The proposal for the method of testing the phytotoxic effect of wood preservatives
2000 - IRG/WP 00-50163
Four methods of testing the phytotoxic effect of wood preservatives are proposed as the unified test by: - direct application of the preservatives to the test plants by spraying; - direct application of the preservative to the soil substrate; - indication plants growing in the vicinity of treated wood; - seed germination rate on the treated substrate....
J Wazny, P Witomski


Inspection results of preservative treated stakes, maximum 33 years in field
1992 - IRG/WP 92-3690
Since in 1958, we have undertaken field experiments in Japan. For these field experiments, we used sapwoods of Japanese cedar called Sugi (Cryptomeria japonica) because of majority of plantation forest soft wood species in Japan. For some preservatives, we added sapwood of Japanese beech called Buna (Fagus crenata), a main Japanese hard wood species. Dimensions of these specimens were 30 x 30 x 60...
K Suzuki, K Yamamoto, M Inoue, S Matsuoka


Wood furfurylation process and properties of furfurylated wood
2004 - IRG/WP 04-40289
The first processes for “furfurylation” of wood (wood modification with furfuryl alcohol) were developed several decades ago. Furfuryl alcohol is a renewable chemical since it is derived from furfural, which is produced from hydrolysed biomass waste. Over the last decade modernised processes for furfurylation of wood have been developed. These new processes are based on new catalytic systems a...
M Westin, S Lande, M Schneider


Aspects of the biology of the wood-boring weevil Pselactus spadix herbst
1997 - IRG/WP 97-10221
The external morphology of the adult and larval digestive tract of the wood boring weevil Pselactus spadix has been reported for the first time. An examination of adult gut ultrastructure showed that the foregut was adapted for the wood boring habit with the presence of chitinous setae, grinding plates and sieve plates. The adult midgut bore eight caecae and numerous palpii. Spherical yeast-like m...
G Cooper, A J Pitman, G S Sawyer


Respiration methods used to follow the decay of wood and the toximetric evaluation of wood preservatives
1975 - IRG/WP 249
When wood is attacked and decayed by fungi, wood substance and oxygen (02) are consumed, while carbon dioxide (CO2), water and heat are liberated. Early in the 1960's workers from England, Canada and Sweden began studying CO2 evolution, with respect to decay and its control using chemical preservatives, while in Germany and the USA O2 utilization was being similarly examined. Oxygen consu...
R S Smith


Valid names for some common decay fungi, their synonyms and vernacular names
1978 - IRG/WP 172
A Käärik


A method of isolating actinomycetes from decayed wood
1974 - IRG/WP 126
This paper deals with a tentative method of isolating Actinomycetes from dacayed wood....
T Haraguchi


Abstracts of papers prepared for the Symposium “Environment and wood preservation”
2001 - IRG/WP 01-60135
IRG Secretariat


The long-term performance of boron treated joinery in service - A case study
2000 - IRG/WP 00-20208
Joinery treated with borates 23 years ago and in service in residential flats was surveyed and analysed for boron content. The levels of boron still present were sufficient to prevent decay. None of the windows surveyed showed any decay despite the fact that moisture and sapwood contents were conducive to decay....
D J Dickinson, R J Murphy


Durability of pine modified by 9 different methods
2004 - IRG/WP 04-40288
The decay resistance was studied for pine modified by nine methods of wood modification: 1) Acetylation, 2) Treatment with methylated melamine resin (MMF), 3) Acetylation followed by post-treatment with MMF-resin, 4) Thermal modification, 5) Furfurylation, 6) Maleoylation (using water solution of MG or ethanol solution of maleic anhydride), 7) Succinylation, 8) NMA-modification and 9) modification...
M Westin, A O Rapp, T Nilsson


Biological control with Trichoderma harzianum in relation to the formation for spores the production of soluble metabolites
1994 - IRG/WP 94-10073
The amount of spores produced by three strains of Trichoderma harzianum on the aerial mycelium of agar cultures and in shake cultures, respectively, correlated with the inhibition zones exerted against Phanerochaete chrysosporium in an agar diffusion test. The amount of soluble antifungal metabolites as well as the protein content also correlated with the inhibition zones and the amount of spores ...
J Bürgel, E Horvath, J Haschka, K Messner


Chemical compounds from Eperua falcata and Eperua grandiflora heartwood and their biological activities against wood destroying fungus (Coriolus versicolor)
2005 - IRG/WP 05-30373
The chemistry analysis of the compounds present in dichloromethane and ethanolic fraction as well as bioassays enables to understand the durability differences of Eperua falcata and Eperua grandiflora. The principal distinction between these two species is the acidic subfraction of diterpenoic extract, which is antifungic in Eperua falcata when tested in in-vitro conditions. This study also enable...
N Amusant, C Moretti, B Richard, E Prost, J M Nuzillard, M-F Thévenon


Some characteristics of Pinus radiata wood from trees subjected to resin extraction
1987 - IRG/WP 3403
35 year old Pinus radiata trees growing in La Puntilla (lat. 37° south, long. 72,4° west), Chile, were subjected to resin extraction 5 years ago. After harvesting them simultaneously with control trees of the same place and age, probes were taken from the bottom of each pole, at 3.4 m, 7.8 m and 11.4 m height. Analysis of ethanol/benzene extract, CCA salt penetration tests and sapstain and brown-rot development rate were performed. The extract content differed in both groups. In the ascendent sense it decreases in unextracted trees and increases in extracted. CCA salt penetration was deeper in treated trees than in untreated. Wood subjectect to resin extraction was less susceptible to sapstain development. No significant difference was detected in both groups in relation to the development of brown-rot.
M C Rose, J Navarrete, G Sandoval, A Bedoya, L Ortega, R Zurita


European standardization for wood preservation
1988 - IRG/WP 2321
G Castan


Results of stake tests on wood preservatives (Progress report to 1974)
1975 - IRG/WP 361
A number of field stake trials on preservative-treated wood have been carried out at Princes Risborough Laboratory from 1928 to the present day, and many of the tests still continue. This paper presents in detail the results obtained to date, covering about 15 000 individual test stakes exposed over the period....
D F Purslow


Circular letter to all members of WG IV Marine Wood Preservation
1985 - IRG/WP 4122
IRG Secretariat


A novel method for delivering fluids into bolted wooden components.
2004 - IRG/WP 04-40280
The paper describes the development of a washer that enables fluids such as wood preservatives and adhesive resins to be delivered to bolted wooden components in-situ. The system was developed to meet the criteria of low cost and the ability to tolerate inaccurate drilling of holes in the wooden members....
G S Sawyer, B Tole


Effect of water repellents on leaching from CCA treated wood
1995 - IRG/WP 95-50044
CCA treated fence boards brushed with a water repellent finish had consistently lower leaching losses of all CCA components compared to the rate for matched samples without the water repellent. These results are after 12 cycles of simulated rainfall in the laboratory (1800 mm rainfall total) and four months of natural rain exposure in Toronto....
P A Cooper, R MacVicar


Use of vermiculite as substrate in assays on phytotoxicity of treated wood
1989 - IRG/WP 3547
It is considered the possibility of using vermiculite instead of soil as substrate in assays on phytotoxicity of wood treated with preservatives for agricultural use. Three organic preservatives were used. It had been tested the behaviour of both, vermiculite and soil in case of preservative leaking due to a leach. So that, assays of germination with cucurbitaceous were carried out, mixing a dose ...
M V Baonza Merino, D Franco


CEN Draft (38 N 460E) Standard: Test method for determining the protective effectiveness of a preservative in the marine environment
1986 - IRG/WP 4132
This European Standard describes a marine test method which provides a basis for asseasing the effectiveness of a wood preservative used to prevent attack of timber in sea-water by marine borers. The method is only suitable for testing preservatives which are intended to prevent attack by marine wood boring organisms of treated timber for use in more or less permanent contact with sea-water. It is...
G Castan


Effects of various preservative treatments on the mechanical and physical properties of plywood
1993 - IRG/WP 93-40007
The technical properties of plywood are related to both the intrinsic characteristics of its composing wood species and the quality and performance of the glue bond which acts as an interface between veneer sheets. Consequently mechanical and physical testing and glue bond strength analysis offer an appropriate means for studying the effect of preservative treatments on the overall quality of plyw...
J Van Acker, M Stevens


Treatability of plywood containing intermountain Douglas fir veneers
1982 - IRG/WP 3203
Eighteen sheets of plywood were obtained which contained intermountain Douglas-fir veneers from two regions of British Columbia. Following pressure treatment with chromated copper arsenate (CCA type C) and ammoniacal copper arsenate (ACA) the preservative penetration and retention in individual veneers was assessed. It was concluded from the study that the intermountain Douglas-fir veneer could no...
J N R Ruddick, A Walsh


Direct measurement of fluid flow within wood
1986 - IRG/WP 2248
The problematics of fluid flow mechanism within wood using a permeability concept are highlighted, and the non-feasibility of a practical and versatile model is explained. An alternative method using a negative temperature coefficient thermistor to measure flow velocity directly is presented. The method has been verified in living trees and shows extreme sensitivity for flow above 1 meter/hour. Fo...
J P Hösli


An investigation of the effects of pre-steaming on the treatment of sawn spruce timber with Celcure A, a copper-chrome-arsenic preservative
1981 - IRG/WP 3150
Difficulties in the treatment of spruce using standard vacuum/pressure techniques with both water-borne and organic solvent preservatives are well known. We have evaluated the influence of steaming on treatability with a waterborne CCA preservative....
C R Coggins


Depletion of boron and copper from CCB treated test specimens using different leaching protocols
2004 - IRG/WP 04-50208
The objective of this study was to measure the depletion of inorganic wood preservative components regarding the proposed OECD guideline "Estimation of emissions from preservative-treated wood to the environment: laboratory method for wooden commodities exposed in the use class 4 and 5" as part of the project "Investigations concerning the influence of test parameters on the release of biocidal ac...
E Melcher, R-D Peek, U Schoknecht, R Wegner


Previous Page | Next Page