Improved preservative penetration of spruce after pre-treatment with selected fungi. I. Fungal pre-treatment of pole sections
1998 - IRG/WP 98-40117
European spruce logs were pre-treated with either Phanaerochete chrysosporium, Dichomitus squalens, Trichoderma viride and Trichoderma aureoviride for incubation periods of between 1-4 weeks prior to pressure treatment with creosote in a commercial treatment plant and analysed for strength and creosote uptake (see part II Tucker et al.). A method to pre-treat logs was optimised. The pole sections ...
B Rosner, K Messner, E J B Tucker, A Bruce


Investigation of extracellular mucilaginous material in some wood decay fungi
1996 - IRG/WP 96-10188
The external morphology of the extracellular mucilagenous material (ECM) produced by Coriolus versicolor and Coniophora puteana during colonization of Scots pine and beech was studies using SEM. Specimens were examined in the frozen hydrated, freeze-dried and critical point dried state. All technics produced artefacts but the ECM was best preserved when examined the frozen hydated state. Critical ...
A R Abu, D J Dickinson, R J Murphy


Biocontrol of Reticulitermes santonensis by entomopathogenic fungi
1999 - IRG/WP 99-10324
Biocontrol of subterranean termites by entomopathogenic fungi has already been studied but little work has been done on Reticulitermes santonensis. This paper deals with the screening of 8 fungi strains for their pathogenicity towards R. santonensis. Spores from Metarhizium anisopliae, Beauveria bassiana and Absidia coerulea were used to contaminate 25 termite workers in petri dishes. Bioassays we...
I Le Bayon, D Ansard, C Brunet, I Paulmier, A-M Pruvost


Silicon tetrachloride: A potential wood preservative
1980 - IRG/WP 3133
In its present form, this paper is a preliminary draft of a paper that will eventually be submitted for publication in the Forest Products Journal. We are continuing the work on the effects of silicon tetrachloride on wood and expect to have additional data for the meeting in May 1980. Specifically we are measuring the penetration rate and depth of SiCl4, and we are chemically analyzing the treate...
C W Owens, W T Shortle, A L Shigo


Remediation of a site contaminated with creosote and CCA - a case study
1998 - IRG/WP 98-50101-12
Over sixty years of wood preservation activity conducted by ImpregNor at Ilseng, Norway, has caused serious contamination of the soil. High concentrations of creosote have been found at two separate sites, one in connection to the creosote wood preservation plant, and one further downstream were residues from the creosote preservation have been deposited. High levels of chromium, copper and arseni...
T Rødsand, K Hellum, H Lillemaehlum


Extracellular hydrogen peroxide-producing and one-electron oxidation system of brown-rot fungi
1990 - IRG/WP 1445
Wood-component-degrading compounds involved in the initial degradation of the cellulose and lignin in wood were isolated from wood-containing culture of brown-rot fungi, Gloeophyllum trabeum and Tyromyces palustris and partially purified by gel filtration on Sephadex G-25 and DEAE-Sepharose ion-exchange chromatography. The compounds were glycoproteins. The molecular weights of the glycoproteins as...
A Enoki, S Yoshioka, H Tanaka, G Fuse


The nature of osmiophilic particles and their distribution during different stages of brown and white rot decay
1983 - IRG/WP 1213
The distribution of osmiophilic particles during the course of brown and white rot decay was investigated by applying transmission electron microscopic (TEM) methods. It was found that it correlates with the brown and white rot pattern.The osmiophilic particles are produced by the fungus and are supposed to be wood rotting enzymes....
K Messner, H Stachelberger


Leaching from CCA-treated wood submerged in seawater: Effect of high loadings, and a comparison between laboratory and marine conditions
1996 - IRG/WP 96-50080
This study of leaching examined the following variables: CCA loading; marine versus laboratory exposure and length of submergence. Blocks of Pinus sylvestris were treated to a range of nominal retentions from 15 to 50 kg/m³. Each block was then divided into three cubes and all transverse faces were sealed. All cubes were allowed to fix at ambient temperature for a minimum of one week. One set of ...
R M Albuquerque, S M Cragg, J D Icely


Growth of the copper tolerant brown rot fungus Antrodia vaillantii on different substrates
1995 - IRG/WP 95-10121
In recent years the copper tolerant brown rot fungus Antrodia vaillantii caused severe damages on impregnated wood in ground contact. The pattern of decay gave the impression that impregnated wood was even more severely attacked than unimpregnated. To investigate this question more closely laboratory tests were carried out. In a "choice test" Antrodia vaillantii grew preferably towards CC-impregna...
H Leithoff, I Stephan, M-T Lenz, R-D Peek


Do CCA treated support stakes cause increased arsenic level in crops?
2003 - IRG/WP 03-50204
Trial of using CCA-C treated eucalypts stakes for supporting banana plants in Guangdong Province, China, began in 1998 and later it was expanded as a demonstration program of a joint International Tropical Timber Organization–Chinese Government timber preservation project in 2000. The greatest concern was whether the crop would be contaminated by the preservatives, arsenic in particular. Data fr...
Li Zhaobang, Su Haitao, Liang Linqing


Ten Year Marine Borer Exposure Trial of Chlorothalonil and Emulsified Preservatives in Australia
2003 - IRG/WP 03-30314
Results of a ten-year marine exposure trial at Townsville and Port Stephens are presented. Sawn Pinus radiata and natural round Eucalyptus obliqua specimens were treated with preservatives including creosote (HTC), pigment emulsified creosote (PEC), chlorothalonil, and the oil emulsions of CCA called PROCCA and HYCON. Basic zinc chloride treatment was also exposed at Townsville. Some of the findin...
L J Cookson, D Scown


Targeted inhibition of wood decay fungi: degradation of cotton cellulose
1999 - IRG/WP 99-10321
Brown-rot decay is responsible for 80% of the damage and replacement of wood in service. For nearly thirty years, researchers have postulated a one-electron oxidase system combining Fe+2 oxalic acid, and H2O2 in the production of hydroxy radicals which ultimately oxidize cellulose in situ. Recently, researchers have been investigating antioxicants, in combination with biocides (Schultz, et al.,199...
F Green III, T A Kuster


Field fencepost test of several species treated with water-borne preservatives by rural methods
1986 - IRG/WP 3385
Fencepost field results in ground-contact treated by rural methods: immersion-diffusion and sap displacement by evaporation are analyzed. Copper-chrome-arsenic and copper-fluor-chrome preservatives were used in two concentrations. The wooden species studied were: Pinus pinaster, Eucalyptus globulus and Quercus rubra. For each of the test units decay index evolution was analyzed after five years ex...
M V Baonza Merino


Influence of variable lignin content amongst hardwoods on soft-rot susceptibility and performance of CCA preservative
1982 - IRG/WP 1151
This paper presents the outline of an argument, based on both new and established data, which relates varying lignin content to variation of soft-rot susceptibility between hardwood species and of performance of CCA preservatives in controlling soft-rot. Although more data need to be generated to prove this relationship, sufficient evidence exists for the hypothesis to be given close attention, pa...
J A Butcher, T Nilsson


Effect of moisture and cellulosic substrate on decay of hardwoods by soft-rot fungi
1982 - IRG/WP 2173
The development by Forintek Canada Corp. of standard test procedures for laboratory preservative evaluations using soft-rot fungi was requested by the American Wood Preservers' Association. In Europe, through cooperative studies in the International Research Group on Wood Preservation, several attempts have been made to produce a standard procedure, but variability in results obtained bet...
A Byrne, R S Smith


Proposal for a simple methodology for the evaluation of the preventive effectiveness of protectors applied in superficial treatments against basidiomycetes fungi
1999 - IRG/WP 99-20167
Due to the considerable effect that the relation between the lateral surface and the volume of wood blocks has on superficial treatments, this work has attempted to determine the ideal size which allows to evaluate the effectiveness of a preservative in the shortest possible time. Three wood blocks of different dimensions were tested. In addition, as it is necessary to neutralise the effect of the...
M T De Troya, A Navarrete, F Rubio, M Yuste, C Rodríguez-Borrajo, D Muñoz-Mingarro, F Llinares


Utilization of coconut timber from north Sulawesi, Indonesia. Part 2: Treatability
1994 - IRG/WP 94-40025
Under tropical conditions coconut wood is quickly degraded by mold and blue stain fungi. Low density wood in ground contact is commonly decomposed by wood destroying fungi within a period of only a few months, higher density wood from the outer stem regions within 24 to 30 months (MOSTEIRO, CASIN, SERIBAN 1976; McQUIRE 1975). Moreover, according to McQUIRE (1975) green wood of lower density is hig...
R-D Peek


Effect of thickened boron in preventing conidial germination of sapwood-inhabiting fungi
1994 - IRG/WP 94-30059
We evaluated the efficacy of thickened boron preservative "Diffusolä" in preventing conidia germination of sapwood-inhabiting fungi using plate bioassay, Southern Yellow Pine and sweetgum block tests, and green pine log sections. The test fungi were sapstain fungi Ceratocystis coerulescens, Ceratocystis minor, and Aureobasidum pullulans and mold fungi, Aspergillus niger, Penicillium spp, and Tric...
S C Croan


Leaching of arsenic, copper and chrome from preservative-treated timber in playground equipment
1984 - IRG/WP 3149
Samples were taken from CCA-treated timber in sand play boxes and other play ground equipment. Sand was also sampled. Sand and wood samples were analysed for copper, chrome and arsenic by AAS. About 20-25% of the arsenic had leached from the timber after 2-4 year's exposure in the playgrounds. Very little of the copper and chrome had been leached. Sand collected in the close vicinity of t...
B Henningsson, B Carlsson


Soft-rot in Tabebuia sp. wood used in water cooling tower: identification and degradation capacity of the fungi
1998 - IRG/WP 98-10253
Tabebuia sp. (ipe), a native Brazilian wood, is considered of high natural resistance to decaying fungi, and has been used in harsh environments, as cooling towers. Fifty-one fungi, belonging to mitosporic fungi group (Fungi Imperfecti), were isolated from deteriorated Tabebuia sp. wood samples, collected from the mist eliminator and packing of a cooling tower in operation for about 23 years. The ...
S Brazolin, M Tomazello, I H Schoenlein-Crusius


Fixation of CCA preservatives in cocos-, oil- and rattan-palm
1986 - IRG/WP 3371
In previous tests with jubaea-palm almost no fixation of a CCA-preservative Type B could be achieved, consequently, further leaching tests were carried out with samples of 1 cocos-, 1 oil- and 2 rattan-palms from Malaysia. A good fixation of chromium and copper took place in cocos-palm after 4 weeks storage at 28°C. Nevertheless the fixation was slower than in pine-wood and demanded an elevated t...
H Willeitner, K Brandt


The efficacy of polymer/preservative treatments in soil-bed exposure
1992 - IRG/WP 92-3729
Southern pine was treated with CCA, CCB, sodium borax/boric acid, or disodiumoctaborate, alone or in combination with an acrylic polymer system containing a water repellent. Treated samples were subjected to an unsterile soil burial test. The addition of polymer reduced the weight loss in borontreated samples at the lower retentions but not at the higher retention. Results with borates indicate th...
R J Murphy, H M Barnes, S M Gray


Soft rot decay in CCA treated eucalypts in Queensland - A comment
1986 - IRG/WP 1301
A survey has been completed concerned with the distribution and severity of groundline soft rot decay in the CCA treated sapwood of eucalypt poles in Queensland. The survey encountered some 1000 poles of which 55% were slightly, 28% moderately and 17% severely decayed. Soft rot decay was more severe in urban than rural locations. Embedment of poles in concrete resulted in severe soft rot. No signi...
L E Leightley


Environmental consequences of various materials in utility poles - A life cycle analysis
1992 - IRG/WP 92-3726
A model for environmental life cycle analysis, LCA, has been created to compare environmental impact from transmission poles, made alternatively of concrete, steel, aluminium and pine wood treated with CCA type B or creosote. The main pollution sources and energy use are included in the LCA. One pole size, 12 meters long, is presented in the study, a so called "45 kV" pole. Poles of different mate...
M Erlandsson, K Ödeen, M-L Edlund


Inhibitory effects of leachates from Scots pine wood on germination of some wood rotting fungi
1986 - IRG/WP 1282
Leachates from sapwood of Pinus sylvestris inhibited or reduced the germination of basidiospores of the wood decay fungi tested. The fungi were selected among those preferentially colonizing hardwood or softwood, representatives for brown rot and white rot fungi, early basidiomycete colonizers and late basidiomycete colonizers in above-ground parts of pine as well as fungi found in high frequencie...