A summary of work carried out to compare natural and artificial weathering for preconditioning test specimens in testing anti-stain chemicals for wood in service
1976 - IRG/WP 266
Since 1972 work has been in progress within CEN to establish a European standard for the testing of wood preservatives designed to prevent blue-staining of wood in service. The method is based on the Butin test and involves pre-weathering of the samples prior to biological testing. The weathering regime employed is 6 months outside exposure from March to October. This imposes severe limitations on...
D J Dickinson, A F Bravery


Remedial treatment of wood attacked by insects
1981 - IRG/WP 3175
A review is presented of remedial treatments against wood-boring insects in wood in service. Preconditions and fundamental principles of insect control are compared with the control of fungal attack and reasons are given for the fact that remedial treatments against insects are more commonly applied than against fungi. With regard to insect control measures with a simultaneous preventive effective...
H Kühne


Comparison of decay rates of preservative-treated stakes in field and fungus cellar tests. Results after 40 months fungal cellar exposure
1983 - IRG/WP 2200
Decay rates of preservative-treated Pinus radiata stakes during 40 months exposure in the FRI fungus cellar were compared with those of similarly treated material in a field test. Decay rates in the fungus cellar were from 4 to 100 times higher than in the field, although for the majority of preservatives the rate was between 7 and 12 times higher. The lag phase before onset of decay, noticeable w...
M E Hedley


Effect of incising depth and density on treatment of Douglas fir, hem fir and spruce-pine-fir lumber with CCA, ACZA or ACQ
1997 - IRG/WP 97-40093
Incising markedly improves both the depth and uniformity of preservative treatment of refractory wood species, but there are few studies directly comparing the effects of incising depth and density on penetration and retention of commonly used waterborne preservatives in wood species from the western United States. The effects of two incision densities (7300 and 8900 incisions/square meter) at two...
M Anderson, J J Morrell, J E Winandy


Retention and distribution of copper/chrome/arsenic (CCA) in pressurised sap-displaced UK grown spruce and pine
1986 - IRG/WP 3366
Increment cores were taken from UK grown Scots pine (Pinus sylvestris L.), Corsican pine (Pinus nigra var. maritima Ait), Sitka Spruce (Picea sitchensis (Bong) Carr), and Norway spruce (Picea abies (L) Karst) distribution poles treated by pressurised sap-displacement using a 1.8% copper, chrome, arsenic (CCA) solution. Each increment core was sectioned radially and the copper, chrome, and arsenic ...
P D Evans, G M Smith, B King


Soft rot fungi as possible sources of odor in impregnated wood in buildings
1993 - IRG/WP 93-20013
Wood preservatives are frequently used inside houses. In several cases impregnated wood, particularly when used in crawlspaces or other near-ground constructions, has been found to be a source of odor. Mold fungi, soft rot fungi actinomycetes or bacteria growing on impregnated wood are possible producers of the odor. Analyses of volatile emissions from impregnated wood with odor and pure cultures ...
J Bjurman, J Kristensson


Blue stain resistance of exterior wood coatings as a function of their typology
1998 - IRG/WP 98-20145
Paints and wood stains were evaluated on their blue stain resistance using both EN 152 method and the reverse method. The typology of these exterior coatings was varied including standard and high solid solvent-borne coatings as well as different types of waterborne coatings. For the water-borne acrylic, alkyd based and hybrid coatings both applied as opaque primer paints and as decorative wood st...
J Van Acker, M Stevens, C Brauwers, V Rijckaert, E Mol


Natural durability of European wood species for exterior use above ground
2003 - IRG/WP 03-10499
The main interest in using more timber for exterior constructions is to protect the environment, where wood is considered an environmentally friendly material. However, chemicals for wood protection are getting more and more restricted, consequently, the focus on the natural durability of wood is increased. Good, well-documented data on the durability of wood species in ground contact exist, which...
B Lindegaard, N Morsing


Detection of termite attack in wood using AE monitoring
1990 - IRG/WP 2355
An acoustic emission (AE) monitoring method for detecting termite activity in wood was applied to lumber of 3 by 3 cm to 10 by 10 cm square, 1 m long. Furthermore, the propagation of AEs due to the feeding activities of termites in the specimens and the locations of AE sources were analyzed. Also discussed was the feasibility of the method applied to posts out in the field of subterranean termites...
Y Fujii, M Owada, M Noguchi, Y Imamura, M Tokoro


Effect of light and ventilation condition on the rate of wood decay by the brown rot basidiomycete, Tyromyces palustris
1991 - IRG/WP 1517
Effect of light and the ventilation conditions of incubation jars on the wood decay by Tyromyces palustris (Berk. et Curt.) Murr. FFPRI 0507 was investigated. Under no irradiation of light, the ventilation conditions gave extensive effect on mass loss of the test pieces when the culturing was performed with culture medium designated in Japanese Industrial Standard (JIS) A 9302 (Medium A; glucose 4...
T Suzuki, M Higaki


Bioassays for rapid assessment of heavy metal toxicity in seawater
1998 - IRG/WP 98-50112
In evaluating the effect of CCA leachate on the establishment of fouling communities on wood exposed in the sea, three organisms were assessed as biological indicators of heavy metal toxicity. These were two macroalgae, Fucus serratus and Undaria pinnatifida. and the motile protist thraustochytrid, Schizochytrium aggregatum. The choice of these organisms for the tests carried out was based on the ...
C J Brown, R L Fletcher, R A Eaton


A study of wood quality of Juglans nigra and hybrid walnut (MJ 209xRA) : durability against Coriolus versicolor, density and MOR
2004 - IRG/WP 04-10522
The study investigated possible effects of harvesting season on some wood properties of Juglan nigra (JN) and a hybrid walnut (MJ209xRA). The samples were taken from trees which were harvested in June July, August, November of the same year, and March in the year after to determine whether there were any significant differences in wood properties as regards the harvesting seasons. In order to test...
B Charrier, F Charrier, D P Kamdem, J B Aurel, G Janin


An evaluation of CCA, CCB and CCP preservatives using a "sandwich test"
1991 - IRG/WP 2370
The last two years has seen some important changes in standards and preservative types used in Scandinavia, which have led to a wider choice for specifiers. In order to identify those treatments suitable for replacement or reinforcement of decayed constructional timbers, it was felt necessary to modify the standard EN 113 test. Impregnated blocks were sandwiched between two untreated blocks, previ...
A P Koch, L B Sheard


The performance of CCA treatment in bamboo against decay fungi
1993 - IRG/WP 93-30027
Samples of culm wall material from young (< 6 month age) and mature (> 3 years age) culms of the bamboo, Phyllostachys virideglaucescens were treated to equivalent% w/w retentions of a CCA preservative. After fixation and leaching the treated samples were exposed to decay by Chaetomium globosum FPRL S70K, Coriolus versicolor FPRL 28A and Coniophora puteana FPRL 11E. Thin section samples of u...
O Sulaiman, R J Murphy


The effect of felling time of year on CCA fixation rate and quality of selected hardwoods
1998 - IRG/WP 98-40116
White birch (Betula papyrifera), poplar (Populus sp.) and red maple (Acer rubrum) trees were harvested in winter, in spring, before the leaves flushed, after leaf flush and later in the summer. Sapwood discs were cut from the freshly felled trees, dried and cut into 25 mm and 19 mm cubes. The cubes were pressure impregnated with CCA-C and fixed under high relative humidity and at 50°C or at room ...
Y T Ung, A Taylor, P A Cooper, D P Kamdem


Effectiveness of Busan 30 treated birch blocks in a soil medium
1987 - IRG/WP 3409
TCMTB based formulation has been anticipated for use in dip-diffusion treatment in Papua New Guinea to replace BFCA Wood preservative. One such formulation is the Penacide (TCMTB + MBT Boron) which is currently being tested against fungi and insects. Accelerated laboratory test in soil exposure was employed to test a related formulation (Busan 30) to determine its effectiveness against soil inhabi...
H C Konabe


The chemical analysis and biological evaluation of wood extractives as potential timber preservatives
1995 - IRG/WP 95-30090
Work involved the biological performance of water and organic solvent soluble extractives of four naturally durable wood species, namely; Matumi, Tamboti, Sneezewood and the Turpentine tree. These timber species are known to be naturally durable against termites and fungi (±25 to 35 years). The extractives were evaluated against termites and fungi using impregnated pine pencil stakes in field tes...
P Turner, D Conradie


Preference of the Formosan subterranean termite for wood previously damaged by conspecifics
1988 - IRG/WP 1338
In a laboratory choice test, groups of termites from five colonies of Coptotermes formosanus Shiraki were presented with wood blocks which had sustained previous termite damage: 1) by nestmates, 2) by conspecifics from another colony, 3) by another termite species, Reticulitermes virginicus Banks, and 4) no damage. Coptotermes formosanus preferred wood previously damaged by conspecifics over that ...
J P La Fage, K S Delaplane


Vapour boron treatment of wood based panels: Mechanism for effect upon impact resistance
1994 - IRG/WP 94-40036
Samples of medium density fibreboard, chipboard and oriented strandboard (OSB) were treated to two retentions of boric acid by a vapour phase treatment. The results of a range of mechanical tests were reported by Hashim et al. (1992, 1993) in which a small reduction in impact resistance was observed. Several investigations were carried out to study how and where this loss in impact resistance occu...
R Hashim, R J Murphy, D J Dickinson, J Dinwoodie


Health hazards and environmental aspects when using Cu-HDO-containing wood preservatives in vacuum pressure plants
1993 - IRG/WP 93-50001-11
Apart from the biological efficacy of wood preservatives, the health and environmental aspects concerning the utilisation of wood preservatives, the use of treated timber and the disposal of impregnated wood are of high significance today. Therefore, information on a possible aerial concentration of wood preservatives, on the mobility of active substances in soil leached from treated timber in ser...
W Hettler, S Breyne, M Maier


The Use of Insect Hormones as Non-Neurotoxic Insecticides in Wood Preservatives
2002 - IRG/WP 02-30277
The ecdyson and juvenile hormone analogues show a clear difference in their effect on the house borer, Hylotrupes bajulus. In the tested dosages, the ecdyson analogues have only a slight ovicidal effect but a very clear effect on old larvae. With a dosage of 1250 mg/m², Halofenozid achieved 100% mortality after 27 weeks and Tebufenozid after 40 weeks. The two juvenile hormone analogues, Fenoxy...
E Graf, M Barkhoff, R Hamberg, H Büttner, M Pallaske


Dynamics of pressure changes in wood during impregnation
1990 - IRG/WP 3615
Conventional methods of impregnation have to be improved for achieving better penetration of refractory wood species. Basic requirements for an adjustment of treatment schedules are, amoung others, a profound knowledge of the course of pressure changes in the wood during treatment. A new method of pressure measurement was developed which supplies exact and reproducible data. The results show that ...
R D Peek, S Goetsch


Development on Damage Functions of Wood Decay for Building Envelope Design
2005 - IRG/WP 05-10556
For the hygrothermal analyses of building envelope systems for insulation design, we tried a natural decay test of wetted wood specimens without any inoculation of fungi. Three principal experimental types: under steady-state conditions (Experiment A), at a cyclic water dripping under Non-steady conditions (Experiment B) and at a cyclic water dipping under-steady conditions (Experiment C), were ca...
H Suzuki, Y Kitadani, K Suzuki, A Iwamae, H Nagai


Photo-discoloration and Degradation of Wood and its Stabilisation by Modification with Benzoyl Chloride
2004 - IRG/WP 04-40274
Photo degradation of Pinus roxburghii (chir pine) and Hevea brasiliensis (rubber wood) was studied under artificial accelerated weathering conditions in a Xenon test chamber. The irradiated samples were analyzed for color changes and chemical changes. Analysis of colour changes in wood surfaces by UV-Vis. irradiation was carried out using a colour measuring (CIELAB) system and chemical changes ...
K K Pandey


Studies on the destruction by marine wood boring organisms of fishing boats in the Eastern Black Sea of Turkey
1977 - IRG/WP 427
The present paper concerns the problem of fishing boats which are attacked by wood boring organisms in the Black Sea of Turkey. The aims of this study are: 1) to identify the marine wood boring organisms attacking fishing boats in the Northern Black Sea of Turkey; 2) to identify the wood species that are used in boat building construction and assess their durability; 3) to assess the degree of att...
R Ilhan, O A Sekendiz