IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 323 documents. Displaying 25 entries per page.


Leaching of CCA components from treated wood under acidic conditions
1993 - IRG/WP 93-50004
The leaching of CCA components from treated wood under acidic conditions were investigated. Western hemlock treated with three types of CCA and two levels of target retention was subjected to leaching at four different levels of pH. After leaching tests, leached samples were subjected to laboratory decay and soft rot tests. The amount of CCA components leached was dependent on acidity of leaching ...
Jae-Jin Kim, Gyu-Hyeok Kim


Artificial drying of impregnated wood
1987 - IRG/WP 3448
Sawn timber (Pinus Sylvestris) of dimension 50x150 mm was impregnated with CCA by a full-cell process. The timber was then dried in a conventional kiln or a special vacuum kiln where the timber was dried by circulating superheated steam. Drying time was 16 days and 2 days respectively. The aim of the investigation was to compare the physical appearence of the wood after drying by the two methods w...
M-L Edlund


Three dimensional computer representations of growth of microbial populations in wood
1984 - IRG/WP 1243
Creosoted distribution poles inoculated with either Lentinus lepideus, biological control organisms including Triochoderma or combinations of both were extensively sampled to monitor the spread of organisms. A computer program which enabled the results to be portrayed in a three dimensional graphic form was developed and is illustrated. Results showed that computer mapping of this type usefully en...
A Bruce, B King, C Bruce, G M Smith


The yeast Pichia sp. As a short-term biological control agent to fungal spoilage of sawn softwood timber
2000 - IRG/WP 00-10362
Previous work has found isolates of the yeast Pichia to be a successful biological control agent toward moulding of fruits. An isolate was tested for the ability to protect sapwood of Pinus sylvestris timber against visual degrade by surface growth of moulds and staining fungi. Successful protection of autoclaved wood sprayed with a mixture of common wood moulding fungi was achieved when the yeast...
C Payne, H J Staines, A Bruce


Remedial treatment of wood attacked by insects
1981 - IRG/WP 3175
A review is presented of remedial treatments against wood-boring insects in wood in service. Preconditions and fundamental principles of insect control are compared with the control of fungal attack and reasons are given for the fact that remedial treatments against insects are more commonly applied than against fungi. With regard to insect control measures with a simultaneous preventive effective...
H Kühne


Effects of Trichoderma harzianum on enzyme activity and oxalic acid production of Gloeophyllum trabeum in ponderosa pine sapwood blocks
1992 - IRG/WP 92-1550
The effect of a bioprotectant, Trichoderma harzianum, on the activity of Gloeophyllum trabeum was investigated using a wood wafer sandwich method. Wood weight loss was greatest with Gloeophyllum trabeum exposed wafers, intermediate with those exposed to both the bioprotectant and decay fungus, and lowest with the bioprotectant exposed wafers. Extracts of wood wafers after 2, 4, or 6 weeks of funga...
C M Sexton, J J Morrell


The chemical analysis and biological evaluation of wood extractives as potential timber preservatives
1995 - IRG/WP 95-30090
Work involved the biological performance of water and organic solvent soluble extractives of four naturally durable wood species, namely; Matumi, Tamboti, Sneezewood and the Turpentine tree. These timber species are known to be naturally durable against termites and fungi (±25 to 35 years). The extractives were evaluated against termites and fungi using impregnated pine pencil stakes in field tes...
P Turner, D Conradie


Chemical, physical and biological factors affecting wood decomposition in forest soils
2003 - IRG/WP 03-20281
Organic matter (OM) decomposition is an important variable in determining the potential of forest soils to sequester atmospheric CO2. Studies using OM from a particular location gives site-specific decomposition information, but differences in OM type and quality make it difficult to compare results among soils and forest ecosystems. By using a “standard” OM in decomposition studies, OM qual...
M Jurgensen, P Laks, D Reed, A Collins, D Page-Dumroese, D Crawford


Biological control of sapstain fungi in wood
1996 - IRG/WP 96-10158
Sapstain fungi can cause serious damage to wood and wood products, resulting in a significant economic loss for the wood products industry. The purpose of the present investigation was to determine whether the sapstain in wood caused by sapstain fungi could be biologically controlled. Biological control of sapstain fungi in wood was demonstrated in field trials with nonpigmented isolates of Cerato...
S C Croan


Assessing the performance of wood preservatives from biological tests - the European approach
1994 - IRG/WP 94-20040
The impetus for the European Standardisation Committee to undertake the development of a performance standard for characterising the effectiveness of wood preservatives from biological tests, lies in the Construction Products Directive. This is effectively the European Community law which provides the basis for Construction Products to be traded across all member states without technical or regula...
A F Bravery


Albumin borate: A new non-toxic, wide-spectrum, long-term wood preservative
1998 - IRG/WP 98-30167
Boron, widely recognized for its broad range of activity towards both fungi and insects and for its low mammalian toxicity, can not provide long term protection to treated timber due to its high leachability. Boron, in the form of boric acid, can be partially fixed to timber by the formation of an association with egg albumin, which is insolubilized by heat-induced coagulation. Chemical investiga...
M-F Thévenon, A Pizzi, J-P Haluk


Effect of media composition on the antagonistic properties of Trichoderma spp. against wood decay fung
1992 - IRG/WP 92-1538
Most screening of potential biocontrol agents of wood decay fungi has previously been undertaken using artificial media. Similarly experiments designed to evaluate the mechanisms involved in antagonism between biological control agents and target fungi, have largely been carried out in conditions which do not accurately reflect the nutrient status of wood. This paper examines the influence of nutr...
U Srinivasan, A Bruce, H J Staines


An in-ground natural durability field test of Australian timbers and exotic reference species. Part 5: Extensive data from a site where both decay and termites are active. Results from a full-replicated set of heartwood specimens from each of ten myrtaceous hardwoods after 18, 19 and 20 years' exposure - A discussion paper
1988 - IRG/WP 2324
Extensive data are presented on the decay situation, the termite situation and the decay-termite associations; all gathered from a fully-replicated set of heartwood specimens of 10 hardwood timbers after 18, 19 and 20 years' exposure in the ground at a single test site, i.e. a semi-arid steppe site. Sixteen tables are presented in addition to the one table providing the rating data; the l...
J D Thornton, G C Johnson, J W Creffield


Kiln drying of CCA-treated wood - Some safety and environmental considerations
1987 - IRG/WP 3443
Vapours and condensate from a condenser kiln in which CCA-treated wood was being dried have been collected and analysed. The concentrations of arsenic, copper and chromium found in the vapours from the drying process were well below Swedish threshold limit values. The contents of arsenic and chromium were also low in the condensate, although the copper content was fairly high. The latter result wa...
J Jermer, B Lundberg


Dip-diffusion of dressed timber - Effect of drying
1989 - IRG/WP 3509
The effect of drying on dip-diffused dressed freshly sawn timber was determined by the depth of penetration of boron achieved on the two test timber species, White cheesewood (Alstonia scholaris) and Light Hopea (Hopea papuana). The results obtained showed that light density White cheesewood was completely penetrated even after 3 days drying while Light hopea, treated immediately achieved 5.2 mm p...
H C Konabe


Chemical and biological studies of organotin treated and painted wood stakes after outdoor exposure
1987 - IRG/WP 3419
Organotin based wood preservatives containing tributyltin oxide (TBTO) or tributyltin naphthenate (TBTN) are used in Sweden mainly for double-vacuum treatments of window joinery of Pinus sylvestris. After impregnation the joinery is painted or stained in different colours. To evaluate this effect (different colours on the degree of degradation of TBTO and TBTN, effected by different temperatures i...
M-L Edlund, B Henningsson


Presteaming radiata pine heartwood to improve treatability
1983 - IRG/WP 3239
Steaming and holding before preservative treatment by the Bethell process greatly improved the treatment of radiata pine heartwood. Maximum penetration of preservative for the shortest holding period was obtained by the use of steam vacuum but the difference between this and steam venting was small when compared with the standard of treatment of air dried samples. A holding period of one day was s...
A J Bergervoet


In vitro sporulation of selected wood decay fungi
1978 - IRG/WP 190
Basidiospores produced axenically without laborious attention in the laboratory are useful in studies of wood decay initiation. Such spores presumably approach those collected from natural sporophores in size and germinability (Morton, 1964). Production of spores in vitro by inversion of cultures grown on 2% malt extract agar in deep glass dishes (100x80 mm²) has been the preferred method (Morton...
E L Schmidt, D W French


Improvement of some technological and biological properties of poplar wood by impregnation with aqueous macromolecular compounds
1992 - IRG/WP 92-3721
Poplars (Populus spp) belong to the most important tree species in afforestation programs of the Netherlands. Due to their rapid growth, the wood quality is usually low. Therefore, studies were performed to elucidate whether some technological properties and the resistance against fungal attack could be improved by impregnation with water-soluble resins. The results showed that swelling and shrink...
R D Peek, H Militz, J J Kettenis


Controlling the sapstain fungus Ceratocystis coerulescens by metabolites obtained from Bjerkandera adusta and Talaromyces flavus
1993 - IRG/WP 93-10024
Sapstain causes severe damage to wood and wood products, posing a major economic problem for the wood industry. The purpose of this study was to determine if metabolites from Bjerkandera adusta and Talaromyces flavus would (1) decolorize stain in wood caused by Ceratocystis coerulescens and (2) prevent sapstain by Ceratocystis coerulescens. We studied the interaction of the sapstain fungus Ceratoc...
S C Croan, T L Highley


Internal pressure monitoring during the treatment of Pinus radiata (D. Don)
1995 - IRG/WP 95-40049
The use of micro-transducers to monitor the internal pressure of wood during treatment is investigated. The rates of pressure transfer in radiata pine sapwood and heartwood are compared during Bethell treatment with copper chrome and arsenic preservative. The effect of pre-conditioning treatments are also evaluated using micro-transducer monitoring. It is anticipated that knowledge of the changes ...
P R S Cobham, P Vinden


Biological resistance of aldehyde-treated wood
1994 - IRG/WP 94-40018
Biological resistance of wood treated with aldehyde cross-linking agents such as glyoxal, glutaraldehyde and dimethylol dihydroxy ethyleneurea (DMDHEU) were investigated. Sapwood blocks of Japanese cedar and Japanese beech, measuring 20 x 20 x 10 mm³ (T x R x L), were vacuum-impregnated at room temperature with 5-25% of aldehyde solutions. Blocks were kept in the solution for 1 week to gain the o...
S Yusuf, Y Imamura, M Takahashi, K Minato


Biological detoxification processes - A check list for assessments
1998 - IRG/WP 98-50120
The number of scientific publications on the biological purification of preservative treated wood implies that the biological treatment of wood wastes becomes more and more important. But an information about a successful industrial application is almost missing in all cases. Therefore the applicability of the proposed purification processes is often uncertain. The feasability of such a biological...
H Leithoff, R-D Peek


Environmentally benign biological wood preservatives by Streptomyces rimosus, SC-36
1997 - IRG/WP 97-10196
Microbiocides obtained from mutant culture Streptomyces rimosus SC-36 were evaluated for their abilities to inhibit the growth of brown-rot, soft-rot, white-rot, and sapstain fungi on wood. The test fungi were the brown-rot fungi Antrodia carbonica, Gloeophyllum trabeum, Neolentinus lepideus, and Postia placenta; soft-rot fungi Chaetomium globosum, Paecilomyces variotti, Phialocephala dimorphospor...
S C Croan


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 1: Treatment of reference samples
1977 - IRG/WP 426
It was agreed in Wildhaus on 15 May 1976 that preparations for the test detailed in Document No: IRG/WP/414 should commence immediately, but that initially only two water-borne preservatives should be used - a copper/chrome/arsenic (CCA) and a copper/chrome/boron (CCB) formulation respectively. PRL, England (R Cockcroft) would be responsible for supplying samples of the reference timbers treated w...
R Cockcroft, T B Dearling, W O Schulz, H V Borck


Previous Page | Next Page