Co-operative Field Experiment: Performance of preservative-treated timber: Report on condition of specimens after seven years installed in New South Wales - Australia
1986 - IRG/WP 3362
R S Johnstone


Surface coatings for impregnated wood
1992 - IRG/WP 92-3684
The use of proper surface coatings enhances the aesthetic and protective properties of impregnated wood. Good results with especially water-borne coatings have been obtained for class-A impregnated L-joints and claddings in field tests started in 1982....
L Kotama


Termite field test results of preservative treated and modified woods in Kumamoto, Japan
2001 - IRG/WP 01-30275
Various preservative treated or modified wood stakes other than CCA, were buried in the soil, maximum for six years in Kumamoto, south west side of Japan. In this area, two main termite species, Coptotermes formosanus and Reticulitermes speratus, are distributed. After two years in field, untreated sapwood of sugi (Cryptomeria japonica) were observed severe attacks by termites, but the preservativ...
K Suzuki


CCA Chemistry
1983 - IRG/WP 3268
A Pizzi


Biological effectiveness of ground-contact wood preservatives as determined by field exposure stake tests
1984 - IRG/WP 3297
Field exposure tests conducted on stakes treated with different creosotes, mixtures of creosote and waxy oil as well as different CCA wood preservatives over a period of 25 years, gave the following results: The CCA preservatives provided excellent biological protection to treated stakes, especially against fungal attack. The CCA Type I, currently approved for use under South African conditions is...
W E Conradie, A Pizzi


300 years water-logged wood: Treatability with CCA-C
1998 - IRG/WP 98-40103
The treatability of 300 years water-logged and recent wood (Abies bornmülleriana M.) was assessed by dip treatment and vacuum and pressure cycling with CCA-C. Treatment runs were evaluated on the basis of weight gain retention and radial and tangential penetration measurements. The preservative penetration and retention levels in the 300 years water-logged wood were higher than in the recent wood...
S N Kartal, N Yilgör


Measurement of VOC emissions from curative treated wood: A new emission test chamber
2001 - IRG/WP 01-50166-13
A poor indoor air quality (IAQ) is now recognized as a potential factor affecting occupants health. There are three basic strategies to improve IAQ: source control, improvement of the ventilation and use of air cleaners. Usually, the most efficient way to improve IAQ is to eliminate the different pollutant sources or to reduce their emissions. In order to precisely measure emissions from building ...
F Maupetit, O Ramalho, C Yrieix


Health and safety aspects of the use of wood preservatives. Preliminary evaluation of the answers to the IRG-Questionnaire on the state of pollution control in the field of wood preservation
1974 - IRG/WP 56
This preliminary evaluation of the answers to the IRG/WP-Questionnaire only gives a general survey on those questionnaires, which the author received until June 13, 1974. Details, such as correlations between importance of wood preservation and pollution control, could not be considered due to lack of time. For the same reason it was not possible so far, to evaluate the additional remarks given in...
H Willeitner


Some statistics on the Brazilian Wood Preservation Industry: 1980-81
1982 - IRG/WP 3214
Statistical data on the production of pressure treated wood and on the consumption of wood preservatives are given for the years of 1980 and 1981 in Brazil....
M S Cavalcante, F C Geraldo, A R De Freitas


Evaluation and approval of wood preservatives in the Nordic countries
1988 - IRG/WP 2311
This paper reviews the system for evaluating and approving the efficacy of wood preservatives for industrial use currently in force in the Nordic countries Denmark, Finland, Iceland, Norway and Sweden....
B Henningsson, J Jermer


The effective control of moulds on freshly impregnated wood
2004 - IRG/WP 04-30352
Beside natural timber it is known, that moulds can also groth at the surface of impregnated wood. This material shows “defects” like resistant dark spots or color changes and causes complaints. During the last years, the problem by moulds seems to increase. Laboratory studies were carried out to show the effect of impregnations against moulds. Wood samples (Pinus sylvestris L.) were impregn...
G Cofta, K Lutomski, P Jüngel


Soft rot decay of 23 CCA-treated hardwoods from Sabah, Malaysia, in ground contact in Australia
1986 - IRG/WP 1280
The performance against soft rot decay of 23 CCA-treated hardwoods from Sabah, Malaysia, was examined after 20 months in ground contact at Pennant Hills, Australia. The results indicate that between these species soft rot decay is excluded by different levels of CCA salt suggesting that the threshold level for exclusion of soft rot in these hardwoods is a function of anatomical structure/ultrastru...
R S Johnstone


The use, approval and waste management of industrial wood preservatives. A preliminary report
1994 - IRG/WP 94-50033
The structure on the wood preservation through the world is heterogenous. Environmental legislation, approval policy and application practices differ in each geographical region and in individual countries. This preliminary report gives a rough estimation of the production of treated timber, the use of wood preservatives and a bief summary of environmental status of wood impregnation in selected c...
A J Nurmi


Environmental risk assessment of preservative treated wood
1998 - IRG/WP 98-50101-19
This paper reviews the status of the environmental risk assessment of preservative treated wood and confirms the distinction between the risks presented by wood preservatives and preservative treated wood. The paper proposes a tiered approach to risk assessment and discusses the rationale. Flowcharts are presented which summarise the tiered approach to risk assessment, show the tests required, and...
E F Baines, S J Davis


Preservative absorption response of planks of Anogeissus acuminata for plank-built catamarans
2002 - IRG/WP 02-40245
Due to shortage of timber coupled with other compelling factors, traditional fishermen along the east coast of India, especially of Andhra Pradesh, of late, are departing from conventional log type wooden catamarans. Instead, they are fabricating catamarans out of timber planks of hard woods and utilizing thermocol for buoyancy. Mostly, locally available timber of a Combretaceae species, Anogeis...
V Kuppusamy, M V Rao, M Balaji, K Rao


How to determine what is a realistic emission from treated wood - basic reflections
1998 - IRG/WP 98-50105
Emissions from treated wood occur by evaporation and by leaching. Up to date by far more experience exists on leaching tests than on evaporation test. The methods applied will be of interest to give answers to the questions about the quantity of possible emissions. Standardisation on leaching started very early. One of the first attempts to quantify the effect of leaching on the remaining efficacy...
H Willeitner, R-D Peek


Performance of treated spruce in Canadian field test sites
1989 - IRG/WP 3506
Spruce material under test in Canadian field test sites is performing better than anticipated. From the comparison of the performance of spruce treated with various preservatives, it appears that penetration may be far more important on durability performance than the preservative itself or the retention of preservatives in the wood. However, there is still insufficient data on the influence of pe...
J P Hösli, E E Doyle


Effect of leaching temperature and water acidity on the loss of metal elements from CCA treated timber in aquatic conditions. Part 2: Semi-industrial investigation
1995 - IRG/WP 95-50040-13
In continuation of previous leaching research on the quantification and modelling of metal elements released from CCA treated timber, a series of experiments has been carried out dealing with the influence of temperature and pH of the relative aquatic environment. The leaching method used is the Dutch prestandard for building materials, a long term static leaching test simulating practical bank-sh...
G M F Van Eetvelde, W J Homan, H Militz, M Stevens


Timber Preservation and Sustainable Construction in Australia
2005 - IRG/WP 05-50224-14
Sustainable development has been described as meeting the needs of the present without compromising the ability of future generations to meeting their own needs. (Bruntland 1987) To achieve the sustainable development goal therefore, the maximum performance has to be obtained from existing resources (timber) so that the remaining resource is protected from over-exploitation. Clearly, wood preserva...
J Norton


Performance of chromated copper arsenate-treated aspen fence posts installed in Forintek's Eastern test plot from 1951 to 1963
1984 - IRG/WP 3272
Aspen poplar fence posts were pressure treated by the full cell process using three formulations of copper chrome arsenate wood preservative. A total of one hundred and fifty nine of the posts were installed in service in Forintek's Chalk River post plot from 1951 to 1962. During the 1982 general inspection of the post plot all 159 posts were still in service. A groundline inspection was ...
C D Ralph


Biological degradation resistance of pine wood treated with dimethylol compounds
1989 - IRG/WP 3528
The study reports the increase of dimensional stability and biological degradation resistance of pine wood (Pinus sylvestris L) after impregnation with dimethyloldibydroxyethyleneurea. Decay resistance was determined according to BS 838:961. Nearly complete protection against Coniophora puteana, (Schum.ex Fr. Karst) weight loss of 2-3% was shown when modification, expressed as weight gain, exceede...
C L Videlov


Performance of CCA treated Eucalyptus round ties
1985 - IRG/WP 3342
After 5.5 years of field exposure in the south of Brazil round Eucalyptus ties treated with CCA type A Oxide (OSMOSE K-33-A) preservative with retentions from 12 to 14 kg/m³ (0.75 to 0.873 PCF) (active ingredient basis) are performing very well. No decay or insect attack was observed in the 100 ties in test in real conditions of use; 10% of ties show incipient checking (what is a natural trend of...
V J Carlos, F R Niederauer, J P P Wehr


36 years of wood preservative tests in Tanzania
1992 - IRG/WP 92-3731
The performanee of major wood presevatives which are used widely commereially are given. These include creosote, CCA's and 5% Pentachlorophenol dissolved in heavy industrial diesel. Tests are conducted at three ecologically different using pine stakes. Results show that the striking performance of creosote and CCA's is noticeable at above 128 kg/m³ and 16 kg/m³ respectively....
K K Murira, P F Nangawe


A method of predicting the average life of field tests on preservative-treated stakes
1977 - IRG/WP 297
The paper presents an analysis of the results of completed field stake tests on untreated and preserved timber, and develops a method of predicting the average life of incomplete stake tests on wood preservatives from the failures that have occurred so far....
D F Purslow


Copper binding capacity of modified wood flour
1992 - IRG/WP 92-3709
Wood flour was modified by reaction with oxidising agents and CCA preservative. The copper chromium and arsenic were removed from the CCA treated wood flour by an acid leaching procedure. The modified wood flours were allowed to react with copper acetate solution and the level of copper fixation achieved was determined. The modified wood flours had greater affinity for copper ions present in solut...
N C Milowych, W B Banks, J A Cornfield