Blue stain in timber in service. Results of further IRG collaborative tests to compare different artificial weathering systems
1981 - IRG/WP 2146
The previous work described in Document No IRG/WP/286 examined 3 preservatives (1% phenyl mercury succinate - PMS, 5% pentachlorophenol - PCP and 1.5% Preventol A4 - PA4) subjected to 5 different artificial weathering systems (BAM Xenotest, Cuprinol Marr, EMPA Xenotest, Gori Atlas and PRL Marr) and after natural weathering at 5 sites (BAM, Cuprinol, EMPA, Gori and PRL). Results showed good correla...
A F Bravery, D J Dickinson


Susceptibility of painted wood to discolouring fungi - influence of binder, solvent and surfactant
1992 - IRG/WP 92-3714
Previous studies have shown that the basic composition of paints, without fungicide addition, can significantly contribute to the varying microbial susceptibility of painted wood. Previously, non-weathered water-borne acrylic paints applied to wood without a primer were shown to be more susceptible to mould attack than solvent-borne alkyd paints. The present study was initiated to reveal if this d...
J Bjurman, C Herder


The selected properties of Scots pine wood blue-stained by fungus Cladosporium herbarum
2003 - IRG/WP 03-10484
The fungi causing primary blue-stain of wood may change wood properties especially when acting in mixture of few fungi species. There were been undertaken investigation to clear the influence of pure culture of one fungus species on selected physical and mechanical properties of Scots pine wood. The twin samples of fresh cut Scots pine sapwood (Pinus sylvestris L.) were exposed into pure culture o...
A Fojutowski


Evaluation of chlorothalonil for stain and mould control on lumber
1992 - IRG/WP 92-3713
Chlorothalonil is a commercially important fungicide with many industrial and agricultural applications. It has a very low mammalian toxicity and is considered to be an environmentally benign material. This paper describes the laboratory evaluation of chlorothalonil as a wood antisapstain treatment. Chlorothalonil was tested as three formulation types - an emulsifiable concentrate (EC), a water-ba...
P E Laks, T L Woods, D L Richter


The use of preservative containing waste wood as substrate for growing greenhouse crops
1993 - IRG/WP 93-50011
In the Netherlands a large amount of waste wood and wood waste is produced every year. An important part of this amount comes from the pallet and packaging industries. One of the possibilities to re-use this relatively clean material is to convert it into substrates for growing crops in glass houses instead of the commonly used materials such as rock wool and glass wool. In this research, the infl...
W J Homan,H Militz


Surface retentions of PCP, TCMTB and MTC obtained during a field trial of antisapstain formulations
1993 - IRG/WP 93-20002
Formulations containing NaPCP or TCMTB and MTC were included as reference products in a recent field trial of antisapstain formulations in Queensland. Retentions of these actives on the surface of treated sawn Pinus elliottii were monitored by ultrasonic solvent extraction of excised samples and analytical determination by high performance liquid chromatography. Distribution of actives with depth ...
D E Ferlazzo, M D Needham, M J Kennedy


Screening of the efficacy of tall oils against wood decaying fungi
2004 - IRG/WP 04-30354
Tall oil is a by-product in pulping of resinous wood by the sulphate process. Tall oil contains a complex mixture of wood extractives. Some of these extractives act as natural protection against wood decaying fungi while other serve as nutrition for the fungi. This report describes a screening of the efficacy of four refined tall oils with different chemical composition on wood decaying fungi. ...
G Alfredsen, P O Flæte, A Temiz, M Eikenes, H Militz


Blue stain in service on wood surface coatings. Part 1: The nutritional requirements of Aureobasidium pullulans
1992 - IRG/WP 92-1556
The nutritional requirements of Aureobasidium pullulans was examined with regard to nutrient sources that are potentially available in fresh and weathered wood. The study was designed to determine how far wood cell wall components need to be broken down during weathering before they provide a useful nutrient source for Aureobasidium pullulans. Various carbon sources were tested, with eight differe...
P R Sharpe, D J Dickinson


Investigation of the suitability of silver fir (Abies alba Mill.) for thermal modification
2004 - IRG/WP 04-40275
In this study the suitability of silver fir (Abies alba Mill.) was examined for thermal modification. Comparative experimental investigations were performed with silver fir and Norway spruce (Picea abies Karst.) after thermal treatments. Besides properties, which characterize the quality of heat treatments, like dimensional stability and resistance against fungal attack, strength properties of the...
C Brischke, A O Rapp


Laboratory studies on control of sapstain and mold on unseasoned wood by bacteria
1991 - IRG/WP 1493
A malt-agar and nonagar laboratory test was used to evaluate the efficacy of bacterial preparations as biological control agents against several sapwood-inhabiting fungi. Both nonsterilized and filter sterilized bacteria preparations prevented attack by the sapwood-inhabiting fungi. Streptomyces rimosus was the most effective bacteria, giving good protection, with a 1-hr soak in a filter-sterilize...
T L Highley, R Benko, S C Croan


A field trial of water repellents as anti-sapstain treatment additives
1987 - IRG/WP 3417
The assessment of water repellents as anti-sapstain treatment additives has been included in a recent FRI research programme investigating improved surface protection of New Zealand Pinus radiata. Laboratory work has shown variation in water repellent effectiveness with chemical type and subsequently a field trial was established to examine the performance of selected water repellent/anti-sapstain...
J A Drysdale, D V Plackett


Comparison of the FRIM and forest research laboratory methods for screening of anti-sapstain formulations
1999 - IRG/WP 99-20170
Two laboratory methods for screening of anti-sapstain formulations were compared. The method adopted by the Forest Research Institute Malaysia (FRIM) involved 3 weeks assessment of rubberwood (Hevea brasiliensis) blocks, dipped in the candidate formulation and inoculated with mycelial/spore suspension of sapstain (Botryodiplodia theobromae) or decay (Schizophyllum commune) fungi, and incubated on ...
A H H Wong, D R Eden, C M Chittenden, M E Hedley, R N Wakeling


Some studies on fungal deterioration of rubber wood (Hevea brasiliensis)
1980 - IRG/WP 2140
For the sreening of anti-stain chemicals trials with selected agricultural fungicides and new chemicals were carried out. Botryodiplodia theobromae, Aspergillus sp. and Penicillium sp. were used at test organisms. For testing the durability of rubber wood (Hevea brasiliensis) suitable local rotting fungi (Basidiomycetes), based on high degrading power, which may later be employed in standard tests...
A Sujan, A G Tan, M Stevens


Detoxification of methylene bisthiocyanate by bacteria isolated from freshly felled, anti-sapstain treated timber
1993 - IRG/WP 93-10017
The microbial defacement of freshly-felled timber treated with organic biocides continues to be a major problem in stored lumber. As part of a study to investigate the depletion in chemical activity of methylene-bis-thiocyanate (MBT) in green timber, bacteria were isolated from freshly-felled boards of Corsican pine (Pinus nigra var. maritima Arnold) previously treated with different biocides. The...
R J Wallace, R A Eaton, G R Williams


Influences of the hydro-thermal treatment on physical properties of beech wood (Fagus orientalis)
2005 - IRG/WP 05-40303
Influences of the hydro-thermal treatment on physical properties of beech wood were studied. Wood specimens (2×2×2cm) were treated in two steps. At first step, samples were treated at 160,180 & 200ºC for 4, 5 & 6 hours. At second step, treated samples were cured based on their first step treatment temperatures (160,180 & 200ºC) for 16 hours. The treated samples were soaked in water...
B Mohebby, I Sanaei


Sapstain development on Jack pine logs in Eastern Canada
2000 - IRG/WP 00-10358
During 1998-99, a study was initiated to investigate the influence of seasons, log types and storage time on the sapstain development on jack pine logs at two sites in Eastern Canada. Jack pine trees (Pinus banksiana) were harvested into whole-tree and cut-to-length logs in spring and in autumn. Sapstain development was examined in these logs at 2 to 4 week intervals after felling. The mean stain ...
Dian-Qing Yang, R Beauregard


A comparative study of some anti-splitting devices, using Eucalyptus saligna and hybrids of Eucalyptus saligna X Eucalyptus spp poles
1983 - IRG/WP 3251
It is commom for some Brazilian wood pole users to require devices such as banding steel, to avoid or reduce splits at the end of Eucalyptus treated poles. On other hand users and manufacturers do not have data to confirm the effectiveness of the banding steel types normally used such as galvanized "Steel-Belt" and galvanized "Wire-Belt". For this reason a comparative study was carried out includi...
F C Geraldo, J A C Sodré


New applications of silafluofen to termite control
2001 - IRG/WP 01-30274
Silafluofen-based termiticides are widely used for soil and timber treatments in Japan, as silafluofen possesses advantageous properties of low fish toxicity and high chemical stability (to light, in soil, in alkaline environments, etc) in addition to high termiticidal activity and low mammalian toxicity. As new applications of silafluofen to termite control, we have developed another type of prod...
K Nakayama, Y Minamite, S Koike, Y Katsuda, K Nishimoto


Reduction of kiln brown stain in radiata pine lumber after log fumigation with methyl bromide
1997 - IRG/WP 97-30129
Methyl bromide fumigation of freshly felled radiata pine log sections effectively killed living cells in parenchyma to at least 75mm into sapwood. Lumber cut from logs (fumigated and control) stored 1 month outdoors (dry) showed slightly reduced brown stain when kiln dried at conventional temperatures. A more dramatic reduction and elimination of brown stain was noted in lumber cut from fumigated ...
E Schmidt, M E Hedley, D R Page, D Cross


Artificial weathering as an aid to assessing the effectiveness of chemicals for preventing blue stain in service - a co-operative study
1984 - IRG/WP 2215
The paper reports co-operative studies carried out within Working Group II of the International Research Group on Wood Preservation to assess the effects of different artificial weathering systems on the performance of fungicides to control blue-stain in service. It has been shown that Atlas, Xenotest and Marr equipments operated according to particular standard schedules can give essentially the ...
A F Bravery, D J Dickinson


The suitability of isothiazolone microemulsions as long term wood preservatives
1997 - IRG/WP 97-30150
Microemulsion formulations of 4,5 dichloro-2-n-octyl-4-isothiazolin-3-one were investigated to determine the leaching potential of these formulation types as well as their efficacy against decay fungi. These patented low leaching formulations exhibited good anti fungal efficacy in standard tests combined with minimal leaching of the active ingredient from the wood. The data suggests that the excel...
B M Hegarty, Bing Yu, L E Leightley


A report on the development of "Technical Recommendations Document for the Canadian wood preservation and protection facilities"
1987 - IRG/WP 3447
The wood preservation and wood protection industry uses chemicals which are similar. However, because the methods of applications of preservatives are different in wood preservation (pressure treatment) and wood protection (surface treatment) plants, their problems need to be resolved separately. As a part of a federal strategy to protect the environment and human health from potentially toxic com...
G Das, V N P Mathur


Screening of modified linseed oils on their applicability in wood protection
2004 - IRG/WP 04-30346
In this study modified linseed oils, rape oil and three waxes were screened on their efficacy as wood protecting agents. By testing all products when impregnated with high retentions in Scots Pine sapwood on water repellence qualities, additionally an accelerated weathering test, drying quality, accelerated brown rot and blue stain test, an indication is formed of the capability of these products ...
A Treu, J Lückers, H Militz


Comparison of two laboratory methods for screening potential anti-sapstain chemicals
1993 - IRG/WP 93-10036
Two methods were used to screen a number of potential anti-sapstain chemicals in the laboratory. In one method miniature boards of freshly felled Scots pine sapwood were dip treated with the candidate chemical, sprayed with a suspension of stainers or moulds and incubated for five weeks. In the other method antibiotic assay discs were treated with precise quantities of chemical, plated out on malt...
S M Gray, D J Dickinson


Commercial antisapstain chemicals in New Zealand
1980 - IRG/WP 3142
Almost all sawn timber of exotic softwoods (principally Pinus radiata) and a large proportion of indigenous sawn timber receives an antisapstain chemical treatment to prevent fungal degrade during subsequent seasoning, storage, or transportation (if exported). Antisapstain chemicals are also widely used to protect freshly peeled round produce during drying. A further, specialised, use is as the fu...
J A Butcher