Surface protection of wood with titanium, zirconium and manganese compounds
2005 - IRG/WP 05-30376
Thin radiata pine veneers were treated with a range of titanium, zirconium and manganese compounds and exposed to natural weathering. Veneer weight and tensile strength losses were used to assess the protective efficacy of the compounds. The oxidative manganese compounds potassium permanganate and manganic acetate restricted both weight and tensile strength loss of treated wood veneers during weat...
K J Schmalzl, P D Evans


Testing blue stain fungicides for joinery timber in combination with natural weathering
1976 - IRG/WP 268
Joinery timber in outside use becomes affected by blue-stain after a short time of exposure. This is especially the case with pine sapwood treated with unpigmented lacquer, but also with other timber species as well as different types of surface treatment. According to the basic investigations of BUTIN this is due to special types of blue-stain fungi, called "Lack-bläue" (lacquer blue-stain), in ...
H Willeitner


FTIR studies on the weathering of didecyldimethylammonium compound (DDAC) treated wood
1993 - IRG/WP 93-30013
Wood treated with alkylammonium compounds (AACs), such as DDAC, weathered more rapidly than untreated wood. In order to examine the influence of DDAC treatment of wood on its weathering, treated and untreated microtomed sections of southern yellow pine earlywood of various thicknesses, were prepared and weathered for approximately one month. The changes in these samples were monitored using FTIR. ...
R Liu, J N R Ruddick


A comparison of analytical and visual techniques used for assessment of weathering properties of chromium and copper azole treated timber
1994 - IRG/WP 94-20023
The weathering properties of preservative treated timber were studied by measuring surface lignin loss and by microscopic examination after weathering, and results were related to qualitative assessments of visual appearance after weathering. Measurement of relative rates of delignification of untreated and preservative treated timber obtained by FTIR analysis, and weight loss determined on thin v...
J A Cornfield, M D C Hale, G Fettis


Comparative study of blue stain resistance of various types of wood stains after artificial and natural weathering
1992 - IRG/WP 92-2411
For the determination of the protective effectiveness of a preservative treatment against blue stain in service, artificial weathering has been proposed as an alternative for the natural weathering period of 6 months in the European standard EN 152. Research on a range of products and on complete finishing systems for external joinery was conducted during 1986-1990. It revealed that the decisions ...
J Van Acker, M Stevens, M Nys


Preliminary observations of the effect of growth ring orientation on the surface checking of flat sawn Southern pine decking
2005 - IRG/WP 05-20313
Checking in decking timber is a serious defect and methods of reducing its severity are required to ensure that wood can compete with alternative decking materials. The first aim of this research was to test the hypothesis that flat sawn Southern pine decking boards with growth rings oriented concave to the exposed surface will develop less severe checking when exposed outdoors than similarly expo...
K Urban, P D Evans


Impregnation of timber with tannin as a mean of improving its dimensional stability
1992 - IRG/WP 92-3695
The results of a joint project carried out at the Timber Division of LNEC under the 2nd research programme of the CEC DGXII - "Wood as a renewable raw material" entitled "Stabilization of wood by impregnation processes" is presented. Pieces Maritime pine timber was impregnated with tannin under pressure to see if the treatment with tannin improved the behavior of wood regarding its dimensional sta...
J S Machado


Some Experiences with Stake Tests at BAM Test Fields and in the BAM Fungus Cellar Part 1: Comparison of Results of Visual Assessments and Determinations of Static Moduli of Elasticity (MOE)
2005 - IRG/WP 05-20319
With examples of routine in-ground stake tests differences are shown in the performance of wood preservatives at the BAM test fields Lehre and Horstwalde and in the BAM fungus cellar. Signs of attack of micro-organisms were assessed visually according to EN 252. Periodical determinations of static moduli of elasticity (MOE) revealed the influence of the attack on the elastic properties of the wood...
M Grinda, S Göller


Blue stain in timber in service. Progress review of Sub-group collaborative tests - 1981/82
1982 - IRG/WP 2178
Following from the discussions after reporting Document IRG/WP/2146 at the Meeting in Sarajevo, 1981, it was decided that 1.) more precise definition was needed of the artificial weathering schedules used in the work - participants to re-check Table 8 and send further details or amendments to Dr Bravery; 2.) a further test employing a wider range of chemicals was necessary using a smaller range of...
A F Bravery, D J Dickinson


Enhancing the Performance of Transparent Coatings by UV Protective Pre-treatments
2006 - IRG/WP 06-30399
Most industry observers anticipate a change from copper-based preservatives to metal-free combinations of organics for residential treated wood products in North America within the next one to five years. While the chromium copper provide considerable protection against UV, metal-free formulations will need UV protection in the form of additives or coatings. While transparent coatings can be made ...
P I Morris, S McFarling


L-joint based testing for service life prediction of exterior plywood in out of ground contact conditions
2006 - IRG/WP 06-20342
Good biological performance of several plywood types in exterior conditions is most probably related to altered wood moisture behaviour compared to solid wood. Therefore a test set up was developed, using EN 330 L-joint testing methodology, to facilitate differentiation of plywood for exterior applications. The proposed test set up is an adaptation of an accelerated L-joint method introduced by V...
J De Smet, I De Windt, J Van Acker


High-energy multiple impact (HEMI)-test – Part 1: A new tool for quality control of thermally modified timber
2006 - IRG/WP 06-20346
Thermal modification processes improve durability and dimensional stability of wood, but the strength properties, especially the dynamic ones, are compromised and need to be considered with respect to industrial quality control. Results from standard dynamic strength testing, such as impact bending tests, suffer from high variability, and therefore require a high number of replicates. To overcome ...
C Brischke, A O Rapp, C R Welzbacher


Wood-Plastic Composites and the Durability Dilemma: Observations from the Field
2006 - IRG/WP 06-40351
Wood-Plastic Composites (WPCs) used for decking, window & door moldings have experienced dramatic growth in North America over the last several years, with annual production increasing at rates greater than 20% per annum since 1998. A key factor contributing to this growth has been the successfully communicated message that they are "virtually maintenance free". The common perception being t...
M J Manning, F M Ascherl, M E Mankowski


Tunneling patterns of the subterranean termite species Reticulitermes grassei (Isoptera: Rhinotermitidae)
2007 - IRG/WP 07-10619
The cryptic habits of subterranean termites restricts detailed analysis of their foraging patterns in situ, but the process is evidently dominated by tunnel constructions connecting the nest with woody resources discovered within the territory of each colony. In this study, tunnel formation and orientation were studied experimentally in the termite Reticulitermes grassei (Clément), using 2D labor...
T Nobre, L Nunes, D E Bignell


Micro- and hydro-sandblasting for wood and wood coatings
2007 - IRG/WP 07-40380
Exterior wood coatings are getting increasingly durable and often more film forming. As a result they become difficult to renovate. Conventional renovation techniques (chemical or thermal stripping, sanding) are demanding techniques which take a long time to implement. Therefore renovation techniques are requested which are easier to use and which ensure that the wood surface is suitable for a re-...
L Podgorski, V Georges, P Svane


Natural Weathering of Coated Oil Heat Treated Wood
2007 - IRG/WP 07-30440
Oil heat-treated (thermally modified) pine wood was coated with 9 different types of solvent- or water-borne exterior finishes. The systems with modified wood substrate as well as unpainted and painted non-modified controls were exposed to weathering (EN 927-3) on two locations with sub-alpine and alpine climate. The influence of natural ageing on surface systems was evaluated after one year of ex...
M Petric, B Kricej, M Pavlic, A Rapp


The Effect of Solar Radiation on the Surface Checking of Wood
2007 - IRG/WP 07-40356
The aim of this research was to investigate whether exposure to solar radiation increases the checking of wood exposed to the weather, and examine the causes and spectral dependency of such an effect. Lodgepole pine samples were exposed outdoors under filters which transmitted selected regions of the solar spectrum while allowing other weathering factors to act on samples. Surface checking in samp...
P Evans, K Urban


Fire, flame resistance and thermal properties of oil thermally-treated wood
2007 - IRG/WP 07-40361
Oil thermal treatment, first developed by German scientists, is a promising technology for improving the durability and dimensional stability of wood for outdoor above-ground residential uses such as siding and shingles. The present authors’ previous research showed that 220ºC is an optimal treatment temperature, with 2 hours’ treatment producing wood with significantly improved moisture and ...
Jieying Wang, P Cooper


Brief introduction of a research project on the wood materials from an ancient Byzantine port unearthed during drilling for underground rail tunnel in Istanbul
2008 - IRG/WP 08-10641
A research project has been recently started to evaluate some properties of wooden materials from the biggest port of ancient times called Port of Theodosius I in Istanbul, Turkey. The ruins of the ancient Byzantine port during the excavations were recently uncovered in the Yenikapi site where an underground rail tunnel construction has been in progress in Istanbul. The wooden objects unearthed fr...
A D Dogu, C Köse, S N Kartal, N Erdin


Anatomical, physical and chemical changes of Bamboo (Phyllostachys puberscence ) during weathering processes
2008 - IRG/WP 08-10650
Bamboo (Phyllostachys puberscence) culms with 1, 2, 3 year old were exposed to natural weathering condition in Gwangju, Korea for 12 months. Changes in color, surface topography, strength and chemical properties were investigated using various microscopic and instrumental techniques. After one year’s weathering, the color of bamboo became lighter but strengths of bamboo did not change significan...
Jong Sik Kim, Kwang Ho Lee, Mi Young Cha, Yoon Soo Kim


Relationship between coating properties and their performance on treated wooden decks
2008 - IRG/WP 08-30454
Preservative treated wood benefits from the application of a surface coating to protect it from weathering (UV and rain). Different preservative formulations may affect surface properties of treated wood differently; therefore compatibility of coatings with different preservative treated wood types should be considered. This paper examines coatings characteristics and their weathering performance ...
M Ahmadinejad, P A Cooper


Service life prediction of wood: scale-dependent tools within a bio-engineering framework
2008 - IRG/WP 08-20387
Service life prediction (SLP) is a complex yet essential method for the building industry. Accurate and precise assessment of the components is crucial for a strong position of wood on the market. As it is a biological material, wood has an inherent variability and is susceptible to fungal attack. Therefore a profound knowledge of these characteristics is the corner stone of SLP for wood products....
J Van den Bulcke, J Van Acker, M Stevens


Development of a Weatherometer to Accelerate the Surface Checking of Wood
2008 - IRG/WP 08-20388
There is significant interest in developing preservatives that are better at preventing wood from checking. Currently, however, there is no accepted test methodology for accelerating the development of checks in wood samples so information on the effectiveness of treatments at restricting checking can be obtained more quickly. This paper describes the development of a new type of weatherometer (Ac...
R Ratu, P D Evans


Depletion and Redistribution of Boron in Bundles of Commercially Treated Lumber Exposed to Artificial and Natural Rainfall
2008 - IRG/WP 08-30474
The depletion and redistribution of boron from stacks of Southern Yellow Pine lumber pressure treated with disodium octaborate tetrahydrate (DOT) and exposed to artificial and natural rainfall was examined. When the lumber was exposed to periodic simulated rainfall, 5.7-8.1% of the measured boron present leached from the lumber after exposure to over 300 mm of rainfall. In tests which exposed bo...
M E Mankowski, M J Manning


Bi-oleothermal treatment of wood at atmospheric pressure: resistance to fungi and insects, resistance to weathering and reaction to fire results
2008 - IRG/WP 08-40418
Bi-oleothermal process is a simple treatment which has been developped by CIRAD in cooperation with FCBA. It allows a deep impregnation of wood with hydrophobic products using cheap facilities. The process includes two steps at atmospheric pressure. The first one is a dipping of wood samples in a hot oil bath (between 110 °C and 200°C) which creates an overpressure inside the wood. The second on...
L Podgorski, I Le Bayon, I Paulmier, J-D Lanvin, V Georges, D Grenier, H Baillères, J-M Méot