Laboratory and field evaluation of Plasmite Reticulation System using bifenthrin as a chemical barrier within wall cavities against subterranean termites.
2005 - IRG/WP 05-20307
Laboratory and field bioassays undertaken to demonstrate Plasmite Reticulation system effectively delivers the termiticide (bifenthrin) within a simulated wall cavity at the required concentration. The chemical assay indicated that the amount of bifenthrin sampled at 5, 10, 15, 20, and 25m along the simulated reticulation system tested (30m) exceeded the manufacturer’s minimum recommendation of ...
J R J French, B M Ahmed, J Thorpe, A Anderson


Involvement of hydrogen peroxide in wood decay by brown-rot and white-rot fungi
1985 - IRG/WP 1256
To gain further understanding of the role of H2O2 in wood degradation by brown- and white-rot fungi, we studied the following: (a) extracellular H2O2 production, (b) effect of various hydroxyl radical (·OH) and singlet O2 (1O2) quenching agents on wood and cellulose degradation, (c) intracellular H2O2 production and catalase activity, and (d) cytochemical localization of H2O2 with diaminobenzidin...
T L Highley, L L Murmanis


Effect of felling time related to lunar calendar on the durability of wood and bamboo -Fungal degradation during above ground exposure test for 2 years- (Preliminary report)
2005 - IRG/WP 05-20311
Current study was carried out to know whether the felling time of trees and bamboos based on lunar calendar affects natural durability of felled wood-bamboo or not. Each of one sugi (Cryptomeria japonica) tree of 28 years old and one Moso bamboo (Phyllostachys heterocycla) of around 3 years old was cut 12 times between February and December in 2003. Six sets of sugi tree and bamboo were felled in ...
K Yamamoto, S Uesugi, K Kawakami


TBTO absorption and penetration in pine joinery treated by various processes
1989 - IRG/WP 3523
Matched sections of several White pine (Pinus strobus) and Ponderosa pine (Pinus ponderosa) mouldings were treated with TBTO by Double vacuum, modified empty-cell, 15 second dip and several preheating treatments followed by a 15 s dip treatments. As expected the double vacuum and empty-cell (batch) treatments resulted in much greater retentions and penetrations than the dip treatments. The absorpt...
P A Cooper, Y T Ung


The preliminary characterization of ß-1,4-xylanase of the brown-rot fungus Gloeophyllum trabeum
1990 - IRG/WP 1447
The extracellular ß-1,4-xylanase of the brown-rot fungus, Gloeophyllum trabeum, was isolated from crude extract by chromatofocusing method (PBE 94 column chromatography). The isoelectric point was estimated to 4.2-4.8 by cromatofocusing and 4.5 by isoelectric focusing (IEF). The molecular weight of the enzyme was estimated to 37,000 dalton by SDS-PAGE. The optimal temperature for the crude extrac...
A-C Ritschkoff, M Rättö, L Viikari


Wood degradation mechanisms by the brown rot fungus Gloeophyllum trabeum
1997 - IRG/WP 97-10229
A mechanism for the degradation of wood by the brown rot fungus Gloeophyllum trabeum is outlined. The mechanism includes the function of redox-cycling, low molecular weight phenolic derivatives which sequester and reduce iron in acidic environments. The role of oxalate for the sequestration of iron (hydr)oxides and the pH dependent transfer of iron to the G. trabeum phenolic chelators, as well as ...
B Goodell, J Jellison


Stability and performance of tributyltin compounds
1984 - IRG/WP 3275
Based on the critical examinations of the disputable permanence of tributyltin compounds in wood, this paper deals with a number of examinations of the relative evaporation, thermal stability and oxidation stability of some TBT-compounds. While thermal and oxidative stability is high for all TBT-species, the relative evaporation at elevated temperature is highly variable, and lowest for the TBT-es...
F Imsgard, B Jensen, H A B Landsiedel, H Plum


Analysis of degradation observed on ancient wooden objects buried underground
2001 - IRG/WP 01-10403
Ancient wooden objects were sometimes excavated from the moat of mounded tombs in Japan. Such wooden objects were in the shape of a sunshade, bird, shield, pole, yugi(a bag that holds arrows) among others. Archaeologists discussed the usage of such shaped objects, but no one could clearly explain their use. Some objects were observed using an ordinary microscope. Deterioration by bacteria was foun...
H Sakai


Leaching of copper, chromium and arsenic from CCA-treated slash pine heartwood
1994 - IRG/WP 94-50020
Drying green slash pine with any of three high temperature drying schedules produced a product in which both the sapwood and the heartwood could be penetrated with CCA using a modified Bethell treatment schedule. Required H3 retentions were achieved in both sapwood and heartwood, from 200 litres per m³ charge uptake. Post-treatment fixation/drying was accomplished by three different regimes, incl...
M J Kennedy, G Palmer


Evaluation of New Zealand staining fungi for degradation of radiata pine
1999 - IRG/WP 99-10310
This investigation sought to determine the potential of selected NZ staining fungi to induce weight loss and changes in toughness (impact bending strength) and composition in unseasoned radiata pine sapwood. Furthermore, assays were performed to eveluate enzyme production by staining fungi. Sets of side-matched specimens were inoculated with Ophiostoma floccosum, Sphaeropsis sapinea and O. plurian...
A Schirp, R L Farrell, B Kreber


Immunogold localisation of catalytic domain of endocellulase in the cellulosic substrates
1997 - IRG/WP 97-10205
The reaction of catalytic domain of endocellulase on the cellulosic substrates was visualised by using immunogold labelling procedures to obtain a better understanding of the mechanism of enzymatic cellulose hydrolysis. Polyclonal antibody was produced against the catalytic domain of endo-l, 4-ß-glucanase (EGI) from a ruminal anaerobic bacterium Ruminococcus albus F-40. Immuno-TEM works showed th...
Yoon Soo Kim, Seung-Gon Wi, Kyu Ho Myung, K Ohmiya, S Karita


Alternative technologies for wood wastes recycling - Part B: Biotreatment of PCP- and creosote-treated wood
1998 - IRG/WP 98-50101-18 b
Alternative technologies have been investigated to detoxify treated wood. Two classes of organic compounds are studied. Creosote-treated wood are classified in France as dangerous wood wastes. A conventional incineration could be provided for these wood wastes but the cost of this elimination could be very high (> 2000 FFR/ton). For these reasons, we have tested two kinds of new processes as al...
S Legay, P Marchal, G Labat


Photo-discoloration and Degradation of Wood and its Stabilisation by Modification with Benzoyl Chloride
2004 - IRG/WP 04-40274
Photo degradation of Pinus roxburghii (chir pine) and Hevea brasiliensis (rubber wood) was studied under artificial accelerated weathering conditions in a Xenon test chamber. The irradiated samples were analyzed for color changes and chemical changes. Analysis of colour changes in wood surfaces by UV-Vis. irradiation was carried out using a colour measuring (CIELAB) system and chemical changes ...
K K Pandey


Kinetic of the wood degradation produced by wood decay fung
1993 - IRG/WP 93-20016
The degradation degree of a wooden structure has a direct influence on its loss of mechanical strength. It's necessary to deepen in non destructive techniques which permit to extrapolate the results obtained in laboratory to structural timber used in the building's construction. This work studies the relationship existing between the pulse velocity of ultrasonic waves and the wei...
M T De Troya, A M Navarrete, A Sanchez, V Bucur


Study of the degradation of retified wood through ultrasonic and gravimetric techniques
1994 - IRG/WP 94-40030
One of the non-polluting processes that increase the natural durability of wood is a thermal treatment in an atmosphere poor in oxygen, producing what is normally denominated "retified wood". In this study the validity of a non-destructive technique (ultrasound) in order to determine the biodegradation suffered by wood across time has been studied. For this reason, the behavior of a wood species (...
D T De Troya, A M Navarrete


Identification of terminal structures in cellulose degraded by the brown-rot fungus Postia placenta
1989 - IRG/WP 1389
To gain insight into the biochemical mechanism employed by brown-rot fungi to depolymerize cellulose, we identified the end-groups of chemically pure cellulose that had been depolymerized by the brown-rot fungus, Postia placenta. The depolymerized cellulose was acid hydrolyzed and the anion fractions isolated by ion chromatography. Sugar acids were identified by gas chromatographic and mass spectr...
T K Kirk, T L Highley, R E Ibach, M D Mozuch


Preservation of two Indonesian timber species for marine environment purposes
1994 - IRG/WP 94-10079
This paper deal with the experiment of CCA full cell processed two non-durable Indonesian species for placed in the marine environment. 80 samples of 5 x 5 x 60 cm³ dried durian (Durio zibethinus) and mahogany (Swietenia mahagony) timber were CCA-full cell processed using 4 combination treatment of: without steaming; one hour steaming; 3% and 5% CCA solution concentration. 40 samples of them were...
P Permadi, I M Padlinurjaji, F Rasmita


Wood protection processes in the Asean countries
1994 - IRG/WP 94-40034
This paper presents the wood processing practices in the Asean countries composing Indonesia, Malaysia, Philippines, Singapore, and Thailand except Brunei. The development of wood preservation industry in these countries started as early as 1922 to 1960. As in other industrial countries, treatment pressure with creosote of utility poles, railway sleepers, and marine pilings are the prime commoditi...
F R Siriban


UV-microspectrophotometry of lignin and accessory compounds in wood cell walls of conifers
1999 - IRG/WP 99-20171
The distribution of lignin in the cell wall of conifer tracheids was determined by UV-VIS microspectro-photometer. Wood sections of one micron thickness were measured between the wavelength 240 and 700 nm. Spectral analyses revealed that the conifer lignin associated with the tracheid secondary wall and middle lamella is composed of guiacylpropane units which exhibit a characteristic UV absorption...
G Kleist, G Koch, J Bauch


Changed permeability and surface properties of hornbeam wood due to its degradation by erosive strain of Phanerochaete chrysosporium
2004 - IRG/WP 04-40290
Specimens of hornbeam wood were submitted to a medium-term degradations by erosive fungus Phanerochaete chrysosporium. Biodegradations of specimens resulted in their apparent structural alterations, changes in permeability and increased intensity of interactions with polar liquids. Modified physical properties of biodegraded wood may significantly influence its penetration with polar media and che...
R Solár, S Kurjatko, L Reinprecht, M Mamon, V Vacek


Enzyme systems of bacterial isolates from ponded logs - Potentials of pectin and/or starch degradation
2000 - IRG/WP 00-10378
This paper deals with the degradation potentials of wood constituents by the bacterial isolates from ponded logs. The potentials to degrade pectin as a constituent of pit-tori as well as starch existing in ray parenchyma cells in the areas of sap- and transition wood with the isolates were examined. The pectinase activity was investigated by means of the degradation degree of a carrot strip used a...
S Doi, S Ohta


Moisture uptake and volumetric swelling as probable factors also affecting leaching in CCA-treated wood. A preliminary study of treated Eucalyptus saligna sapwood
2003 - IRG/WP 03-30318 IRG/WP 03-30318
A number of factors affecting leaching of CCA from treated wood have been variously investigated and discussed. However, the possible effects of moisture movement in treated timbers on leaching have not received attention yet. The present study examines and compares moisture uptake and volumetric swelling in CCA-treated and untreated sapwood of Eucalyptus saligna, and tries to establish a correl...
R Venkatasamy


The effect of hemicellulose degradation on the mechanical properties of wood during brown rot decay
2001 - IRG/WP 01-20219
Incipient decay of wood by brown rot fungi causes measurable strength losses in wood before measurable weight loss occurs. Previous studies have shown that the high levels of strength loss that occur during incipient brown rot decay may be related to loss in hemicellulose. This paper investigates the effect of decay on hemicellulose composition and the relationship to the mechanical properties of ...
S F Curling, C A Clausen, J E Winandy


Chemical and biological studies of organotin treated and painted wood stakes after outdoor exposure
1987 - IRG/WP 3419
Organotin based wood preservatives containing tributyltin oxide (TBTO) or tributyltin naphthenate (TBTN) are used in Sweden mainly for double-vacuum treatments of window joinery of Pinus sylvestris. After impregnation the joinery is painted or stained in different colours. To evaluate this effect (different colours on the degree of degradation of TBTO and TBTN, effected by different temperatures i...
M-L Edlund, B Henningsson


Moisture requirements and wood degradation of pine and spruce wood by some Basidiomycetes-fungi
1989 - IRG/WP 1406
The minimum moisture requirements for the growth of the brown rot fungi, Coniophora puteana, Gloeophyllum trabeum and Serpula lacrymans were near or above the fibre saturation point of pine and spruce, sap and heartwood, during 160 days incubation according to the standard method EN 113. The moisture of wood for the optimum growth of Coniophora puteana and Serpula lacrymans was about 35-80% and fo...