IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1274 documents. Displaying 25 entries per page.


A Prediction of Arsenic Groundwater Concentrations Influenced by Construction and Demolition Debris Landfills in Florida Containing CCA-Treated Wood
2006 - IRG/WP 06-50242
Groundwater fate and transport models can provide an indication of the potential impacts of arsenic from the infiltration of leachate from unlined C&D debris landfills containing CCA-treated wood. A solute transport model, Migration of Organic/Inorganic Chemicals (MYGRT), was chosen to predict groundwater contaminant concentrations at specified locations from a hypothetical source (C&D lan...
J Jambeck, T Townsend, H Solo-Gabriele


An Investigation of the use and Durability of some Industrial and Domestic woods of Iran against Destructives factor in Caspian Sea
2007 - IRG/WP 07-10613
Use of domestic and commercial woods of the Caspian Sea forest fringes and evaluation of their durability against marine destructive factors were investigated. The samples of species of elm (Zelkova carpinifolia), oak (Quercus castanifolia), beech (Fagus orientalis), Maple (Acer insgin), Alder (Alnus subcordata), and horn beech (Carpinus betulus) were impregnated with CCA (Chrome–Cupper-Arsenic)...
S M Kazemi


Wood decay fungi from New Zealand ‘leaky’ buildings: PCR identification and laboratory decay tests of wood preservative-treated Pinus radiata (Part 1)
2007 - IRG/WP 07-10620
Fungi colonising Pinus radiata D. Don framing timber of ‘leaky’ New Zealand buildings were isolated to produce pure cultures. Mycelia from these cultures on agar media were collected to extract DNA. To identify the fungi to the species level, polymerase chain reaction (PCR) with primer pairs ITS1-F and ITS4 were performed followed by sequencing of the internal transcribed spacer (ITS) region. ...
D Stahlhut, R L Farrell, R Wakeling, M Hedley


Corrosion of metal fasteners in contact with copper preservative treated wood
2007 - IRG/WP 07-20370
The corrosion rates of metal fasteners in contact with alkaline copper quat (ACQ) treated wood with or without commercially available water repellent was compared to that of cedar. In this experiment, fasteners were sandwiched between two pieces of treated wood and exposed to a humid environment at a slightly elevated temperature. The use of a “sandwich” design allowed periodic examination of ...
BaekYong Choi, J N R Ruddick


Use of the Digital Refractometer for the On-site Analysis of Copper-based Preservative Systems
2007 - IRG/WP 07-20371
In some counties, there are no on-site chemical analysis methods available for treatment plants to use to determine the key active ingredients in the preservative treatment solutions. The complexity of the sophisticated methodology; cost of analytical instruments and training required for operating these instruments in treating plant level are the reasons for lacking such practice. In this paper...
L Jin, T Cashman, A Preston, J Trompetter, H Trompetter


Permethrin: A Critical Review of an Effective Wood Preservative Insecticide
2007 - IRG/WP 07-30413
Permethrin is a synthetic pyrethroid used in the wood preservation industry. The generally favorable environmental profile of pyrethroids coupled with their high efficacy led to their wide substitution of the chemically resistant organochlorines dieldrin, lindane, and chlordane formerly used for protection of buildings against wood destroying organisms. Much of the research on performance of perm...
M H Freeman, D N Obanda, T F Shupe


Efficacy of chitosan in combination with GRAS (Generally Recognised As Safe) compounds as a potential wood preservative
2007 - IRG/WP 07-30414
In vitro studies were undertaken to evaluate the synergy between chitosan and selected GRAS (Generally Recognised As Safe) compounds against two sapstain fungi Sphaeropsis sapinea and Leptographium procerum. Bioassays performed on nutrient medium suggested that some of the GRAS compounds tested including sodium benzoate, potassium sorbate and ascorbic acid had a synergistic effect when combined w...
C Chittenden, K Thämelt, T Singh


Silver – The Next Generation Wood Preservative
2007 - IRG/WP 07-30419
The successful introduction and commercial use of products designed to have controlled release of silver ion over long time periods prompted the Silver Research Consortium and the US Forest Products Laboratory to undertake research to see if silver could also be an effective wood preservative to be used in place of chromated copper arsenate (CCA) now prohibited for use in the United States and els...
J R Ellis, K Jayachandran, D Nicholas


Silver as a Wood Preservative Environmental Requirements and Concerns
2007 - IRG/WP 07-30420
The pesticide uses of silver and its compounds fall under the jurisdiction of the United States Environmental Protection Agency (USEPA) under the US Federal Insecticide Fungicide and Rodenticide Act. In addition, many other national and international organizations maintain close observance of the effects of silver in different environments. The US EPA has also issued a specific announcement that t...
J R Ellis


Preservative treatment of Golla cane (Daemonorops jenkinsiana) by pressure process
2007 - IRG/WP 07-40379
The feasibility of preservative treatment of golla cane (Daemonorops jenkinsiana (Griff) Mart). by pressure process has been studied using water borne preservatives CCB (copper-chrome-boron). Cane samples of three different lengths 1m, 2m and 3 m. were treated at different pressure and time period to evaluate the extent of penetration and retention of preservative chemicals. It was observed that t...
K Akhter, M Hoque Chowdhury


Use of Moisture Meters with Treated Wood
2007 - IRG/WP 07-40382
Drying wood treated with waterborne preservatives after treatment to near outdoor EMC conditions improves its physical performance characteristics. This is primarily due to the reduced checking, splitting and warping which can occur when wet wood, particularly if restrained from shrinking by being nailed or otherwise fastened, shrinks in use. Monitoring of the drying process, rate, and end point...
W B Smith, Hwan Myeong Yeo, C Stark, B Morey, C Tascioglu, P Schneider, D Herdman, M Freeman


Influence of Grain Direction on Penetration, Retention, and Leaching of CCA(C) in Sapwood and Heartwood of Kenyan-Grown Eucalyptus saligna and Acacia mearnsii
2007 - IRG/WP 07-40383
Penetration, retention, and leaching of CCA (C) in relation to grain orientation were tested in small (50mm x 50mm x 200mm) sapwood and heartwood samples of Eucalyptus saligna and Acacia mearnsii. In both sapwood and heartwood of the two species, the results showed a consistent pattern: Transverse > Radial > Tangential. Whereas penetration, retention, and leaching were significantly high i...
R Venkatasamy


Influence of Grain Direction on Penetration, Retention, and Leaching of CCA(C) in Sapwood and Heartwood of Kenyan-Grown Cupressus lusitanica and Pinus patula
2007 - IRG/WP 07-40384
The influence of grain orientation on penetration, retention, and leaching of CCA (C) was tested on small samples of sapwood and heartwood of Cupressus lusitanica and Pinus patula. Samples measuring 50mm x 50mm, and 200mm in the longitudinal axis were sealed to expose only transverse, or radial, or tangential faces, pressure treated with 6% CCA (C), and penetration, retention and leaching of the ...
R Venkatasamy


Influence of ethanolamine on lignin depolymerization and copper leaching from treated Norway spruce and beech wood
2007 - IRG/WP 07-30423
Copper-ethanolamine based wood preservatives are replacing several classical copper-chromium based solutions, due to foreseen ban of chromium. Fixation of copper-ethanolamine based wood preservatives is not as good as fixation of copper-chromium ones. The main object of this manuscript was to prove, that ethanolamine is the prime reason for insufficient fixation of copper-ethanolamine formulations...
M Humar, B Bucar, M Zupancic, D Žlindra, F Pohleven


Copper fixation in ACQ-D treated Chinese fir at various temperature and relative humidity conditions
2007 - IRG/WP 07-30436
In this study, the effect of different conditions of temperature, relative humidity, and duration of post-treatments on accelerating copper fixation in ACQ-D treated Chinese fir wood blocks was investigated. The conditions include the combination of three temperatures (21, 50, and 70?) and two relative humidity levels (20% and 80%), also include four temperatures (50, 70, 90, and 110?) without con...
Jinzhen Cao, Lili Yu


Tropical In-Ground Durability of CCB-treated Keruing and other Structural Sarawak Timbers after 8 – 10 Years Exposure
2007 - IRG/WP 07-30439
The heartwood of 12 mainly low-durability native timber species of Sarawak [4 Dipterocarpus (Keruing) species, Anisoptera grossivenia (Mersawa kunyit), Canarium apertum (Seladah), Dacryodes incurvata (Seladah laut), Dryobalanops oblongifolia (Kapur kelansau), Mesua macrantha (Mergasing), Podocarpus micropedunculatus (Kayu cina), Shorea compressa (Engkabang langgai), and Pterospermum javanicum (Ba...
A H H Wong, Ling Wang Choon


Micro-Distribution of Metals in Wood Treated with a Nano-Copper Wood Preservative
2007 - IRG/WP 07-40360
The microdistribution of copper in southern pine treated with a newly-developed nano-copper wood preservative was examined to determine if it differed from that reported for wood treated with conventional copper-based wood preservatives. Field Emission Scanning Electron Microscopy (FE-SEM) in combination with x-ray microanalysis (EDX) revealed the presence of nano-sized copper and iron particles i...
H Matsunaga, M Kiguchi, P Evans


Effect of barriers on moisture content of treated and non-treated utility poles
2007 - IRG/WP 07-40369
The potential for non-biocidal barriers to slow moisture sorption was investigated using butt treated western redcedar poles immersed in either water or moist soil over a 2 year period. Moisture sorption was initially slowed by the barriers, but openings at the bottoms of the barriers eventually allowed moisture to migrate upward. Moisture levels in wrapped poles eventually reached those found in...
C S Love, J J Morrell


Durability of some alternatives to preservative-treated wood. Progress report 2: Results from field tests after 5 years’exposure
2007 - IRG/WP 07-30442
A number of alternatives to preservative-treated wood have been tested according to EN 252 (stake test) and a specially designed ground-proximity field test, the latter in Sweden as well as in Hawaii, USA. Seven untreated wood species and four alternative wood treatments labelled as environmentally friendly (acetylation, linseed oil, heat treatment, vinyl polymer) were included in the study. Four ...
M-L Edlund, J Jermer


Development of preservative treatment method using sub and super critical carbon dioxide
2007 - IRG/WP 07-40385
Significant efforts have been devoted for developing biocide impregnation method into wood materials using supercritical fluid. Developing better understandings of fluid phase and its effect on treatment results would facilitate a more rational development of supercritical fluid (SCF) impregnation. In this project, the preservative treatabilities under super- and sub-critical fluid conditions we...
Myeung-Won Cho, Sung-Mo Kang, Gyu-Hyeok Kim


Kd values of Cu, Cr, As in different soil matrix
2007 - IRG/WP 07-50247
Chromated copper arsenate (CCA), a long history of successful preservative, have raised environmental concerns. Adsorption characteristics of domestic soils for chromium, copper, and arsenic were assessed by measuring distribution coefficient (Kd) values of these metal components. The results revealed that Kd values were higher in chromium, followed by arsenic and copper in soil matrix. Different...
Sung-Mo Kang, Seung-Hun Shin, Ja-Oon Koo


Development of boron/linseed oil combined treatment as a low-toxic wood protection. Evaluation of boron fixation and resistance to termites according to Japanese and European standards
2007 - IRG/WP 07-30448
Combinations of boric acid as a first step of treatment and linseed oil as a second step have been performed in order to enhance boron retention to leaching and wood resistance to termites. Classic leaching and termites resistance standards are inappropriate to evaluate this combination which can be considered as both a wood core preservation treatment and a coating. Japanese Industrial Standard...
F Lyon, M-F Thevenon, Y Imamura, J Gril, A Pizzi


An Investigation on Use and Durability of Some Industrial and Domestic Woods of Iran against Destructive Factors in Caspian Sea
2008 - IRG/WP 08-10636
In this study the use of domestic and commercial woods of the Caspian Sea forest fringes and evaluation of their durability against marine destructive factors were investigated. The samples of elm (Zelkova carpinifolia), oak (Quercus castanifolia), beech (Fagus orientalis), Maple (Acer insgin), Alder (Alnus subcordata), and horn beech (Carpinus betulus) species were impregnated with CCA (Chrome–...
S M Kazemi


Performance of softwood preservative treated stakes after 4 years exposure in-ground to decay fungi and termites in tropical Australia
2008 - IRG/WP 08-10643
This field study was based on the 1993 IUFRO method and designed as a graveyard (in-ground) test in the tropical region of the Northern Territory to examine the efficacy of novel preservative formulations developed as alternative protection for softwood timber against decay fungi and termites for Hazard Class 3 and 4. This study was supported by the Forest and Wood Products Research and Develop...
B M Ahmed (Shiday), J R J French, S R Przewloka, P Vinden, J A Hann, P Blackwell


Validity of above ground testing according to ENV 12037
2008 - IRG/WP 08-20379
The standard ENV 12037 for testing of treated and untreated wood (lap-joint) exposed above ground was issued in 1996 by The European Committee for Standardization. A draft for the development of the standard was presented by CEN-TC 38/WG 25/DOC N 076 in 2002. For a test to become valid the median rating of decay for untreated control replicates (Scots pine sapwood) must be equal or greater than ...
Ö Bergman, U Råberg, N Terziev


Previous Page | Next Page