Limited variability in biological durability of thermally modified timber using vacuum based technology
2011 - IRG/WP 11-40567
The SmartHeat® thermal timber treatment is a new technology based on the process parameters being steered very precisely mainly due to the vacuum applied and heating system involved. Timber treated with this technology shows a potential for less variability of biological durability in one batch. Several batch treatments were sampled and assessed on statistical variability of decay resistance agai...
J Van Acker, S Michon, J Van den Bulcke, I De Windt, B Van Swaay, M Stevens


The Technical Criteria on Biological Evaluation of Wood Preservatives for Use Category C4.1 in Southern China
2012 - IRG/WP 12-20481
According to the Regulations on Pesticide management of the People's Republic of China, wood preservatives belong to agrochemicals. The establishment of registration system on wood preservatives would be benefit to management of preservatives, including the market entrance and safety insurance to the human beings, livestock and the environment associated by the application of these preservati...
Xingxia Ma, Mingliang Jiang


Durability of timber products – Part 2: Proposal for an IRGWP - Durability Database
2012 - IRG/WP 12-20497
A proposal for a web-based platform for scientific exchange of test data in the field of wood durability and wood protection has been made. The overall aim of the durability data base is to improve the usability of existing test data and to create an added value for durability research and service life prediction. The database allows for test results from standardized and non-standardized laborat...
C Brischke, L Meyer, G Alfredsen, M Humar, L Francis


Durability of timber products –Part 1: Inventory and evaluation of above ground data
2012 - IRG/WP12-20498
The material-inherent resistance of wood is one of the most important qualities influencing the durability of timber. Hence, it has also a major effect on the service life to be expected from a timber construction. In addition, design details and the respective climatic conditions determine durability and make it impossible to treat wood durability as an absolute value. Moreover, the reference mag...
C Brischke, L Meyer, G Alfredsen, M Humar, L Francis, P O Flæte, P Larsson Brelid


Tannin resin-boron associations: Leaching and biological resistance
2012 - IRG/WP 12-30587
The easy leaching of boron in wood preservation formulations has allowed to use this fungicide only for short term applications. The recently discovered adduct with flavonoids allows boron to resist longer periods of time within wood and consequently extend its life. Two different leaching treatments were compared and the fungal and termite decay was examined. The biological tests have shown extre...
G Tondi, S Wieland, N Lemenager, A Petutschnigg, A Pizzi, M-F Thevenon


Glueline fungicides in veneer based engineered wood products - results from laboratory work for the H1.2 hazard class in New Zealand
2012 - IRG/WP 12-30593
The use of glueline insecticides in plywood and laminated veneer lumber is commonplace in several countries. However, few glueline fungicides are registered for commercial use with previous work suggesting that achieving control of decay from the glueline is very challenging. This paper summarises two tests completed on Pinus radiata plywood with a new glueline fungicide comprising the active in...
A Siraa, K Day, P Lobb


Biological performance of wood- and bamboo-polypropylene composites: Effects of particle content, particle size and Zn borate
2012 - IRG/WP 12-40577
Particle content and size of wood material in wood plastic composites (WPCs) can affect efficacy of WPCs against fungi and termites. This study evaluated fungal and termite resistance of WPCs manufactured by using two different levels of particle content (50 and 70%) and three different particle sizes (30, 60, and 100 mesh). In fungal resistance tests, Tyromyces palustris, a standardized test fung...
S N Kartal, S Aysal, E Terzi, T Yoshimura, K Tsunoda


The assessment of biological and mechanical properties of wood treated with ionic liquids – N,N-dimethylamine and 1-decylimidazole derivatives
2012 - IRG/WP 12-40582
This paper presents the results of tests of the effectiveness of action of new imidazolium and bis-ammonium ionic liquids against Basidiomycotina and Ascomycotina wood-destroying fungi. All the investigated ionic liquids showed high fungicidal action against Coniophora puteana. In order to characterize the influence of ionic liquids on mechanical wood properties, the compression strength along the...
W Przybylska


Improvement of the biological performance and dimensional stability of two tropical woods by thermal modification
2012 - IRG/WP 12-40605
Pink cedar wood and rubberwood were thermally modified at 230°C in air for 4 h or for 8 h, and then subjected to bending, compression and hardness tests to evaluate the effect of the treatment on these mechanical properties. The biological performance of the modified wood was also determined, according to EN113, and the dimensional stability measured by means of the anti-swelling efficiency. The ...
M M González-Peña


Wood-leather panels – A biological, fire retardant building material
2012 - IRG/WP 12-40615
The poor flame retardant properties of wood-based products are among the severest obstacles, hindering its use in the commercial building sector. Recently, some attempts to improve the fire properties, relying on inflammable salts or reactive halogen compounds, have been presented, although they either cause problems with machining or embody harmful compounds (halogen derivates). In this paper, ...
S Wieland, U Stöckl, T Grünewald, S Ostrowski, A Petutschnigg


System treatments of Pinus sylvestris - influence on moisture, decay and discoloration
2013 - IRG/WP 13-30612
Biological activity can cause challenges for the use of wood in outdoor exposure. Decay and discolouring fungi influence the service life of wooden constructions, and the moisture content of the wood is often an important factor. The aim of this study was to evaluate the performance of different combinations of preservative/modified wood protection treatments and surface treatments for wooden deck...
A Schabacker, G Alfredsen, L Ross Gobakken, H Militz, P O Flæte


The development of accelerated test systems to evaluate the durability of framing timber
2014 - IRG /WP 14-20547
Various accelerated decay resistance trials including small simulated wall units, samples exposed in enclosed tanks and ‘I’ samples in stacks have been explored and used to test the durability of treated and untreated radiata pine framing at Scion since 2001. These testing methods have been established to determine the effectiveness of commercial formulations in preventing decay in framing sub...
T Singh, D Page, J van der Waals


Modern Instrumental Methods to Investigate the Mechanism of Biological Decay in Wood Plastic Composites
2014 - IRG/WP 14-40674
Various instrumental techniques were used to study the fungal decay process in wood plastic composite (WPC) boards. Commercial boards exposed near Hilo, Hawaii (HI) for eight years in both sun and shadow locations were inspected and tested periodically. After eight years of exposure, both boards were evaluated using magnetic resonance imaging (MRI), while a selected area of the board exposed in sh...
G Sun, R Ibach, M Gnatowski, J Glaeser, M Leung, J Haight


Biological durability of natural fibre reinforced composites
2014 - IRG/WP 14-40681
Composite materials reinforced with wood or non-wood natural fibres have the potential to be a lighter and lower-cost alternative construction material. Until better availability and properties and a lower cost price of degradable polymers makes their use more prevalent, the application of natural fibre reinforcements in synthetic polymers is an intermediate step towards products that are complete...
N Defoirdt, I De Windt, J Van den Bulcke, J Van Acker


Study on Biological Distribution to Conserve the Tripitaka Koreana woodblocks in Haeinsa Temple
2015 - IRG/WP 15-10844
Tripitaka Koreana is the Wood-carved Buddhist scriptures which were made in 13th century. And Janggyeong Panjeon that is depository for the Tripitaka Koreana was built in 15th century. In recent days, biological damage becomes a serious problem to wooden cultural heritage including historical wooden buildings with global warming. In this study, termite monitoring on whole Haein-sa temple area and ...
Si Hyun Kim, Hyun Ju Lee, Yong Jae Chung


Durability of treated wood Corymbia torelliana and Eucalyptus grandis x Eucalyptus urophylla against subterranean termite
2015 - IRG/WP 15-20563
This work aimed to analyze the durability of woods against termite Nasutitermes corniger Motsch. Fence posts from this study were collected in Pinheiros, north of Espírito Santo state, Brazil. Used the Corymbia torelliana and Eucalyptus grandis x Eucalyptus urophylla species with 11 and 9 years, respectively and plant spacing of 3.00 x 2.00 m. Were used 72 samples from discs removed the 0.50 m of...
D Junior Verly Lopes, J Benigno Paes, P N de Medeiros Neto, G dos Santos Bobadilha


Biological Performance of Triadimefon in combination with Tebuconazole in laboratory and field tests
2015 - IRG/WP 30668
The usage of Triazole-combinations for wood preservatives is common practice in several countries. Especially the combination of Tebuconazole and Propiconazole is preferred for this application due to its broad spectrum of efficacy against wood destroying fungi. 1-(4-Chlorphenoxy)-3,3-dimethyl-1-(1,2,4-triazol-1-yl)-butanon, also known as Triadimefon provides a good efficacy against the wood destr...
P Meckler, T Jaetsch


Development of decay hazard maps based on decay prediction models
2016 - IRG/WP 16-20588
Durability plays a very central role in timber engineering, especially when working with wood in use class 3 and above where the risk of decay is high. As one of the primary decay influencing factors, the external condition, i.e. the local climate, is often graded by some type of climate index value. Predominately, climate indices are based on a direct relationship between weather data and decay. ...
J Niklewski, E Frühwald Hansson, C Brischke, D Kavurmaci


Assessment of the biological durability of wood treated with organosilicon compounds
2016 - IRG/WP 16-30685
The European wood construction market is in need of environmentally friendly wood-based products whose service life meets the expectations of end users. Non-biocidal silicon-based water repellents, which can be applied to different materials, help minimize their vulnerability/susceptibility to liquid water. Consequently, they have the potential of increasing wood’s resistance against decay fungi...
M Kutnik, M Montibus, S Derocker, S Salivati, J-P Lecomte


Effects of Bio-oil Obtained from Laurel (Laurus nobilis) Residues on Biological, Physical, and Mechanical Properties of Treated Wood
2016 - IRG/WP 16-30692
In this study, the effects of bio-oil obtained from Laurel (Laurus nobilis) residues on biological (decay, insect, termite resistance), physical (water absorption, tangential and radial swelling), and mechanical properties (MOE, MOR and CSPG) of treated wood samples were studied. The bio-oil used in this paper was produced by the help of fixed bed reactor type pyrolyzer. GC/MS analysis showed that...
S Akbas, A Temiz, N Terziev, M H Alma, S Palanti, E Feci


Effect of Nano-Silane on Permeability in MDF as a Result of Susceptibility to Moulds and Fungi
2016 - IRG/WP 16-40716
Effects were studied of vapor chamber on specific gas permeability of nanosilane-treated medium-density fiberboards (MDF). Size range of nanoparticles was 20 – 80 nm. Nano-silane (NS) was used at four consumption levels of 0, 50, 100, and 150 g/kg dry wood fibers. Density of all treatments was kept constant at 0.67 g/cm3. Specimens were kept for 18 weeks in vaporized chamber; their specific gas ...
H R Taghiyari, J Norton, A Moradiyan, M Sadegh Taher Tolou Del, H Siahposht, B Moradi-Malek, M Noferesti


Resistance of heat treated Ash wood under steam pressure: rot fungi, soil micro-organisms and termites
2016 - IRG/WP 16-40724
Thermal modification processes have been developed to increase the biological durability and dimensional stability of wood. The aim of this paper was to study the influence of ThermoWood® treatment intensity on wood decay resistance improvement against soil-inhabiting micro-organisms, brown/white rots and termite’s exposures. All of the tests were carried out in the laboratory with two differen...
K Candelier, S Hannouz, M-F Thévenon, D Guibal, P Gérardin, M Pétrissans, R Collet


Incorporation of raw boron minerals to protect particleboard against decay and mold fungi, termites and insects
2016 - IRG/WP 16-40729
This paper evaluated the biological performance of particleboards incorporated with the raw boron minerals ulexite and colemanite against decay, mold fungi, termites and insect larvae in comparison with that of particleboards with zinc borate, or boric acid plus a borax mixture. The results showed that ulexite and colemanite were highly effective against the decay fungi and termite attack in labor...
S N Kartal, E Terzi, P Gerardin, C M Ibanez, T Yoshimura


Development of a new method for wood hydrophobizing and fixation of copper compounds by chemical hardening of vegetable based modified oils
2016 - IRG/WP 16-40754
Wood products with ground and direct water contact, but without sufficient biological durability, have to be protected against biological degradation by fungi and other microorganisms. Due to European legislation (Biocidal Products Regulation 528/2012), the selection of possible chemical agents, which are still allowed to be used, is diminishing rapidly. The use of previously widely applied, very ...
C Swaboda, M Fischer, K Jacobs


Effects of wollastonite nanofibers on biological resistance of historical paper against Aspergillus niger
2017 - IRG/WP 17-10878
Effect of wollastonite nanofibers on biological resistance of historical paper against Aspergillus niger was studied. Specimens from A4 papers were also prepared for comparison purposes. Paper specimens were dipped in aqueous nanowollastonite (NW) with 10, 20, 30, and 40% concentrations and compared with control specimens. In order the nanofibers be fixed on paper specimens, 5% of polyvinyl acetat...
H R Taghiyari, A Kalantari, A Ershad-Langroudi, A Kalantari