Comparison of performance of wood preservatives in laboratory and field tests of treated commodities
1993 - IRG/WP 93-20010
The purpose of laboratory tests for evaluating efficacy of wood preservatives is usually to establish toxic values against standard strains of wood decay fungi. Exposure conditions are usually chosen as optimal for fungal growth. Toxic values so determined serve as a guide as to expected performance of the preservative in field stake tests or in above ground exposure tests. Test material is select...
M E Hedley


Non-destructive detection of the presence and behaviour patterns of wood-destroying insects
1988 - IRG/WP 2302
An apparatus, designed for the automatic recognition of the presence and of specific behaviour patterns of wood-boring insects, is introduced. From a wood sample, a mixture of noise and action induced substratum vibrations is picked up, amplified, filtered and translated into a sequence of computer-readable numbers which are passed to a microcomputer-based signal-pattern-recognition. If an incomin...
M Pallaske


Siderophore production by Trichoderma spp. and its importance in the biological control of wood decay fungi
1994 - IRG/WP 94-10070
Competition for iron as well as other micro-nutrients is an essential component of the microbial ecology of many ecosystems. A wide range of micro-organisms including fungi and bacteria have been shown to increase their ability to efficiently capture iron through the production of specialised iron chelating compounds called siderophores. Since iron is in low supply in wood and has been implicated ...
U Srinivasan, A Bruce, T L Highley


Alternatives to preliminary oven-drying prior to spot-testing treated timber for borate or TBTN preservative penetration
1995 - IRG/WP 95-20067
Commonly-used penetration test procedures for timber treated with borate or organotin wood preservatives demand preliminary oven-drying before application of the spot-testing reagent(s), in order to achieve reliable results. The delay of 12 hours or more during oven drying is often a nuisance. Modifications to the spot-testing procedures, involving alternative solvents and acidification conditions...
M J Kennedy, A Zosars, J Norton


The effect of alternative pre-conditioning procedures on the durability of wood based board materials to decay fungi
1997 - IRG/WP 97-20105
In the biological testing of wood based board materials it has been shown that exposure of boards in a closed vessel system may lead to inaccurate results due to the build up of volatile substances that inhibit the test fungi. It is thought that this is a transitory effect of freshly manufactured boards. In the European standard for testing fungal durability of board materials which is currently u...
S F Curling, R J Murphy, J K Carey


A soil-less test of treated wood
1978 - IRG/WP 2105
The objective of this work is to devise an accelerated test for preservatives to be used in places away from soil contact. There may be compounds or mixtures which will protect wood or wood derived materials from decay in such articles as sash and doors, boardwalks, steps, laminated arches and the like, and possess properties that make them preferable to the heavy-duty preservatives used for poles...
E A Behr


Status of Work on OECD Test Guidelines for Emissions of Wood Preservatives to the Environment
2005 - IRG/WP 05-50224-3
In April, 2003, OECD published an ESD on wood preservatives that provides guidance on how to estimate emissions: 1) during the wood preservative application processes and storage of treated wood prior to shipment; and 2) from treated wood-in-service. The ad hoc Expert Group that developed the wood preservatives ESD identified the need to develop Test Guidelines to estimate the amount of biocides ...
W Jakob


A bioassay for appraising preservative protection of wood above ground
1978 - IRG/WP 2124
A bioassay, using the mold fungus Aspergillus niger, gave results that were correlated with amounts of pentachlorophenol and tributyltin oxide in pine sapwood treated with solutions ranging in strength from 0.016 or below to 5%. Limited bioassay estimates of penta in commercially treated millwork corresponded to estimates by lime ignition. The assay fungus exhibited somewhat greater tolerance of t...
T C Scheffer, L Gollob


Co-operative research project on L-joint testing. Sampling after 18 months exposure
1984 - IRG/WP 2233
In September 1983, Document No: IRG/WP/2208 was distributed giving guidance on sampling after 8 months exposure (due 1 December 1983 for those L-joints exposed on schedule on 1 April 1983), and including tables on which to record the test results. No major problems have been notified to Princes Risborough Laboratory concerning the sampling method. It is therefore proposed that the next sampling, a...
J K Carey, A F Bravery


Detection and estimation of Hylotrupes bajulus L. wood damages by ultrasonics
1990 - IRG/WP 2350
To evaluate the validity of the ultrasonic application in the detection and evaluation of wood damages produced by Hylotrupes bajulus L. larvae, some laboratory tests were made with small wood samples. The pulse through transmission method was used. The transit time of ultrasonic pulses in transversal sections, radial and tangential, of the samples was measured. The increment of the transit time o...
G Prieto


An attempt to grow dry rot fungus Serpula lacrymans on mortar substrate in non-sterile conditions
1989 - IRG/WP 1385
According to many experts, Serpula lacrymans is probably the most dangerous wood destroying fungus in houses. Investigations of KOCH, A.P. (2) showed that incidence of this fungus in percent was around 20% when the frequency of some other standard fungi was far below (Coriolus versicolor: 0.2% for example). The work presented here is a part of a program carried out at CTFT for assessing the resist...
L N Trong


Interactions between water-borne preservatives and emulsion additives that influence the water repellency of wood
1991 - IRG/WP 2374
Incorporation of non-polar additives into water-borne treatments through of emulsion technology can greatly improve the physical characteristics of wood in service. Of specific interest with these emulsions is their effectiveness in reducing the rate of wood swelling. We have observed that the presence or absence of preservatives can often significantly influence the resultant effectiveness of the...
A R Zahora


A bioassay to determine preservative retention in hardwoods and southern pines
1982 - IRG/WP 2183
In this paper the author discusses and suggests a new method of evaluating preservative retention in treated woods by means of bioassays. Twelve North American species were tested with different retention levels of pentachlorophenol (PCP) and copper/chrome/arsenic (CCA) preservatives. The results observed in this work show that among other fungi, Aspergillus niger responds to both preservatives, w...
J C Moreschi


A test method to simulate above-ground exposure
1978 - IRG/WP 2112
The simulated above-ground exposure technique described is worthy of consideration as a simple procedure to determine the relative decay resistance of preservative-treated wood exposed to a moderate decay hazard. The method may readily be modified to allow testing of other materials such as plywood by simply enlarging the slots cut in the modified feeder strips. The method by no means completely s...
J A Butcher


The need for realism in wood preservation research. A key address
1983 - IRG/WP 3254
The approval of a chemical for use as a timber preservative and the design of in service retention requirements represents an act linking fundamental research and commercial timber preservation. How difficult is it to translate figures generated through controlled experimentation into working specifications and how confident can we be in the methods used to provide such figures? The chairman of Wo...
L E Leightley


Preservation of wood-based panels against fungi and insects and and testing its efficiency
1976 - IRG/WP 270
Wood-based panel products which are made of susceptible wood species may be destroyed by fungi under wet conditions and by termites. The glues do not provide sufficient protection unless very high concentrations are applied. Particle boards and fibre boards are not susceptible to beetle infestation, although some species may attack plywood. Various types of preservatives provide sufficient protect...
G Becker, M Gersonde


Micromorphology of decay in Keruing heartwood by the basidiomycetes Phellinus contiguus and Dacrymyces stillatus
2002 - IRG/WP 02-10454
This study aimed to characterise the micromorphology of fungal decay in a wooden handrailing in an above ground exposure at the Thames embankment in London. Keruing heartwood (Dipterocarpus spp.) was determined as the construction timber and the two basidiomycetes Phellinus contiguus and Dacrymyces stillatus identified as main decay organisms. Their decay patterns within Keruing heartwood were...
G Kleist, M Ray, R J Murphy


Some aspects of testing water repellents
1998 - IRG/WP 98-40113
Several test methods are used to determine the efficiency of water repellent treatments on wood. The most common are: contact angle measurement, swelling rate of samples immersed under water and, the increase in mass of wood samples with time or after a fixed period of time either fully immersed under, or partially immersed in or floating on water. In this paper, some fundamental aspects of the l...
D Lukowsky, M Farnow, T Rypstra


Preliminary evaluations of a small wafer assay for screening potential biological control agents
1989 - IRG/WP 2332
Screening potential biological agents for controlling wood decay fungi poses a dilemma. The ideal test would eliminate as many variables as possible. Most tests utilize pure cultures of the test organism on an artificial media which in no way resembles wood. The use of sawdust improves this approach, but the sawdust increases fungal access to the lignocellulose matrix, potentially inflating the im...
C M Freitag, J J Morrell


Leaching of active components from preservative-treated timber. Stages 2 & 3: Laboratory testing and comparison with semi-field testing
2004 - IRG/WP 04-20303
This part of the project is focussed on leaching from preservative-treated wood obtained by the laboratory test method CEN/OECD draft guideline, February 2003 ”OECD guideline for the testing of chemicals proposal for new guideline XXX. Estimation of Emissions from Preservative-treated Wood to the Environment: Laboratory Method for wood held in the storage yard after treatment and for wooden comm...
N Morsing, B Lindegaard


Co-operative research project on L-joint testing. Progress report to March 1986
1986 - IRG/WP 2272
Further sets of data received from CTFT (France) after 18 months exposure, BAM (Germany) after 18 months exposure, STU (Sweden) after 9.5 months exposure and TI (Denmark) after 12 and 17.5 months exposure are presented and discussed in conjunction with data previously reported. The new data are generally in agreement with those presented previously and indicate the major difference between the co-...
J K Carey, A F Bravery


Intraspecific variability of durability of Wapa courbaril (Eperua grandiflora) against Antrodia sp. and Coriolus versicolor: effect of radial and height position in the stem
2004 - IRG/WP 04-10531
The variation of a lesser-used species, Eperua grandiflora attacked by brown and white rot has been examined. Trees of this specie showed differences in their behaviour against the type of rot used and also showed evidence of intra and inter tree variation. The “tree” effect is very significant concerning natural resistance. In the same way, there is variation of durability observed according ...
N Amusant, J Beauchêne, M Fournier


Improved preservative penetration of spruce after pre-treatment with selected fungi. II. Creosote treatment, analysis and strength testing
1998 - IRG/WP 98-40106
This paper describes the creosote treatment and analysis of logs pre-treated with selected fungal agents as a method of increasing the porosity of the wood prior to preservative treatment. The paper also reports the subsequent strength testing of the timber to evaluate the effects of the fungal pre-treatment on the structural integrity of the wood. European spruce logs were pre-treated with eithe...
E J Tucker, A Bruce, H J Staines, B Rosner, K Messner


Suitability of cotton strip testing as a screening method for the development of wood preservative formulations
2003 - IRG/WP 03-20270
This paper outlines a simple and rapid test method for screening the efficacy of wood preservative formulations against microbiological attack using cotton strips. The method was evaluated against soft rot and was found to provide reliable information on the protection of lignocellulosic material against microbiological attack. The assessment is based on visual interpretation of decay and on a sim...
H Leithoff, I Stephan, H Härtner


Creosote losses due to ageing methods prior to laboratory efficacy testing
2002 - IRG/WP 02-20256
Laboratory efficacy testing of creosote is affected by the impact of volatile components on the fungal growth. European test methods for assessing efficacy against Basidiomycetes and soft rot fungi is based on two standard methods, EN 113 and ENV 807 respectively. Combined with both fungal tests two pre-treatment methods are commonly used, namely EN 84 (leaching) and EN 73 (evaporation). Within th...
J Van Acker, K Ghekiere, M Stevens


Previous Page | Next Page