IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 968 documents. Displaying 25 entries per page.


Recycling of impregnated timber: Part 2: Combustion trial
1999 - IRG/WP 99-50132
Totally 270 m3 (61,3 t) of CCA impregnated wood was chipped and incinerated at the combustion plant of Jalasjärvi. After the normal gas cleaning venture scrubbers were tested. After the trial a metal balance was calculated. Ash was treated at the copper smelter of Outokumpu Harjavalta Metals Oy. Condensate waters were transfered to the Outokumpu's CCA production plant and utilized by the...
L Lindroos


Proposals for a field experiment to determine the performance of preservative treated hardwoods with particular reference to soft rot
1975 - IRG/WP 342
It is proposed to treat a series of hardwood stakes in the UK and install them in different sites around the world. The stakes will include 3 reference species common to every site and 2 locally selected species. The hazard of termites should be avoided in order to limit the study to action of micro-organisms....
D J Dickinson


Water-borne preservative marine trials in Western Canada
1981 - IRG/WP 470
Red pine boards treated with chromated copper arsenate, ammoniacal copper arsenate, copper zinc arsenic additive, a modified ammoniacal copper arsenate, and zinc arsenic additive, have been installed in a marine field test at West Vancouver, British Columbia. After two and a quarter years exposure, all the test samples are in excellent condition with the exception of those treated with the zinc ar...
J N R Ruddick


Disposal of Pressure Treated Wood in Construction and Demolition Debris Landfill
2005 - IRG/WP 05-50235
Pressure treated wood is often disposed in landfills in the US, very frequently in construction and demolition (C&D) debris landfills. C&D debris disposal facilities in many states are not equipped with liner systems to protect underlying groundwater. In this paper, issues associated with the disposal of metal-containing treated wood in C&D debris landfills are discussed. C&D de...
T G Townsend, B Dubey, J Jambeck, H M Solo-Gabriele


Disposal of CCA treated waste wood by combustion - An industrial scale trial
1996 - IRG/WP 96-50068
Totally 272 m³ (62.7 t) of CCA treated utility poles were chipped and incinerated at Jalasjärvi Gasification Plant. In average the whole batch of chips contained 57 kg of elementary copper, 95 kg chromium and 76 kg arsenic. During the 56 h combustion trial the measured arsenic emission to the air was 76 g in total. Copper and chromium emission was less than 1 g. The condensing water from the coo...
A J Nurmi


Preservación de maderas en Bolivia
1986 - IRG/WP 3360
Este documento ofrece datos generales concerníentes a los recursos forestales de Bolivia, las facilidades existentes para preservación de maderas, la investigación y educación en esa materia. Se proporciona información sobre instituciones vinculadas a la actividad y las perspectivas del tratamiento de maderas en el país....
A S Viscarra


An interim report on trials with 'Boliden K33' and 'Celcure A' in water of different salinities in the Baltic Sea and in the UK
1974 - IRG/WP 406
It was felt necessary to undertake field trials using large test samples exposed in natural water of different salinity in order to determine preservative leaching and to assess the degree of biological attack....
R A Eaton, D J Dickinson


Ground contact performance of wood treated by the MSU process
1990 - IRG/WP 3609
Environmental concerns have prompted a renewed interest in accelerated fixation schemes for CCA-treated wood. Results from stake tests of southern pine (Pinus sp.) treated using a conventional Bethell cycle are compared with matched stakes treated using the MSU Process. The effects of adding boric acid to the preservative formulation are also discussed. Differences among test plots are discussed....
H M Barnes, T L Amburgey, R W Landers


Copper based water-borne preservatives: The use of a thin section technique to compare the protection of wood by copper based preservatives against soft-rot and bacterial decay
1987 - IRG/WP 2286
This paper describes the techniques developed and gives examples of results obtained for the performance of copper based wood preservatives against both the bacterial and fungal hazards....
A M Wyles, D J Dickinson


The use of image analysis to quantify soft rot decay
1992 - IRG/WP 92-2410
Image analysis techniques can provide quantitative information from visual images. As part of a wider interest in decay assessment methods we have investigated the application of image analysis techniques for quantifying soft rot decay by Chaetomium globosum in transverse sections of birch wood and bamboo. A method for reducing contamination of the section (and image) by the fungal hyphae and of s...
P J Wickens, R J Murphy


Wood preservation in Kenya
2000 - IRG/WP 00-40191
Current research on wood preservation in Kenya is mainly on the development of biological control of wood-destroying termite species, using mycoinsecticides. The major research institutions include the Kenya Agricultural Research Institute (KARI), Kenya Forestry Research Institute (KEFRI), Moi University and the International Centre for Insect Physiology (ICIPE). Training institutions include Fore...
G Ochiel


Evaluation of termiticides in field trials
1990 - IRG/WP 3633
Termiticide-treated posts and stakes have been tested at the field test site in Kagoshima, Southern Kyushu, Japan. Various commercial and alternative termiticides have been evaluated annually as TAI (termite attack index), calculated by the equation: TAI = R x P, where R is the mean of attack rating of 0 (sound), 10 (sign of tasting), 30 (slight attack), 50 (moderate attack), 100 (severe attack), ...
M Takahashi, Y Imamura, K Tsunoda, A Adachi, K Nishimoto


Available iron promotes brown rot of treated wood
1992 - IRG/WP 92-1526
Exposure of treated wood blocks to rusting iron increased the toxic threshold of chromated copper arsenate and ammoniacal copper arsenate to a brown-rot fungus Leucogyrophana sp. This supports the hypothesis that the movement of iron ions into wood contributes to the unexpectedly high decay rate of treated wood at the stake test site at Westham Island BC. To what extent this phenomenon may occur e...
P I Morris


Germination of basidiospores on preservative treated wood after leaching or natural weathering
1981 - IRG/WP 2150
In tests of residual toxic efficacy after leaching or natural weathering, spore germination with Gloeophyllum trabeum has proved to be a less reliable criterion of attack than when used with unaged preservative treatments. Since spores sometimes prove more tolerant than their parent mycelium, their use should be continued....
J K Carey


Effects of the addition of polyethylene glycol to the CCA-C preservative treatment
1985 - IRG/WP 3337
A modification of the CCA-C wood preservative system for utility poles has been investigated to see if spur penetration into the poles is assisted during climbing. Addition of polyethylene glycol to the CCA system has been shown to accomplish this purpose. This paper addresses the effects of the addition of polyethylene glycol to other physical properties germane to utility poles....
W P Trumble, E E Messina


Computer-assisted numerical clustering analysis of various strains of Serpula lacrymans (Wulfen:Fr.) Schroeter apud Cohn
1992 - IRG/WP 92-2396
Eight strains of Serpula lacrymans were compared in relation to their previously determined factors (5 physiological and 10 toxicometrical). A numerical clustering analysis was used along with, as coefficient of similarity, "cos Q" after standardization of all results. Results with respect to the combined factors showed a mutual similarity within four groups of strains. The first of these groups c...
J Wazny, J D Thornton, P Stenzel


The use of the Pilodyn for detecting soft-rot decay in CCA treated eucalypt poles
1986 - IRG/WP 2251
A 6 Joule Pilodyn unit with 2.5 mm diameter pin was used to inspect CCA treated eucalypt poles, suspected of suffering groundline soft-rot decay. Pole plugs were removed at the inspection region and the amount of soft-rot decay present determined microscopically. High correlation (R² = 0.73) was obtained between the amount of soft-rot and Pilodyn pin penetration. The Pilodyn is recommended as a u...
L E Leightley, G A Willoughby


Patterns of bacterial attack in preservative treated eucalypt power transmission poles
1984 - IRG/WP 1223
Patterns of bacterial decay have been examined using light and scanning electron microscopy. Two morphologically distinct patterns have been recognised in preservative treated eucalypt power transmission poles. Bacterial Decay I (BDI) involves the removal of the secondary wall layers initiating with erosion of the S3 layer from the cell lumen. As decay progresses the S2 layer and S1 layer are degr...
G A Willoughby, L E Leightley


Laboratory simulation of leaching from creosote treated wood in aquatic exposures
2000 - IRG/WP 00-50157
Creosote has a long history of use as a preservative particularly in industrial wood products, but its use has come under increasing scrutiny as a result of concerns about its potential effects on aquatic and terrestrial non-target organisms. Despite its long use, there is relatively little data on the rates of creosote loss in many exposures. In this report, we describe small scale leaching tank ...
Ying Xiao, J Simonsen, J J Morrell


The potential for accelerated ageing to determine the persistence of active ingredients in timber
2006 - IRG/WP 06-20323
Fast screening methods for evaluating the persistence of active ingredients in timber are proposed. This is an outline proposal which is intended to provoke discussion and further development of the methods. Reliable and accurate analytical methods are key to these tests....
L D A Saunders, M R Powell


Collaborative soft rot experiments 1974. Preliminary analysis of results
1975 - IRG/WP 251
J K Carey, J G Savory


A behaviour of CCA penetration of fir (Abies bornmulleriana Mattf.) at different ramp times and constant vacuum/pressure applications
2006 - IRG/WP 06-40346
A behaviour of CCA penetration of Bornmulleriana fir (Abies bornmulleriana Mattf.) at different ramp times and constant vacuum/pressure applications was illustrated for the main flow directions by the experimental pictures....
I Usta, R Despot, M Hasan


The variability of preservative distribution in test blocks
1973 - IRG/WP 220
The techniques for the assessment of likely effectiveness of preservative systems have long been the subject of much discussion. The whole field has recently been reviewed by Hilditch and Hamblyn (1971) who described in detail many of the laboratory test procedures used, but who also indicated the deficiencies in many of these techniques. It has long been the view of many associated with the wood ...
F W Brooks, M R Gayles, R W Watson


Visualization of inorganic element distribution in preservative treated wood by SEM-EDXA
2001 - IRG/WP 01-40208
SEM-EDXA was found to be an effective way of visualizing inorganic element distribution in wood as it was possible to examine some inorganic elements at the same time and map the concentration differences in color. Japanese cedar sapwoods were impregnated by vacuum treatment with CuAz or by pressure treatment with CCA preservatives and then distribution of Cu, Cr and As elements in wood were exami...
H Matsunaga, R Matsumura, K Oda


Water-borne wood preservatives against marine borers. Results from NWPC marine trials started in 1972 and 1976
1990 - IRG/WP 4162
The paper presents the results from NWPC (Nordic Wood Preservation Council) marine trials started in 1972 and 1976. The trials are carried out according to the NWPC Standard No. 1.4.2.2./73 "Marine test - a test against marine wood boring organisms in sea water". The test site is Kristineberg Marine Biology Station on the west coast of Sweden. The wood blocks used in the trials were made from sapw...
Ö Bergman, C Lundberg


Previous Page | Next Page