Micromorphology of Schizophyllum commune attack in pine (Pinus sylvestris) wood
1983 - IRG/WP 1184
The decay pattern caused by Schizophyllum commune in pine latewood tracheids was studied using both light and transmission electron microscopy. The attack began as isolated concentric slits within the S2 layer with extensive lamellation and separation of individual wall layers observed in subsequent stages of decay. The slits resulting from attack appeared to be formed in thin, regular concentric ...
T Nilsson, G F Daniel


Respiration measurement of dry-rot
1995 - IRG/WP 95-10095
Methods for measuring the production of carbondioxide from wood infected with the dry-rot fungus were evaluated. By enclosing whole wood blocks and measuring the concentration of gas in the headspace by gas chromatography, an exponential increase in the concentration of CO2 was observed for at least 2 months. This technique could therefore present a method for evaluating various treatments of dry-...
L Toft


On the biotope of dry rot (Serpula lacrymans) in the wild
1995 - IRG/WP 95-10123
The True Dry rot fungus was found in the Himalayas several times in this century. The finds were able to cross breed with Serpula lacrymans from Denmark and therefore all belong to this species (Harmsen 1960). In order to understand its successful colonisation in buildings we were interested in studying the natural biotope, i.e. the moisture, temperature and soil relationships. All together 15 fru...
J Bech-Andersen, S A Elborne, K Bech-Andersen


Susceptibility of CCA treated North American hardwoods to Chaetomium globosum decay
1998 - IRG/WP 98-10278
Seven species of hardwood, Beech (Fagus grandifolia), Basswood (Tilia americana), Maple (Acer rubrum), Oak (Quercus rubra), Trembling Aspen (Populus tremuloides), White birch (Betula papyrifera) and Yellow poplar (Liriodendron tulipifera) were vacuum or pressure impregnated with CCA, at four retention levels. The CCA was allowed to fix in the wood at 35°C. Red pine (Pinus resinosa) was also inclu...
U Srinivasan, Y T Ung, P A Cooper


Factors affecting decay rates in a fungus cellar II
1986 - IRG/WP 2259
Tests were initiated to investigate the influence of various factors on the decay rate in a "Fungus Cellar". Birch and pine stakes treated with chromated copper arsenate and didecyldimethyl ammronium chloride, as well as untreated control stakes, were incubated in two soils in a Fungus Cellar test and installed at two field sites for comparative purposes. The visual rating vs actual stake weight l...
P A McKaig


Effect of soil type and moisture content on soft rot testin
1986 - IRG/WP 2270
Several soils of different types were tested at a range of moisture contents for their suitability for use in a soil burial soft rot test. Their effectiveness was assessed by weight loss in CCA treated and untreated beech and birch outerwood. A horticultural loam (John Innes No. 2) was the most appropriare soil in terms of amount of weight loss caused, tolerance to changes in soil moisture content...
S M Gray


Effects of cyproconazole and copper sulphate on the length of the hyphal growth unit (HGU) of the white-rot fungus Coriolus versicolor
2003 - IRG/WP 03-10473
Wood decay basidiomycetes have been shown to produce appreciable quantities of extracellular mucilaginous materials (ECMM). The relationship between ECMM and total biomass production has been investigated in the white-rot fungus Coriolus versicolor (CTB 863 A). Differences in the amount of ECMM produced by the fungus proportionally to the total biomass, were observed under a range of physiological...
D Vesentini, D J Dickinson, R J Murphy


Incidence of soft rot in creosoted poles
1992 - IRG/WP 92-1554
A further population of creosote-treated poles has been assessed for the occurrence of soft rot, as a continuation of work reported in IRG Document No. IRG/WP/1368. The outer 1 cm of each core was assessed microscopically and graded for the presence of soft rot cavities in the wood cell walls; with further assessments taken at a consecutive 1cm interval for cores showing positive findings. Followi...
D J Dickinson, P W McCormack, B Calver


Settlement of fouling organisms on CCA-treated Scots pine in the marine environment
1997 - IRG/WP 97-50094
As part of an EU project to investigate the effects of CCA loading on non-target marine fouling animals, exposure panels of Scots pine treated to 12, 24 and 48 kgm-3 CCA and untreated controls were submerged at seven coastal sites (Portsmouth, UK: Kristineberg, Sweden: La Tremblade (2 sites), France: Ria Formosa, Portugal: Sagres, Portugal: Athens, Greece). Inspections were made at 6 and 12 months...
C J Brown, R A Eaton


Extracellular substance from the white rot basidiomycete Irpex lacteus involved in wood degradation
1992 - IRG/WP 92-1571
Cellulases, phenol oxidase, and a substance that both produced and reduced H2O2 were isolated from cultures containing wood or glucose on which the white-rot fungus Irpex lacteus was growing. The rate of wood degradation by the fungus with different amounts of glucose in the medium was measured. More of the substance that produced and reduced H2O2 was found extracellularly in cultures containing w...
H Tanaka, T Hirano, G Fuse, A Enoki


Destruction of two tropical timbers by marine borers and micro-organisms in Goa waters (India)
1992 - IRG/WP 92-4176
The paper deals with the pattern of microbial attack in relation to marine borer damage of test panels of African rosewood and Brazilian jackwood exposed in Goa waters (Western India) for a period of seven months. The degradation of wood cell walls in both the timber samples occurred due to infestation of soft-rot fungi and tunnelling bacteria. African rosewood, which was severely damaged by tered...
L N Santhakumaran, A P Singh


The effectiveness of three tributyltin compounds in beech against soft rot fungi using a soil-bed technique: A preliminary report
1986 - IRG/WP 3390
The effectiveness, towards soft rot fungi, of bis (tributyltin) oxide, tributyltin ethanesulphonate (TBTES) and benzyltributylammonium tributyldichlorostannate in both leached and unleached beech stakes is compared to that of a CCA preservative (Tanalith CT 106), using a soilbed technique. In addition, the effect of test solvent (water or toluene) on the performance of TBTES is evaluated. Total ti...
R Hill, A H Chapman, B Patel, A Samuel, J K Carey


An investigation of the factors influencing the rate of deterioration of timber samples due to microfungi in laboratory tests
1997 - IRG/WP 97-20116
An investigation was performed into the comparative performances of test 1 (vermiculite burial) and test 2 (soil burial) as described in ENV 807. Two test preservatives were used - copper naphthenate and propiconazole. Copper chromate was included as a reference preservative. The wood species used was beech (Fagus sylvatica). Test 1 was performed using both a mixed inoculation of the five stipulat...
I J Herring, D J Dickinson, S M Gray, J K Carey


Soil treatment tests with the three products of boric acid for the prevention of the hyphal growth of Serpula lacrymans
1992 - IRG/WP 92-3693
Laboratory soil treatment tests were conducted for the evaluation of fungicidal or fungistatic effect of boric acid products against Serpula lacrymans. Boric acid products tested were the following three: a thickened boric acid solution in triethanolamine, boric acid-silica gel complex granules, and a nonwoven fabric laminated with a polypropylene film and coated with boric acid granules on one si...
S Doi, A Yamada, Y Mineki, M Mori


Alkaline building materials and controlled moisture conditions as causes for dry rot Serpula lacrymans growing only in houses
1985 - IRG/WP 1272
Dry rot Serpula lacrymans ( Fr.) S.F. Gray is commonly found in houses, though never with certainly in nature, like other wood destroying fungi which grow both indoors and outdoors. In investigating series of dry rot instances it was shown that this fungus is always found in covered places, close to a moisture source, the distance being from 0 a maximum of 600 cm. Owing to the dry rot has been abl...
J Bech-Andersen


Old and new facts on the dry rot fungus Serpula lacrymans
1991 - IRG/WP 1470
The article collates some of the recent literature on the biology of the dry rot fungus Serpula lacrymans. The fungus can grow at 28°C, and maximum wood moisture is above 55%. Serpula Iacrymans degrades crystalline cellulose. The intensive production of extracellular oxalic acid is neutralized by calcium and iron. There is considerable variation among the strains with regard to factors such as gr...
O Schmidt, U Moreth-Kebernik


An attempt to grow dry rot fungus Serpula lacrymans on mortar substrate in non-sterile conditions
1989 - IRG/WP 1385
According to many experts, Serpula lacrymans is probably the most dangerous wood destroying fungus in houses. Investigations of KOCH, A.P. (2) showed that incidence of this fungus in percent was around 20% when the frequency of some other standard fungi was far below (Coriolus versicolor: 0.2% for example). The work presented here is a part of a program carried out at CTFT for assessing the resist...
L N Trong


Cytoplasmic and extracellular localization of manganese II dependent peroxidase(s) in white rot fungi during degradation of woody materials
1989 - IRG/WP 1416
The manner by which lignin is degraded in-situ in natural substrates by white rot fungi still remains a controversial issue particularly the distribution and role(s) played by lignin degrading enzymes (i.e. manganese II peroxidase and lignin peroxidase). In the present study, use was made of anti-manganese II peroxidase and immunolabelling techniques in conjunction with transmission electron micro...
G F Daniel, B Pettersson, T Nilsson, J Volc


European standardization for wood preservation
1991 - IRG/WP 2365
Since the last IRG 21 conference in New-Zealand, there one meeting of the plenary committee and several meetings of working groups. The interprative documents prepared by CCE for expliciting the essential requirements of the CCE Directive on the construction products and specially: mechanical resistance and stability / hygiene, health and environment / safety in use are waited to valid the progra...
Anonymous


Synergistic combination of an antioxidant and wood preservative: a preliminary study
1998 - IRG/WP 98-30172
We previously proposed that extractives in highly durable angiosperm heartwood may protect wood against white-rot fungal colonization and subsequent degradation by a dual mechanism: extractives have some fungicidal activity and are also free radical scavengers (antioxidants) and thus interfere with the fungal free radical degradative mechanisms. We tested this hypothesis using the commercial bioci...
T Schultz, D D Nicholas, J Minn, K D McMurtrey, T H Fisher


The high decay resistance in the sapwood of the naturally durable Malaysian hardwood Belian (Eusideroxylon zwageri)
2001 - IRG/WP 01-10410
It has long been assumed that the observed natural durability of the heartwood in certain timbers is perhaps associated with a relatively lower decay susceptibility also of the sapwood of these species. While the heartwood of Belian is reputedly highly decay resistant among the tropical hardwoods of Southeast Asia, laboratory decay tests reported in this paper have also confirmed the high decay re...
A A H Wong, A P Singh


Microscopic analysis of southern pine utility pole core segments
1992 - IRG/WP 92-1542
Fifteen macroscopic core descriptive categories were evaluated by microscopic analysis for accuracy in detecting decay and judging decay severity. Five categories were good indicators of decay as decay was detected in 28 of 48 samples. Five categories were possible indicators of early decay as decay was detected in 6 of 40 core segments and an additional 18 contained hyphae. The remaining five cat...
S E Anagnost, C J K Wang, M Wright


Performance of Tuff Brite C™ and other formulations against blue-stain, mold and brown-stain in freshly-sawn rubberwood (Hevea brasiliensis) in the humid tropics of Peninsular Malaysia
1997 - IRG/WP 97-30163
The relative anti-sapstain and anti-mold efficacies, including brown-stain development in freshly-sawn rubberwood (Hevea brasiliensis) in the Malaysian tropics, between selected water-based product concentrations of formulations Tuff Brite CTM without/with added Borax (at 1.5/0, 1/1.5, 1.5/1.5 and 2%/1.5%), PQ8TM without/with added Borax (at 2.5/0, 1.5/1.5, 2/1.5 and 2.5%/1.5%) and NeXgenTM/NeX-Br...
A H H Wong, T L Woods


Suitability of cotton strip testing as a screening method for the development of wood preservative formulations
2003 - IRG/WP 03-20270
This paper outlines a simple and rapid test method for screening the efficacy of wood preservative formulations against microbiological attack using cotton strips. The method was evaluated against soft rot and was found to provide reliable information on the protection of lignocellulosic material against microbiological attack. The assessment is based on visual interpretation of decay and on a sim...
H Leithoff, I Stephan, H Härtner


Dimensional stabilization and decay resistance of wood treated with brown-rotted lignin and copper sulfate
1990 - IRG/WP 3608
The objective of this study was to evaluate the potential usefulness of brown-rotted lignin (BRL) as a dimensional stabilization and copper complexing agent for wood treatment. For dimensional stabilization, aqueous solutions of the lignin extract were combined with either copper sulfate, glyoxal or other additives. Anti-shrink efficiency (ASE) values as high as 42% were obtained with wood treated...