Treatment details for the field experiment to determine the performance of preservative treated hardwoods with particlar reference to soft rot
1977 - IRG/WP 384
These notes are compiled to complement and supplement Document No: IRG/WP/367 which described the plan for the treatment of the stakes, using a CCA preservative, for the field experiment. This document gives extra details of the treatment characteristics of the different timber species and as such may give IRG members useful information on the sapwood permeability of a range of hardwoods. The repo...
F W Brooks, M R Gayles


Biochemical aspects of white-rot and brown-rot decay
1987 - IRG/WP 1319
This paper presents an overview of the decomposition of wood by white- and brown-rot fungi - the most important and potent of known wood-decay fungi. These organisms are unique among cellulose destroyers because of their strong capability to enzymatically degrade lignified material. Special emphasis is given to the following aspects of wood decomposition by white- and brown-rot fungi: (1) effects...
T L Highley


An investigation of the effects of pre-steaming on the treatment of sawn spruce timber with Celcure A, a copper/chrome/arsenic preservative
1981 - IRG/WP 3180
Difficulties in the treatment of spruce using standard vacuum/pressure techniques with both water-borne and organic solvent preservatives are well known. The growth characteristics of spruces (Picea spp) make them attractive candidates for forestry schemes. In 1975 the UK Forestry Commission had about 400 000 hectares, about 20% of total UK forest area, planted with Sitka spruce (Picea sitchensis)...
C R Coggins


Effects of fixation conditions and seawater on leaching of wood treated with marine retention CCA
1997 - IRG/WP 97-50088
The effect of post-treatment conditioning temperature and humidity on leaching of chromated copper arsenate (CCA) was compared in seawater and deionized water. Southern pine cubes treated to 40 kg/m3 CCA were stored at 2° C and 82% relative humidity (RH), 24° C and 65% RH, or 32° C and 30% RH for 3, 10, or 17 days. Cubes were then leached in deionized water or artificial seawater. The rate of l...
S T Lebow


The use of the Shigometer® and Pilodyn® as non-destructive test methods for detecting decay in CCA treated eucalypt poles
1981 - IRG/WP 2153
The groundline condition of sixty C.C.A. treated eucalypt poles comprising six different species was examined using the Pilodyn® and Shigometer®. Although sensitive to the presence of soft-rot decay, the Shigometer® would seem to offer little practical advantage in the eucalypt soft-rot decay situation, since a comparable visual examination could reveal the presence and extent of decay. Initial...
L E Leightley


Determination of absorption, accumulation and transport of copper in mycelium of some wood decay fungi
1999 - IRG/WP 99-10323
Copper compounds are common wood preservatives. However, tolerance of some wood decay fungi to copper compounds has been observed recently. Therefore, we tried to elucidate possible causes of this phenomenon. We investigated uptake, accumulation and secretion of copper in the mycelium of potentially copper tolerant fungi (Antrodia sp.) and non tolerant fungus Trametes versicolor. We observed that ...
F Pohleven, S Breznikar, P Kalan, M Petric


The critical moisture and temperature conditions for the growth of some mould fungi and the brown rot fungus Coniophora puteana on wood
1988 - IRG/WP 1369
The growth of some mould fungi on pine and spruce sapwood was studied in 40 different constant moisture and temperature conditions. The temperature range was between +10 and +40°C and the relative humidities varied from 76 to 100% relative humidity (RH). The incubation time was 12 weeks. The mixed mould inoculation used included typical fungi growing on wood: Aspergillus versicolor, Cladosporium ...
H Viitanen, L Paajanen


Fixation of copper-chrome-arsenic treated timber: A comparison of leaching methodologies
1996 - IRG/WP 96-50075
Five packs of kiln dried radiata pine heartwood were treated with copper-chrome-arsenic preservative treated, utilising a modified Bethell treatment schedule. Two methods of determining the level of preservative fixation were compared. These included the diphenylcarbazide method and simulated rainfall testing. The fixation levels were generally higher for tests involving simulated rain leaching. F...
S Walley, P R S Cobham, P Vinden


Relative performance of copper/chrome/boron (CCB) and copper/chrome/arsenate (CCA) in ground contact
1992 - IRG/WP 92-3694
The performance of four retentions each of an oxide CCA formulation and a salt formulation of CCB in radiata pine and European beech was compared after 18 years' field exposure. In radiata pine CCA oxide was more effective (4 failures out of 40) than CCB (9 failures out of 40). However, in European beech CCB was substantially more effective (22 failures) than CCA oxide (all failed). Analy...
M E Hedley


L-joint trials: Part 2: The relationship between colonisation by decay fungi and long-term performance
2002 - IRG/WP 02-20251
Many of the L-joint trials conducted at BRE were assessed during the early stages to establish the rate of colonisation by fungi, principally basidiomycetes. At that time, a system of assessment incorporating colonisation studies was proposed for inclusion within the European Standard EN 330 but was rejected for the final version of the standard. The long-term trials associated with the colonisa...
J K Carey


Comparison of three methods for assessing the in-ground termite resistance of treated timber, durable timber and plastics at sites in Australia, USA and Thailand - First results
1998 - IRG/WP 98-20132
The in-ground resistance of materials to attack by subterranean termites is most commonly assessed with one form or another of the conventional graveyard method, despite the significant shortcomings of this method. In Australia, an alternative method, in which all samples of test materials are placed below-ground, has been in use for more than 10 years. The method provides reliable exposure of sam...
M Lenz, A F Preston, J W Creffield, K J Archer, B M Kard, C Vongkaluang, Y Sornnuwat


Resistance of painted wood to mould fungi. Part 3. The effect of weathering, wood substrate and fungicides on mould growth
1998 - IRG/WP 98-10284
The effect of 6 month outdoor weathering on the resistance of acrylate paint systems on different types of pine and spruce sapwood to mould fungi was studied. Dipping into the preservative prior to painting, a primer with and without a fungicide (propiconazole + IPBC 0.50 + 0.2%) and a topcoat with and without a fungicide (propiconazole + IPBC 0.25 + 0.12%) were combinations of the treatments stud...
H Viitanen, P Ahola


Which fungi should be included in the laboratory evaluation of anti-stain chemicals?
2001 - IRG/WP 01-20236
Test fungi for efficacy tests of anti-stain formulations were selected based on the assumptions that test fungi should be fungicide-tolerant antagonists and fungi resistant to both fungicides and fungicide- tolerant antagonists, and such fungi should be re-isolated from treated samples with the highest fungicidal concentration used for laboratory evaluation of fungicides. This paper discusses the ...
Hyung-Jun Kim, Jae-Jin Kim, Gyu-Hyeok Kim


Interim report on the use of borate rods for the in-situ treatment of joinery
1980 - IRG/WP 3159
In the U.K. in recent years, it has been recognised that there is a major need for in-situ treatment of joinery at risk from or showing the early signs of decay. Several techniques have been developed to provide such a treatment, one of which is based on the insertion of anhydrous borate glass rods. The tests in hand are long term and this report is confined to the mycological isolation data from ...
D J Dickinson


Use of wood-decay fungi for disposal of PCP-treated wood
1995 - IRG/WP 95-50040-33
Although PCP has been classified as a priority pollutant, PCP-treated wood products are currently allowed to be disposed of as ordinary solid (non-hazardous) wastes in the US. Non-regulated disposal of these materials is allowed because PCP concentrations in extracts from PCP-treated products such as utility poles and crossarms, determined by the Toxicity Characteristic Leaching Procedure (TCLP) h...
R T Lamar


Observations on the performance of copper-based wood preservatives in fungal cellar (soil-bed) tests
1994 - IRG/WP 94-20047
Fungal cellar (soil-bed) tests are considered to be an important tool for the evaluation of the performance of ground contact wood preservatives. Facilities of this type have been established world wide although caution has been exercised in their introduction into standard testing methods for the approval of wood preservatives. This is the result of concerns over the variability in the biological...
G R Williams, D Rudolph, M E Hedley, J A Drysdale, R F Fox


Effect of cyclic change of temperature on fungal growth and mass loss
1994 - IRG/WP 94-10065
For estimating the effect of cycling change of temparature on fungal growth, four Japanese species, sugi (Cryptomeria japonica), hinoki (Chamaecyparis obtusa), akamatsu (Pinus densiflora) and buna (Fagus crenata), four fungal species, Tyromyces palustris, Gloeophyllum trabeum, Coriolus versicolor, Pycnoporus coccineus, and five temperature conditions, 10, 20, 27, 35°C and cyclic temperature (20°...
K Suzuki, K Okada


Description of a trial with wood preservatives against marine wood boring organisms
1975 - IRG/WP 412
Wood situated in sea water along the Atlantic coasts of the Nordic countries is attacked by marine wood boring organisms. Timber constructions in these waters therefore must be preservative treated. In order to evaluate the effect of various preservatives against marine wood borers, the Nordic Wood Preservation Council (NWPC) organized a rather extensive trial in 1972. In the absence of and while ...
E Norman, B Henningsson


The effect of extent and location of decay on strength loss in constructional timber
1994 - IRG/WP 94-30039
Radiata pine heartwood billets, 50 x 100 x 1000 mm³ were end-sealed and treated with copper-chrome-arsenate preservative (NZ Type I) to a range of retentions and penetration patterns. Cross-sections, 10 mm thick, were cut from the centre of each billet and used for determination of preservative distribution, for preservative analysis and for decay tests. The decay test consisted of laying samples...
M E Hedley, H Bier


Preservative effect of cellulose insulation material against some mould fungi and brown rot fungus Coniophora puteana in pine sapwood
1991 - IRG/WP 1484
The influence of mineral wool and loose-fill cellulose wool on biodeterioration of pine sapwood was studied. The test fungi were mould fungi Aspergillus versicolor, Cladosporium sphaerospermum, Penicillium sp. and Aureobasidium pullullans and brown rot fungus Coniophora puteana. Cellulose wool inhibited the growth of mould fungi on the face of wood contacted with insulation material at RH of 97 an...
H Viitanen


On the effectiveness of fumigants against wood-destroying insects and fungi in wooden cultural property
1993 - IRG/WP 93-10030
Based on a survey of the history of the use of fumigants the actual agents are mentioned in relation to their biogenic effect on wood-destroying insects and fungi as well as their corrosive behavior on cultural property. Furthermore the conditions for the use of reactive fumigants in buildings are discussed. Trials to control wood-destroying insects and fungi by nitrogen and bromomethane are the m...
W Unger, A Unger


Unsuitability of the limiting dose as a criterion for assessing the toxicity of preservatives to wood-destroying fungi
1974 - IRG/WP 243
In the majority of methods for investigating preservatives for wood-destroying fungi their toxicity is assessed by determining what is called the "limiting dose". This normally denotes a range of preservative solution concentrations or retentions of dry preservative in the timber, the lower value serving to indicate the amount of preservative at which is observed the expected effect, e.g. the grow...
D A Belenkov


The probable mechanism of action of boric acid and borates as wood preservatives
1990 - IRG/WP 1450
The tetrahydroxyborate ion [B(OH)4-] acts by complexation with poly-ols and probably attacks decay fungi through extracellular substrate sequestration; intracellular substrate sequestration; enzyme inhibition; and change in membrane function. Work was carried out to investigate this further and to try to explain certain phenomena observed in the area of boron preservation. The effect of Na borate ...
J D Lloyd, D J Dickinson, R J Murphy


Treatability of waterstored poles of Norway spruce by sap-displacement and pressure treatment with Boliden K33 and creosote
1973 - IRG/WP 328
Poles of windthrown Norway spruce were stored in bark under water sprinklers for 11-20 months or fully submerged in a lake for 3 years (tab. 1 and 2). Water content after storage is shown in fig. 1 and 8. Treatment with Boliden K33 by sap-displacement (open tank suction) gave a poor result. The Danish requirements of delivery claim a penetration of 20 mm and a net retention of 12 kg/m³ in outer 2...
P Moltesen, E Borsholt, B Bang


Poplar wood and its damages in Iran
1987 - IRG/WP 1332
In Iran poplar planting has been used for many centuries ago specially in regions without forests. It had rural uses in ancient time, but recently many fast growing poplar species have been planted and many hybrids also have been planted; the following species had been cultivated widely in Iran: Populus nigra L. var. italica, Populus alba L., Populus caspica Bornm, Populus deltoides L., Populus X....
D Parsapajouh, P Niloufari