Errata to Document No: IRG/WP/3276
1984 - IRG/WP 3285
W E Conradie


Disposal of treated wood - Canada
1990 - IRG/WP 3563
It is estimated that treated wood removed from service each year in Canada contains about 16,000 tonnes of creosote, 1000 tonnes of pentachlorophenol and 245 tonnes of CCA or ACA. The amount of CCA treated wood for disposal is expected to increase more than ten-fold by the year 2020. At present, most treated wood is disposed of in landfills, burned (creosote only) or recycled as other products. Ot...
P A Cooper


Development of a method for testing wood preservatives with soft rot fungi
1975 - IRG/WP 250
Although the first publications on experimental soft rot attack date back 20 years ago, so far no test method for evaluating the efficacy of wood preservatives against soft rot attack (Ascomycetes and Fungi Imperfecti) has been generally accepted. The reasons are diverse and the shortcomings and the disadvantages of the methods described are well known and have repeatedly been discussed. The soil ...
M Gersonde, W Kerner-Gang


Involvement of hydrogen peroxide in wood decay by brown-rot and white-rot fungi
1985 - IRG/WP 1256
To gain further understanding of the role of H2O2 in wood degradation by brown- and white-rot fungi, we studied the following: (a) extracellular H2O2 production, (b) effect of various hydroxyl radical (·OH) and singlet O2 (1O2) quenching agents on wood and cellulose degradation, (c) intracellular H2O2 production and catalase activity, and (d) cytochemical localization of H2O2 with diaminobenzidin...
T L Highley, L L Murmanis


Treatability of Siberian larch and spruce with chromated copper arsenate
1996 - IRG/WP 96-40060
Heartwood of Siberian larch (Larix gmelini) and spruce (Picea jezoensis) was pressure treated with chromated copper arsenate (CCA) Type B using a full cell process. Larch heartwood was somewhat difficult to treat than the spruce, although both species did not meet a minimum requirements of penetration and retention specified by the American Wood Preservers' Association (AWPA) for difficul...
Gyu-Hyeok Kim, Woo-Gue Jee, Jae-Jin Kim


Fungicidal properties of boron containing preservative Borosol 9
2004 - IRG/WP 04-30348
The fungicidal properties of new boron containing wood preservative Borosol 9 is described in this paper. These properties were of particular interest as this new boron containing preservative, exhibit very good performance against wood damaging insects. But because the tested boron formulation contain also nitrogen compounds, we wanted to verify if nitrogen as a nutrient could promote...
G Babuder, M Petric, F Cadež, M Humar, F Pohleven


CCA fixation experiments. Part 2
1989 - IRG/WP 3505
CCA fixation in wood was measured by both squeezing solution from treated wood that had not been dried and analyzing the solution for copper, chromium and arsenic, as well as using a chromotropic acid test to detect the presence of chromium VI. Both methods provide useful information on the CCA fixation process and illustrate that chromium VI disappears as CCA becomes fixed within wood....
W S McNamara


Progress report on collaborative experiments on testing with basidiomycetes
1982 - IRG/WP 2184
The present Document reviews results provided by participants as at 1 May 1982 and draws preliminary conclusions....
A F Bravery


Biodeterioration and preservation of rubberwood (Hevea brasiliensis)
1994 - IRG/WP 94-10084
Plantation-grown rubber trees (Hevea brasiliensis) in the tropics is fast emerging as a significant provider of quality hardwood for a variety of non-structural products, as the aesthetics of the timber is its creamed colour resembling perhaps the priced but depleting Ramin wood or even American beechwood. However rubberwood logs and sawn materials are highly sensitive to sapstain, fungal decay an...
L T Hong, A H H Wong


Leaching of chromium and other cca components from wood-cement composites made with spent CCA treated wood
2000 - IRG/WP 00-50153
Wood cement composites are an attractive option for recycling spent treated wood, since the CCA treatment enhances the physical, mechanical and biological resistance properties of the composite. However, we have noted a higher than normal leaching of chromium from these products and this appears to result from conversion of some of the trivalent chromium to the more leachable and toxic hexavalent ...
D Qi, P A Cooper


Experience with an industrial scale-up for the biological purification of CCA-treated wood waste
1997 - IRG/WP 97-50095
The biological purification of CCA-treated wood waste was tested in co-operation of the BFH and the Italian impregnation plant SoFoMe. Chipped poles were infested with the chromium and arsenic tolerant brown-rot fungus Antrodia vaillantii which can transform in the laboratory ca. 90% of the chromium and arsenic into watersoluble salts. These can be leached to 100-200 ppm residual metal content. Th...
H Leithoff, R-D Peek


Potential toxicants for controlling soft rot in preservative treated hardwoods. Part 4: Evaluation of combined diffusion and toxicity
1979 - IRG/WP 2129
A large number of inorganic and organic preservatives were evaluated as potential soft rot control chemicals, by their degree of inhibition of fungal growth after allowing them to diffuse through a 6 mm thick wood slab. The tests were inoculated with wood powder from soft-rotted CCA treated poles. Pentachlorophenol was unable to diffuse quickly through the wood slab, although formulations with hex...
E W B Da Costa, O Collett


Wood preservation in China
1989 - IRG/WP 3546
Huiming Zhou, Zhongwei Jin


Performance of CCA treated Eucalyptus round ties
1985 - IRG/WP 3342
After 5.5 years of field exposure in the south of Brazil round Eucalyptus ties treated with CCA type A Oxide (OSMOSE K-33-A) preservative with retentions from 12 to 14 kg/m³ (0.75 to 0.873 PCF) (active ingredient basis) are performing very well. No decay or insect attack was observed in the 100 ties in test in real conditions of use; 10% of ties show incipient checking (what is a natural trend of...
V J Carlos, F R Niederauer, J P P Wehr


36 years of wood preservative tests in Tanzania
1992 - IRG/WP 92-3731
The performanee of major wood presevatives which are used widely commereially are given. These include creosote, CCA's and 5% Pentachlorophenol dissolved in heavy industrial diesel. Tests are conducted at three ecologically different using pine stakes. Results show that the striking performance of creosote and CCA's is noticeable at above 128 kg/m³ and 16 kg/m³ respectively....
K K Murira, P F Nangawe


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. 3rd Interim Report
1983 - IRG/WP 4101
This paper updates the results of microbiological examination and marine borer assessment of untreated wood samples (15 x 2 x 2 cm³) and samples treated with 3, 6 and 10% CCA and CCB preservatives. Three reference species - Alstonia scholaris, Fagus sylvatica, Pinus sylvestris were used at all the test sites in addition to local species chosen by participants in the test....
R A Eaton


Sap displacement treatment of utility poles in Papua New Guinea
1977 - IRG/WP 3102
Rapid growth of rural electrification in P.N.G. has created a considerable demand for treated poles. In the past power lines have been run on steel poles but the Government of P.N.G. is now seeking to make maximum use of the country's own resources rather than continue to rely upon imported materials such as steel poles. To some extent, this demand is being met by expansion of existing va...
C R Levy


Antifungal properties of new quaternary ammonium and imidazolium salts against wood decay, staining and mould fungi
2004 - IRG/WP 04-30347
The biological activity of twenty-four potential wood preservatives – imidazolium and quaternary ammonium salts with a modified anion structure was determined employing screening agar-plate and agar-block methods. Experiments were carried out on Scots pine (Pinus sylvestris L.) wood. The aim of the performed studies was to investigate the effect of structure modification of IC and QAC with organ...
J Zabielska-Matejuk, W Wieczorek


Copper binding capacity of modified wood flour
1992 - IRG/WP 92-3709
Wood flour was modified by reaction with oxidising agents and CCA preservative. The copper chromium and arsenic were removed from the CCA treated wood flour by an acid leaching procedure. The modified wood flours were allowed to react with copper acetate solution and the level of copper fixation achieved was determined. The modified wood flours had greater affinity for copper ions present in solut...
N C Milowych, W B Banks, J A Cornfield


HCB - a new preservative combination for wood pole maintenance
1996 - IRG/WP 96-30122
New combination of heavy creosoted boron (HCB) applied on hardwood and softwood logs at different moisture content revealed successful diffusion of boron in all sapwoods within 7 days and in all sapwoods plus hardwoods within 15 days. The new cost effective paste sterilizes wood through diffusion and suitable for pole maintenance at groundline and above groundline e.g. cut ends, drilled holes, woo...
A K Lahiry


Isolation and identification of the fungal flora in treated wood
1976 - IRG/WP 144
J F Levy


Characterization of glycopeptide from white-, brown- and soft rot fungi
2002 - IRG/WP 02-10424
Extracellular low-molecular-weight substances that catalyze a redox reaction between O2 and electron donors to produce hydroxyl radicals have been isolated from wood degrading cultures of white-rot, brown-rot, and soft-rot fungi. They contained protein, neutral carbohydrate, and Fe(II). These substances were glycosylated (glycated) peptides and suggested to form Amadori product (ketoamine). The...
H Tanaka, S Itakura, A Enoki


An experimental method to simulate incipient decay of wood by basidiomycete fungi
2000 - IRG/WP 00-20200
At very early stages of decay of wood by basidiomycete fungi, strength loss can be measured from wood before any measurable weight loss. Therefore, strength loss is a more efficient measure of incipient decay than weight loss. However, common standard decay tests (e.g. EN 113 or ASTM D2017) use weight loss as the measure of decay. A method was developed that allowed progressive removal of samples ...
S F Curling, J E Winandy, C A Clausen


The influence of age on retention and fixation of CCA in pressure-treated Kenyan-grown Eycalyptus saligna: Summary of findings
2002 - IRG/WP 02-30296
The present study investigates the influence of age on retention and fixation of copper-chrome-arsenate (CCA) in Kenyan-grown Eucalyptus saligna. Samples for the study were obtained from sound trees aged 4, 8, 12, 16, 20 and 24 years. Test samples were radially cut from round material to represent total sapwood and heartwood for each age class, and measured 50mm in thickness, 100mm long, with wi...
R Venkatasamy


Leaching of inorganic wood preservatives – Investigating the relationship between leachability, dissociation characteristics and long-term leaching potential
2003 - IRG/WP 03-50199
Estimation of the leaching properties of preservative components is greatly affected by the leaching test method applied since not all methods equally consider the physical components responsible for leaching. These include: wetting of the wood and penetration of water (affected by dimensions, amount of end grain, permeability, duration and nature of water exposure); solution of preservative comp...