IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3612 documents. Displaying 25 entries per page.


An attempt to evaluate wood resistance against fungal decay in non-sterile conditions by measuring the variation of resistance to bending test
1988 - IRG/WP 2308
The main object of this work was to determine the variation of strength on large test specimens of wood (800 x 45 x 45 mm³) when exposed to accelerated fungal attacks close to natural conditions, out of test vessels. The modulus of elasticity (MOE) and the modulus of rupture (MOR) have been assessed. Thereby, the natural resistance of the wood species to fungal decay, the efficiency of preservati...
L N Trong


Gloeophyllum trabeum and Gloeophyllum abietinum, the most frequent brown rot fungi in fir wood joinery
1999 - IRG/WP 99-10319
In Croatia the primary raw material for joinery production is silver fir wood (Abies alba Mill). L-joints made of home-grown fir sapwood and prepared according to EN 330: 1993 were used to establish the infection and colonisation of micro-organisms, particularly wood decay fungi, to compare the performance of untreated and 1% TnBTO treated L-joints. The L-joints were coated with two types of coat,...
R Despot, M Glavas


IRG test of preservative-treated hardwoods with particular reference to soft rot. Report on condition of specimens installed in Victoria, Australia
1982 - IRG/WP 3207
J Beesley


European standardization for wood preservation
1989 - IRG/WP 2335
G Castan


Conservation of wooden cultural property
1994 - IRG/WP 94-30038
A survey of the conservation of wooden archtitectual monuments, art objects and archaeological finds is presented. Each of the three areas has typical conservation problems which reqire the use of selected wood preservatives and consolidation agents. Furthermore specific protection and consolidation methods are necessary. A precise damage diagnosis with non-destructive testing methods is the first...
A Unger, W Unger


The resistance of painting materials and consolidants against wood-destroying insects
1997 - IRG/WP 97-10239
Natural and synthetic adhesives, varnishes, painting materials and consolidants were used in investigations of bioresistance against newly hatched larvae and beetles of Hylotrupes bajulus (L.). Animal glues, casein, drying oils and natural resins such as dammar resin and shellac, were not resistant to attack by these larvae. Similarly, semi- and all-synthetic polymers tested including hydroxypropy...
W Unger, H Fritsche, A Unger


Wood preservation in the USA
1982 - IRG/WP 3215
This report is a comprehensive survey of the status of the wood preservation field in the U.S.A. at the start of the 1980s. The importance of wood preservation is discussed and its industry described. Various statistics and analyses regarding the use of treated wood have been compiled. Both pressure and non-pressure applications have been covered, as well as remedial treatments and pest control op...
D D Nicholas, R Cockcroft


Leaching of copper, chromium and arsenic from CCA-treated Scots pine exposed in sea water
2000 - IRG/WP 00-50149
A laboratory leaching trial combining a static and a flowing seawater system was carried out to measure the leaching rates of copper, chromium and arsenic from the surface of Scots pine panels vacuum-pressure treated to 3, 6, 12, 24, and 48 kgm-3 CCA. Untreated and treated panels were exposed in flowing seawater for up to 8 weeks followed by 2 weeks submersion in static seawater which was taken fo...
C J Brown, R A Eaton


The susceptibility of 35 Amazon wood species to Cryptotermes brevis (Walker)
1982 - IRG/WP 1160
Laboratory tests were carried to evaluate the susceptibility of 35 Amazon hardwoods to Cryptotermes brevis (Walker). The results were analysed statistically and showed that five wood species were non resistant, nine were resistant and the other twenty-one in between those classes of resistance....
M D Canedo


The Ninth Annual Report of the International Research Group on Wood Preservation 1978-1979
1979 - IRG/WP 579
IRG Secretariat


The leaching of copper, chrome and arsenate from CCA-impregnated poles stored for ten years in running water
1978 - IRG/WP 3122
There is no evidence to indicate that the chromium and copper components are leached from the outermost 5 mm of sapwood in poles impregnated with Boliden K33 and Tanalith C and stored in running water for ten years. The arsenic component, however, seems to be leached out during the first few months to an extent of about 20% of the initial amount. The leaching time is dependent on the preservative ...
F G Evans


Radical changes in the requirements for more safe pressure impregnation in the Nordic countries in 1988
1990 - IRG/WP 3581
After introduction of quality control schemes and standards in the Nordic countries during the seventies, the first radical change of the standards and practice of work took place after pressure from the labor unions and authorities in 1988 and 1989 in Denmark and in Sweden. A new class of preservation with less retention for out of ground contact use was introduced, fixation times were prolonged ...
B Moldrup


Short-term field test method with accelerated infection of Basidiomycetes in wood
1981 - IRG/WP 2155
In the ŠIPAD - IRC Wood Protection Laboratory an attempt has been made to develop a simple short-term method for field testing out-of-ground contact wood using accelerated infections with Basidiomycetes. This method makes it possible to obtain a preliminary assessment of a preservative's quality and to estimate the possibility of achieving promising results in more expensive long-term te...
N Vidovic


Vertical distribution of fouling and wood-boring organisms in the Trondheimsfjord (Western Norway)
1981 - IRG/WP 467
Results of a detailed study on the vertical distribution of fouling and wood-boring organisms of Trondheimsfjord at an interval of 3 m from intertidal level to a depth of 30 m, has been presented, based on data collected from two series of panels, exposed from 15 March 1977 to 15 July 1977 (Series I) and from 22 July 1977 to 13 March 1978 (Series II). The intensity of fouling generally decreased w...
L N Santhakumaran


Working Group I 'Biological Problems' Sub-group 'Insects in dry wood (other than termites)', Scope of work
1976 - IRG/WP 152
S Cymorek


Tebuconazole, a new wood-preserving fungicide
1990 - IRG/WP 3634
TEBUCONAZOLE, an anti-fungal triazole compound, has been tested to assess the effectivness as wood preserving fungicide. Tests were made with the active ingredient and also in formulations against basidiomycetes, blue-staining fungi and mould. Results of the DESOWAG laboratories and also from official institutes will be presented. In addition to this there were made different toxicological and eco...
B Wüstenhöfer, H-W Wegen, W Metzner


Decay resistance of wood removed from poles treated with Trichoderma
1989 - IRG/WP 1386
Wood blocks removed from a distribution pole previously treated with a biological control product (Binab FYT pellets) were exposed in soil block tests to selected basidiomycetes. The blocks were removed from regions of poles where Trichoderma colonization had been confirmed by extensive sampling and computer mapping of microbial inhabitants. The results indicate that material from pole interiors c...
A Bruce, B King, T L Highley


What information can we glean from field testing
1995 - IRG/WP 95-20057
To mathematically compare the performance of preservatives in a field test, equations were formulated to describe the relation between log score and time and between rate of decay and retention. By combining these equations, a model was derived for the performance of a number of waterborne preservatives. Some relations between the estimated parameters for different preservatives were noted and the...
P I Morris, S Rae


Biological Durability of Laminated Veneer Lumber from Durable and Non-Durable Wood Species
2005 - IRG/WP 05-10567
Laminated Veneer Lumber (LVL) was laboratory manufactured using veneers from decay and non decay resistant species in order to evaluate changes in the durability as a result of the LVL manufacturing process, and to test if the mixing of decay resistant species and non decay resistant species can improve durability. Laboratory soil block test and field test were conducted. The durability of solid w...
P Nzokou, J Zyskowski, S Boury, D P Kamdem


A discussion of current theories concerning CCA fixation
1983 - IRG/WP 3238
The understanding of the fixation mechanism of CCA and related preservatives in wood has been greatly improved by a significant series of recent scientific papers. In view of recent concerns in New Zealand regarding the long-term efficacy of CCA in high decay-hazard situations, it was considered appropriate to review this recent work and to contrast it with theories presented by previous workers....
D V Plackett


Collaborative soft rot tests: Interim report on PRL tests of Cu/Cr/As preservative using method of Document No: IRG/WP/208
1972 - IRG/WP 211
Preservative: Tanalith CT.106 - Results obtained with beech are given in the table and indicate a toxic limit of 16.7-19.2 kg/m³ - The initial soil moisture content was adjusted to 27.8% (the water holding capacity). Noticeable drying out has occurred in some of the test bottles....
J G Savory


Establishment of a laboratory method to characterise the ecotoxicity of a polluted soil
1998 - IRG/WP 98-50101-23
This method consists in using the underground grub of the Oxythyrea funesta beetle as a bioindicator of the soils pollution. Due to the significant tolerance of the organism, a large type of substrate of different nature and grain size could have been studied. We have tested substances and preparations such as wood preservation products even under powder or liquid form but also some wastes of di...
P Martinet


Selective adsorption of antisapstain actives from two aqueous suspensions, and movement of actives into wood
1996 - IRG/WP 96-30103
Green-off-saw rough sawn Pinus elliottii (slash pine) boards were dipped in aqueous suspensions of two antisapstain formulations, NeXgenâ and Busanâ Sap Stain Preventative (Busan 1009), at three product concentration levels. Concentrations of active ingredients (NeXgen: CTL (chloro-thalonil) and MTC (methylene bisthiocyanate); Busan 1009: TCMTB (2(thiocyanomethylthio)-benzothiazole) and MTC) wer...
M J Kennedy, T L Woods


Blue stain in service on wood surface coatings. Part 2: The ability of Aureobasidium pullulans to penetrate wood surface coatings
1992 - IRG/WP 92-1557
The ability of Aureobasidium pullulans to penetrate seven different wood surface coatings was examined. Eight isolates of Aureobasidium pullulans were used. Following penetration, light microscopy was used to examine the effect of the fungus upon the coating, and growth at the wood-film interface. The fungus showed different growth capabilities with different types of surface coatings. Some isolat...
P R Sharpe, D J Dickinson


The effect of treatment method on CCA efficacy in Corsican pine
1992 - IRG/WP 92-3723
As part of a study into the influence of application method on preservative efficacy Corsican pine (Pinus nigra) samples (50 x 50 x 400 mm³) were treated with a CCA formulation using Bethel, Steam/Bethel or Lowry processes. Full penetration of the preservative at a gross level was confirmed using a copper disclosing reagent. The preservative was allowed to fix and then samples were converted into...
P R Newman, R J Murphy