Insects in dry wood (other than termites)
1977 - IRG/WP 153
S Cymorek


Copper naphthenate performance: A new way to look at old data
2000 - IRG/WP 00-30215
Although copper naphthenate has over a 50-year test history, it is still considered as a "new" preservative in the United States when it is used for utility poles. It has also been extensively used in remedial treatments for poles and has considerable retail or over-the-counter sales. The test history includes a number of different tests and a rationale for evaluating this data and comparing the p...
C R McIntyre


Wood furfurylation process and properties of furfurylated wood
2004 - IRG/WP 04-40289
The first processes for “furfurylation” of wood (wood modification with furfuryl alcohol) were developed several decades ago. Furfuryl alcohol is a renewable chemical since it is derived from furfural, which is produced from hydrolysed biomass waste. Over the last decade modernised processes for furfurylation of wood have been developed. These new processes are based on new catalytic systems a...
M Westin, S Lande, M Schneider


The biostatic effect of copper on decay of fire retardant-treated mining timber
1991 - IRG/WP 1507
Blocks of Eucalyptus grandis were treated with 20kg/m³ ammonium sulphate as fire retardant and challenged with Coriolus versicolor. Replicates were soil buried. A second set of blocks was treated with retardant and copper at 6.6 kg/m³ (ie 1% w/w), and challenged similarly. After 8 weeks weight losses produced by Coriolus versicolor in untreated, retardant treated and copper supplemented blocks w...
G D Shelver, E A Shelver, A A W Baecker


The Seventh Annual Report of the International Research Group on Wood Preservation 1975-1976
1976 - IRG/WP 551
IRG Secretariat


Programme section 3, Wood protecting chemicals
1997 - IRG/WP 97-30159
IRG Secretariat


Effect of medium-term degradation of beech wood by erosive (Phanerochaete chrysosporium) and lignin-selective (Ceriporiopsis subvermispora) strains of white rot fungi on its selected physical properties
2004 - IRG/WP 04-40292
At the Faculty of Wood Sciences and Technology a fungal delignification of normal and tension beech wood by erosive and lignin-selective strains white-rot fungi has been studied. The pre-treatment of both kind of wood samples was accompanied by partial delignification and apparent changes of their physical properties influencing the polar liquids penetration....
R Solár, S Kurjatko, M Mamonová, J Hudec


Protocol for evaluation and approving new wood preservative
1985 - IRG/WP 2159
M E Hedley, J A Butcher


CCA modifications and their effect on soft rot in hardwoods
1982 - IRG/WP 3201
Decay tests were carried out on wood samples treated with three waterborne compounds all identical in composition but applied in different forms. There were significant differences in the effectiveness of the treatments particularly as regards the control of soft rot....
S M Gray, D J Dickinson


Aspects of the biology of the wood-boring weevil Pselactus spadix herbst
1997 - IRG/WP 97-10221
The external morphology of the adult and larval digestive tract of the wood boring weevil Pselactus spadix has been reported for the first time. An examination of adult gut ultrastructure showed that the foregut was adapted for the wood boring habit with the presence of chitinous setae, grinding plates and sieve plates. The adult midgut bore eight caecae and numerous palpii. Spherical yeast-like m...
G Cooper, A J Pitman, G S Sawyer


Respiration methods used to follow the decay of wood and the toximetric evaluation of wood preservatives
1975 - IRG/WP 249
When wood is attacked and decayed by fungi, wood substance and oxygen (02) are consumed, while carbon dioxide (CO2), water and heat are liberated. Early in the 1960's workers from England, Canada and Sweden began studying CO2 evolution, with respect to decay and its control using chemical preservatives, while in Germany and the USA O2 utilization was being similarly examined. Oxygen consu...
R S Smith


Durability of pine modified by 9 different methods
2004 - IRG/WP 04-40288
The decay resistance was studied for pine modified by nine methods of wood modification: 1) Acetylation, 2) Treatment with methylated melamine resin (MMF), 3) Acetylation followed by post-treatment with MMF-resin, 4) Thermal modification, 5) Furfurylation, 6) Maleoylation (using water solution of MG or ethanol solution of maleic anhydride), 7) Succinylation, 8) NMA-modification and 9) modification...
M Westin, A O Rapp, T Nilsson


Biological control with Trichoderma harzianum in relation to the formation for spores the production of soluble metabolites
1994 - IRG/WP 94-10073
The amount of spores produced by three strains of Trichoderma harzianum on the aerial mycelium of agar cultures and in shake cultures, respectively, correlated with the inhibition zones exerted against Phanerochaete chrysosporium in an agar diffusion test. The amount of soluble antifungal metabolites as well as the protein content also correlated with the inhibition zones and the amount of spores ...
J Bürgel, E Horvath, J Haschka, K Messner


The proposal for the method of testing the phytotoxic effect of wood preservatives
2000 - IRG/WP 00-50163
Four methods of testing the phytotoxic effect of wood preservatives are proposed as the unified test by: - direct application of the preservatives to the test plants by spraying; - direct application of the preservative to the soil substrate; - indication plants growing in the vicinity of treated wood; - seed germination rate on the treated substrate....
J Wazny, P Witomski


A case study on quality control on telephone poles as a cost saving tool in Tanzania
1987 - IRG/WP 3418
A sample of 28 CCA treated Eucalyptus poles from a lot of 2,000 poles awaiting delivery to the field, was studied to reveal the quality of treatment. Results showed a product of very poor quality. Average figures for penetration and retention were 8.4 mm and 2.2 kg/m³; these results are 66% and 91% below the required standards, respectively. Consequences of such results are estimated to amount to...
K K Murira


Chemical compounds from Eperua falcata and Eperua grandiflora heartwood and their biological activities against wood destroying fungus (Coriolus versicolor)
2005 - IRG/WP 05-30373
The chemistry analysis of the compounds present in dichloromethane and ethanolic fraction as well as bioassays enables to understand the durability differences of Eperua falcata and Eperua grandiflora. The principal distinction between these two species is the acidic subfraction of diterpenoic extract, which is antifungic in Eperua falcata when tested in in-vitro conditions. This study also enable...
N Amusant, C Moretti, B Richard, E Prost, J M Nuzillard, M-F Thévenon


Valid names for some common decay fungi, their synonyms and vernacular names
1978 - IRG/WP 172
A Käärik


A method of isolating actinomycetes from decayed wood
1974 - IRG/WP 126
This paper deals with a tentative method of isolating Actinomycetes from dacayed wood....
T Haraguchi


Abstracts of papers prepared for the Symposium “Environment and wood preservation”
2001 - IRG/WP 01-60135
IRG Secretariat


The long-term performance of boron treated joinery in service - A case study
2000 - IRG/WP 00-20208
Joinery treated with borates 23 years ago and in service in residential flats was surveyed and analysed for boron content. The levels of boron still present were sufficient to prevent decay. None of the windows surveyed showed any decay despite the fact that moisture and sapwood contents were conducive to decay....
D J Dickinson, R J Murphy


European standardization for wood preservation
1988 - IRG/WP 2321
G Castan


Depletion of boron and copper from CCB treated test specimens using different leaching protocols
2004 - IRG/WP 04-50208
The objective of this study was to measure the depletion of inorganic wood preservative components regarding the proposed OECD guideline "Estimation of emissions from preservative-treated wood to the environment: laboratory method for wooden commodities exposed in the use class 4 and 5" as part of the project "Investigations concerning the influence of test parameters on the release of biocidal ac...
E Melcher, R-D Peek, U Schoknecht, R Wegner


Influence of aliphatic acids on spore germination of wood decay fungi
1984 - IRG/WP 2224
Influences of eight saturated fatty acids (C5-C10, C12 and C16) on spores of four isolates of wood decaying basidiomycetes (white rot fungi: Poria tenuis and Trametes hispida; brown rot fungus: Gloeophyllum trabeum [two isolates]) were observed in-vitro. Spore response after 24 hr on malt extract agar containing 10, 10² , or 10³ ppm of each fatty acid included: no effect on normal germination, d...
E L Schmidt


Results of stake tests on wood preservatives (Progress report to 1974)
1975 - IRG/WP 361
A number of field stake trials on preservative-treated wood have been carried out at Princes Risborough Laboratory from 1928 to the present day, and many of the tests still continue. This paper presents in detail the results obtained to date, covering about 15 000 individual test stakes exposed over the period....
D F Purslow


Circular letter to all members of WG IV Marine Wood Preservation
1985 - IRG/WP 4122
IRG Secretariat


Previous Page | Next Page