IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1832 documents. Displaying 25 entries per page.


Treatment of dried sawn spruce and redwood building timbers with water-borne preservatives under a scheme for the quality control of the preservation and preserved wood in the Netherlands
1978 - IRG/WP 3123
Treatment of dried sawn spruce and redwood Building Timbers with water-borne preservatives under a scheme for the quality control of the preservation and preserved wood in the Netherlands. The aim of this article is to give the reader a modest description of the evaluation of fundamental research in wood preservation into a practical application....
H F M Nijman, N Burgers


Evaluation of wood treated with copper-based preservatives for Cu loss during exposure to heat and copper-tolerant Bacillus licheniformis
1999 - IRG/WP 99-20155
Copper-based wood preservatives need to be effective against exposure to all types of microorganisms. Wood treated with six copper-based preservatives was exposed to 121°C and 20 psi pressure for 15 minutes under standard autoclave conditions and the copper-tolerant bacterium, Bacillus licheniformis CC01, for 10 d at 28°C and 150 rpm. Sixteen to 37 percent of the copper was released from the woo...
D M Crawford, C A Clausen


Short term preconditioning of preservative-treated wood in soil contact in relation to performance in field trials
2000 - IRG/WP 00-20185
The effect of pre-exposure to primary colonising micro-organisms on preservative-treated wood, prior to a basidiomycete decay test, was determined by preconditioning in two soil types. Scots pine EN 113 blocks treated with 3 model systems (a triazole, a copper quaternary compound and a copper boron triazole) were leached according to EN 84 and subjected to 6 weeks and 8 weeks burial in either John...
S Molnar, D J Dickinson


Chemical investigation of 23-year-old CDDC treated southern yellow pine
1997 - IRG/WP 97-30141
The effect of 23 years exterior exposure on CDDC treated southern yellow pine was evaluated by the application of solid state analytical instrumentation. Analytical methods including environmental scanning electron microscopy (ESEM),energy dispersive X-ray analysis (EDXA), X-ray photoelectron spectroscopy (XPS), X-ray diffraction (XRD), inductively coupled plasma (ICP) and atomic absorption spectr...
D P Kamdem, C R McIntyre


Fungicidal and termiticidal effectiveness of alkylammonium compounds
1983 - IRG/WP 3232
This paper is related to effectiveness of several AAC's against wood decay fungi and termites by Japanese standardized test methods....
K Tsunoda, K Nishimoto


Forest products laboratory methodology for monitoring decay in wood exposed above ground
1995 - IRG/WP 95-20074
Research at the Forest Products Laboratory on the durability of wood in service has included a full complement of laboratory and field tests. In this report, we present a review of past and current methods used to evaluate the condition of preservative-treated wood exposed above ground. Current protocols are described for tests on wood packaging, roofing, and dimension lumber....
R C De Groot, T L Highley


Fiji wood preservation regulations
1980 - IRG/WP 3138
A S Alston


Microbial biofouling of 10-40% naphthalene in creosote treated and untreated wooden pilings in the marine environment
1978 - IRG/WP 442
R R Colwell, P L Fish, D A Webb, A J Emery


Collaborative field experiment: Analysis of copper and chromium in stakes of the four reference timbers
1982 - IRG/WP 3213
The stakes analysed belong to the Swedish set of the four reference timbers of the collaborative field experiment (Document No: IRG/WP/367). Before the field exposure 60 mm were cut off the end of each stake. This was done in order to be able to carry out chemical analyses as well as different types of testing. Some of the material has been used in softrot tests (Document No: IRG/WP/1151)....
T Nilsson


Sequential exposure of borate treated Douglas-fir to multiple Formosan subterranean termite colonies in a 40-week field test
1993 - IRG/WP 93-10006
Douglas-fir boards (ca. 74.5 g) pressure-treated with disodium octaborate tetrahydrate (DOT) retentions of 0 (controls), 0.88, 1.23, 1.60, or 2.10% (weight/weight) DOT were sequentially exposed to four active field colonies of Formosan subterranean termites, Coptotermes formosanus Shiraki (Isoptera: Rhinotermitidae), in an above-ground field test. Samples were placed in contact with each colony fo...
J K Grace, R T Yamamoto


Long-term performance of a "wax" type additive for use with water-borne pressure preservative treatments
2000 - IRG/WP 00-40159
Field performance results are updated for matched CCA treated decking boards with and without an emulsion water repellent additive incorporated with the initial pressure treatment. Decks have been exposured for over 9 years in Harrisburg, NC. Boards were evaluated for in-service and laboratory performance for water repellent efficacy, as well as additive loadings in the boards after this exposure....
A R Zahora


Volatile borates in the treatment of wood and wood based panel products against subterranean termites
1995 - IRG/WP 95-30094
Blocks of pine solid wood, oriented strand board and plywood were treated with trimethyl borate by vapour treatment. It was meant to obtain either a full impregnation of the specimens or a shell treatment of the outer three millimetres. The efficacy of the treatments against subterranean termites (Reticulitermes lucifugus) was evaluated using an European Standard method....
L Nunes, D J Dickinson, R J Murphy


Evaluation of polystyrene as a protective of wood in sea-water
1986 - IRG/WP 4129
A test is described on the biological protection of wood by treatment with polystyrene. The results, obtained in marine trials, after 18 months, show that the treatment with polystyrene is not all that effective in preventing the attack of marine borers....
A Gambetta


Collaborative soft rot tests: 2nd interim report
1975 - IRG/WP 258
J G Savory, J K Carey


Marine borers as wood degraders in Bangladesh and their protection
1996 - IRG/WP 96-10186
Field study on timber piles used in Bangladeshi brackish waters revealed that untreated and pentachlorophenol treated piles drastically degraded by the attack of molluscs and pholads (marine borers). Adequately CCA-C impregnated (30 kg/m³ or 6% W/W dry oxide retention) timber piles can protect the attack of molluscs. It is very difficult to protect pholads which can invade naturally very durable ...
A K Lahiry


The utilization of preserved rubberwood
1982 - IRG/WP 3186
The paper examines the use of processed and kiln-seasoned rubberwood for manufacturing furniture and doors and windows, discusses methods tested and found acceptable for preserving the timber as well as for drying the treated timber in conventional kilns. It considers a type of furniture where narrow width timber of preserved and kilned rubberwood has been used with great success. It recommends th...
V R Sonti, B Chatterjee, M S Ashraf


Migration of active ingredients from treated timber into fresh water
1991 - IRG/WP 3669
Spruce roundwoods and segments were treated with three different wood preservatives. Two of them containing copper and chromium the other one free of chromium. After fixation (3 weeks, 20°C) the specimens were leached by using artifical rain or by shaking the segments for one hour in contact with demineralized water. The water was analysed for the relevant elements of the preservative tested. Lea...
H Klipp, H Willeitner, K Brandt, A Müller-Grimm


Diffusion of fused borate rods in top ends of poles
1989 - IRG/WP 3518
Diffusion tests of fused borate rods were carried out on extremities of sapwood poles in service. Rods were set in drills under the cone with or without addition of liquid Boracol 40. After one year of weathering, a good diffusion in the slice under the cone and even below the slice and in the cone itself was observed in Scots pine and spruce poles. The rods were still intacts and constitute, in f...
D Dirol, J P Guder


Influence of storage on mould susceptibility of wood at relative humidity values lower than 100%
1989 - IRG/WP 1413
It is well known that wood material changes with time because of different environmental influences. The effects of such changes on the subsequent mould susceptibility are less known. In this paper we report on increased mould susceptibility of pine wood after storage. Mould growth was detected by indirect methods....
J Bjurman


CEN Draft Standard (38 N 460F): Méthode d'essai pour determiner l'efficacité d'un produit de préservation du bois en milieu marin
1986 - IRG/WP 4132 F
G Castan


Detection of brown rot decay in wood by ion mobility spectrometry
1991 - IRG/WP 2377
A test method for the detection of brown rot decay in wood is described and involves a two-step procedure: thermal release of vapours from wood samples followed by analysis using Ion Mobility Spectrometry (IMS), with results being obtained in 5-10 seconds. The advantages, limitations as well as the detection limit of the technique are presented....
A H Lawrence, T Nilsson


The internal-external diffusion process: Table salt treated poles
2005 - IRG/WP 05-50224-25
This new technique of preservation of wooden poles consists of keeping preservative in stock, in a reservoir drilled inside the pole, in its whole length. This permits the use of non toxic, common products such as table salt, grease, etc, in the preservation of utility poles, building columns, or the like. Some major obstacles to a good implementation of a good preservation with the classical pr...
L Nitunga


Proposed test procedure to determine the effect of timber substrate on the effectiveness of a copper/chrome/arsenic preservative in seawater
1975 - IRG/WP 411
R A Eaton


Analysis of organotin fungicides in wood preservative solutions and double-vacuum treated wood
1983 - IRG/WP 3250
A new analytical method using high-performance thin-layer chromatography (HPTLC), for the assay of organotin compounds in preservative-treated wood, is presented. The organotin compounds are extracted from the ground wood sample with a mixture of hydrochloric acid and ethanol. After HPTLC-separation, exposure of the thin-layer plate to ultraviolet light, and dipping of the plate into a 0.1% pyroca...
W Hintze, S V Ohlsson


Accelerated wood decay in a soil bed test under greenhouse conditions compared with a stake test under field condition
1991 - IRG/WP 2384
The rate of decay of oak, beech, Douglas fir, pine and spruce stakes in an outside test field were compared with the decay rate of the same species in a greenhouse soil-bed test. Strength loss after four and six months respectively was measured by determining the compression strength parallel to the grain. The results show that all species, strength loss in the greenhouse was 2 to 4 times higher t...
J E Polman, S G Michon, H Militz