Collaborative soft rot tests: Interim report on PRL tests of Cu/Cr/As preservative using method of Document No: IRG/WP/208
1972 - IRG/WP 211
Preservative: Tanalith CT.106 - Results obtained with beech are given in the table and indicate a toxic limit of 16.7-19.2 kg/m³ - The initial soil moisture content was adjusted to 27.8% (the water holding capacity). Noticeable drying out has occurred in some of the test bottles....
J G Savory


Efficacy of anhydrides as wood protection chemicals - II. Performance against soft rot fungi
1998 - IRG/WP 98-30174
Pine sapwood modified with various anhydrides and with butyl isocyanate was tested for its resistance to soft rot decay. Small stakes were exposed for 20 months in unsterile soil in a fungal cellar test. Wood modified with butyl isocyanate performed better than any of the anhydrides tested, with a threshold level of protection (less than 3% weight loss) at 12% weight percent gain (WPG). Stakes ac...
S C Forster, M D C Hale, G R Williams


Rational weight per weight (w/w) qualifying retention from a pole bank in Bangladesh
2000 - IRG/WP 00-40187
Weight per weight (w/w) vs weight per volume (w/v) retention study revealed that the w/w % retention is found to be appropriate and uniform for all timber species in respect of its real effectiveness. The pole species having density below 512 kg/m3 (32pcf.) showing w/v retention below 20kg/m3 (1.25pcf.) have equal w/w retention of 4%. The apparently reduced w/v retention of low density poles will ...
A K Lahiry


Recent soft-rot research in softwoods and hardwoods
1980 - IRG/WP 1108
The purpose of this paper is to describe briefly the current status of our research on soft-rot fungi. The work to be discussed is still in progress and any results described must be regarded as provisional....
J A Butcher


Resistance to soft rot of hardwood plywood treated with CCA salt
1983 - IRG/WP 3258
Plywood made from indigenous hardwoods was treated at an average loading of 34 kg Celcure A per m³ and was installed in a field test. After 20 years the samples were only slightly attacked by soft rot and the glue bonds were still intact....
R S Johnstone


Proposals for a vermiculite burial soft rot test method
1980 - IRG/WP 283
J G Savory, J K Carey


Soft rot and bacterial decay in preservative treated eucalypt power transmission poles
1982 - IRG/WP 1155
Bacterial type decay was observed in CCA and PCP treated eucalypt power transmission poles. Detailed observations made with the SEM revealed bacterial colonisation and decay, especially in fibres. Plug samples taken from poles throughout Queensland were examined for preservative retention and presence of soft-rot decay. The severity of decay was different according to location, retention and speci...
L E Leightley


Biological performance of gypsum products containing borates
2000 - IRG/WP 00-30237
At suitable retentions borates have biostatic properties enabling them to be used for biodeterioration control in wood. They provide protection against decay fungi, mould, and termites, which are known to also attack gypsum products. Currently, many gypsum products contain added borates, which are used to improve physical and processing characteristics. Work examining the effect of borates at cont...
J L Fogel, J D Lloyd


The effectiveness test of chemicals against Serpula lacrymans
1984 - IRG/WP 2222
The effectiveness tests of wood preservatives against Serpula lacrymans were conducted in accordance with Japan Industrial Standard A 9302 and Japanese Wood Preserving Association Standard No. 1. Also, the soil treatment test against this fungus was carried out with two chemicals. The preservatives tested without Creosote oil (out of JIS) had sufficient preservative effect against Serpula lacryman...
S Doi


Biological control of Serpula lacrymans using Trichoderma spp
1994 - IRG/WP 94-10069
The effectiveness, or otherwise, in killing Serpula lacrymans, of a range of Trichoderma spp. in a variety of media and using two different incubation systems has been tested. In agar based systems with normal nutrients or minimal nutrients with high or low nitrogen contents and high or low iron content Trichoderma harzianum 25 proved to be the most efficient and killing Serpula lacrymans. Other s...
A J Score, J W Palfreyman


Some thoughts on the future strategy for eradicating Serpula lacrymans from a building
1989 - IRG/WP 1405
We now have a clear view of the mechanism of translocation of nutrients in the mycelium of Serpula lacrymans which is one of the physiological processes underlying the remarkable capacity of this fungus to spread through a building. Here the elements of the mechanism of translocation are dissected out to suggest avenues which might be followed in the search for new ways for eradicating the fungus ...
D H Jennings


Wood in concrete. Summary of discussion at IRG 14, Surfers Paradise, Australia
1984 - IRG/WP 3264
The performance of untreated and preservative treated wood when placed in direct contact with concrete was considered in a discussion session at IRG 14. While published reports in this area are scarce, research is in progress internationally and a variety of practices are currently available to minimize any additional hazard posed by contact with concrete. This report summarizes the points raised ...
R J Murphy


Fungus cellar and stake tests with tall oil derivatives. Progress Report after 5 years' testing
1987 - IRG/WP 3442
Two derivatives of tall oils have been tested for five years in fungus cellar and stake tests. The samples were relatively quickly attacked on the surface by decay fungi, mainly soft rot, but the decay has progressed very slowly. The performance of the stakes in the tests has so far been equivalent or even better than some CCA preservatives and creosote....
J Jermer, Ö Bergman, T Nilsson


Collaborative soft rot tests
1981 - IRG/WP 2151
There appears to be need for reconsideration of attitudes towards Standardisation of laboratory tests for determining the toxicity of preservatives to soft rot fungi. The original approach was that a limited number of test methods were available and that collaborative effort would determine the suitability of the methods for Standardisation. It has been established so far that pure culture testing...
J G Savory


Comparative studies on the distribution of lignin and CCA elements in birch using electron microscopic X-ray microanalysis
1987 - IRG/WP 1328
The microdistribution of metal preservatives in treated wood has received considerable research over the last two decades. Despite this, little effort seems to have been made to try and correlate the distribution of CCA elements with respect to naturally occurring wood cell wall components in wood. In the present preliminary study an attempt is made to relate the distribution of lignin in-situ wit...
G F Daniel, T Nilsson


Collaborative soft rot tests: Summary of comments on 'Proposals for a standardized soil burial test'
1971 - IRG/WP 202
J G Savory


Collaborative soft rot tests: 2nd interim report
1975 - IRG/WP 258
J G Savory, J K Carey


Collaborative experiments in testing the toxicity of wood preservatives to soft rot fungi
1970 - IRG/WP 25
Eight Institutes from seven countries, Austria, England, France, Germany, Holland, Sweden and Switzerland have collaborated in an attempt to assess the suitability of various laboratory test procedures for acceptance as standard methods of determining the toxicity of wood preservatives to the cellulose-attacking micro-fungi which cause 'soft rot' of wood. Pure culture methods wit...
J G Savory, A F Bravery


Short term preconditioning of preservative-treated wood in soil contact in relation to performance in field trials
2000 - IRG/WP 00-20185
The effect of pre-exposure to primary colonising micro-organisms on preservative-treated wood, prior to a basidiomycete decay test, was determined by preconditioning in two soil types. Scots pine EN 113 blocks treated with 3 model systems (a triazole, a copper quaternary compound and a copper boron triazole) were leached according to EN 84 and subjected to 6 weeks and 8 weeks burial in either John...
S Molnar, D J Dickinson


Synergistic effects between 2-HPNO, Irganox 1076 and EDTA on the inhibition of wood degradation by Coriolus versicolor
2004 - IRG/WP 04-30331
The efficiency of 2-hydroxypyridine-N-oxide (2-HPNO) as wood preservative has been investigated. As shown using classical experiments as well as using response surface methodology, the efficiency of 2-HPNO as wood preservative is strongly improved in presence a chelator like EDTA and/or of Irganox 1076 an industrial antioxidant. In these conditions, wood preservative efficiency of the mixture the ...
A Mabicka, S Dumarçay, N Rouhier, M Linder, J P Jacquot, P Gérardin, E Gelhaye


A short note on fungal decay in K33-treated poles
1982 - IRG/WP 1169
Soft rot cavities and erosion of the lumen have been found in K33-treated Pinus sylvestris poles from the years 1956-66 by microscopic studies. Poor treatment quality has been proved for some of these poles. The microscopy showed an unusual pattern of attack, and pre-treatment decay is suspected but not yet proved. Sounding the poles and using the Pilodyn indicated decay, but poking did not. Quant...
H Friis-Hansen


IRG test of preservative-treated hardwoods with particular reference to soft rot. Report on condition of specimens installed in Victoria, Australia
1983 - IRG/WP 3269
G C Johnson, J D Thornton


A preliminary report on lignicolous marine fungi in the Java Sea, Indonesia
1982 - IRG/WP 488
This report is part of a study on the natural durability of Indonesian timbers against marine borers conducted in Pari Island waters, Java Sea (Suhirman and Eaton, 1981), and contains preliminary information which has not yet been published....
Suhirman, R A Eaton


Efficacy of some extractives from Pinus heartwood for protection of Pinus radiata sapwood against biodeterioration. Part 1: Fungal decay
1995 - IRG/WP 95-30072
Chemical compounds thought to contribute to the natural durability of heartwood of Pinus spp. were either chemically synthesised in the laboratory or extracted from the heartwood of Pinus elliottii or Pinus caribaea. These compounds included the stilbenes, pinosylvin and its mono- and di-methyl ethers, and the flavonoids, pinobanksin and pinocembrin. Small blocks of Pinus radiata sapwood were impr...
M J Kennedy, J A Drysdale, J Brown


Changed susceptibility of the chemically and thermally degraded spruce wood to its attack by the dry rot fungus Serpula lacrymans
1999 - IRG/WP 99-10322
In buildings, some intentional or unintended situations can occur at which some wood products are exposed to aggressive chemicals and also to higher temperatures. Occasional activity of fungi on such pre-attacked wood products can be either higher or lower. This paper deals with changes in the susceptibility of spruce wood (Picea abies L. Karst.) to attack by the dry rot fungus Serpula lacrymans, ...
L Reinprecht