Chapter 13 - Slow fixation of CCA-treated bamboo
2007 - IRG/WP 07-10635-13
Chromated copper arsenate (CCA) leachability tests on full-cell pressure impregnated (with 2-3% CCA solution) and slow dried (six months air-drying under cover) bamboo block of three major bamboo species of Bangladesh revealed initial insignificant leaching of CCA within first week and no leaching in next week. Use of low concentration of CCA, release of particle form of CCA due to exposure ...
A K Lahiry


Chapter 14 - Accelerated fixation of CCA-treated bamboo
2007 - IRG/WP 07-10635-14
Chromated copper arsenate type C (CCA-C) fixation study on impregnated (with adequate w/v 6% CCA solution) then boiled, oven-dried, normal, air-dried and steamed bamboo slices of airdried borakbamboo (Bambusa balcooa Roxb.) of Bangladesh, revealed almost complete fixation in steamed (accelerated fixation) and air-dried (3 weeks, slow fixation) bamboo slices compared to moderate to low fixati...
A K Lahiry


Gene expression analysis of a copper-tolerant brown rot fungus on MCQ-treated wood
2011 - IRG/WP 11-10748
Most brown rot fungi are copper-tolerant, which makes them difficult to control with copper-based wood preservatives like MCQ. To better understand what biological processes are regulated, we used our model species, Antrodia radiculosa, to examine expression of genes on MCQ-treated wood. Our hypothesis was genes that decreased copper bioavailability would be up-regulated early, when wood showed ...
J D Tang, A Perkins, S V Diehl


Decay resistance attributes of teak (Tectona grandis L. f.) wood: comparison of the fungicidal activities of quinones
2011 - IRG/WP 11-10752
The implication of quinones in decay resistance of teak wood is controversial. To better understand the role of individual quinone in this property, we studied the correlations between this latter and the content of 2-(hydroxymethyl)anthraquinone, tectoquinone, anthraquinone-2-carboxylic acid, 1,4-naphthoquinone, lapachol and the new compound 4’,5’-dihydroxy-epiisocatalponol found in teak wood...
F B Niamké, N Amusant, N Lemenager, G Chaix, M-F Thévenon, C Baudassé, S Kati-Coulibaly, A Amissa Adima, I Gossan Ado, C Jay-Allemand


Measuring fungal cellulolytic enzyme activity in degrading wood
2011 - IRG/WP 11-10753
An enzyme assay which measures enzyme activity directly from wood will assist in the fundamental understanding of the enzyme components of the decay mechanism of rot fungi and any changes in the presence of wood protectants. At present, to measure fungal carbohydrate degrading enzyme activity in the presence of wood, two methods are used: either 1) the enzyme is measured in the growth media contai...
S M Duncan, J S Schilling


Quantification of four dark colored mould fungi by real time PCR
2011 - IRG/WP 11-10754
Coated wooden claddings in building facades are widely used in the Scandinavian countries, and are often preferred to other materials. Wood is facing increasing competition from other materials that are less labor intensive at the construction site and materials with less demand for maintenance thru service life, and makes further development of wooden claddings essential. Growth of discoloring mo...
E Larnøy, L Ross Gobakken, A M Hietala


Novel Approaches to the Development and Testing of Anti After-glow Additives for CCA-based Treatments of Poles
2011 - IRG/WP 11-30561
In this paper, a field fire stake testing screen method is described. This method uses stake samples from matched wood sources allowing replicates from different boards to be included. The method is easy to control and can provide quick comparative fire resistance test results. The parameters measured from the tests are percentage weight loss, minimum residual circumference and residual thicknes...
L Jin, P Walcheski, A Preston


Characterisation and evaluation of various chitosan oligomers, and decay resistance
2011 - IRG/WP 11-30562
Chitosan, a polymer of D-glucosamine, is known for its antimicrobial activity. However, the physicochemical properties of chitosan depend upon three principal factors, i.e. source of raw material, molecular weight and degree of deacetylation. Here, we report synthesis and characterization of chitosan oligomers prepared by deaminative depolymerization of chitosan (s) obtained from Sigma Aldrich and...
I Hussain, C Chittenden, T Singh


The resistance to Basidiomycetes fungi of chipboard 35 years after their industrial preservation with wood preservative on fluoroborate basis
2011 - IRG/WP 11-40546
The research on wood-based panels’ (WBP) behaviour towards fungi impact demonstrated rather low resistance of wood-based materials to wood rotting fungi. However, these materials are used in construction under conditions favourable to fungi growth. In such conditions WBP treated with wood preservatives should be used. Preservation durability is of great importance in such cases. The resistance o...
A Fojutowski, A Kropacz


Study of the durability of the Maderon® against wood decay fungi and insects
2011 - IRG/WP 11-40548
Many industries produce residues that are not easily degradable. One of these is nut husks which, due to their high level of resistance to biological and environmental degradation, have become an ecological problem. Maderón® is a material invented and patented in Spain employed as an ecological substitute and a modern alternative to certain uses of wood. At present, Maderón® is commercialized ...
M T Troya, F Llinares, P Jiménez, J I Fernández-Golfín, M Conde, R Díaz


Evaluation of an optimized industrial process aiming to improve the natural durability and mechanical behavior of bamboo for outdoor use
2011 - IRG/WP 11-40554
Mao Bamboo (Phyllostachys pubescens) is characterized by high contents of sugar and starch and by high hygroscopicity, which makes it susceptible to biodegradation, and specifically to fungal decay. Still, many bamboo based products regularly enter the European wood construction market, competing with traditional solid wood products used for outdoor decking and cladding. The performance of a heat ...
F Simon, M Kutnik, I Le Bayon, G Moisset, V Gatimel


Challenges and new developments in testing electro osmotic pulsing technology (PLEOT) by means of conventional laboratory methods
2011 - IRG/WP 11-40555
A new wood protection system, electro-osmotic pulsing technology, called PLEOT, is tested in lab trials using different test setup. The technology is tested on Scots pine sapwood and beech wood samples exposed to brown- and white rot fungi. Mass loss and moisture content is calculated after testing and a chitin analysis are performed on the sample powder. Two different electrodes are used in ord...
A Treu, E Larnøy


Performance of Zinc Borate-Treated Oriented Structural Straw Board against Mold Fungi, Decay Fungi and Termites–A Preliminary Trial
2011 - IRG/WP 11-40571
The performance of zinc borate (ZB)-treated oriented structural straw board (OSSB) against mold fungi, decay fungi and termites was examined in standard laboratory evaluations. OSSB was fabricated with split wheat straw and diphenylmethane diisocyante (pMDI) resin. The ZB was added during panel manufacture to achieve preservative levels (wt.%) of 1.0%, 1.5%, 2.0%, and 3.0%. Untreated (0.0% ZB) OSS...
Guangping Han, M Manning, Wanli Cheng, E Pierre, W Wasylciw


Laboratory evaluation of the natural durability and treatability of Cryptomeria japonica grown in La Reunion Island
2012 - IRG/WP 12-10772
The Japanese cedar Cryptomeria japonica is the main resource for timber construction in La Reunion Island, an overseas territory belonging to France. The natural durability of C. japonica originating from East-Asia has been considered so far as quite poor and the European standard EN 350-2 classifies this species ‘not durable’ with regard to its resistance to termites, xylophageous beetles and...
M Kutnik, J Vuillemin, I Paulmier, I Le Bayon, S Legay, E Raphalen, M Jequel, N Farnier, T Glandut


Connecting fungal genomic variations to wood chemical composition: A way to understand the adaptation of wood decaying fungi
2012 - IRG/WP 12-10776
The development of new sequencing methods allows now exploring the detoxication systems of wood-decaying fungi. These systems, called xenome, are mainly composed of oxidative enzymes (phase I) and of conjugation enzymes (phase II). These enzymes belong to superfamilies, which are extended in the plant cell-wall interacting fungi. From different approaches coupling in particular comparative genomic...
E Gelhaye, Y Mathieu, E Meux, A Thuillier, M Mélanie


Inhibition of Basidiospore Germination by Copper from MCQ, ACQ and CCA Leachates
2012 - IRG/WP 12-10778
The long-term decay resistance of refractory wood shell-treated with chromated copper arsenate (CCA) in above-ground exposures has been attributed to mobile copper that migrates into checks and inhibits the germination of basidiospores. Copper from micronized copper quat (MCQ) has also been shown to migrate into checks suggesting similar performance as a shell treatment, but questions have been ra...
R Stirling, J Drummond, P I Morris


Coconut lumber for wood decks (Cocos nucifera L.): decay resistance against Basidiomycetes fungi
2012 - IRG/WP 12-10784
Since a couple of years, manufactured products of coconut wood for outdoor uses like wood decks have been proposed on the European market. These are presented as an alternative for traditional tropical timbers. In the past, coconut wood was neglected and burned for sanitary reasons and lack of interest at industrial scale. Plantation coconut trees at end of production of copra constitute a renewab...
B Jourez, C Verheyen, J Van Acker


Effects of microclimate, wood temperature and surface colour on fungal disfigurement on wooden claddings
2012 - IRG/WP 12-20490
Wooden claddings are common in façades in Norway, and Norway spruce (Picea abies) is the most frequently used species. The cladding is a major part of the facade, and it has visual requirements that may define the aesthetic service life. The visual changes that occur during weathering can be colour changes, abrasion or wear, blistering, flaking, and even cracks in the wood or coating, but more of...
L Ross Gobakken, G I Vestøl


Performance of Wood Protection Systems at Multiple Field Test Sites Using the Ground Proximity Test Method
2012 - IRG/WP 12-20499
A series of preservative systems were used to treat southern pine ground proximity test samples which were then exposed at a range of test sites located throughout the world. The sites were chosen on the basis of having vastly different Scheffer Climate decay indices. After almost 14 years exposure, distinct differences are apparent in how different preservative systems perform at the different ...
A Zahora, A Preston, L Jin


Performance superiority of CCA-C treated wooden jetty poles and piles used for 30 years in Bangladesh against marine borers
2012 - IRG/WP 12-30582
Observational study along with previous investigation and records revealed that chromated copper arsenate type C (CCA-C) impregnated southern pine poles and piles of jetty constructed in most vulnerable brackish water in Bangladesh are stable and resistant to attack of all types of marine borers after 30 years of use. It is evident from the service records of other construction materials that CCA-...
A K Lahiry


Performance of wood treated with linseed and tung oil against wood decay fungi and wetting
2012 - IRG/WP 12-30598
Most of the European wood species does not have durable wood. In order to use it in outdoor conditions nondurable material has to be protected. Nowadays, non-biocidal solutions for wood protection are attracting a lot of attention, particularly in use class 2 and 3 applications. One of the non-biocidal techniques is treatment of wood with water repellents like wax emulsions and oils. Linseed oil a...
M Humar, B Lesar


Analyses of premature failure of utility poles
2012 - IRG/WP 12-40584
In this study a total number of 18 utility poles of Scots pine (Pinus sylvestris) impregnated with a copper-chromium containing preservative were investigated. They were part of different lower voltage transmission lines in the western part of Germany and failed before predicted minimum service life. All poles in this study were less than 15 years in use. The type of decay and fungi were evaluated...
S Bollmus, N Rangno, H Militz, A Gellerich


The resistance of thermo and thermo-oil modified black poplar wood (Populus nigra L.) to Basidiomycetes fungi
2012 - IRG/WP 12-40585
The share of area taken by poplar tree species in Poland account for 2.0% of the area of state forests, 4.8% of national parks and for 2.3% in the privately-owned forests. It is shown and expected an increase in the share of poplar stands connected with plantation of fast growing trees. The poplar wood is not resistant to Basidiomycetes fungi, easy attacked by insects and in consequence is regarde...
A Fojutowski, A Kropacz, A Noskowiak


A survey of factors affecting decay resistance of wood modified with acetic anhydride
2012 - IRG/WP 12-40594
From the range of information published, acetylation appears well suited to provide adequate protection against biological attack for materials derived from typically non-durable wood species. Acetylated wood is now commercially available both in Europe and in the USA. But still there are a lot of unanswered questions related to fungal decay mechanisms in acetylated wood. The paper summarize exist...
G Alfredsen, P O Flæte, H Militz


Environmental safeness of 60% and 72% concentrated CCA-C solution and paste for wood treatment
2012 - IRG/WP 12-50284
In this study 30-years practical and observational experience of the present author about using of 72% concentrated CCA-C paste for preparing treating solutions and for treating wooden poles, anchor logs and cross arms has revealed that the 60% concentrated CCA-C solution is superior to the 72% concentrated CCA-C paste regarding solubility, homogeneity, cleanliness, treatability, sludge formation,...