Comparison of culturable fungi found on two types of modified wood cladding
2023 - IRG/WP 23-11025
Modified woods are rapidly gaining popularity in the United States and are appearing on more public buildings. Because these are biocide-free products, they can support the growth of non-wood degrading fungi on their surfaces, many of which produce dark pigments and deface the cladding. Even growth of dark pigmented fungi on modified woods yields an even grey-black color, giving the materials a we...
G Presley, J Cappellazzi, B Held, R Blanchette


Glued laminated poles - Progress report after 43 years of testing
2023 - IRG/WP 23-20692
In 1979, a number of glued laminated poles treated with CCA and creosote were placed in a greenhouse in Uppsala, in the Simlångsdalen test field in south-western Sweden and in a power lane in Vuollerim in northern Sweden, in order to study their resistance against biological degradation. The test poles were treated in a two-step process. All laminations of Scots pine (Pinus sylvestris) were first...
J Jermer, M Westin, N Terziev


Simulations of microclimates for wood-decaying fungi in the built environment using environmental analysis
2023 - IRG/WP 23-20703
Simulations of fungal decay risk were run on two similar building geometries exposed to typical annual climate conditions of two different geographical locations, Brunswick (Germany) and Cairns (Australia). The simulations were conducted to capture the effect of wind-driven rain and solar irradiation exposure over nodes of the common building geometry. The moisture content and temperature variatio...
P B van Niekerk, J Niklewski, S H Hosseini, B N Marais, I Frimannslund, T Kringlebotn Thiis, C Brischke


A six-year ground proximity trial of TRU-CORE treatments at Innisfail, Queensland
2023 - IRG/WP 23-30775
This article describes an H3 (above ground outdoor) ground proximity field trial that compares the performance against decay fungi of TRU-CORE (also known as the Buffered Amine Oxide Enhancement System) Copper Quat (CQ) with CCA and commodity Alkaline Copper Quat (commodity-CQ) treatments, all in Pinus radiata. The retentions achieved reflected commercial practice, where higher mean retentions are...
L Cookson


Challenges in managing very long-term field tests
2023 - IRG/WP 23-30779
Field testing of wood preservatives has been on-going in Petawawa, Ontario, Canada since at least 1937. Many of the treated roundwood posts from these early experiments are still in test, and include preservatives still used today, including creosote, copper naphthenate, pentachlorophenol and CCA. Performance data from selected experiments more than 50 years old are reported and we discuss some of...
R Stirling, D Wong


Influence of weathering of wood surfaces before and after treatment with iron(II) sulphate
2023 - IRG/WP 23-30786
Outdoor wood is exposed to various factors that cause the wood to grey or age. The ageing processes can vary greatly depending on the exposure. Parts of the wood that are not exposed to external factors, e.g. under the eaves, are less exposed and the ageing process is therefore slower. This can be accelerated by solutions based on iron ions. In this way, the wood greys quickly and evenly. However,...
B Lesar, M Humar, F Osvald


Outdoor performance of Tanalith® K treated timber: Dimensional stability and corrosivity towards metal fasteners
2023 - IRG/WP 23-30798
This study was carried out to investigate dimensional stability and corrosivity towards metal fasteners in radiata pine (Pinus radiata D. Don) treated with Tanalith® K to Hazard class 4 (H4) retentions in comparison with chromated copper arsenic (CCA) treated timber. For corrosion test, untreated and treated matched specimens were prepared from Australian-grown radiata pine, tested with mild stee...
G Rassam, J Hague, D Humphrey


Multi-scale Experimental Study on Self-sustained Smouldering of CCA-treated Timber Poles
2023 - IRG/WP 23-40988
While it is accepted that appropriate treatment with chromated copper arsenate (CCA) will extend the design life of wood markedly, there are concerns regarding the effect of treatment on fire performance. Smouldering combustion in CCA-treated timber infrastructure can self-sustain, destroying the timber elements, as the chromium and copper present in the CCA can act as catalysts of the smouldering...
W Wu, L Yerman, J J Morrell, F Wiesner


Research on gaseous COS degradation by brown-rot fungus Gloeophyllum trabeum
2024 - IRG/WP 24-11033
Physiological studies of wood rotting fungi have mostly focused on the metabolism of carbon and nitrogen sources, which constitute the dominants components of wood. On the other hand, despite the physiological importance of trace elements such as sulfur, studies on their acquisition sources and metabolic pathways are limited. Until now, wood rotting fungi have been thought to utilize slight amount...
R Iizuka, R Tsukida, Y Katayama, M Yoshida


Characterization of cell wall morphology and water-soluble extractives in Japanese larch decayed by white-pocket-rot fungi
2024 - IRG/WP 24-11034
Porodaedalea chrysoloma (Fr.) Fiasson & Niemelä is a basidiomycete that can cause white-rot decay in Japanese larch (Larix kaempferi) heartwood. P. chrysoloma is a white-rot fungus with a unique pattern that causes white-pocket-rot in the xylem of Japanese larch. However, the mechanism by which P. chrysoloma yields the pattern of white-pocket-rot in Japanese larch heartwood remains unclear. Thus,...
Y Mori, H Arai, T Ito, H Hashitani, K Yamashita, Y Ota, M Kiguchi


Cellulose nanomaterials in growth media for wood decay fungi
2024 - IRG/WP 24-11035
Cellulose nanofibrils (CNFs) were investigated as a partial substitution for agar in growth media for wood decay fungi. Radial growth measurements of eight basidiomycete fungi were taken on solid growth media with and without CNFs. Additionally, fungal strain virulence was evaluated using the European CSN Standard EN 113-2 wood decay durability test. The inclusion of CNFs did not significantly aff...
K M Ohno, R A Arango, R Sabo, C M Clemons, G T Kirker, A B Bishell


Cellulose nanomaterials in growth media for wood decay fungi
2024 - IRG/WP 24-11035
Cellulose nanofibrils (CNFs) were investigated as a partial substitution for agar in growth media for wood decay fungi. Radial growth measurements of eight basidiomycete fungi were taken on solid growth media with and without CNFs. Additionally, fungal strain virulence was evaluated using the European CSN Standard EN 113-2 wood decay durability test. The inclusion of CNFs did not significantly aff...
K M Ohno, R A Arango, R Sabo, C M Clemons, G T Kirker, A B Bishell


On the use of miniaturized wood specimens in fungal decay experiments – mini-blocks versus EN 113 test specimens
2024 - IRG/WP 24-11044
Preliminary evaluation and classification of wood durability against decay fungi using laboratory monoculture experiments has been a longstanding practice because these tests offer quicker results than field tests. Various methods, including miniaturized specimen formats and different incubation periods, have been explored to expedite decay processes and assess wood preservation efficacy. The 'min...
C Brischke, G Alfredsen


A novel cellulose-binding domain from the brown-rot fungus that can be used to evaluate cellulose in wood
2024 - IRG/WP 24-11046
Wood-rotting basidiomycetes are the primary microorganisms that decay wood in nature. They are classified as white-rot fungi and brown-rot fungi by the difference in decaying types. White-rot fungi secrete a variety of cellulolytic enzymes during wood degradation. These enzymes often have an additional cellulose-binding domain (CBD) that adsorbs to the cellulose surface and localizes the catalytic...
Y Kojima, N Sunagawa, S Tagawa, T Hatano, S Nakaba, M Aoki, M Wada, K Igarashi, M Yoshida


Potential of heartwood extracts as wood preservatives combined with linseed oil in 8-year above-ground and in-ground field trials
2024 - IRG/WP 24-20719
The current study assessed the efficacy of heartwood extracts from Tectona grandis, Dalbergia sissoo, Cedrus deodara, and Pinus roxburghii, combined with linseed oil, as protectants for two non-durable wood species against termites and decay fungi. Stakes measuring 45.7 × 1.9 × 1.9 cm and blocks measuring 12.5 × 3.75 × 2.5 cm of the sapwood of southern pine (Pinus sp.) and cottonwood (Populus ...
M E Mankowski, G T Kirker, B Hassan


Changes in decay risk of wood in ground contact over Europe, from analysis of historic climate conditions
2024 - IRG/WP 24-41008
Changing climate conditions will affect global temperature and precipitation patterns, shifting some geographical areas into states that are more suitable for fungal wood decay. Climate normals, which are taken over a 30-year period, capture vast spatial and temporal variations in these conditions and comparing these can show changes over time. Importantly, being able to identify locations that ha...
P B van Niekerk, B N Marais, G Alfredsen, C Brischke


Leaching and chemical redistribution of CCA components in refractory heartwood of E. nitens
2024 - IRG/WP 24-41011
Chromated Copper Arsenate (CCA) is a wood preservative widely used to protect against fungal and insect attack. The fixation mechanism of CCA involves complex chemical reactions, including the reduction of chromium (VI) to chromium (III) and the formation of insoluble complexes. Despite fixation efforts, a portion of CCA components tends to leach from treated wood, influenced by factors like wood ...
J R Vargas, L Yermán, K C Wood, T Singh