IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3718 documents. Displaying 25 entries per page.


A collaborative test to determine the efficacy of polyurethane coatings on wood samples exposed in the marine environment
1984 - IRG/WP 4113
Aims are: a) to determine the effectiveness of elastomeric polyurethane as a protective coating against marine wood boring animals in a range of tropical and tempreate sites; b) to compare the adhesion of polyurthane coatings on different wood species exposed in seawater; c) to record the severity of attack in failed samples and to identify the causal marine organisms....
R A Eaton


Changed susceptibility of the chemically and thermally degraded spruce wood to its attack by the dry rot fungus Serpula lacrymans
1999 - IRG/WP 99-10322
In buildings, some intentional or unintended situations can occur at which some wood products are exposed to aggressive chemicals and also to higher temperatures. Occasional activity of fungi on such pre-attacked wood products can be either higher or lower. This paper deals with changes in the susceptibility of spruce wood (Picea abies L. Karst.) to attack by the dry rot fungus Serpula lacrymans, ...
L Reinprecht


In-situ pressure injection for preservation of rubber wood (Hevea brasiliensis Muel Arg.)
1992 - IRG/WP 92-3688
Rubber wood is widely used for the manufacture of furniture, doors for housing and packing cases. However in an untreated condition it is highley susceptible to sapstain and decay fungi and borers. Its utility gets considerably reduced if the wood is not treated well in time. Preservative treatment has to be given within the period of felling and transport to prevent not only loss of structural pr...
H S Ananthapadmanabha, V R Sivaramakrishnan


Evaluation of polystyrene as a protective of wood in sea-water
1986 - IRG/WP 4129
A test is described on the biological protection of wood by treatment with polystyrene. The results, obtained in marine trials, after 18 months, show that the treatment with polystyrene is not all that effective in preventing the attack of marine borers....
A Gambetta


European standardization for wood preservation
1990 - IRG/WP 2359
G Castan


On the problem "House Longhorn Beetle" in hardwoods and an aid to distinguish between Hylotrypes bajulus and Hesperophanes cinereus larvae
1981 - IRG/WP 1141
S Cymorek


Collaborative soft rot tests: 2nd interim report
1975 - IRG/WP 258
J G Savory, J K Carey


Influence of storage on mould susceptibility of wood at relative humidity values lower than 100%
1989 - IRG/WP 1413
It is well known that wood material changes with time because of different environmental influences. The effects of such changes on the subsequent mould susceptibility are less known. In this paper we report on increased mould susceptibility of pine wood after storage. Mould growth was detected by indirect methods....
J Bjurman


Report of an investigation of damage by wood ants in buildings in Sweden
1976 - IRG/WP 148
Wood ants in buildings occur everywhere in Sweden, particularly in maritime districts and in vicinity of larger lakes. The damage caused by Camponotus herculeanus does not differ from that caused by Camponotus ligniperda. The former occurs in all Sweden, the latter only in southern Sweden. The damage is to be found almost exclusively in dwelling houses (week-end cabins and "all-the-year round" hou...
V Butovitsch


The effect of storage or simulated internal use on the durability of wood based panels to decay fungi
1997 - IRG/WP 97-20106
Wood based panels such as particleboard and medium density fibreboard are experiencing a steady increase in use, in areas from structural to decorative applications. Understanding the "natural" durability of these panel products against basidiomycete fungal decay is therefore of great importance. Various methods have been proposed or are under development to test the durability/susceptibility of v...
S F Curling, R J Murphy, J K Carey


Natural resistance of twenty-six Guianese wood species against marine borers
1988 - IRG/WP 4144
This note is a contribution on the study of the natural resistance of some wood species from French Guiana, some of which could be found too in the neighbourhood. Here are presented the results after one year exposure in the marine environment....
L N Trong


Report on a field demonstration of methods for detecting defects in wood poles
1984 - IRG/WP 2232
P I Morris, H Friis-Hansen


Detection of brown rot decay in wood by ion mobility spectrometry
1991 - IRG/WP 2377
A test method for the detection of brown rot decay in wood is described and involves a two-step procedure: thermal release of vapours from wood samples followed by analysis using Ion Mobility Spectrometry (IMS), with results being obtained in 5-10 seconds. The advantages, limitations as well as the detection limit of the technique are presented....
A H Lawrence, T Nilsson


Accelerated wood decay in a soil bed test under greenhouse conditions compared with a stake test under field condition
1991 - IRG/WP 2384
The rate of decay of oak, beech, Douglas fir, pine and spruce stakes in an outside test field were compared with the decay rate of the same species in a greenhouse soil-bed test. Strength loss after four and six months respectively was measured by determining the compression strength parallel to the grain. The results show that all species, strength loss in the greenhouse was 2 to 4 times higher t...
J E Polman, S G Michon, H Militz


Research on the effects of wood preservatives on the physical and mechanical properties of Iranian beech (Fagus orientalis Lipsky)
1985 - IRG/WP 3351
This research work was conducted with the aim of using preservatives such as Basilit and Wolman Salts with Iranian beech and to study any physical and mechanical changes these might have on the beech species of Iran. Samples were divided into three groups; one group were used as untreated controls, the second group was treated with Basilit and the third group was treated with Wolmanit. Results obt...
P Niloufari


Effects of pretreatments for the amelioration of preservative impregnability using the Oscillating pressure method (OPM)
1995 - IRG/WP 95-40044
For the purpose of an amelioration of preservative impregnability, three types of pretreatment: the steaming, the explosion and the boiling, were tested. The specimens were prepared by the domestic four species: Itajii, Ryukyumatsu, Sugi and Hinoki, and 1 refractry imported species: Douglas-fir. The dimension of specimens was 20 x 20 x 300 mm³ and were treated with CCA in a laboratory OPM machine...
K Suzuki, I Asaoka, S Tani, K Okada, T Hidaka


Preventive action against fungal decay: A comparative experiment on the effects of natural and artificial infection of wood by Basidiomycetes
1981 - IRG/WP 2160
M Fougerousse


Report on Sub-group 5 in Raleigh, 6 May 1980
1980 - IRG/WP 1123
S Cymorek


Performance of untreated French Guianan piling in marine exposure
1992 - IRG/WP 92-4173
Round piling of seven French Guianan species, greenheart, and preservativ-treated Southern Pine were installed as fender piling in Key West, FL. After 12½ years, none of the tropical hardwoods performed as well as dual-treated Southern Pine. Of the hardwoods, kouata patou and maho noir were the most resistant to decay and marine borers....
B R Johnson


Durability of different heat treated materials from industrial processes in ground contact
2005 - IRG/WP 05-40312
In this study the durability of heat treated wood originating from four different European industrial heat treatment processes in ground contact was examined. The manufacturers of heat treated material were: PLATO Hout B.V./Netherlands, Thermo Wood/Finland, New Option Wood/France and Menz Holz/Germany where Oil-Heat treated Wood (OHT) is produced. All heat treated materials showed significantly i...
C R Welzbacher, A O Rapp


Effect of fatty acid removal on treatability of Douglas-fir
1993 - IRG/WP 93-40008
Treatment of Douglas-fir with chromated-copper-arsenate (CCA) poses a major challenge. Several hypotheses based on the anatomical aspects as well as chemical reactivity of the preservative formulations with cell wall constituents and deposits have been proposed. Techniques to prevent pit aspiration or slow fixation reactions have, however, not significantly improved treatment. The presence of high...
S Kumar, J J Morrell


Report of field test results for dichloro-n-octyl-isothiazolone: A potential new wood preservative
1988 - IRG/WP 3495
In a previous report (IRG/WP/3306) we presented preliminary laboratory test results on 4,5-dichloro-2-n-octyl-4-isothiazolone (RH 287). Laboratory data indicated toxic threshold values for RH 287 ranging from 0.37 to 0.50 kg/m³. In this report we present field test results on an IRG L-joint test and an in-ground stake test for RH 287, pentachlorophenol and biocide free test units. (a) L-joint tes...
D E Greenley, B M Hegarty


United States Federal Committee on Wood Protection
1971 - IRG/WP 43
A C Jewett


Proposed test procedure to determine the effect of timber substrate on the effectiveness of a copper/chrome/arsenic preservative in seawater
1975 - IRG/WP 411
R A Eaton


The effects of heat treatment on the toughness of beech wood
2004 - IRG/WP 04-40283
The effects of heat treatment on toughness of beech (Fagus orientalis) wood naturally grown and intensively used in forest products industry in Turkey were studied. The wood samples were cut into 5 x 5 x 5 cm. Heat treatment was than applied to the wood samples at three different temperatures (130 °C, 150 °C and 180 °C) and three different durations (2 h, 6 h and 10 h) under air atmospheres. ...
S Yildiz, Ü C Yildiz, E D Gezer, Ali Temiz, E Dizman


Previous Page | Next Page