Performance of borate-treated lumber in a protected, above-ground field test in Japan
2004 - IRG/WP 04-30344
This document is supplemental to the previous IRG document (Tsunoda et al., 2002). An experiment to simulate the sill plate (dodai) of the Japanese houses was conducted at the termite field test site of the Wood Research Institute in Kagoshima, Japan where two economically important subterranean termite species [Coptotermes formosanus Shiraki and Reticulitermes speratus (Kolbe)] are established. ...
K Tsunoda, A Byrne, P I Morris, J K Grace


Anti-sapstain chemicals for diffusion treatment of rubber wood
1986 - IRG/WP 3367
Performance of Sinesto B and Akzo EN 494, two formulated products of alkyl ammonium compounds, was tested as fungicidal additive in the boron solution to control mould and stain during diffusion storage of rubber wood. Sinesto B at 2.0% (a.i.) concentration has given good control over mould and its protection against sapstain was only satisfactory. Akzo EN 494 at 0.7% (a.i.) concentration has give...
R Gnanaharan


Gelatin encapsulated fumigants for wood fumigations: Current research status
1985 - IRG/WP 3336
The fumigants chloropicrin (trichloronitromethane) and methylisothiocyanate (MIT) were encapsulated in gelatin as an alternative to liquid fumigant treatments for control of decay fungi in wooden utility poles. Gelatin-encapsulated MIT was stored for over 2 years under dry conditions without significant fumigant leakage. Gelatin encapsulated MIT and chloropicrin were released from capsules when pl...
A R Zahora, M E Corden, J J Morrell


A bioassay of remedially treated pole material
1987 - IRG/WP 3453
Stubs prepared from treated and untreated utility poles were installed in a test plot and pressure spade treated at the groundline with one of four preservative greases. At one and three year intervals, core samples were removed from the stubs and the improvement in the preservative efficacy due to the greases was assessed. The bioassay investigation showed that only bis(tributyltin) oxide (TBTO) ...
J N R Ruddick, L Parker


Effects of pre-harvest girdling on selected properties of red pine, red maple and Eastern larch
1999 - IRG/WP 99-40137
Trees of three species - tamarack (Larix laricina), soft maple (Acer rubrum) and red pine (Pinus resinosa) - were girdled immediately below the crown,one to two years before felling. The wood from these trees was compared with wood taken from un-girdled control trees felled at the same. Sapwood and heartwood, from the controls, and from above and below the girdle of treated trees, were examined fo...
A Taylor, P A Cooper


The effect of oil-borne preservative treatments on the shear strength of FRP/wood composite adhesive bonds
2003 - IRG/WP 03-40265
Reinforcement of structural wood components with Fiber Reinforced Polymer (FRP) will enhance the beam’s strength, but actual data on long-term durability is sparse, not well documented or not readily accessible. In this study, bond properties of FRP-wood composite materials were investigated following treatment with creosote or copper naphthenate preservatives. The properties investigated inclu...
B Herzog, B Goodell, R Lopez-Anido


A review of the current status of the estimation of emissions from preserved wood and their use in the environmental risk assessment of wood preservatives under the Biocidal Products Directive
2005 - IRG/WP 05-50224-7
A review and update of the status of the issues concerning the estimation of emissions from preserved wood (e.g. amendments to the proposed ‘OECD Guidelines’), and the environmental risk assessment of wood preservatives under the Biocidal Products Directive (e.g. compartmental sizes, emissate ecotoxicity testing)....
E F Baines


The functional anatomy of the digestive caecae and gut residence times for the marine wood borer Limnoria (Crustacea: Isopoda)
1997 - IRG/WP 97-10204
A scanning and transmission electron microscope study of the digestive caecae of the marine wood boring isopods Limnoria tripunctata and Limnoria quadripunctata, was undertaken. Two cell types were identified, containing structures indicative of absorption, secretion and storage. Cell types were distinguished according to size, the largest cell type having a large free surface area, a well develop...
C Wykes, S M Cragg, A J Pitman


Evaluation of literature on adenocarcinomas in wood workers
1997 - IRG/WP 97-50092
Occupational exposure to wood dust alone or chemically treated is suspected to be associated with an increased risk of developing adenocarcinoma of the nasal cavity, which in the general population is very rare; fewer than 10% of nasal cancer deaths are adenocarcinomas, which have an annual incidence of 1-2 per million. However, the epidemiological data available are not sufficient to make a defin...
A Voss, R-D Peek


Microbial ecology of treated Lap-joints exposed at Hilo, Hawaii for 24 months
1997 - IRG/WP 97-20107
This paper is a continuation of previous work reported in IRG/WP 96-20089 by Molnar et al. (1996) in which Lap-joints, made from Southern yellow pine and treated with ACQ, DDAC or propiconazole were sampled over 12 months exposure at Hilo, Hawaii. 18 and 24 month samplings have since taken place and are reported here. TnBTO treated Lap-joints made of scots pine which were exposed later as a standa...
S Molnar, D J Dickinson, R J Murphy


Selecting fumigants for treatment of internal decay in wood
1986 - IRG/WP 3370
A number of potential fumigants were screened with respect to their toxicity to decay fungi, (Poria carbonica, and Lentinus lepideus) and their sorption characteristics on Douglas Fir (Pseudotsuga menziesii Mirb. Franco) wood. Wafers of infected wood were exposed to different fumigant concentrations for various times then cultured to determine viability. The lethal concentration X time (ct) factor...
P A Cooper


Moisture Adsorption Behaviour of Rubber Wood Decayed by Brown and White rot Fungi
2005 - IRG/WP 05-40306
Moisture adsorption behaviour of rubber wood blocks decayed by each brown rot and white rot fungi was studied. The adsorption isotherms of decayed wood were compared with the isotherm of undecayed wood. The wood decayed by brown rot adsorbed less moisture as compared to sound or undecayed wood at all humidity levels. No significant difference was observed in adsorption behaviour of white rot dec...
S S Chauhan, H C Nagaveni


Collaborative soft rot tests: Specific gravity loss resulting from soft rot
1973 - IRG/WP 227
It was proposed at the 5th meeting of Working Group II of the IRG in June 1973 in Lahti, Finland, that the specific gravity (swollen volume basis) of test blocks used in the IRG Collaborative Soft Rot Tests should be determined on all the blocks at the completion of the exposure period. Specific gravity determined on the basis of the oven dry weight and water swollen volume was selected because (1...
C R Levy


The use of organic wood preservatives in ground contact and the suitability of laboratory test procedures to determine their efficacy
1999 - IRG/WP 99-20175
Organic fungicides, such as propiconazole, have proven to be highly effective when used as a co-biocide in recently developed wood preservative formulations. They have however been ineffective when used as a stand alone preservative, particularly when used in ground contact (European Hazard class 4). Previous research, using the test methods of ENV 807 (1993), provided conflicting evidence regardi...
I J Herring, D J Dickinson


Characterization of wood decay enzymes by MALDI-MS for post-translational modification and gene identification
2002 - IRG/WP 02-10442
The recent sequencing of the Phanerochaete chrysosporium genome presents many opportunities, including the possibility of rapidly correlating specific wood decay proteins of the fungus with the corresponding gene sequences. Here we compare mass fragments of trypsin digests, determined by MALDI-MS (Matrix Assisted Laser Desorption Ionization-Mass Spectrometry), with predicted mass fragments derive...
T H de Koker, P J Kersten


A simple field apparatus for measuring relative gaff penetration and assessing the effect of additives for improving pole climbability
2000 - IRG/WP 00-20187
A simple apparatus for measuring and comparing the relative "hardness" of utility poles is described. This "slide-hammer" gaff penetration apparatus was designed as a field testing unit to measure the depth of gaff penetration into test poles after application of a uniform and reproducible force to the gaff. The apparatus is simple to use in both the laboratory and field. Data is provided for resu...
A R Zahora


Co-operative tests concerning the influence of solvent and drying method on the toxic limit of wood preservatives against Coniophora cerebella
1972 - IRG/WP 216
In the working group II of the IRG it was agreed that more knowledge was necessary concerning the influence of the solvent on the toxic limit of organic solvent types of wood preservatives against Basidiomycetes. A test program was drawn up and after discussion in the mentioned working group the final program was accepted by the co-operating institutes in 1969. In the test program two fungicides, ...
T Hof


The effect of kerfing on check formation in treated white spruce (Picea glauca) poles
1981 - IRG/WP 3167
62 white spruce poles, 6 m in length, were cut from full size utility poles commercially pressure treated with preservative. 21 of the poles were treated with pentachlorophenol, while of the remainder, all of which were treated with ammoniacal copper arsenate, 22 were kerfed and 19 were unkerfed. The poles were installed in the Westham Island field test site, near Vancouver, and inspected annually...
J N R Ruddick


Water transfer in wood in relation to fungal attack in building - Effect of condensation and diffusion
1992 - IRG/WP 92-1543
Wood is continuously exchanging moisture with the surrounding atmosphere, the temperature and relative humidity are important factors. Wood moisture in this case is not enough to provoque decay by fungi. However, when, during the night, condensation appears cyclically, wood absorbs water and moisture content may be sufficiently high to allow development if drying does not take place. The water tra...
D Dirol, J-M Vergnaud


Potential use of an emulsified tar oil fraction as a wood preservative: Preliminary technological and environmental assessment
1994 - IRG/WP 94-50028
In order to meet the recent environmental concern specifications of creosote are altered, the B[a]P content is limited and restrictions on the emission of volatile organic compounds (VOC) and higher polyaromatic hydrocarbons (PAH) are expected in some countries. Research has been conducted on an emulsion of a selected tar oil fraction. Using a waterborne formulation opens new perspectives for targ...
G M F Van Eetvelde, R Leegwater, M Stevens


Bethoguard; A new wood protecting fungicide for use in metal free ground contact wood preservatives
2002 - IRG/WP 02-30301
Research has identified the limitations in both the spectrum of activity and permanence of organic biocides placed in wood in high hazard environments, particularly in the absence of heavy metals such as copper. More specifically, the control of soft rot decay in wood in soil contact has proven to be most problematic. The new organic biocide, Bethoguard; an oxathiazine, has demonstrated excellen...
S C Forster, G R Williams, M Van Der Flaas, M Bacon, J Gors


Aggressiveness of Reticulitermes species in laboratory test
1993 - IRG/WP 93-10026
In European Standards concerned with the preventive action of wood preservatives against termites, i.e. EN 117, EN 118 the obligatory test species is Reticulitermes santonensis. It is argued that this species is more aggressive than the second European Reticulitermtes species, Reticulitermes lucifugus. Since Reticulitermes santonensis is confined to certain smaller areas in France and thus not rea...
H Hertel, S Pantos, D Rudolph


Soft rot - Soil burial - Tests. Influence of the addition of nitrogen compounds to the soil on wood decay by soft rot
1972 - IRG/WP 213
The decay of wood specimens buried in soil is influenced by various factors. Decisive are the water content, the content of organic substances, the pH-value, the content of mineral nutritive salts, nitrogen content, etc. of the soil. These tests were carried out in order to investigate if the decay of wood in the soil will be influenced by additions of various nitrogen-compounds in different conce...
O Wälchli


Antagonism of Gliocladium virens against wood decay fungi
1995 - IRG/WP 95-10102
Antagonistic abilities of a commercial biofungicide, Gliocladium virens (GL-21, Grace) were evaluated against three white-rot fungi, Trametes versicolor, Phlebia brevispora, Irpex lacteus, and three brown-rot fungi, Postia placenta, Neolentinus lepideus, Gloeophyllum trabeum. In dual culture of Gliocladium virens and wood decay fungi, Gliocladium virens rapidly overgrow the decay fungi and killed ...
T L Highley, L Ferge


Changes of copper and chromium content after leaching in wood impregnated with the CCB and CB preservatives
2000 - IRG/WP 00-50147
The objective of the study was impregnated with CCB and CB preservatives pine wood of moisture content varying from 12% to 55% subjected to leaching. Losses of copper and chromium were determined for individual layers of wood up to 3 cm from the girth. The results were compared to the total amount of metals determined in water extracts. The degree of leaching of metal ions from wood of 55% moistur...