as carbendazim, tebuconazole, fludioxonil, difenoconazole, prochloraz, benomyl and 8-hydroxy-quinoline copper (copper oxine) were selected to conduct the laboratory test of fungicidal activity by method of inhibition zone against Botryodiplodia theobromae Pat., Fusarium sp., Alternaria tenuis Nees., Penicillium purpurogenum Stoll, Tr...
Xingxia Ma, Airui Sun, Mingliang Jiang, Daochun Qin


Laboratory and above ground exposure efficacy of silicon-boron treatments
2009 - IRG/WP 09-30510
The study deals with silicon compounds, namely tetraethoxysilane (TEOS), phenyltriethoxysilane (PhTES) and methyltriethoxysilane (MTES) at concentrations of 23, 16 and 10% in combination with 1.2-1.5% boric acid. The aim with the study was to combine the chemical approach with the necessary biological tests of the impregnated wood. The tested silicon-boron combinations ensured mass loss less than ...
N Terziev, D Panov, A Temiz, S Palanti, E Feci, G Daniel


Environmental Emission of Wood Preservatives: Interpretation of Data Relevant to BPD Risk Assessments
2009 - IRG/WP 09-50259
The risk assessments for the use of wood preservatives proposed by the OECD and used under the Biocidal Products Directive (BPD) (98/8/EC) require the derivation of leaching rates for active substances. These rates are to be used as input data in to agreed exposure scenarios. The leaching rates can be derived from laboratory testing and from field testing. The relationship between laboratory and f...
D G Cantrell


Rapid Microwave-Assisted Acid Extraction of Metals from Chromated Copper Arsenate (CCA)-Treated Southern Pine Wood
2009 - IRG/WP 09-50262
The effects of acid concentration, reaction time, and temperature in a microwave reactor on recovery of CCA-treated wood were evaluated. Extraction of copper, chromium, and arsenic metals from chromated copper arsenate (CCA)-treated southern pine wood samples with three different acids (i.e., acetic acid, oxalic acid, and phosphoric acid) was investigated using in microwave reactor. Oxalic acid wa...
Bin Yu, Chung Y Hse, T F Shupe


Estimating the heat treatment intensity through various properties of thermally modified timber (TMT)
2009 - IRG/WP 09-40459
The suitability of different measures for prediction of the heat treatment intensity was investigated. Therefore, the resistance to impact milling (RIM), the lightness L*, the equilibrium moisture content (EMC), the anti swelling efficiency (ASE) and the total amount of soluble carbohydrates (TSC) of heat treated specimens were correlated with corresponding fungal resistance achieved by heat treat...
C R Welzbacher, C Brischke, A O Rapp


Biological Performance of Boron-based Chemicals Treated Wood Composites
2009 - IRG/WP 09-40464
In this study, the biological performance of wood-based composites panels treated with boron containing chemicals against to a fungus was determined. Boric acid, borax, zinc borate and agricultural borate (Tarım-bor™), developed and patented by National Boron Research Institute, were mixed with wood chips or fibers and then particleboard, medium strand board and middle density fiberboar...
Ü C Yıldız, H Kalaycıoğlu, S Yıldız, A Temiz, E Tomak Dizman, A Çavdar Dönmez


Termite Resistant Properties of Wood and Natural Fiber Plastic Composites - AWPA E1 Test Data
2009 - IRG/WP 09-40466
This paper deals with resistance properties of wood plastic composites against Formosan Subterranean Termites (FSTs) based on the AWPA E1 test standard. Sixteen laboratory WPC formulations, four WPC commercial materials, and southern pine (Pinus sp.) wood control were tested for termite mortality, sample weight loss, and sample damage rating. The results show that FSTs did attack WPC products in ...
Q Wu, T Shupe, J Curole, K Ragon, M Voitier, M Freeman, D Ring


Seasonal shifts of fungal community structure at the interface of treated or untreated wood and soil
2010 - IRG/WP 10-10721
Many wood species are degraded rapidly in soil by the fungal community. In order to preserve wood and structures in which it is used, chemical preservatives are used. Little is known about the interaction of treated wood and the surrounding soil fungal community. For this work, presented at IRG 41, wooden specimens (Pinus sylvestris sapwood, sizes 25 mm x 50 mm x 500 mm (longitudinal)) were treate...
M Noll, I Stephan


Chemical mediated depolymerization of cotton cellulose for the understanding of non-enzymatic fungal decay
2010 - IRG/WP 10-10731
Small, low molecular weight non-enzymatic compounds have been linked to the early stages of brown rot decay as the enzymes involved with holocellulose degradation are found to be too large to penetrate the S3 layer of intact wood cells. The most pronounced of these which were analyzed in this study are hydrogen peroxide, iron, and oxalic. The compounds related to the Fenton reaction: the combinati...
A C Steenkjær Hastrup, B Jensen, F Green III


Glued laminated poles - Progress report after 30 years testing
2010 - IRG/WP 10-20427
In 1979 a number of glued laminated poles treated with CCA and creosote were placed in a greenhouse at Uppsala, at the Simlångsdalen test field in southern Sweden and in a power lane in Vuollerim in northern Sweden in order to study their resistance against biological degradation. The tests have shown that the best performance will be obtained if each lamination is treated with a water-borne pre...
Ö Bergman, J Jermer


The Relative Performance of an Organic Preservative System under UC3A and UC3B Conditions using Two Test Methods
2010 - IRG/WP 10-20429
Coated L-joints have been used for decades to evaluate the performance of wood preservatives in protected environments. This study was conducted using matched coated and uncoated L-joints to simulate above ground protected and unprotect exposures. When exposed to constant moisture in a greenhouse environment, coated and uncoated L-joints give very similar performance results. In contrast, exposi...
C F Schauwecker, A Zahora, A F Preston


Determination of a fixation time of wood preservatives: A discussion paper
2010 - IRG/WP 10-20436
The intention of that paper is to initiate a discussion on the basis of a French method in combination with a German approach regarding the need of a method for the determination of a fixation time and especially to obtain input as well as ideas concerning a possible test design. Since no harmonised European approach exists up to now concerning the determination of a fixation time, CEN TC 38 (2009...
E Raphalen, E Melcher


Service life prediction of wooden components – Part 1: Determination of dose-response functions for above ground decay
2010 - IRG/WP 10-20439
Scots pine sapwood (Pinus sylvestris L.) and Douglas fir heartwood (Pseudotsuga menziesii Franco) specimens were exposed in double layer field trials at 24 different European test sites under different exposure conditions (in total 28 test sets). The material climate in terms of wood moisture content (MC) and wood temperature was automatically recorded over a period of up to eight years and compar...
C Brischke, A O Rapp


Impact of climate change on wood deterioration - Challenges and solutions for cultural heritage
2010 - IRG/WP 10-20441
Deterioration of wood in cultural assets follows the same physiological mechanisms as in modern structures. Therefore rules and data for prediction of service life derived from old wooden structures can be used to model the service life of recent wooden structures and vice versa. The latter is done in this paper: From experimental test set ups in the field spread over Europe, climatic data, wood t...
C Brischke, A O Rapp, M Hasan, R Despot


Previous Page | Next Page