Your search resulted in 425 documents. Displaying 25 entries per page.


Bioresistance of Poplar Wood Compressed by Combined-Hydro-Thermo-Mechanical Wood Modification (CHTM) Process
2010 - IRG/WP 10-40532
Bioresistance of treated Poplar wood by CHTM process (Combined-Hydro-Thermo-Mechanical Wood Modification) was studied in the current research work. Resistance against brown rot fungus Gloeophyllum trabeum as well as the soft rot decay was the main concern of this work. Poplar wood blocks were hydrothermally treated at temperatures of 120,150 and 180°C for holding time of 0, 30 and 90 min. afterwa...
L Khademi-Bami, B Mohebby


Biological resistance of acetylated particleboards exposed to white (Trametes versicolor (and brown (Coniophora puteana) rot fungi
2010 - IRG/WP 10-40534
This research was conducted to investigate the effect of acetylation on bioresistance of particleboard produced from acetylated wood chips of Fagus orientalis exposed to white (Trametes versicolor (and brown (Coniophora puteana) rot fungi. After 12 hours soaking in acetic anhydride, in order to achieve three level of weight gains, 5, 9 and 16%, acetylated particles were heated in an oven at 120 c...
M Ghorbani kokandeh, K Doosthoseini, A N Karimi, B Mohebby, H Asghari


Gene expression analysis of a copper-tolerant brown rot fungus on MCQ-treated wood
2011 - IRG/WP 11-10748
Most brown rot fungi are copper-tolerant, which makes them difficult to control with copper-based wood preservatives like MCQ. To better understand what biological processes are regulated, we used our model species, Antrodia radiculosa, to examine expression of genes on MCQ-treated wood. Our hypothesis was genes that decreased copper bioavailability would be up-regulated early, when wood showed ...
J D Tang, A Perkins, S V Diehl


Decay resistance attributes of teak (Tectona grandis L. f.) wood: comparison of the fungicidal activities of quinones
2011 - IRG/WP 11-10752
The implication of quinones in decay resistance of teak wood is controversial. To better understand the role of individual quinone in this property, we studied the correlations between this latter and the content of 2-(hydroxymethyl)anthraquinone, tectoquinone, anthraquinone-2-carboxylic acid, 1,4-naphthoquinone, lapachol and the new compound 4’,5’-dihydroxy-epiisocatalponol found in teak wood...
F B Niamké, N Amusant, N Lemenager, G Chaix, M-F Thévenon, C Baudassé, S Kati-Coulibaly, A Amissa Adima, I Gossan Ado, C Jay-Allemand


Study of the durability of the Maderon® against wood decay fungi and insects
2011 - IRG/WP 11-40548
Many industries produce residues that are not easily degradable. One of these is nut husks which, due to their high level of resistance to biological and environmental degradation, have become an ecological problem. Maderón® is a material invented and patented in Spain employed as an ecological substitute and a modern alternative to certain uses of wood. At present, Maderón® is commercialized ...
M T Troya, F Llinares, P Jiménez, J I Fernández-Golfín, M Conde, R Díaz


Influence of soil moisture, Sarawak soil types and decay types on decay susceptibility of rubberwood and kelempayan
2012 - IRG/WP 12-10780
Wood and soils are important natural resources of the land, the former widely used as structural supports in contact with the latter. Many low durability wood species exposed to soil contact has reportedly high incidence of decay failures in poorly treated and untreated materials depending on soil types, properties and soil microbial virulence. This paper probes the relationship of the main soil t...
A H.H. Wong, P K.F. Chong, J Sabang


Effects of microclimate, wood temperature and surface colour on fungal disfigurement on wooden claddings
2012 - IRG/WP 12-20490
Wooden claddings are common in façades in Norway, and Norway spruce (Picea abies) is the most frequently used species. The cladding is a major part of the facade, and it has visual requirements that may define the aesthetic service life. The visual changes that occur during weathering can be colour changes, abrasion or wear, blistering, flaking, and even cracks in the wood or coating, but more of...
L Ross Gobakken, G I Vestøl


In-ground variability of decay intensity within a test field
2012 - IRG/WP 12-20496
Timber exposed in the ground faces most severe conditions in terms of exposure to wetting and fungal decay in the terrestrial environment, therefore wood durability tests are often conducted in test fields preferably ensuring the occurrence of all relevant decay organisms. One can also expect differences in decay within an individual field-test site due to localized distribution of certain organis...
C Brischke, S Olberding, L Meyer, T Bornemann, C R Welzbacher


Evaluation of Five Novel Organotin(IV) Complexes as Wood Preservatives
2012 - IRG/WP 12-30590
Three selected non durable tropical wood species namely Alstonia scholaris (pulai), Macaranga triloba (mahang) and Hevea brasiliensis (rubber) were chemically impregnated with five novel organotin(IV) complexes using vacuum-pressure treatment method. The objectives of this study were to determine the treatability and efficacy of novel organotin(IV) complexes against white and brown rot decay fungi...
M M Rahman, I Jusoh, M A Affan, A Husaini


Field-testing of Norway Spruce Claddings with Monitoring of Moisture Content, Material Temperature and Microclimate
2012 - IRG/WP 12-20502
The physical function of a cladding is to protect the interior construction. Under normal circumstances the performance requirements can be met for a very long time, meaning that the technical service life of a wooden cladding can be very long. Since the cladding is a major part of the facade, it also has visual requirements that may define the aesthetic service life, and often it is much shorter ...
G I Vestøl, L Ross Gobakken


Influence of a pulsed electric field on the growth of surface fungi
2013 - IRG/WP 13-10795
The colonization of mold and staining fungi are not only an aesthetical problem. Blue stain fungi are able to penetrate paint films. Maintenance of coatings on wood are time consuming and costly. A new approach uses a pulsed electric field (PLEOT) in order to protect wood against surface fungi. This technology is evaluated in non-sterile laboratory conditions on different coated and uncoated Scots...
M Starck, A Treu


Determination of the natural durability of solid wood against wood-destroying fungi - a European round-robin test
2013 - IRG/WP 13-20511
In Europe the durability of wood against wood-destroying basidiomycetes is tested according to CEN/TS 15083-1 (2005). Hitherto existing experience with this standard is quite heterogeneous and results from previous round-robin tests have stayed unreported or have been reported incompletely. In particular the need for natural pre-weathering of the test specimens to allow potential detoxification of...
C Brischke, C R Welzbacher, A Gellerich, S Bollmus, M Humar, K Plaschkies, W Scheiding, G Alfredsen, J Van Acker, I De Windt


Predicting the Rate of Decay, and the Potential for Misinterpretation of Proper Scientific Method
2013 - IRG/WP 13-20525
Predicting the rate of fungal attack in wood-based materials and its effect on properties remains the holy grail of wood products pathologists; however, achieving this goal is difficult because of the many variables associated with the process. This paper reviews some of the more important aspects of the decay process in relation to test methodology and then discusses how data are sometimes used b...
B S Goodell, J J Morrell


The activity of a wood-decaying fungus during drying and rewetting cycles measured by isothermal calorimetry
2013 - IRG/WP 13-20526
Wood decaying fungi are an essential part of any ecosystems as they are the main decomposers of cellulose and lignin-containing materials. But as wood is a common building material the risk for decay fungi growth and subsequent degradation of our construction material is a concern. There are important physiological aspects of the growth and activity of decay fungi that are unknown today, and witho...
S Johansson, L Wadsö, A Pilgård, G Alfredsen


Effect of biodiesel on Performance of Isothiazolone
2013 - IRG/WP 13-30625
Biodiesel has a number of attractive properties, including the ability to readily solubilize a number of biocides and a tendency to reduce odors associated with other solvents such as petroleum-based diesel. Biodiesels, however, have also been implicated in reduced performance of some, but not all preservatives. It is important to assess the effects of biodiesel on each biocide. Soil block tests ...
Cheng Hua-Kang, L Jin, C Freitag, J J Morrell


Postia placenta cellulase gene expression in modified wood during incipient decay
2013 - IRG/WP 13-40626
In optimization of modified wood, it is important to understand the mode of action of the wood modification and how the fungi response to it. The aim of this study was to investigate the expression of cellulases during the first two weeks of Postia placenta exposure in acetylated, DMDHEU-treated and thermally modified as well as in untreated wood. Using real-time PCR, the gene expression patterns ...
R Ringman, A Pilgård, K Richter


Influence of Heat Treatment Medium on Fungal Resistance of Beech Wood
2013 - IRG/WP 13-40643
Hydrothermal treatment of beech wood (Fagus orientalis) performed in acidic, neutral and alkaline buffered mediums in 160 and 180°C. White rot fungi (Coriolus versicolor) and brown rot fungi (Coniophora puteana) were used to determine the influence of heat treatment mediums on the behaviour of fungal resistance. White rot of wood digest lignin rather than cellulose; while brown rot digests the ce...
A Talaei, A Karimi, M-F Thévenon


Using hyperspectral imaging to detect and quantify mould and blue stain on coated and uncoated wood
2014 - IRG/WP 14-10822
Hyperspectral imaging has been applied on the surface of samples of coated and uncoated Norway spruce (Picea abies) as a new technique to detect and quantify growth of mould and blue stain fungi. Principal Component Analysis of the hyperspectral images resulted in a clear visualization of the fungi and the amount of mould coverage could be estimated. This indicates that NIR hyperspectral imaging c...
L Ross Gobakken, I Burud, A Flø, K Kvaal, T K Thiis


The effects of copper proximity on oxalate production in Fibroporia radiculosa
2014 - IRG/WP 14-10823
Copper remains a key component used in wood preservatives available today. However, the observed tolerance of several critical wood rotting organisms continues to be problematic. Tolerance to copper has been linked to the production and accumulation of oxalate, which precipitates copper into insoluble copper-oxalate crystals, thus inactivating copper ions. The purpose of this study was to assess d...
K M Jenkins, C A Clausen, F Green III


Protein extraction from wood decay fungus Postia placenta
2014 - IRG/WP 14-10827
Wood decay fungi (often distinguished as white rot and brown rot) belonging to the basidiomycetes, are common inhabitants of forest litter, where they play an important role in carbon cycling. Brown rot fungi are perhaps the most important organism involved in the degradation of wood products, and of considerable economic importance. Brown rotted wood loses strength very early because of the rapid...
A Pilgård, P Arnold, K Richter


The Chelator Mediated Fenton System in the Brown Rot Fungi: Details of the Mechanism, and Reasons Why it has Been Ineffective as a Biomimetic Treatment in some Biomass Applications – a Review
2014 - IRG/WP 14-10828
The chelator-mediated Fenton (CMF) reaction requires the action of two types of chelating compounds. The first chelator, oxalate, solubilizes and then sequesters iron, and the second chelator reduces iron. Iron reduction must be controlled near the fungal hyphae to prevent damaging Fenton chemistry from occurring in that location. Similarly, iron reduction must be promoted within the wood/plant ce...
B S Goodell, M Nakamura, J Jellison


A comparison of the resistance of pyrethroid-treated wood to damage by Coptotermes acinaciformis in Australia and C. formosanus in China and the USA
2014 - IRG/WP 14-10830
Field trials, using a single aboveground method of exposure, were used to assess a range of retentions of two pyrethroids (bifenthrin and permethrin) in Pinus radiata D. Don sapwood against two species of Coptotermes in three countries to provide directly comparable results. Coptotermes acinaciformis (Froggatt) in Australia, C. formosanus Shiraki in China and C. formosanus in the USA consumed simi...
J Creffield, M Lenz, D Scown, T Evans, Junhong Zhong, B Kard, J Hague, K Brown, E Freytag, J Curole, R Smith, T Shupe


Effectiveness of Copper Indicators in Treated Wood Exposed to Copper Tolerant Fungi
2014 - IRG/WP 14-20554
Wood treated with a copper based wood preservative will typically turn a green color. While the depth of copper penetration can be readily discerned from the green color of the copper it is standard practice in research and commercial treating plants to make use of a color reagent such as Chrome Azurol S, Rubeanic acid or PAN indicator to reveal the penetration more clearly. When copper treat...
L Jin, K Brown, A Zahora, K Archer


Reducing Extractives Stain in Western Red Cedar Sidewall Shingles
2014 - IRG/WP 14-30654
One of the aesthetic challenges that western red cedar shingles face is extractives redistribution stain, particularly in unpainted sidewall applications. Dip and pressure treatments with a mixture of quaternary ammonium compounds and alkyl amine oxides were investigated for their ability to prevent this stain. After nine months of exposure in Vancouver, extractives stain was present on nearly all...
R Stirling


Decay resistance of wood-plastic composites reinforced with extracted or delignified wood flour
2014 - IRG/WP 14-40655
The moisture and decay resistance of wood-plastic composites (WPCs) reinforced with extracted or delignified wood flour (WF) was investigated. Three different extractions were preformed: toluene/ethanol (TE), acetone/water (AW), and hot water (HW). Delignification (DL) was performed using a sodium chlorite/acetic acid solution. All WPCs specimens were made with 50% by weight HDPE and WF, first com...
R E Ibach, Yao Chen, N M Stark, M A Tshabalala, Yongming Fan, Jianmin Gao