An illustrated comment on the soft rot problem in Australia and Papua New Guinea
1977 - IRG/WP 296
A brief survey of soft rot is presented, with particular reference to attack of preservative treated hardwood transmission poles in Australia. Possible explanations of why the preservatives are failing to protect the poles are discussed, together with current efforts to produce control measures. Examples of soft rot in variously treated eucalypt or pine specimens are shown to illustrate the morpho...
H Greaves


Changed permeability and surface properties of hornbeam wood due to its degradation by erosive strain of Phanerochaete chrysosporium
2004 - IRG/WP 04-40290
Specimens of hornbeam wood were submitted to a medium-term degradations by erosive fungus Phanerochaete chrysosporium. Biodegradations of specimens resulted in their apparent structural alterations, changes in permeability and increased intensity of interactions with polar liquids. Modified physical properties of biodegraded wood may significantly influence its penetration with polar media and che...
R Solár, S Kurjatko, L Reinprecht, M Mamon, V Vacek


CCA modifications and their effect on soft rot in hardwoods. Part 2
1983 - IRG/WP 3244
The work outlined in this document is a continuation of that presented in Document No: IRG/WP/3201. The findings described in the previous paper are summarised below: a double treatment of CCB followed by arsenic (CCB+A) is more effective than a double treatment of boron followed by CCA (B+CCA) or a single treatment of CCA, CCB or CCAB in controlling soft-rot due to Chaetomium globosum in birch. C...
S M Gray, D J Dickinson


Supplementary experiment to the main trial (IRG/WP/367, 384) to determine the performance of preservative treated hardwoods with particular reference to soft rot
1977 - IRG/WP 3101
The field experiment being carried out by the IRG (described in document IRG/WP/367) is designed to obtain information on the performance of a preservative in different hardwoods in ground contact. A total of 57 timber species is being examined and 36 different field sites are involved representing a complete range of climatic conditions. IRG document WP/384 describes the treatment details of the ...
F W Brooks, C R Coggins, D J Dickinson


The natural durability assessment of secondary hardwood species - laboratory tests
1998 - IRG/WP 98-10295
Laboratory tests have been undertaken to assess the natural durability of 16 species of lesser known hardwoods, or hardwoods from non-traditional sources, including teak from three different plantations. Resistance to decay by both basidiomycetes and soil-inhabiting micro-fungi has been established. ´The data indicated that published information on the durability of these timbers should be treat...
J K Carey, S J Hendry


Assessment of the toxicity of some copper-, zinc- and boron-based wood preservatives to the cellar fungus Coniophora cerebella Schröet
1974 - IRG/WP 242
This article reports the use of a method based on the determination of the probability of the protection of timber against destruction by fungi. By converting the probability values to probit values and plotting them as a function of the amount of preservative retained in the timber, curves of the toxic effect are obtained, enabling any timber protection probability to be assessed....
V N Sozonova, D A Belenkov


Collaborative soft rot tests: Paper for discussion in Working Group II
1970 - IRG/WP II 5A
An account of the major part of the collaborative work on laboratory tests of toxicity of preservatives to soft rot fungi initiated by the European Homologation Committee at Delft in 1966 has been published in ‘Material und Organismen’ (1970) as a report of progress. The main objective of these collaborative tests, namely to establish a reliable and acceptable standard test method was not acco...
J G Savory, A F Bravery


Occurrence, prevention and repair of Dry Rot
1990 - IRG/WP 1439
Information about the frequency, detection, identification and repair of Dry Rot attacks (Serpula lacrymans) is summarized from 13 European countries. Based on 28 completed and returned questionnaires it appears that Dry Rot attacks are recognized in all countries participating, and that there is an appreciable similarity in the frequency of attacks and methods of detection and identification. How...
A P Koch


Variation in infection rates of blue-stain, mould and white rot tropical fungi on mixed light Malaysian woods
2000 - IRG/WP 00-10334
The modified 3-week FRIM laboratory method for screening of anti-sapstain formulations against three representative tropical fungi causing blue-stain (Botryodiplodia theobromae), mould (Paecilomyces variotii) and white rot (Schizophyllum commune) infection of sapwood species was used to examine the relative resistance of the sapwood of eight mixed light Malaysian woods, Scots pine (Pinus sylvestri...
A H H Wong, S Ahmad


Final proposals for a field experiment to determine the performance of preservative treated hardwoods with particular reference to soft rot
1976 - IRG/WP 367
A series of hardwood stakes have been prepared and treated in the UK from samples (mainly sapwood) supplied from participants around the world. The stakes include 4 reference species common to each site and, in most cases, at least 2 local species of importance. The treated stakes will be despatched to the co-operating scientists and installed under local conditions. It is hoped that with periodic...
D J Dickinson


Evaluation of fungal remediation of creosote treated wood
1998 - IRG/WP 98-50101-25
Biotechnological remediation of creosote treated wood may be of interest in connection with novel recycling processes. White rot fungi and/or their ligninolytic enzyme systems are supposed to be valuable tools for such processes. This paper reports about results achieved when creosoted wood was treated in solid substrate fermentation with selected white rot fungi after different extraction procedu...
K Messner, S Böhmer


Laboratory tests on light organic solvent preservatives for use in Australia. - Part 6: Soft rot resistance of three fully formulated preservatives on different timber substrates
2000 - IRG/WP 00-30245
The above-ground soft rot resistance of substrates treated with three fully formulated light organic solvent preservatives (Cuprivac Green WR, Impresol WR 205 and Vacsol) was studied using a modified vermiculite burial method. The substrates were sapwood of Pinus elliottii and P. radiata and heartwood of Eucalyptus regnans, Pseudotsuga menziesii, Shorea sp. (a lower and a higher density source) an...
G C Johnson, M A Tighe, J D Thornton


Co-operative work on the performance of treated timber in ground contact
1975 - IRG/WP 344
At the 6th meeting of The International Research Group on Wood Preservation in Vienna, it was decided to approach all interested parties in order to: collate available information, set up collaborative work and to stimulate research on the performance of treated timber, especially hardwoods, in ground contact. In recent years, considerable concern has been expressed about the performance of preser...
D J Dickinson, J F Levy


The use of modulus of rupture and modulus of elasticity in natural durability testing
1997 - IRG/WP 97-20117
Losses in weight, losses in bending strength and changes in elastic behaviour were assessed in a fungus cellar test with beech wood stakes (Fagus sylvatica). Results were gained after 8, 12, 16 and 20 weeks resp . The outcomes show, that the non-durable species beech is very rapidly attacked by fungi and loses up to 60% of its initial bending strength even within the first 8 weeks. Earlier researc...
L Machek, H Militz, W Gard


Natural exposure weathering tests: Their role in the assessment of wood preservative efficacy
1993 - IRG/WP 93-20006
Previous work has demonstrated the potential and usefulness of natural ageing procedures in e evaluation of wood preservative efficacy. This results from the combination of physico-chemical influences and microbiological interactions with both substrate and wood preservative. In this paper, results are presented for a range of biocide types. Discussions are centred on the value of natural exposure...
G R Williams, J Brown


Formation of soft rot cavities in relation to concentric layers in wood fibre walls
1983 - IRG/WP 1185
A large number of timber species attacked by soft rot have been examined using light microscopy. The S2 layers in a large number of the timbers exhibited special structural features in the form of thin concentric layers. Several observations indicate that these layers may be characterised as "weak" zones by being more easily degradable than the surrounding wall layers. The chemical structure of th...
T Nilsson, G F Daniel


Acetylated solid wood. Laboratory durability test (part 2) and field trials
1995 - IRG/WP 95-40048
Degradation of acetylated beech, pine and poplar by soft rot fungi was related to strength loss in a laboratory test. No strength loss was noticed for poplar acetylated to a weight percent gain (WPG) of more than 11.2% and beech with a WPG of 12.8%. Several field trials were set up to determine the durability of acetylated products in practice. They included a field test to determine the durabilit...
E P J Beckers, H Militz, M Stevens


Controlling the sapstain fungus Ceratocystis coerulescens by metabolites obtained from Bjerkandera adusta and Talaromyces flavus
1993 - IRG/WP 93-10024
Sapstain causes severe damage to wood and wood products, posing a major economic problem for the wood industry. The purpose of this study was to determine if metabolites from Bjerkandera adusta and Talaromyces flavus would (1) decolorize stain in wood caused by Ceratocystis coerulescens and (2) prevent sapstain by Ceratocystis coerulescens. We studied the interaction of the sapstain fungus Ceratoc...
S C Croan, T L Highley


Soft rot test of copper/chrome/arsenic treated heartwood of three Malaysian timbers
1991 - IRG/WP 2381
Standardized heartwood blocks of kempas (Koompassia malaccensis), keruing (Dipterocarpus sp.) and tualang (Koompassia excelsa) were impregnated with 0 to 6.3% (w/v) CCA and challenged to decay by a mixed inocula of Chaetomium globosum, Glenospora graphii, Humicola grisea, Petriella setifera and Trichurus spiralis in a containerized vermiculite-burial decay system according to draft CEN/TC 38 WG 4....
A H H Wong, R-D Peek


Soft rot decay of Belian (Eusideroxylon zwageri) wood
1995 - IRG/WP 95-10119
The heartwood of Belian (Eusideroxylon zwageri), an East Malaysian timber species, is naturally durable due to its certain unique anatomical features and high content of extractives. The timber can tolerate years of exposure to hazardous conditions in ground contact and other situations without any significant loss in its strength. A few Belian transmission poles sampled from one locality in Saraw...
A H H Wong, A P Singh


The growth and behaviour of Australian isolates of dry rot fungi, mainly Serpula lacrymans (Schum. ex Fr.) S.F. Gray. A comparision with the world literature
1983 - IRG/WP 1190
In Australia Serpula lacrymans occupies a rather unique environment, being restricted to growth within basal regions of buildings containing masonry. Its rate of timber attack in these situations appears to be far faster than that experienced in other parts of the world. Therefore the question arises as to how Australian isolates (particularly 16508 which has become a "standard" test fungus for so...
J D Thornton, O Collett


Soft rot - Soil burial - Tests. Influence of the water content of the soil on wood decay
1972 - IRG/WP 212
The decay of wood samples buried in the soil is influenced by various factors. Decisive are the water content, the content of organic substances, pH-value content of mineral nutritive substances etc. of the soil. For the tests, carried out by the EMPA until now, it was always started with a water content of 35%, refered to the dry weight of the EMPA-soil = 75% of its water capacity. In order to in...
O Wälchli


A chemical and mycological evaluation of fused borate rods and a borate/glycol solution for remedial treatment of window joinery
1983 - IRG/WP 3225
The possibility of using fused borate rods (Impel Borpatron) and a borate/glycol solution (Boracol-40) for depot impregnation of window joinery has been examined in a co-operative project between The Swedish Forest Products Research Laboratory, The Swedish University of Agricultural Sciences and Prolignum AB. The fused Impel rod is a glassy rod composed of disodium octaborate which readily dissolv...
M-L Edlund, B Henningsson, A Käärik, P-E Dickèr


Treatment details for the field experiment to determine the performance of preservative treated hardwoods with particlar reference to soft rot
1977 - IRG/WP 384
These notes are compiled to complement and supplement Document No: IRG/WP/367 which described the plan for the treatment of the stakes, using a CCA preservative, for the field experiment. This document gives extra details of the treatment characteristics of the different timber species and as such may give IRG members useful information on the sapwood permeability of a range of hardwoods. The repo...
F W Brooks, M R Gayles


Evaluation of the pulsed-current resistance meter (Shigometer®) for determination of the internal condition of utility poles
1979 - IRG/WP 2128
A number of Telecom poles, which had been removed from service to be replaced by a radio link, were inspected using an electrical resistance meter (Shigometer®). These poles were creosoted, non-durable Victorian species in service in New South Wales. Six of these poles, chosen to represent various internal conditions typical of the range of the population tested, are discussed here. Data, from tr...
J D Thornton, W G Seaman, M McKiterick