IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3367 documents. Displaying 25 entries per page.


Treatability and natural durability of some lesser used or unused wood species of Bangladesh
2000 - IRG/WP 00-40170
A research study was conducted to determine the natural durability and treatability of heartwood of some lesser used or unused wood species. The treatability of species has been studied along with certain anatomical concepts association with preservative penetrability of the wood. It was observed that grain structure and presence of tyloses appeared to be correlated with penetrability of the wood....
K Akhter, M Younusuzzaman, M H Chowdhury


The Efficacy of Wood Preservative Treatments in Laboratory Soil-Bed Test
2004 - IRG/WP 04-20289
The efficacy of wood preservatives were determined in laboratory soil-bed test. Pine and alder wood samples (10 x 10 x 10 mm) were treated with CCA (1, 2%), ACQ-1900 (2, 3%), ACQ-2200 (1, 2%), Tanalith E 3491 (2, 2,8%), Wolmanit CX-8 (1, 2%). The leached and unleached samples were exposed 76 days at Simlångsdalen soil and determined mass loss. The results of this study showed that mass losses o...
A Temiz, T Nilsson, Ü C Yildiz, E D Gezer, S Yildiz


A novel guide for the determination of the physical properties of wood including kiln drying and full-cell preservative treatment
2004 - IRG/WP 04-20298
An ideal flow chart for the sequential experimental determination of a range of physical properties relevant to wood drying and subsequent preservation was designed as a novel guide to assist wood scientists. In this manner, data assembly and experimental processing are shown. This was designed according to experience and published literature. Aspects emphasised in this review were the physical p...
I Usta, M D C Hale


Kinetics and mechanism of fixation of Cu-Cr-As wood preservatives. Part 5: Effect of wood species and preservative composition on the leaching during storage
1975 - IRG/WP 354
Conversion reactions during storage of CCA treated wood take place even at and below the fiber saturation point as long as ion transport is possible. Increase in drying temperature increases the final pH of the treated wood and the leachability of Cu and decreases slightly the leachability of Cr, while the leachability of As is not affected. This temperature effect is considered to be of no techni...
S-E Dahlgren


Application of energy dispersive X-ray fluorescence spectrometry to the quantitative analysis of organotin preservative solutions and treated wood
1978 - IRG/WP 3125
One technique frequently used for the quantitative analysis of material containing inorganic compounds is energy dispersive X-ray fluorescence spectrometry. It has been shown previously that this technique can be readily used to determine the retentions of chromated copper arsenate and ammoniacal copper arsenate treated wood. This paper reports the results of a preliminary study to determine wheth...
J N R Ruddick


Characterization of checks and cracks on the surface of weathered wood
2000 - IRG/WP 00-40153
The surface roughness of unweathered and untreated pine; unweathered copper chromium arsenate type C (CCA) - treated pine; weathered CCA-treated pine; and weathered CCA-plus-water-repellent (WR) - treated pine was evaluated by a stylus tracing method. Surface roughness parameters Ra, Rz, Rmax, Rk, Rpk, and Rvk were measured. Ra, Rpk, and Rvk were the most appropriate parameters for describing modi...
D P Kamdem, Jun Zhang


Preservative treatment of Golpata (Nypa fruticans) using CCA (Chromated Copper Boric Acid)
1999 - IRG/WP 99-40131
Golpata (Nypa fruticans) leaves provide a cheap but practical source of roof thatches. This study was carried out to determine whether the life span of Golpata could be extended by using CCB (Chromated Copper Boric Acid) treatment. Both leaves and midribs of Golpata , with different moisture contents ranging 16.63% to 70.67%, at the start of the experiment were treated with four different concentr...
G N M Ilias, F Abdullah, M O Hannan, S M Feroz


New conception for shortering the duration of fungitoxic test of wood preservatives. Part 2: Computer-assisted miniaturisation of wood specimens
1994 - IRG/WP 94-20052
The mass loss of wood used as a criterion in the standarised agar-block method of evaluation of toxic value of preservatives depends upon the relationship between volume of specimens, their outspread planes and ratio of areas of particular anatomic sections. Upon the computer-assisted mathematical basis the dimensions of miniaturized specimens which make 1/2, 1/4, and 1/8 part of standarized ones ...
J Wazny, K J Krajewski


Future Directions Regarding Research on the Environmental Impacts of Preservative-Treated Wood: Environmental Impacts of Preservative-Treated Wood. February 8-11, 2004, FL, USA Workshop – Research Needs
2004 - IRG/WP 04-50222
This paper presents a series of documents that focus on research needs for potential future work focusing on the environmental impacts of preservative-treated wood. These documents were developed through a conference sponsored by the Florida Center for Environmental Solutions (FCES), located in Gainesville, Florida. The conference was held in Orlando, Florida, February 8 – 11, 2004 and the tit...
H M Solo-Gabriele, J D Schert, T G Townsend


On the occurrence of Phialophora species in preservative treated wood in ground contact
1977 - IRG/WP 163
Phialophora is a fairly large genus comprising about thirty described species. They are widespread in very diverse environments, such as soil, sea water, wood and wood pulps. Some species are known as parasites on plants and animals, including man. Phialophora species were early known for their ability to produce blue stain in timber. Later it was discovered that several species were able to produ...
T Nilsson, B Henningsson


Screening techniques for potential wood preservative chemicals. Proceedings of a special seminar held in association with the 10th Annual Meeting of the IRG, Peebles 1978. Report No 136, 1979
1980 - IRG/WP 2138
This paper continues following issues: I. SCREENING INSECTICIDES 1) R W Berry (BRE/PRL, UK): Screen testing of insecticides for use in remedial wood preservatives. 2) D J Cross (FRI, New Zealand): Rapid screening of contact insecticides for use on forest products. 3) C R Coggins; A Forsyth; A E Glaser (Rentokil, UK): Experience in the use of indicative screening techniques for termiticides. ...
Anonymous


Effect of test site, preservative and wood species on decay type Glenbervie pastoral and radiata pine forest sites
2000 - IRG/WP 00-30248
Pinus radiata stakes were treated with 0.8, 1.2, 1.8, 2.7 and 4.1 kg/m3 of CCA and Fagus sylvatica with 2.7, 4.1 and 6.1 kg/m3 of CCA. Both wood species were also treated with equivalent retentions of a copper plus triazole preservative (CT) (0.89, 1.3, 2 and 3 kg/m3 of copper for pine & 2.5 and 4 for beech) and chlorothalonil plus chlorpyriphos in oil (CC) (1.4, 2.1, 3.2 and 4.8 kg/m3 of chlo...
R N Wakeling


Water-Borne Copper Naphthenate: An Emerging Wood Preservative
2002 - IRG/WP 02-30280
Waterborne copper naphthenate (WB Cu-N) was used to treat southern yellow pine (Pinus spp) and red maple (Acer rubrum) stakes. The treated stakes were exposed in test sites located in Florida, Michigan and Mississippi for 3 to 6 years. Copper Chromium Arsenate (CCA), Ammoniacal Copper Quat (ACQ) and Oil-borne Copper Naphthenate (OB Cu-N) were also used to treat some stakes for comparison. Results...
P Nzokou, D P Kamdem, M H Freeman


Preservative treatment of two bamboo species Borak (Bambusa balcooa Roxb) and Talla (Bambusa tulda Roxb) by Boucherie method
2003 - IRG/WP 03-40262
Bamboo is widely used as a construction material in rural and urban areas of Bangladesh. It is perishable in nature and highly susceptible to the attack of borer, termites and fungi. As a result, bamboo products do not last long. This short life of bamboo is increasing demand thereby increasing pressure on our homestead and natural reserve of bamboo. For this reason, it is needed to make the bambo...
M N Islam, A S M A Huda, A K Saha, S M Mithue


Determination of N-cyclohexyl-diazeniumdioxide (HDO) containing compounds in treated wood using GC-MS
2000 - IRG/WP 00-20201
Beside the biological effectiveness the approval of a chemical wood preservative requires also techniques for the analytical determination of active ingredients in different matrices. Fulfilling of the last requirement is particularly difficult in the case of impregnated timber treated with wood preservatives containing organic compounds. This paper describes a procedure for the determination of t...
P Jüngel, J Wittenzellner, E Melcher


The use of preservative containing waste wood as substrate for growing greenhouse crops
1993 - IRG/WP 93-50011
In the Netherlands a large amount of waste wood and wood waste is produced every year. An important part of this amount comes from the pallet and packaging industries. One of the possibilities to re-use this relatively clean material is to convert it into substrates for growing crops in glass houses instead of the commonly used materials such as rock wool and glass wool. In this research, the infl...
W J Homan,H Militz


Status of wood preservation industry in India
2005 - IRG/WP 05-30388
The paper traces the history of wood preservation industry in India, listing various mile stones for creation of treating capacity. The preservation industry developed with the development of rail road system on the line of most other developed countries. The most popular wood preservatives are CCA, CCB, ACC, Creosote and recently LOSP have also appeared in the market. The major users of CCA is th...
S Kumar


Fundamentals on steam fixation of chromated wood preservatives
1988 - IRG/WP 3483
Weathering of treated wood directly after impregnation leaches up to 2% of copper-chromate-containing wood preservatives. Almost total fixation of Cr+6 is achieved by steaming the treated wood at 100°C to 120°C, preferably 110°C. To initiate such spontaneous fixation 85°C to 90°C inside the wood are essential, which requires heating times ranging from 20 to 80 min, depending on timber species...
R-D Peek, H Willeitner


Need to develop processing technologies (for value addition) of the species evaluated for their properties and uses
2005 - IRG/WP 05-40307
The demand of timber in India for different industrial as well as domestic applications is ever increasing mostly due to urbanization and industrialization. This demand can only be met either from the imported timber or from the plantation resources outside the reserved and natural forests. There are a number of timber species grown under plantation forestry have their heartwood refractory to any ...
S R Shukla, S K Sharma, Y M Dubey, P Kumar, R V Rao, K S Shashidhar


Performance of preservative-treated wood not in ground contact
1975 - IRG/WP 254
Experimental sash units of Pinus strobus L. and Pinus resinosa Ait. wood were removed from a test fence at Ottawa, Canada after outdoor exposure of over 20 years. The units were superficially treated, prior to painting, with preservatives containing either copper naphthenate, pentachlorophenol or a combination of zinc naphthenate and pentachlorophenol. Results indicated that all treatments were ef...
J K Shields, J Krzyzewski


Influence of acidification on decay processes of CCB treated wood
2004 - IRG/WP 04-10514
The phenomenon of copper tolerance by brown rot fungal strains has been known for a long period but the complete mechanism of copper tolerance by these fungi is not understood yet. Copper tolerance has previously been linked to oxalic acid excreted by copper tolerant brown rot fungal strains. This acid reacts with copper in the wood to form an insoluble and therefore less toxic copper oxalate. The...
M Humar, S A Amartey, M Šentjurc, F Pohleven


The remaining concentration of inorganic wood preservative components in EN 252 stakes after ground contact
2000 - IRG/WP 00-50159
In order to determine the biological efficiency and the remaining concentration of different inorganic and organic active ingredients during service, EN 252 specimens were impregnated with 3 copper based wood preservatives. The stakes were installed in the test field of the DESOWAG GmbH, Rheinberg, for at least 7 years. At the end of the field test some of these stakes were divided into 10 uniform...
E Melcher, H-W Wegen


A bioassay for appraising preservative protection of wood above ground
1978 - IRG/WP 2124
A bioassay, using the mold fungus Aspergillus niger, gave results that were correlated with amounts of pentachlorophenol and tributyltin oxide in pine sapwood treated with solutions ranging in strength from 0.016 or below to 5%. Limited bioassay estimates of penta in commercially treated millwork corresponded to estimates by lime ignition. The assay fungus exhibited somewhat greater tolerance of t...
T C Scheffer, L Gollob


Preservative treatment of wood by diffusion processes - Simulation of commercial treatment processes
1988 - IRG/WP 3498
Spruce (Picea abies), Scots pine (Pinus sylvestris) and birch (Betula pendula) were preservative treated by diffusion with mixtures of copper sulphate and arsenic pentoxide. The preservative was fixed after a suitable diffusion storage period by soaking in ammonia solution. A high standard of treatment could be achieved in spruce sapwood. This was attributed to its low wood density, and high wood ...
P Vinden


Persistance of active ingredients in treated wood
1993 - IRG/WP 93-50001-20
Disposing of chemically protected waste wood implies the distinction between surface and pressure treatment. Considering that barked round-wood merely contains, after 7 months open storage, less than 30 g per ton of bark or 25 mg per ton of sapwood, depending on the type of insecticide, the bark or sapwood shavings may be incinerated normally, according to less severe legal prescriptions than for ...
E Graf, P Manser, S Rezzonico, B Zgraggen


Previous Page | Next Page