Chapter 6 - Preservatives of bamboo
2007 - IRG/WP 07-10635-06
Almost all currently available oil-borne, water-borne and compound types of preservatives suitable for the preservation of bamboo or wood have been described along with their classifications, applications, formulations, merits and demerits, history of invention or discovery and development. The preservatives suitable for wood are also considered suitable for bamboo....
A K Lahiry


Collaborative tests on the influence of solvent and drying method on the toxic limit of wood preservatives against Basidiomycetes
1974 - IRG/WP 248
Seven institutes from five countries, Austria, England, France, Germany and the Netherlands have collaborated in a study on the influences of solvent and drying method on the toxic limits of wood preservatives against Basidiomycetes tested according to the agar-block method. Two preservatives, a 25% pentachlorophenol-concentrate and tributyltinoxide were applied to pine sapwood and beech and teste...
T Hof


Environmental exposure to wood preservatives
2000 - IRG/WP 00-50165
The OECD Working Group on Pesticides will hold a workshop on Assessing Environmental Exposure to Wood Preservatives within the context of its Biocides Programme (cf. IRG/WP 99-20182). In the area of risk assessment, OECD countries have given highest priority to developing guidance on how exposure assessments for biocides should be performed. Wood preservatives have been selected since most countri...
R-D Peek


Biological effectiveness of ground-contact wood preservatives as determined by field exposure stake tests
1984 - IRG/WP 3297
Field exposure tests conducted on stakes treated with different creosotes, mixtures of creosote and waxy oil as well as different CCA wood preservatives over a period of 25 years, gave the following results: The CCA preservatives provided excellent biological protection to treated stakes, especially against fungal attack. The CCA Type I, currently approved for use under South African conditions is...
W E Conradie, A Pizzi


Practical testing of wood preservatives to prevent weathering damage and infection by micro-organisms on spruce and pine
1989 - IRG/WP 3530
Brush application, is generally used to prevent wooden window frames from decay caused by influence of weathering and fungi. Accordingly 10 boards of pine (Pinus sylvestris) and spruce (Picea abies) were treated with 10 commercially used wood preservatives. The efficiency of fungicides by using chiptest and blue stain test (EN 152), the effectiveness against weathering as well as the course of col...
R Gründlinger, O Janotta, H Melzer, K Messner


Health and safety aspects of the use of wood preservatives. Preliminary evaluation of the answers to the IRG-Questionnaire on the state of pollution control in the field of wood preservation
1974 - IRG/WP 56
This preliminary evaluation of the answers to the IRG/WP-Questionnaire only gives a general survey on those questionnaires, which the author received until June 13, 1974. Details, such as correlations between importance of wood preservation and pollution control, could not be considered due to lack of time. For the same reason it was not possible so far, to evaluate the additional remarks given in...
H Willeitner


Fungal degradation of wood treated with metal-based preservatives. Part 2: Redox states of chromium
1996 - IRG/WP 96-10164
Concerns have arisen about the leaching of heavy metals from wood treated with metal-based preservatives, such as chromated copper arsenate (CCA). Of particular concern is the toxic redox state of chromium and arsenic in aging and decayed CCA-treated wood. Generally, hexavalent chromium is more toxic than trivalent chromium and trivalent arsenic is more toxic than pentavalent arsenic. The desired ...
B Illman, S Bajt, T L Highley


The effective control of moulds on freshly impregnated wood
2004 - IRG/WP 04-30352
Beside natural timber it is known, that moulds can also groth at the surface of impregnated wood. This material shows “defects” like resistant dark spots or color changes and causes complaints. During the last years, the problem by moulds seems to increase. Laboratory studies were carried out to show the effect of impregnations against moulds. Wood samples (Pinus sylvestris L.) were impregn...
G Cofta, K Lutomski, P Jüngel


Performance of treated spruce in Canadian field test sites
1989 - IRG/WP 3506
Spruce material under test in Canadian field test sites is performing better than anticipated. From the comparison of the performance of spruce treated with various preservatives, it appears that penetration may be far more important on durability performance than the preservative itself or the retention of preservatives in the wood. However, there is still insufficient data on the influence of pe...
J P Hösli, E E Doyle


The use of zirconium as an inert fixative for borates in preservation
2001 - IRG/WP 01-30256
Stand-alone borates have been used in internal protected situations as wood preservatives for about 60 years. They have not been deemed acceptable for external situations because of their leaching characteristics. Work carried out to reduce the leachability of borates has been reviewed briefly here, and a specific fixation agent based on zirconium has been tested in standard leaching and decay tes...
J D Lloyd, J L Fogel, A Vizel


Patterns of long-term performance - How well are they predicted from accelerated tests and should evaluations consider parameters other than averages?
1998 - IRG/WP 98-20130
This paper is a discussion of whether different service-life distribution patterns of products treated with unlike preservatives can be predicted, modeled, characterized, or even anticipated from accelerated laboratory tests. Graphic displays of data from Forest Products Laboratory field plots with preservative-treated and fire-retardant-treated stakes demonstrate the importance of local environme...
R C De Groot, J W Evans


Risk assessment and the approval of wood preservatives in the United Kingdom
1995 - IRG/WP 95-50040-23
An approval system operates in the United Kingdom (UK) for the regulation of wood preservatives. The regulatory authority uses a risk assessment approach to evaluate how far the potential for harm to people and the environment from wood preservatives is likely to be realised in practise, and hence the controls required for products to be, used safely. The evaluation for approval purposes also take...
R M Turner


Effect of double-vacuum and vacuum-pressure impregnation with water-borne preservatives on the dimensional characteristics of spruce
1990 - IRG/WP 3613
Air-dried planed spruce (Picea abies) samples were treated with a water-borne preservative (micro-emulsion) and one oil-borne type both containing azaconazole and deltamethrin. Each set of samples contained equal number of specimens with different growth ring orientation, heartwood content and density. In addition to the preservative retention and the penetration of a.i., the swelling of the sampl...
J Van Acker, M Stevens, G Rustenburg


Literature survey on the permanence and distribution of salt-type wood preservatives
1969 - IRG/WP III 1B
The objective of this survey is generally to review some of the more important published work dealing with the distribution and permanence of salt-type waterborne wood preservatives in treated timber. The survey is limited to the major chrome-containing formulations and the classification system proposed by Becker (1964) has been adopted throughout. CK - chromium, copper (copper, chrome); CKA - c...
Anonymous


Preservatives treatment and field test monitoring of spruce pole stock: CCA and fumigant treatments
1990 - IRG/WP 3619
The fumigants trichloronitromethane (chloropicrin) and sodium N-methyldithiocarbamate (SNMDC) were used to treat red spruce pole stock, either CCA treated or untreated, through holes bored through the pole's center. The poles were analyzed for the presence of microorganisms immediately before ground installation and again after installation at a pole test site. Monitoring of fumigant move...
A J Pendlebury, B Goodell


Methods of treatment of wood preservatives. The selection of appropriate preservation process with particular reference to mixed tropical forest resources. A key address
1982 - IRG/WP 3177
All wood is biodegradable. Many timber species have, however, sufficient natural durability to permit their use, particularly in protected situations, without any special precautions. Many others, of course, are readily attacked by insects and where there is sufficient moisture and air, by wood-decaying fungi. It is these timber species which benefit most from treatment with wood preservatives. Ev...
C R Levy


Washboard effect: A surface deformation of spruce resulting from vacuum-pressure impregnation with water-borne preservatives
1987 - IRG/WP 3450
The washboard effect has been observed in sawn spruce after both commercial and laboratory based preservative treatments and is of increasing economic importance. The effect is defined as a specific phenomenon at the wood surface. It is distinct from internal collapse in the wood, but it may occur in association with internal collapse damage. Experimental investigations on the causes of washboardi...
H Willeitner, R J Murphy


Development of a method for testing wood preservatives with soft rot fungi
1975 - IRG/WP 250
Although the first publications on experimental soft rot attack date back 20 years ago, so far no test method for evaluating the efficacy of wood preservatives against soft rot attack (Ascomycetes and Fungi Imperfecti) has been generally accepted. The reasons are diverse and the shortcomings and the disadvantages of the methods described are well known and have repeatedly been discussed. The soil ...
M Gersonde, W Kerner-Gang


Field and laboratory studies on anti-sapstain preservatives
1982 - IRG/WP 3205
The field tests included 11 different anti-sapstain preservatives and were carried out at different sawmills in southern Sweden. Drying conditions, climate and the local fungus flora were not identical for the different preservatives and comparisons between the preservatives should therefore be made with caution. Results obtained in the field tests are, however, in relatively good agreement with t...
M-L Edlund, B Henningsson


Evaluation and approval of wood preservatives in Japan
1988 - IRG/WP 2303
Japanese standardized decay test methods, performance requirements and approving system are briefly described. JIS (Japanese Industrial Standard) A 9302, which is related to a testing method for evaluating effectiveness of wood preservatives when applied to pressure treatment, is fundamentally a sand-block laboratory test method. According to performance requirements in JIS A 9201, mean percentage...
K Tsunoda


Incorporating insect behaviour in standard tests of wood preservatives - A possible way to reduce pesticide loadings
2000 - IRG/WP 00-20190
The application of wood preservatives to protect timber against insect infestation is common practice world wide. The effectiveness of wood protecting insecticides is usually determined in various standard tests. Depending on the target pest species and the test method, larvae of different developmental stages and sizes or adult insects are exposed artificially to the insecticide-treated commodity...
H Hertel, R Plarre


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. 3rd Interim Report
1983 - IRG/WP 4101
This paper updates the results of microbiological examination and marine borer assessment of untreated wood samples (15 x 2 x 2 cm³) and samples treated with 3, 6 and 10% CCA and CCB preservatives. Three reference species - Alstonia scholaris, Fagus sylvatica, Pinus sylvestris were used at all the test sites in addition to local species chosen by participants in the test....
R A Eaton


Leaching of inorganic wood preservatives – Investigating the relationship between leachability, dissociation characteristics and long-term leaching potential
2003 - IRG/WP 03-50199
Estimation of the leaching properties of preservative components is greatly affected by the leaching test method applied since not all methods equally consider the physical components responsible for leaching. These include: wetting of the wood and penetration of water (affected by dimensions, amount of end grain, permeability, duration and nature of water exposure); solution of preservative comp...
L Waldron, Y T Ung, P A Cooper


Water-borne preservative marine trials in Western Canada
1981 - IRG/WP 470
Red pine boards treated with chromated copper arsenate, ammoniacal copper arsenate, copper zinc arsenic additive, a modified ammoniacal copper arsenate, and zinc arsenic additive, have been installed in a marine field test at West Vancouver, British Columbia. After two and a quarter years exposure, all the test samples are in excellent condition with the exception of those treated with the zinc ar...
J N R Ruddick


Protection of beech veneer for fruit and vegetable boxes
1981 - IRG/WP 3176
In Yugoslavia about 50,000 m³ of low quality beech logs annually are rotary cut into veneer from which boxes are made for transporting fruit and vegetables. Because of steaming before rotary cutting, beech veneer becomes extremely sensitive to mould attack which decreases the quality and commercial value of the final product. To avoid mould attack, veneer sheets are dried to 16% moisture content ...