Your search resulted in 3612 documents. Displaying 25 entries per page.


Fiji wood preservation regulations
1980 - IRG/WP 3138
A S Alston


The Fourth Annual Report of the International Research Group on Wood Preservation 1972-1973
1973 - IRG/WP 522
IRG Secretariat


nvestigation of anomalous fixation and leaching of CCA-treated red maple
2004 - IRG/WP 04-30341
The fixation of CCA-C preservative was investigated in red maple sawdust (Acer rubrum L.) at target retentions of 4.0, 6.4, 9.6 and 30.0 kg/m3. The effect of water-soluble extractives on the course of fixation was evaluated comparing the non-extracted with pre-extracted samples treated to 6.4 and 30 kg/m3. Leaching of the CCA components was monitored after complete fixation for all retentions. Fix...
S Radivojevic, P A Cooper


Environmental issues: Messages for the wood preservation industry
1985 - IRG/WP 3353
A review of the origins and structure of environmental legislation throughout those territories of the world where wood preservation is a major industry is given. The implications of media, industry and legislation interaction is discussed and suggestions made as to the key issues the wood preservation industry should concentrate its attentions on in the immediate future....
D G Anderson, P Waldie


Environmental impact of CCA poles in service
1997 - IRG/WP 97-50087
Soil samples from different depths and distances from CCA treated utility poles in Canada were analyzed for copper, chromium and arsenic content for a number of soil types, two wood species red pine (Pinus resinosa) and jack pine (P. banksiana) and different pole ages in service. A limited number of poles were equipped with water traps to collect rain water that dripped down the poles and where su...
P A Cooper, Y T Ung, J-P Aucoin


Ecotoxicological risks of anti-sapstain preservatives washed off from treated timber
2000 - IRG/WP 00-50144
A field method for ecotoxicity assessment of rain water wash-off from anti-sapstain treated timber was developed. In the course of this study freshly sawn timber treated with 1.5% Busan 30 L (reference preservative) and a control stack with untreated pine were exposed to weathering. The run-off water was ecotoxicologically tested with organisms from three trophic levels (Vibrio fischeri, Kirchneri...
G Aschacher, R Gründlinger


The Eleventh Report of the International Research Group on Wood Preservation 1980-82
1982 - IRG/WP 5154
IRG Secretariat


Extracellular layers of wood decay fungi and copper tolerance
1983 - IRG/WP 1180
Extracellular layers around the hyphae of brown, white and soft rot fungi have been examined using electron microscopy. These layers were isolated for identification. Particular interest was directed towards the extracellular layers of copper-tolerant soft rot fungi....
D M Francis, L E Leightley


Volatile borates in the treatment of wood and wood based panel products against subterranean termites
1995 - IRG/WP 95-30094
Blocks of pine solid wood, oriented strand board and plywood were treated with trimethyl borate by vapour treatment. It was meant to obtain either a full impregnation of the specimens or a shell treatment of the outer three millimetres. The efficacy of the treatments against subterranean termites (Reticulitermes lucifugus) was evaluated using an European Standard method....
L Nunes, D J Dickinson, R J Murphy


Short term preconditioning of preservative-treated wood in soil contact in relation to performance in field trials
2000 - IRG/WP 00-20185
The effect of pre-exposure to primary colonising micro-organisms on preservative-treated wood, prior to a basidiomycete decay test, was determined by preconditioning in two soil types. Scots pine EN 113 blocks treated with 3 model systems (a triazole, a copper quaternary compound and a copper boron triazole) were leached according to EN 84 and subjected to 6 weeks and 8 weeks burial in either John...
S Molnar, D J Dickinson


Reliability-based service life prediction methodology for assessment of water protection efficiency for coatings on wood
2003 - IRG/WP 03-20268
Assessment of water protection efficiency according to EN 927-5 has been shown to give significant differences in water absorption values for different types of coatings on wood. It is shown that the combination of EN 927-5 and an artificial weathering procedure gives more information regarding expected durability and long-term performance than a single measurement of water absorption on fresh, un...
J Ekstedt


Chemical investigation of 23-year-old CDDC treated southern yellow pine
1997 - IRG/WP 97-30141
The effect of 23 years exterior exposure on CDDC treated southern yellow pine was evaluated by the application of solid state analytical instrumentation. Analytical methods including environmental scanning electron microscopy (ESEM),energy dispersive X-ray analysis (EDXA), X-ray photoelectron spectroscopy (XPS), X-ray diffraction (XRD), inductively coupled plasma (ICP) and atomic absorption spectr...
D P Kamdem, C R McIntyre


The present classification of wood degradation factors
1994 - IRG/WP 94-10071
The revised version of classification of wood degradation factors is presented after discussion and remarks sended by IRG-Members. The classification contains the biotic and abiotic factors in two aspects: etiological and symptomatical....
J Wazny


A collaborative test to determine the efficacy of polyurethane coatings on wood samples exposed in the marine environment
1984 - IRG/WP 4113
Aims are: a) to determine the effectiveness of elastomeric polyurethane as a protective coating against marine wood boring animals in a range of tropical and tempreate sites; b) to compare the adhesion of polyurthane coatings on different wood species exposed in seawater; c) to record the severity of attack in failed samples and to identify the causal marine organisms....
R A Eaton


Evaluation of polystyrene as a protective of wood in sea-water
1986 - IRG/WP 4129
A test is described on the biological protection of wood by treatment with polystyrene. The results, obtained in marine trials, after 18 months, show that the treatment with polystyrene is not all that effective in preventing the attack of marine borers....
A Gambetta


European standardization for wood preservation
1990 - IRG/WP 2359
G Castan


On the problem "House Longhorn Beetle" in hardwoods and an aid to distinguish between Hylotrypes bajulus and Hesperophanes cinereus larvae
1981 - IRG/WP 1141
S Cymorek


Sequential exposure of borate treated Douglas-fir to multiple Formosan subterranean termite colonies in a 40-week field test
1993 - IRG/WP 93-10006
Douglas-fir boards (ca. 74.5 g) pressure-treated with disodium octaborate tetrahydrate (DOT) retentions of 0 (controls), 0.88, 1.23, 1.60, or 2.10% (weight/weight) DOT were sequentially exposed to four active field colonies of Formosan subterranean termites, Coptotermes formosanus Shiraki (Isoptera: Rhinotermitidae), in an above-ground field test. Samples were placed in contact with each colony fo...
J K Grace, R T Yamamoto


The resistance of fifteen Indonesian tropical wood species to the powder post beetle Heterobostrychus aequalis
1990 - IRG/WP 1429
A preliminary laboratory test on the resistance of 15 tropical wood species to Heterobostrychus aequalis has been carried out using small samples of 7.5 x 5 x 1.5 cm³. The results reveal that Pinus merkusii and Agathis borneensis are very susceptible to Heterobostrychus aequalis. Other 13 species vary between susceptible to resistance There is no signifisant relation between starch content and th...
Jasni, Nana Supriana


Natural durability and basic physical and mechanical properties of secondary commercially less accepted wood species from Brazil
2002 - IRG/WP 02-10451
The natural durability towards basidiomycete fungi and termites of several secondary timber from Brazil (Vatairea sp., Hymenolobium sp., Inga sp., Manilkara sp., Caryocar sp., Terminalia sp., Apuleia sp.) has been evaluated according to the EN 350-1. Some basic physical and mechanical properties (density, shrinkage, hardness, colour, static strength in flexion and compression) were also measured a...
M-F Thévenon, A Thibaut


Improved resistance of Scots pine and Spruce by application of an oil-heat treatment
2000 - IRG/WP 00-40162
Spruce (Picea abies L. Karst.) and Scots pine (Pinus sylvestris L.) were subject to a heat treatment which was carried out in an oil-bath. The aim was to improve the dimensional stability of the treated wood and its resistance against fungi. The bath of vegetable oil provides a uniform heat transfer at temperatures of 180°C, 200°C and 220°C and protects the submersed wood from oxygen. Heat trea...
M Sailer, A O Rapp, H Leithoff


Collaborative soft rot tests: 2nd interim report
1975 - IRG/WP 258
J G Savory, J K Carey


Influence of storage on mould susceptibility of wood at relative humidity values lower than 100%
1989 - IRG/WP 1413
It is well known that wood material changes with time because of different environmental influences. The effects of such changes on the subsequent mould susceptibility are less known. In this paper we report on increased mould susceptibility of pine wood after storage. Mould growth was detected by indirect methods....
J Bjurman


CEN Draft Standard (38 N 460F): Méthode d'essai pour determiner l'efficacité d'un produit de préservation du bois en milieu marin
1986 - IRG/WP 4132 F
G Castan


Natural resistance of twenty-six Guianese wood species against marine borers
1988 - IRG/WP 4144
This note is a contribution on the study of the natural resistance of some wood species from French Guiana, some of which could be found too in the neighbourhood. Here are presented the results after one year exposure in the marine environment....
L N Trong


Previous Page | Next Page