IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3713 documents. Displaying 25 entries per page.


The Fifth Annual Report of the International Research Group on Wood Preservation 1973-1974
1974 - IRG/WP 531
IRG Secretariat


Model questionnaire for preparation of monographic cards for wood-destroying fungi
1972 - IRG/WP 103
C Jacquiot


A bibliography of organic solvent-based wood preservatives
1973 - IRG/WP 322
H Alliot


The role of communication in the field of environment protection: A case study "Wood Protection"
1990 - IRG/WP 3574
L Wöss


The potential of 2-deoxy-D-glucose as an active ingredient in wood preservation
1999 - IRG/WP 99-30205
2-deoxy-D-glucose (2-DOG) is a potential active ingredient against wood decaying fungi. When dissolved in water, it can be used in pressure treatment of wood. Thereby the wood is protected from attack by wood decaying fungi. A concentration of 1.5% (mean retention 9.7 kg/cubic meter sap-wood) is adequate for brown rot fungi, and 3% (mean retention 19.5 kg/cubic meter sapwood) will also provide protection against white rot fungi. 2-DOG is easily soluble in water, and is therefore easily leached from the wood upon completion of the preservation process. Different types of fixa-tion methods have been tried and evaluated. It is possible to produce 2-DOG by the hydrolysis of chitin, a constituent of the exterior skeleton of shellfish and insects. There is a potential for exploita-tion of this waste product provided by the crab and shrimp industry. The yield of 1 kg of fresh shrimp is 75 g of 2-DOG.
O V Frederiksen, A P Koch


Kinetic modelling of adsorption of quaternary ammonium compounds by Scots pine wood sawdust (Pinus sylvestris L.)
2005 - IRG/WP 05-30369
The adsorption of new quaternary ammonium compounds from aqueous solutions onto Scots pine wood (Pinus sylvestris L.) sawdust was studied. The pseudo first- and second- order kinetic models were used for the mathematical description of the sorption dynamic process of QACs onto wood. The highest correlation coefficients were obtained for the pseudo-second order kinetic model, those suggest that che...
J Zabielska-Matejuk


Water-based water repellents for treatment of wood
1987 - IRG/WP 3446
The water uptake by wood can be reduced by treatment with a water repellent. The water repellents most commonly used are solvent based. In the present work a new type of water repellent that is water-based has been investigated. Two different treatments have shown an effect of the same order as a commercial solvent based product. The cellular distribution of the water repellents has been investiga...
I G Svensson, G Hägglund, I Johansson, W B Banks


The use of C CP/MAS NMR in the chemical identification of decayed and undecayed, tropical timber species
1984 - IRG/WP 1224
13C CP/MAS NMR was found to be an extremely powerful tool for elucidating the chemical composition of Eucalyptus maculata, Pinus elliottii and Alstonia scholaris. The differences in lignin composition were different for each timber and discussed in relation to decay caused by soft-rot and white rot fungi. In particular the presence of syringyl and guaiacyl lignin types are discussed.
L E Leightley


Editorial corrections to Document No: IRG/WP/304
1972 - IRG/WP 305
Anonymous


The Second Annual Report of the International Research Group on Wood Preservation 1970-1971
1971 - IRG/WP 502
IRG Secretariat


Biological control of decay in standing creosote-treated poles
1976 - IRG/WP 156
Internal decay caused by basidiomycetes in standing creosoted poles can be controlled biologically, it seems, by artificial inoculation near the ground line. For such inoculation IC-type facultative mycoparasites, Scytalidium sp FY strain or Trichoderma spp for example, may be used. Apparent residual action can be explained by the release of non water soluble chemically stable antibiotics from the...
J Ricard


The Fifteenth Annual Report of the International Research Group on Wood Preservation 1985-1986
1986 - IRG/WP 5243
R Cockcroft


Airborne algae as a wood degradation factor
1992 - IRG/WP 92-1549
The occurrence of airborne (aerophytic) algae on wood is a very frequent phenomenon. However, there is currently a lack of information concerning their effect on the wood tissue. Some important genus of algae infesting wood under natural conditions are listed, as well as the results of experimental studies in the "in vitro" culture concerning the effect of two selected algal species on some physic...
K J Krajewski, J Wazny


Differences in feeding activity among colonies of Formosan subterranean termite Coptotermes formosanus Shiraki
1983 - IRG/WP 1202
Feeding activities of 7 colonies of the Formosan subterranean termite, Coptotermes formosanus Shiraki, were examined. Wood-consumption rates among colonies differed significantly, ranging from 23.80-78.48 mg/g/day. This large intraspecific variation raised a question of whether differences in feeding activity reported for other termite species were due to interspecific differences. When rates were...
N-Y Su, J P La Fage


Wood preservatives ecotoxicology on Gammarus pulex (L.) - toward an environmental monitoring method and a getting rid of pollution process
2005 - IRG/WP 05-50224-9
Wood preservatives can have a strong impact on freshwater invertebrates when used close to aquatic ecosystems. It has been reported in Jura that different arthropod taxa, specially crustaceans, have disappeared along several kilometers downstream from factories using insecticides and fungicides as wood preservatives. The crustacean Gammarus pulex (L.) is a relevant bioindicator to characterize th...
O Adam, F Degiorgi, G Crini, P-M Badot


The rate of redistribution and loss of leachable preservatives under service conditions
1993 - IRG/WP 93-30026
This paper describes experiments carried out to determine patterns of preservative redistribution and any associated losses which occur when wood containing unfixed water-soluble wood preservatives is exposed to service conditions where leaching is possible. Scots pine sapwood treated with disodium octaborate was used as a model system. Results are recorded and discussed for trials representing pa...
R J Orsler, G E Holland


The International Research Group on Wood Preservation
1979 - IRG/WP 582
J M Baker


New developments in wood preservation
1974 - IRG/WP 335
Most of the developments in wood preservation in recent years have been stimulated by changing circumstances, particularly the increasing interest in reducing hazards and environmental, pollution but also the serious difficulties that are now being encountered in obtaining economic supplies of established preservatives. There is perhaps a danger that new controls to reduce pollution dangers may be...
B A Richardson


Wood preservation in East European countries
1989 - IRG/WP 3527
The paper discusses the main problems of wood preservation in Bulgaria, Czechoslovakia, German DR, Hungary, Poland, Rumania and the USSR. The main types of wood preservatives produced have been presented, as well as the state of standarization to test their properties. There have been considered methods of wood treatment in use and application range of treated wood....
J Wazny


Water-repellent additive for CCA
1991 - IRG/WP 3655
Hickson have developed a water repellent additive for incorporation into copper-chromium-arsenate timber treatment solutions. The water repellent emulsion shows good stability in the treatment solution, is easily incorporated and applied in a single stage treatment. No modifications to the additive is safe to treatment schedule are usually needed and use. Weathering of the treated wood is substant...
P Warburton, R F Fox, J A Cornfield


The performance of wood preservatives in soil-bed soft rot tests
1993 - IRG/WP 93-20007
Testing the efficacy of wood preservatives in soil is recognised as a fundamental part of the assessment of long-term wood protection in ground contact. Laboratory based tests can provide a hazardous environment in which a preservative can be challenged by a range of micro-organisms. This paper presents the results of tests carried out to investigate the performance of wood preservatives in a wet ...
G R Williams, S Caswell


The interaction of polyflavonoid tannins with CCA in Pinus radiata
1987 - IRG/WP 3422
Polyflavonoid tannins complex easily and rapidly with metal ions such as copper, chromium, and arsenic. such complexes in high-tannin-containing CCA treated hardwoods might result in essentially under-treated timber. Four aspects of this interaction were investigated: 1) The relationship between tannin contents of seven hardwoods (Betula pendula, Alstonia scholaris, Fagus sylvatica, Liquidambar st...
K G Ryan, D V Plackett


Framework document for an international code of good practices for wood preservation and wood protection (anti-sapstain) facilities
1992 - IRG/WP 92-3683
At the Kyoto meeting, the Health & Safety committee agreed to form a task force to prepare a global plan for writing a code of good practices (Code) for wood protection and preservation facilities (Doc. No. IRG/WP/3681). The Canadian document had been presented to the IRG group earlier (Doc. No. IRG/WP/3447) and similar documents were solicited from other countries for preparing a framework do...
V N P Mathur, G Das


The isolation of actinomycetes from wood in ground contact and the sea
1980 - IRG/WP 1110
M S Cavalcante, R A Eaton


Detection of incipient brown rot decay in wood by fourier transform infrared spectrometry
1987 - IRG/WP 2275
Fourier transform infrared spectrometry was evaluated as a possible method for detecting different levels of brown-rot decay in pine sapwood. By using first derivative spectra and regression analysis, an equation based on 4 absorption peaks, normalized with an internal standard peak, was developed. The correlation between weight loss and absorption was highly significant indicating that this is a ...
D D Nicholas, T Schultz