Wood plastic composites from modified wood. Part 2 - Durability in laboratory decay tests
2006 - IRG/WP 06-40353
The decay resistance of wood plastic composites, WPCs, was tested according to modified versions of AWPA E10 (soil-block test) and ENV 807 (tests in three un-sterile soils, terrestrial microcosms, TMCs). The WPC materials were conically extruded profiles with 30% polypropylene content. The 70% wood content was untreated Scots pine sapwood, acetylated pine and heat treated Norway spruce, respective...
M Westin, P Larsson Brelid, M L Edlund, G Alfredsen


Laboratory Leaching Tests to Study the Effects of Post-Treatment Storage Periods on CCA Leachability and Fixation in Treated Permeable and Refractory Malaysian Hardwoods
2006 - IRG/WP 06-50240
The biological resistance and environmental safety of CCA-treated wood relies on the extent of post-treatment storage fixation of CCA in wood prior to being utilized. A study on the comparative leachability (fixation) of CCA-treated refractory and permeable heartwoods of 3 Malaysian hardwoods subjected to different post-treatment storage (fixation) periods of up to 4 weeks, at 2 laboratory leachin...
A H H Wong, H C Lai, N P T Lim


Accelerated assessment tests of new termiticides
2007 - IRG/WP 07-20353
One of the biological agents, which cause major damage to wood in Spain, is the subterranean termites. The systems used for controlling termites don’t eradicate them, and the products presently used to treat wood against them, due to their toxicity and their persistence in the environment, could be prohibited in the near future in Europe as consequence of the 98/8/EC Directive (usually called t...
M T Troya, M J Prieto, D Lorenzo, F Rubio


Wood decay fungi from New Zealand ‘leaky’ buildings: PCR identification and laboratory decay tests of wood preservative-treated Pinus radiata (Part 1)
2007 - IRG/WP 07-10620
Fungi colonising Pinus radiata D. Don framing timber of ‘leaky’ New Zealand buildings were isolated to produce pure cultures. Mycelia from these cultures on agar media were collected to extract DNA. To identify the fungi to the species level, polymerase chain reaction (PCR) with primer pairs ITS1-F and ITS4 were performed followed by sequencing of the internal transcribed spacer (ITS) region. ...
D Stahlhut, R L Farrell, R Wakeling, M Hedley


A roadmap for performance-based specification of wooden components based on service life prediction
2007 - IRG/WP 07-20351
The need for an unified and harmonised system for performance classification and specification of wood and wood-based products in Europe emanates from requirements of users and the European Construction Products Directive, CPD. A road to a feasible specification system is outlined. Exposure-related performance prediction was worked out as a key task on the way to product specification. Therefore s...
C Brischke, A O Rapp


Comparison of laboratory termite test methods
2007 - IRG/WP 07-20365
Seven standardized laboratory tests with termites were evaluated. The bioassays were made in accordance with EN 117, SAA32 E08, SAA32 E09, Ebw 02, the American Wood-Preservers’ Association (AWPA) Standard E1-97, the Japan Wood Preserving Association (JWPA) Standard 11 (1) and The Protocols for Assessment of Wood Preservatives. Two different wood preservatives each in three concentrations and add...
H-U Kruschinski, W Unger, A F Preston


Predicting the decay resistance of timber above-ground: 2. When can reliable field data be obtained?
2007 - IRG/WP 07-20368
Application of modern performance-based engineering and design requires building products that are thoroughly characterised in terms of their ability to perform as expected over time. The engineering community is attempting to use this information to provide predicted service-lives for various building elements. Increasingly, this service-life prediction must be based on objective measurement coup...
L P Francis, A J Swain, J J Morrell


Durability of some alternatives to preservative-treated wood. Progress report 2: Results from field tests after 5 years’exposure
2007 - IRG/WP 07-30442
A number of alternatives to preservative-treated wood have been tested according to EN 252 (stake test) and a specially designed ground-proximity field test, the latter in Sweden as well as in Hawaii, USA. Seven untreated wood species and four alternative wood treatments labelled as environmentally friendly (acetylation, linseed oil, heat treatment, vinyl polymer) were included in the study. Four ...
M-L Edlund, J Jermer


Development of boron/linseed oil combined treatment as a low-toxic wood protection. Evaluation of boron fixation and resistance to termites according to Japanese and European standards
2007 - IRG/WP 07-30448
Combinations of boric acid as a first step of treatment and linseed oil as a second step have been performed in order to enhance boron retention to leaching and wood resistance to termites. Classic leaching and termites resistance standards are inappropriate to evaluate this combination which can be considered as both a wood core preservation treatment and a coating. Japanese Industrial Standard...
F Lyon, M-F Thevenon, Y Imamura, J Gril, A Pizzi


Utilizing Cypress to improve the decay and termite resistance of OSB panels
2008 - IRG/WP 08-10658
OSB panels were manufactured with mixture of pine and cypress heartwood and lignin and tannin based resins in order to propose an eco-friendly wood composite. The resistance of OSB panels was tested against Reticulitermes santonensis according to the EN 118 and EN 117 standards and field tests methods. OSB made from cypress showed more resistance against the tested termite, the resistance decrease...
N Amusant, O Arnould, A Depres, R H Mansouris, T Pizzi, C Baudassé


Field Stake Tests with Copper-based Preservatives
2008 - IRG/WP 08-30459
The performance of field test stakes derived from commercially produced ground contact retention copper quat preservatives based on either soluble copper complexed with ethanolamine, or from a water-based suspension of particulate micronized copper compounds, as well as untreated southern yellow pine controls, is compared at two decay test sites. After less than one year in field test some of t...
A Preston, L Jin, D Nicholas, A Zahora, P Walcheski, K Archer, T Schultz


Above and Below-Ground Copper-Azole and Copper, Chrome Arsenate Depletion from Pinus radiata and Fagus sylvatica at Thirteen New Zealand & Australian Sites
2008 - IRG/WP 08-30460
The objective was to determine the significance of site on preservative depletion from Pinus radiata D. Don and Fagus sylvatica L. 20 x 20 x 500 mm field test stakes treated with a ground contact retention of copper amine plus tebuconazole (CuAz) and copper chrome arsenate (CCA) after approximately 5 years exposure to widely different soil and climate conditions. Site, wood species and their inter...
R Wakeling


Depletion and Redistribution of Boron in Bundles of Commercially Treated Lumber Exposed to Artificial and Natural Rainfall
2008 - IRG/WP 08-30474
The depletion and redistribution of boron from stacks of Southern Yellow Pine lumber pressure treated with disodium octaborate tetrahydrate (DOT) and exposed to artificial and natural rainfall was examined. When the lumber was exposed to periodic simulated rainfall, 5.7-8.1% of the measured boron present leached from the lumber after exposure to over 300 mm of rainfall. In tests which exposed bo...
M E Mankowski, M J Manning


Bending Properties of Southern Pine Treated with Micronized Preservative Systems
2008 - IRG/WP 08-40414
This study indicates that treatment of southern pine with micronized copper systems have no deleterious effect on the residual strength property values. No statistical differences between wood treated with micronized systems and water-treated controls were noted when means were compared using either Tukey’s test or S-N-K mean comparison tests. Using the more discriminating Least Squares anal...
H M Barnes, G B Lindsey, J Hill, M Pompeo, R Hodge


Cantilever bending test of furfurylated poles
2008 - IRG/WP 08-40424
Ten, 8 m long poles of Scots pine (Pinus sylvestris) were treated with furfuryl alcohol to a WPG of approximately 40 %. A bending test was performed according to the principles in the draft European standard for wooden poles, prEN 14229 - Structural timber - Wood Poles for overhead lines. The bending strength and stiffness (MOE) for the poles tested were compared to an earlier study by the Swedish Wood Preservation Committee. In the latter study untreated, CCA-treated, ammoniacal Cu-PCP treated and creosoted poles were tested in bending. These types of poles were considered not to differ in strength and stiffness. The results of the furfurylated poles fit well with the results from the previous study. The bending strength and MOE values obtained are compared to the upper and lower 95-percentile values of the results from the previous study and all poles treated with furfuryl alcohol fit within this interval.Thus, this study indicates that a treatment with furfuryl alcohol does not result in a decrease of strength or stiffness. Further testing with a larger population of poles is necessary in order to get a statistically reliable result. In addition to further demonstration of the durability, the treatment process must be optimised to ensure full sapwood penetration and measures have to be taken to avoid the serious cracking observed in this trial before furfurylation can be considered for treatment of Pinus sylvestris poles.
R Ziethén, J Jermer, A Clang


Field Tests of naturally Durable North American Wood Species
2008 - IRG/WP 08-10675
There has been little field test performance data published on North American naturally durable species in general, and no published data on second growth material in particular. Yellow cedar (Callitropsis nootkatensis), western red cedar (Thuja plicata), eastern white cedar (Thuja occidentalis), and three wood species reputed to be moderately durable were installed in ground-contact (stakes) an...
P E Laks, P I Morris, G M Larkin, J K Ingram


Control de calidad eficiente de proteccion superficial sobre madera
2008 - IRG/WP 08-20397
Quality control is important to assure efficient protection of wood surfaces. When wood is exposed to the environment, it degrades due to weathering or environmental factors alone. Aging tests are utilized to test coating products. Quality control techniques are performed on exposed products according to standardized methods (NCh, ASTM, ISO, DIN, EN, FTMS, NTF, NBINT, or equivalents). Certified l...
A M Fernández S


Utilidad práctica de mini estacas en ensayos de campo
2009 - IRG/WP 08-20395
For testing chemicals for the wood against degradation agents of biotic, known as preservatives, both testing in the laboratory and in the fields are used. Field trials (Cemetery stakes) are often accepted as more "real" whose frequency of observation is set to more or less a year in temperate climates and six months or less in tropical situations, taking into accounts the aggressiveness of the so...
O Encinas, J V Puentes, N K Sarmiento, N Mora


Effectiveness of MOQ® OX 50 (CCB-Oxide) wood preservative – Part 2: Field tests
2008 - IRG/WP 08-30483
MOQ® OX 50 is a chromated copper borate preservative known around the world as CCB. In Brazil, this product is the only CCB-oxide type preservative with fungicide and insecticide properties registered at the Brazilian Institute for the Environment and Renewable Resources (IBAMA) that complies with the requirements of the Brazilian and European markets for preserved wood. For over five decades, s...
A Gandolfi Jr, C Salvela, D R Macedo, J M Vidal


Biological Performance of micronized copper wood preservative formulations in field and laboratory tests
2008 - IRG/WP 08-30488
Micronized Copper wood preservative formulations with different co-biocides were exposed to brown rot fungi in an 8-week AWPA E10 soil block decay test and two AWPA E7 ground-contact decay tests in Hawaii. The micronized copper formulations performed well against decay at or above the AWPA UC3 and UC4 retentions stipulated by the ICC-ES. Micronized copper preservatives performed comparably to a ...
G M Larkin, J Zhang, D L Richter, R J Ziobro, P E Laks


Effects of cold treatment on wood destroying fungi important in cultural heritage
2009 - IRG/WP 09-10706
The dry rot fungus Serpula lacrymans (Wulfen:Fr.) Schroeter is notorious in building environments for its vitality, destructive potential, and the huge costs associated with remediation of damage caused to wood of cultural heritage. Due to the potentially adverse of effects of chemical treatment methods such as have been attempted in the past, more benign physical methods of treatment, e.g. heat t...
M Lüdicke, W Unger, G Binker


Evaluation of variables that influence dynamic MOE in wood decay studies
2009 - IRG/WP 09-20409
The effect of wood moisture content (MC) and outdoor exposure of southern pine lap-joint components on dynamic MOE values was investigated. The use of dynamic MOE as a method of measuring progressive biodeterioration of above ground test samples shows promise, but the accuracy of this method for evaluating test samples subjected to fluctuating environmental conditions has not been reported. The re...
D Nicholas, J Shi, T Schultz


Utilidad práctica de mini estacas en ensayos de campo
2008 - IRG/WP 08-20395
For testing chemicals for the wood against degradation agents of biotic, known as preservatives, both testing in the laboratory and in the fields are used. Field trials (Cemetery stakes) are often accepted as more "real" whose frequency of observation is set to more or less a year in temperate climates and six months or less in tropical situations, taking into accounts the aggressiveness of the so...
O Encinas, J V Puentes, N K Sarmiento, N Mora


Natural durability of African Padauk and Niove. Comparison of new trials and former data from the CIRAD database
2010 - IRG/WP 10-10743
African Padauk (Pterocarpus soyauxii) and Niove (Staudia kamerunensis) were tested in laboratory against Basidiomycetes. The results were calculated according to the requirements of EN 350-1 (1994) and XP CEN/TS 15083-1 (2006). Padauk samples showed a high durability and very small variations between trees and within tree. Niove presented a high durability, but with notable differences according ...
Y N N’Kolo Meze’e, N Leménager, C Baudassé, M-F Thévenon


Diagnosis of failures in wood beams from historical house in Banská Štiavnica – Relations between ultrasonic measurements and bending properties
2010 - IRG/WP 10-20437
Various degrees of rot and other damages in ceiling beams with dimensions of 6500-8800 x 160-200 x 240-310 mm (length x height x width) situated in one historical bourgeois house in the UNESCO town Banská Štiavnica, Slovakia were determined visually and by the PUNDIT-plus ultrasonic device. Subsequently, for seventeen of the most bio-damaged fir (Abies alba Mill.) beams chosen for exchange were ...