Durability of Bamboos in India against termites and fungi and chemical treatments for its enhancement
2005 - IRG/WP 05-10553
Bamboo is a very important forest resource that benefits the life of people in a myriad ways including meeting the need for structural uses like posts, pole fencing, scaffoldings, house building, etc. Although it is one of the strongest structural material available, often succumbs to fungal decay and biodeterioration by insects (termites and powder post beetles) during storage and usage. Studies...
O K Remadevi, R Muthukrishnan, H C Nagaveni, R Sundararaj, G Vijayalakshmi


Strength properties of preservative treated pine and spruce wood after super-heated steaming
1984 - IRG/WP 3313
Possible changes of strength properties of CCF pressure impregnated pine and spruce with subsequent steaming at 110°C respective 120°C for 30 min were examined. For spruce analysis of variance indicated that none of the processes had a significant effect on bending strength, compression strength and the corresponding modulus of elasticity as well as on impact bending strength and shear strength ...
R-D Peek


An appraisal of methods for environmental testing of leachates from salt-treated wood; part 1
1998 - IRG/WP 98-50115
The magnitude and diversity of leaching tests with salt-treated wood, performed by institutes as well as industry, strongly appeal for harmonisation towards one single method. That procedure should be well-defined, cost- and time-effective and moreover be extended with a clear detection and interpretation scheme. The paper(s) presented here tend to evaluate 2 existing leaching methods, the ENV 12...
G M F Van Eetvelde, M Stevens, F Mahieu, H-W Wegen, A Platen


Use of wood-decay fungi for disposal of PCP-treated wood
1995 - IRG/WP 95-50040-33
Although PCP has been classified as a priority pollutant, PCP-treated wood products are currently allowed to be disposed of as ordinary solid (non-hazardous) wastes in the US. Non-regulated disposal of these materials is allowed because PCP concentrations in extracts from PCP-treated products such as utility poles and crossarms, determined by the Toxicity Characteristic Leaching Procedure (TCLP) h...
R T Lamar


Observations on the performance of copper-based wood preservatives in fungal cellar (soil-bed) tests
1994 - IRG/WP 94-20047
Fungal cellar (soil-bed) tests are considered to be an important tool for the evaluation of the performance of ground contact wood preservatives. Facilities of this type have been established world wide although caution has been exercised in their introduction into standard testing methods for the approval of wood preservatives. This is the result of concerns over the variability in the biological...
G R Williams, D Rudolph, M E Hedley, J A Drysdale, R F Fox


Description of a trial with wood preservatives against marine wood boring organisms
1975 - IRG/WP 412
Wood situated in sea water along the Atlantic coasts of the Nordic countries is attacked by marine wood boring organisms. Timber constructions in these waters therefore must be preservative treated. In order to evaluate the effect of various preservatives against marine wood borers, the Nordic Wood Preservation Council (NWPC) organized a rather extensive trial in 1972. In the absence of and while ...
E Norman, B Henningsson


The effect of extent and location of decay on strength loss in constructional timber
1994 - IRG/WP 94-30039
Radiata pine heartwood billets, 50 x 100 x 1000 mm³ were end-sealed and treated with copper-chrome-arsenate preservative (NZ Type I) to a range of retentions and penetration patterns. Cross-sections, 10 mm thick, were cut from the centre of each billet and used for determination of preservative distribution, for preservative analysis and for decay tests. The decay test consisted of laying samples...
M E Hedley, H Bier


Risk of pulmonary damage as a result of an evaporation of ca. 50 ppb = 42 mg HF, evaporated from wood treated by difluorides
1987 - IRG/WP 3401
In this review of the literature the effects of fluorides and fluorine on man are described, especially the low level effects of inhaled HF on human beings. The term "fluoride" is used as a general term everywhere, where exact differentiation between ionic and moluecular forms or between gaseous and particulate forms is uncertain or unnecessary. The term covers all combined forms of the element, r...
H F M Nijman


Effects of alkali treatment on some mechanical and chemical properties of creosote treated oaks
1991 - IRG/WP 2366
To date, there is a lack of information on the effects of chemical treatment on the performance of creosote preservative treated oak sleepers. This factorial experiment was designed to analyze three main effects: species (Quercus alba and Quercus rubra) creosote treatment (treated and untreated), and alkali (NaOH) soaking (0, 1, and 10 percent). The modulus of elasticity (MOE) and fiber stress at ...
P Chow, A J Reinschmidt, E J Barenberg, L C Chang


Treatability of waterstored poles of Norway spruce by sap-displacement and pressure treatment with Boliden K33 and creosote
1973 - IRG/WP 328
Poles of windthrown Norway spruce were stored in bark under water sprinklers for 11-20 months or fully submerged in a lake for 3 years (tab. 1 and 2). Water content after storage is shown in fig. 1 and 8. Treatment with Boliden K33 by sap-displacement (open tank suction) gave a poor result. The Danish requirements of delivery claim a penetration of 20 mm and a net retention of 12 kg/m³ in outer 2...
P Moltesen, E Borsholt, B Bang


On-site test for indicative determination of leaching of components of preservatives from treated timber
1993 - IRG/WP 93-50001-12
In the late eighties the environmental concern about treated timber increased and it is still a hot issue in the Netherlands. From the environmental point of view three phases in the timbers life cycle can be distinguished: - the production phase - the service life - the waste phase. In the Netherlands at this moment much emphasis is laid on the production phase. In 1992 this has led to a new legi...
W J Homan, H Militz


Accelerated decay tests on DNBP-treated Pinus patula and Eucalyptus grandis
1987 - IRG/WP 3441
Blocks (10 x 10 x 5 mm³) of Pinus patula and Eucalyptus grandis were impregnated to 0, 1.5, 3.0 and 4.5 kg/m³ 2-sec-butyl, 4, 6 dinitrophenol (DNBP). They were monitored microscopically and for weight losses over 16 weeks against monocultures of Coriolus versicolor and Coniophora puteana. Treated ministakes (10 x 10 x 100 mm³) and blocks in soil contact were similarly monitored to determine wei...
L D Abraham, A A W Baecker


Hardwood field experiment - 10 year report
1989 - IRG/WP 3560
The international hardwood field experiment was planned in 1976 and set up in some 34 different sites around the world. The test stakes include 4 reference species common to each site and in most cases at least 2 species of local importance (supplementary species). It was hoped that a picture of performance of a range of economically important timber species would be built up and at the same time ...
D J Dickinson, S M Gray


Decay and termite durabilities of heat-treated wood
2004 - IRG/WP 04-40272
Decay and termite resistances of Plato-treated timbers were evaluated using a modified JIS decay test method, feeding test in a laboratory scale and a field exposure against Reticulitermes speratus (Kolbe) or Coptotermes formosanus Shiraki. The results showed that no significant decay durability of the treated timbers although mass loss from decay slightly decreased in case of treated timbers. ...
S Doi, K Hanataa, E Kamonji, Yuuji Miyazaki


Behaviour of some selective Indian species towards treatment with solvent based water repellent preservative
1984 - IRG/WP 3309
This paper discusses a solvent based preservative using PCP and a water repellent for preserving three species of timber commonly used in India for the manufacture of doors and windows. It examines the method of treatment to achieve desired levels of penetration and retention of the preservative-cum-water repellent, and tests made on these timbers to examine the success of the processing methods a...
V R Sonti, B Chatterjee


A marine borer test with water-borne preservatives
1980 - IRG/WP 452
The use of preservative treated timber in sea-water where marine borers are active is of great economic importance, since untreated wood immediately will be damaged. Vacuum/pressure treated timber has been tested in several marine exposure trials on the Swedish west coast since the 1930s (Hager 1941, Hultman 1949, Sandstrom 1951, Nylinder-Norman et al. 1974). Since new interesting materials or pre...
B Henningsson, E Norman


Equilibrium distribution of toxic elements in the burning of impregnated wood
2001 - IRG/WP 01-50172
The current work focuses on predicting the behavior of arsenic, chromium, and copper in the burning of impregnated wood. A theoretical method is used to study the chemistry of the system, with special interest directed towards the vaporization tendency of the potentially toxic elements. The core of the study is the global equilibrium analysis that simultaneously takes into consideration all chemic...
K Sandelin, R Backman


Protection of wood blocks treated with Trichoderma isolates selected on the basis of preliminary agar screening studies
1996 - IRG/WP 96-10154
Previously reported results of agar interaction screening studies for biocontrol agents of wood decay basidiomycetes showed two Trichoderma viride isolates, killed 16 of 19 target fungi (Tucker and Bruce, 1995). Testing of these isolates in wood was required to assess their performance at preventing decay of wood blocks. Standard testing of chemical wood preservatives is used to determine the toxi...
E J B Tucker, A Bruce, H J Staines


Effect of treating process on efficacy of CCA in a laboratory decay test
1990 - IRG/WP 3628
Test samples of Pinus radiata sapwood measuring 40x40x500 mm³ were treated with a range of concentrations of the copper-chrome-arsenate (CCA) formulation "Tanalith C" using Rueping (empty cell), Lowry (empty cell) and Bethell (full cell) treatment processes. Samples were then reduced to 40x40x7 mm³ test blocks and exposed to the decay fungus Coniophora puteana using an agar/block technique. Repl...
M E Hedley, K Nasheri, J G Van der Waals


Risk assessment of energetic valorization of treated wood - wooden recycling
1996 - IRG/WP 96-50072
The most useful method for the valorization of wood wastes and wooden wastes is energetic valorization. In France the percentage of wood treated by antisaptain products is around 30%. Currently with the growing regulation, there is a need for cleaner methods and technology to allow sustainable valorization. The preservatives concerned are common organochlorine compounds (NaPCP) less used nowadays ...
G Deroubaix, P Marchal, G Labat


Remedial ground-line treatment of CCA poles in service. Results of chemical and microbiological analyses 6 months after treatment
1986 - IRG/WP 3388
CCA-treated poles in service with incipient internal soft rot were remedially treated by inserting borate rods, brushing with a boron/glycol solution and injecting boric acid paste, copper/creosote paste or a commercial product (DFCK paste). The spread of active chemicals in the treated zone as well as the change in microflora have been studied with time. After six months chemicals had spread to m...
B Henningsson, H Friis-Hansen, A Käärik, M-L Edlund


Termite Field Tests of Various Timber Species Treated with permethrin using supercritical carbon dioxide
2005 - IRG/WP 05-10560
Termite field tests were conducted on permethrin-treated Eucalyptus obliqua heartwood, Pinus radiata sapwood and P. radiata LVL. The permethrin was impregnated using either supercritical carbon dioxide (scCO2) or light organic solvent preservative (LOSP) systems. Comparative permethrin retentions were most accurately achieved in P. radiata sapwood, where no difference between impregnation systems ...
A Qader, L J Cookson, J W Creffield, D Scown


Alternatives to CCA for ground contact protection of timber: a perspective from UK on performance and service life expectations
2002 - IRG/WP 02-30289
The proposed amendment to the European Union's Marketing and Use Directive (1976/769/EEC) in respect of arsenic in CCA wood preservatives seeks to restrict the use of CCA across the European Union. CCA is an extremely important wood preservative in the UK from the manufacturing of the product to the extent of use of CCA-treated timber. Based on our experience and judgement on the use of ...
E D Suttie, A F Bravery, T B Dearling


Studies on the preservative treatment of round bamboos by a new technique
1989 - IRG/WP 3536
Nature has offered a versatile and cheap material bamboo, which is generally found to grow principally in forest areas from sea level to about 400 m wherever suitable combination of ecological factors prevail. This potential renewable natural resource has been since times immemorial, exploited by mankind for a variety of purposes specially in developing countries like Asia, Africa and South Americ...
V R Sonti, S Sonti, B Chatterjee


Analysis of water repellents in wood treated with water borne formulations using FTIR
2000 - IRG/WP 00-40176
The use of aqueous water repellent emulsion formulations has increased significantly in the wood treatment industry. These products are primarily used to enhance the weathering characteristics of wood products treated with water borne preservatives systems used in exterior above ground applications. They are also used in pole treatments to improve climbing characteristics and in low VOC millwork t...
P J Walcheski, L Jin