Improvements of monitoring the effects of soil organisms on wood in fungal cellar tests
1996 - IRG/WP 96-20093
Accelerated testing the durability of preservative treated timber in a so called "fungal cellar" or "soil-bed" to evaluate its performance in ground contact is widespread practice. In order to obtain a more accurate and reproducible estimate of preservative performance, several institutes, among them the BAM in Berlin, have routinely carried out static bending tests in addition to visual examinati...
I Stephan, S Göller, D Rudolph


A suggested method to test the toxicity of wood preservatives towards the house longhorn beetle
1977 - IRG/WP 275
This method was developed in the Institute for Wood Technology in Sarajevo, Yugoslavia and is used to get quick information on the toxicity of wood preservatives against house longhorn beetle (Hylotrupes bajulus). The method can be used for superficially treated or deeply impregnated wood blocks, and by using small or normal size test material it can be used as a laboratory or field test, and also...
N Vidovic


Aspects of diffusion of boron through wood
1984 - IRG/WP 3298
Boron compounds have been shown to be toxic to a wide range of wood destroying insects and fungi. They are cheap, have low mammalian toxicity and their application in the treatment of wood does not demand specialized equipment. These attributes make them specially attractive to developing countries. Currently, however, little is known about the mechanism of diffusion of boron through wood. Effecti...
S Iddi


Marine testing of selected waterborne preservatives
1987 - IRG/WP 4137
In 1978 a marine test was established at West Vancouver, B C. to determine the performance of selected waterborne preservatives. The preservatives in test were chromated-copper-arsenate (CCA-C), ammoniacal copper arsenate (ACA), a modified formulation of ACA which contained a higher copper content (modified ACA), ammoniacal copper zinc arsenate (ACZA) and ammoniacal zinc arsenate (AZA). The wood s...
J N R Ruddick


Utilization of curcumin for detection of presence of boron in wood
1982 - IRG/WP 3191
It has been shown that curcumin is not a reliable reagent for detecting boron in wood that has been attacked by fungi...
M-L Edlund


Performance of treated fence posts after 6 years in five test plots in the State of Sao Paulo - Brazil
1976 - IRG/WP 376
Fence posts treated with creosote, pentachlorophenol and creosote/ pentachlorophenol mixtures showed good performance after 6 years of exposure in five test plots located in the State of Sao Paulo - Brazil. Good results were also achieved with copper sulphate/sodium arsenate and copper sulphate/potassium dichromate mixtures. Fungi and termites were the main destroying agents found attacking the po...
M S Cavalcante


Pinus and Eucalyptus fenceposts treated with creosote and solvex tar by hot and cold open-tank process
1987 - IRG/WP 3455
A comparative study of the behaviour of two different wood preservatives, creosote and solvex-tar, was made, using two wood species, Pinus pinaster Ait and Eucalyptus globulus Labill, by the hot and cold open-tank process. Results showed that the creosote behaved better in relation with the uniformity of its distribution in wood. On the other hand, better results were obtained on Pinus for both pr...
M V Baonza Merino


The applicability of life cyle analysis and alternative methods in the wood preservation industry
1994 - IRG/WP 94-50023
In the Netherlands, several case studies have been performed using the life cycle analysis method (LCA). This type of research is aimed at an inventory and classification (sometimes including also evaluation) of the environmental impacts of a product, from the raw material to waste stage ("cradle to grave" approach). In a LCA each environmental impact is assessed in terms of, for example, mass of ...
P Esser, J Cramer


Registration and approval of wood preservatives in Australia and New Zealand
2001 - IRG/WP 01-50166-06
Wood preservatives are treated as agricultural chemicals in Australia and, at the time of writing, as pesticides in New Zealand. Antisapstain products are currently considered to be agricultural chemicals in New Zealand while wood preservatives in the future will be considered as hazardous substances under the Hazardous Substances and New Organisms Act when this Act is fully implemented. They are ...
H Greaves


Inhibition of wood-inhabiting fungi by actinomycetes
1981 - IRG/WP 1137
Actinomycetes of the genera Streptomyces, Micromonospora, Microtetraspora, Nocardia and Rhodococcus, isolated from wood, were laboratory tested for their inhibitory effects against the Basidiomycete fungi Polystictus sanguineus and Sistrotrema brinkmannii. One-third of the representatives of the genus Streptomyces which were tested produced significant inhibitory zones whereas actinomycetes belong...
M S Cavalcante, R A Eaton


Strength loss associated with steam conditioning and boron treatment of radiata pine framing
1987 - IRG/WP 3438
The combined effect of included defects and wood moisture content on the strength loss of second rotation radiata pine framing following conventional steam conditioning is investigated. The green Modulus of Elasticity (MOE) is reduced by approximately 13% after steaming. When dried after steaming, however, neither the MOE nor MOR is significantly different from unsteamed dried controls....
M J Collins, P Vinden


Field performance of wood preservative systems in secondary timber species
1997 - IRG/WP 97-30152
The objective of this ongoing study is to evaluate the performance of new, potential, and standard wood preservative systems in secondary North American timber species. Eleven preservative systems were evaluated in this study - ACQ Type B, Copper Citrate 2: l, CDDC, chlorothalonil/chlorpyrifos, copper-8-quinolinolate, tebuconazole/chlorpyrifos, RH287, propiconazole/chlorpyrifos, copper naphthenate...
P E Laks, K W Gutting, R C De Groot


Blue stain in service on wood surface coatings. Part 3: The nutritional capability of Aureobasidium pullulans compared to other fungi commonly isolated from wood surface coatings
1993 - IRG/WP 93-10035
The nutritional capability of Aureobasidium pullulans was previously examined, using agar plate tests, with regard to nutrient sources that are potentially available in fresh and weathered wood (Sharpe and Dickinson, 1992). This study compared these findings with the nutritional capability of four other fungi (Alternaria sp., Cladosporium cladosporoides, Stemphylium sp. and Trichoderma sp.) common...
P R Sharpe, D J Dickinson


Trend in entomology of wood in use and in storage in Nigeria
1978 - IRG/WP 180
The current and potential impact of biotic agents of wood deterioration in Nigeria is reviewed, with emphasis on the insects and marine borers, their recognition and mode of damage. Some essential areas have no doubt been neglected and these are highlighted, while future lines of approach are outlined....
M O Akanbi


IRG - wood preservation - annual report 1999; wood preservation in Slovak Republic
2000 - IRG/WP 00-40192
This report gives basic information about wood preservation in Slovak Republic, related to the wood preservation research and education, to the most important wood-destroying organisms, to the wood preserving industry, and also to the problems of standards, market and environment....
L Reinprecht


Testing of wood preservatives against marine borers (Part 1). Method of testing wood preservatives against marine borers (Part 2)
1971 - IRG/WP 37
P C Trussell, C C Walden


Comité International Permanent pour la Recherche sur la Préservation des Matériaux en Milieu Marin. Information from the Wood Group
1980 - IRG/WP 460
E G B Jones


Influence of different fixation and ageing procedures on the leaching behaviour of copper from selected wood preservatives in laboratory trials
2003 - IRG/WP 03-20264
The paper focuses on the role of different parameters, such as fixation, sample size, wood species, and leaching in internationally standardized ageing procedures for wood preservatives from Europe, Japan and the United States. The leaching protocols used were EN 84, JIS K 1571 and AWPA E11 protocols. The wood species were Scots pine, Sugi and Southern Yellow Pine respectively. Three types of com...
J Habicht, D Häntzschel, J Wittenzellner


The evaluation of permethrin for wood preservation
1977 - IRG/WP 3107
The toxicity of the synthetic pyrethroid permethrin (NRDC 143) to a range of wood destroying insects has been investigated. In tests using Hylotrupes bajulus, Anobium punctatum, Lyctus brunneus and Reticulitermes santonensis permethrin showed a similar order of toxicity to that of gamma-BHC. Although the toxicity of permethrin to adult Anobium punctatum was of the same order as that of gamma-BHC, ...
R W Berry


The International Research Group on Wood Preservation. A Short Presentation
1979 - IRG/WP 92
IRG Secretariat


The Seventeenth Report of The International Research Group on Wood Preservation 1987-1988
1988 - IRG/WP 5322
R Cockcroft


New technique to analyze impregnation processes
1988 - IRG/WP 2304
Equipment has been developed to measure liquid flow in wood during impregnation processes. Basic principles of flow measurements using directly heated negative temperature coefficient thermistors, and some characteristics of the hardware developed are presented in this paper....
J P Hösli


Developments in the protection of wood and wood-based products
1980 - IRG/WP 340
Technology is playing an increasingly important role in the field of wood protection. This current review highlights how modern techniques have provided greater insight into the biological and physical processes affecting the durability of wood and wood-based products. Emphasis is also given to developments in preservative testing methodology and to the encouraging changes towards both the correct...
J M Baker


Low temperature drying conditions of Pinus radiata wood for avoiding internal stain
1989 - IRG/WP 3507
It has been observed that, if in little sawmills, timber is dried with a low temperature schedule, it arrives at destination with internal sapstain besides of superficial mould. In this study, the lowest drying temperature at which wood should be exposed for sterilization, which results to be 52°C, is searched. It is not possible to avoid entrainment of pentachlorophenol, even though a waiting pe...
M C Rose


Co-operative studies on determining toxic values against wood-destroying Basidiomycetes: Progress report to May 1989
1989 - IRG/WP 2339
This document reports progress on the co-operative study between nine laboratories set up following the proposals contained in Document IRG/WP/2316. Results have been received from two laboratories. Toxic values data have been established successfully using the test fungus Coniophora puteana but problems have been encountered with the other test fungi....