Characteristics of treated oriented strand lumber using recycle chips
2006 - IRG/WP 06-40343
The Kyoto Protocol for preventing global warming has come into effect, and the Cabinet Council was decided on the amount of carbon dioxide exhaust to be reduced in Japan. Moreover, the recycling of demolition waste wood is mandated under the “Construction Material Recycling Law” as one of the mechanisms for Japan to form the recycling society. The law encourages the utilization of demolition w...
T Shibusawa, A Miyatake, K Yamamoto, K Hashimoto, H Sonobe


The effect of an ionic liquid of imidazolium tetrafluoroborates series on Scots pine wood properties
2007 - IRG/WP 07-40357
Ionic liquids (ILs) of imidazolium tetrafluoroborates series penetrate Scots pine wood very well and are active against wood destroying fungi. The requirement to use ILs as wood preservatives is determined by the liquid influence on the functional properties of wood. Investigations were undertaken to clarify the influence of an ionic liquid, 3-heptyloxymethyl-1-methylimidazolium tetrafluoroborate ...
A Fojutowski, R Szukala, J Pernak


Effects of sodium hypochlorite on compression strength and copper retention of spruce wood treated with copper azole and alkaline copper quat
2007 - IRG/WP 07-40362
This work investigates the effects of sodium hypochlorite on compression strength values and copper retention ratios of refractory spruce wood (Picea oriental L.) treated with the waterborne preservative Copper Azole, (CBA-A, Tanalith-E 3492) and alkaline copper quat (ACQ-2200). Before the copper azole and alkaline copper quat treatment, the samples were immersed in 500 ml of sodium hypochlorite s...
S Yildiz, E Dizman, A Temiz, Ü C Yildiz


Fire Safety of Wood Floor Assembly: Model and Full-scale Test
2007 - IRG/WP 07-20375
The present paper describes the model for the prediction of fire safety of wood floor assemblies. The model includes heat transfer model for the calculation of the flow of heat in floor assembly and structural model for the analysis of the mechanical performance of wood joists. The floor assemblies considered in this paper are constructed with nominal 2x10 (38x241mm) wood joists lined by Type X ...
H Takeda


Anatomical, physical and chemical changes of Bamboo (Phyllostachys puberscence ) during weathering processes
2008 - IRG/WP 08-10650
Bamboo (Phyllostachys puberscence) culms with 1, 2, 3 year old were exposed to natural weathering condition in Gwangju, Korea for 12 months. Changes in color, surface topography, strength and chemical properties were investigated using various microscopic and instrumental techniques. After one year’s weathering, the color of bamboo became lighter but strengths of bamboo did not change significan...
Jong Sik Kim, Kwang Ho Lee, Mi Young Cha, Yoon Soo Kim


Evaluation and identification of extractives from Iranian walnut (Juglans regia L.) by GC/MS technique for protection of non-decay resistant species
2008 - IRG/WP 08-10670
The use of walnut extractives is interest as environment friendly wood preservatives in the wood preservation industry. In this study, organic solvents were used to remove extractives from Iranian walnut heartwood samples. The solvent was removed by rotoevaporation, and Identification of chemical compounds in the Walnut extractives was done by using GC/MS technique. The toxicity of various extract...
S K H Hashemi, D Parsapajouh, H Khademi Eslam


Mechanical strength of wood from the Vasa shipwreck
2008 - IRG/WP 08-20381
Samples from three ancient ship wrecks (Vasa, Elefanten, and Gröne Jägaren) and recent oak samples as reference were examined with regard to mechanical strength using the high-energy multiple impact (HEMI) - test method, which delivers the resistance to impact milling (RIM) of a material. Adoption and optimisation of the test method for the particular sample size of the wooden drilling cores was...
A O Rapp, C Brischke, C R Welzbacher, T Nilsson, C Björdal


Effects of Murgul Copper Process flue gases (SO2) on compression strength parallel to the grain of Beech (Fagus orientalis Lipsky.) wood
2008 - IRG/WP 08-40404
In this study was investigated the effect on the compression strength parallel to the grain as mechanical properties of Fagus orientalis Lipsky. wood exposed to SO2 gas and non-exposed. In the experiments the two of four (total) were obtained from Artvin-Ortaköy region and the other two from Artvin-Murgul region. The compression strength parallel to the grain was calculated at the compare of ...
N Ay, E Topaloglu, A Uncu


Effect of CCA and Tanalith E on the performance of surface finishing
2008 - IRG/WP 08-40405
Effect of CCA and Tanalith E treatment on the performance of surface finishing properties was the objectives of this study. Sapwood of scots pine, (Pinus sylvestris L.) and oriental beech (Fagus orientalis Lipsk.) specimens (300 x 100 x 15 mm along the grain) were impregnated with aqueous solution of CCA 2% and Tanalith E 2%. Surface roughness, dry film thickness, adhesion strength, gloss measur...
T Ozdemir, A Temiz, I Aydin


Bending Properties of Southern Pine Treated with Micronized Preservative Systems
2008 - IRG/WP 08-40414
This study indicates that treatment of southern pine with micronized copper systems have no deleterious effect on the residual strength property values. No statistical differences between wood treated with micronized systems and water-treated controls were noted when means were compared using either Tukey’s test or S-N-K mean comparison tests. Using the more discriminating Least Squares anal...
H M Barnes, G B Lindsey, J Hill, M Pompeo, R Hodge


The effect of treatments in boron steaming medium on boron leaching and strength properties of wood
2008 - IRG/WP 08-40409
The combined effect of boric acid impregnation together with boron steaming and steaming heat treatments were evaluated in this study. Boric acid pre-treated wood samples and untreated ones subjected to steaming heat and direct steaming treatment in a close reactor at 13 bar pressure and 180 ºC for 30 minutes. Compression strength parallel to grain of wood samples, leaching test and pH measuremen...
E D Tomak, Ü C Yildiz, S Yildiz, E Pesman


Effects of CCB on wood strength of Eastern spruce (Picea orientalis L.)
2008 - IRG/WP 08-40416
The effects of CCB (chromate copper boron) on the static bending properties of Eastern spruce (Picea orientalis L.) based on MOE (modulus of elasticity) and MOR (modulus of rupture) were evaluated after full-cell vacuum/pressure treatment using a 3.0 % concentration followed by kiln-drying at 15 and 30 % moisture contents with heating the preservative at 30 and 40 ºC. The results showed that MOE ...
I Usta, M Hale


Measurement of wood decay by dynamic MOE in an accelerated soil contact test
2008 - IRG/WP 08-20390
Current laboratory and field testing of preservatives involves various techniques to determine the extent of fungal attack, including visual inspection, mass loss, and static bending and compression strength measurements. The objective of this study was to compare decay measurement by conventional compression strength versus dynamic MOE, employing small wood stakes in an accelerated laboratory so...
Gan Li, D D Nicholas, T P Schultz


Laboratory and field exposures of FRT plywood: Part 1. Physical test data
2008 - IRG/WP 08-40426
Our understanding of the laboratory induced degradation with fire retardant systems is currently limited since we are unable to correlate laboratory steady-state experiments with actual in-service field degradation. Current model studies have generally been limited to isothermal rate studies with selected model FR chemicals. Other factors also play a major role in the degradation of FR-treated woo...
H M Barnes, J E Winandy, C R McIntyre


Categorization of 300 timber, bamboo and cane grown in Bangladesh based on their families, origins, growths, physical and mechanical properties
2009 - IRG/WP 09-10684
In this study the 300 timber, bamboo and cane plants grown in Bangladesh have been classified into various categories based on their taxonomic families, origin of species, rate of growth, color of wood, texture of wood, shrinkage of wood, equilibrium moisture content (EMC) of wood, flammability of wood, cutting and sawing properties of timber, finishing and polishing qualities of wood, machining p...
A K Lahiry


Impact of decay and blue stain causing fungi on the structural integrity of wood
2009 - IRG/WP 09-10699
The potential influence of diverse decay patterns caused by different brown rot provoking basidiomycetes on the structural integrity of wood was investigated. Additionally the potential impact of blue stain on the structural integrity was examined. Therefore decayed Norway spruce (Picea abies Karst.) specimens representing a wide range of mass loss, caused by four different brown-rot fungi and one...
C Brischke, C Welzbacher, T Huckfeldt, F Schuh


Degradation of wood veneers by Fenton’s reagents: effects of low molecular weight phenolic compounds on hydrogen peroxide decay and tensile strength loss
2009 - IRG/WP 09-20400
Pine wood (Pinus sylvestris) veneers strips were incubated in acetate buffer containing hydrogen peroxide and iron to mimic mechanisms of brown rot decay and assess the degradation of cellulose through analysis of the tensile properties of the decayed wood. The tensile properties of thin wood strips treated with Fenton system reagents or precursors were determined and correlated to weight loss as ...
Yanjun Xie, R Well, Zefang Xiao, B Goodell, J Jellison, H Militz, C Mai


Effects of concentration and temperature of CCA and CCB on wood strength of Turkish fir (Abies bornmulleriana Mattf.)
2009 - IRG/WP 09-40450
The purpose of this study was to present evidence for the effects of concentration and temperature of solutions of water-borne preservatives (chromated copper arsenate, CCA and chromated copper boron, CCB) on the static bending properties (modulus of elasticity, MOE and modulus of rupture, MOR) of Turkish fir (Abies bornmulleriana Mattf.). Wood samples were mechanically tested after a mild full ce...
I Usta, M Hale


Wettability and bonding strength of wood thermally-treated with different combinations of soy oil and chemical additives
2009 - IRG/WP 09-40454
Thermal treatment is a method which has gained wider acceptability as an alternative to the chemical treatment in wood preservation. In order to maximize the benefits of this technique several options have been adopted including the use of soy oil in transferring the heat to the wood. Available information on thermal treatment in general and the oil method in particular show that there are still n...
L Awoyemi, P A Cooper, T Ung


The Use of Micro-Tensile Testing to Assess Weathering Decay and Oxidative Degradation of Wooden Items
2010 - IRG/WP 10-20433
This paper presents a method to study the weathering performance of wooden items and to assess the oxidative degradation of wood via the Fenton reaction. Weathering resistance and photo-stability of wood was tested using pine wood (Pinus sylvestris) veneer strips measuring approximately 60 µm in thickness. The veneer strips were treated using a reactive chemical to impart surface protection. The ...
C Mai, Yanjun Xie, Zefang Xiao, P D Evans, H Militz


Diagnosis of failures in wood beams from historical house in Banská Štiavnica – Relations between ultrasonic measurements and bending properties
2010 - IRG/WP 10-20437
Various degrees of rot and other damages in ceiling beams with dimensions of 6500-8800 x 160-200 x 240-310 mm (length x height x width) situated in one historical bourgeois house in the UNESCO town Banská Štiavnica, Slovakia were determined visually and by the PUNDIT-plus ultrasonic device. Subsequently, for seventeen of the most bio-damaged fir (Abies alba Mill.) beams chosen for exchange were ...
L Reinprecht, M Pánek


Photostabilization of Wood with Higher Molecular Weight UV Absorbers
2010 - IRG/WP 10-30524
Higher molecular weight UV absorbers were created by reacting the epoxy-functionalized UV absorber 2-hydroxy-4(2,3-epoxypropoxy)-benzophenone (HEPBP) with maleic, phthalic or succinic anhydride. The ability of the UV absorbers to photostabilize wood was then examined. FTIR-spectroscopy confirmed that HEPBP reacted with phthalic anhydride to create a polyester that preserved the UV-absorbing benzop...
P D Evans, M J Chowdhury


Evaluation of ACQ-D treated Chinese fir and Mongolian Scots pine with different post-treatments after 20 months of exposure
2010 - IRG/WP 10-30530
The performance of alkaline copper quat-type D (ACQ-D) treated Chinese fir (Cunninghamia lanceolata Hook.) and Mongolian Scots pine (Pinus sylvestris Linn. var. mongolica Litv.) stakes after 20 months exposure in Chengdu and Guangzhou of southern China were evaluated according to AWPA standard E07-07. The ACQ-D treatments used two concentration levels (0.5 and 1.0%) and four different post-treatme...
Lili Yu, Jinzhen Cao, Wei Gao, Haitao Su


Influence addition of boron compounds to adhesives on the bonding quality and fungicidal properties of glued wood
2010 - IRG/WP 10-40497
Wood is one of the most important construction materials. However, users of wood face two issues: limited dimensions and insufficient durability. These issues have been overcome with the development of bonding and wood preservation. The preservation of glued wood is elucidated in this paper. Through the addition of boric acid to adhesives, we tried to improve the fungicidal properties of glued woo...
M Humar, B Lesar, A Ugovsek, M Kariz, P Kralj, M Šernek


Preliminary Observations of the Photostabilization of Wood Surfaces with Cerium Oxide Nanoparticles
2010 - IRG/WP 10-40504
Reactive transition metal compounds, wood modification and grafting of UV absorbers have all been used to photostabilize wood. Some of these approaches are promising, but the toxicity of certain reactive transition metal compounds and the cost of wood modification and grafting have restricted their commercial applications. Hence, more cost-effective and environmentally friendly methods of protecti...
Chunling Liu, A Ahniyaz, P Evans


Previous Page | Next Page