IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1532 documents. Displaying 25 entries per page.


Collaborative soft rot tests: Results of analyses of soil samples
1976 - IRG/WP 263
C R Levy


The influence of building design on wood decay
2000 - IRG/WP 00-10339
The cheapest and most effective way to prevent wood decay is to KEEP THE WOOD DRY! You and I know that, but we often forget and attempt a preservative solution to a problem better solved with good design and construction. It's also the answer to a frequently missed exam question in my Architecture class. Just as caulking is a poor substitute for proper design, so preservative treatment sh...
W W Wilcox


A short note on the subject of pretreatment decay in wood
1984 - IRG/WP 1245
The paper reviews five national standards for wood utility poles and some literature that concerns the problems of pretreatment decay. Finally it is proposed to form a new sub-group to study that problem....
J A Taylor


Results from soft rot tests in vermiculite jars
1976 - IRG/WP 272
T Vihavainen


Monographic information on Serpula (Merulius) lacrymans (Schum. ex Fr.) S. F. Gray, according to the 'Model Questionnaire for preparation of monographic cards for wood-destroying fungi'
1978 - IRG/WP 170
J Segmüller, O Wälchli


Chemical analysis of TnBTO in lap-joints
1999 - IRG/WP 99-20173
This research was performed as part of the EU project FACT (contract SMT4-CT96-2135) on field tests out of ground contact and ageing methods. The results reported here are part of the work on the experimental lap-joint standard (ENV 12037). TNO investigated the TBTO content of 32 lap-joints by analysing the tin content of 90 samples. The lap-joints were treated with two different TBTO-concentratio...
A Voss, P Esser, W L D Suitela


The Pilodyn instrument as a non-destructive tester of the shock resistance of wood
1978 - IRG/WP 2107
A new non-destructive shock resistance tester, the PILODYN, has been developed. The instrument measures the fracture surface area created by a constant amount of energy. It operates by shooting a blunt pin into wood by an exact amount of energy. The penetration depth is read on a scale. A wide field of application is open to a non-destructive shock resistance tester such as: 1) assessment of the r...
P Hoffmeyer


Surface coatings for impregnated wood
1992 - IRG/WP 92-3684
The use of proper surface coatings enhances the aesthetic and protective properties of impregnated wood. Good results with especially water-borne coatings have been obtained for class-A impregnated L-joints and claddings in field tests started in 1982....
L Kotama


Soil-bed studies
1982 - IRG/WP 2181
This paper discusses factors affecting the design and use of a soil-bed....
P Vinden, J G Savory, D J Dickinson, J F Levy


Ultrastructural observations on wood-degrading erosion bacteria
1986 - IRG/WP 1283
G F Daniel, T Nilsson


Rapid leaching test
1991 - IRG/WP 2367
An accelerated test which is suitable for measuring the extent of metal fixation in both chromium and non chromium containing preservatives is described....
J A Cornfield, M Bacon, A Lyman, C Waldie, M R Gayles


A deflection test for monitoring decay in miniature beams
1986 - IRG/WP 2269
A laboratory apparatus for assessing decay in small stakes is described. It involves the measurement of deflection in a static bending apparatus using a displacement transducer linked to a microcomputer. Measurements are non-destructive, rapid, accurate and automatic and decay can be assessed repeatedly over long time periods....
S M Gray


Spatial arrangement of lignin peroxidase in pine decayed by Phanerochaete chrysosporium and Fomitopsis pinicola
1988 - IRG/WP 1343
By applying immunoelectronmicroscopic methods, lignin peroxidase of the white rot fungus Phanerochaete chrysosporium has been localized in the cytoplasm of hyphae, close to the plasmalemma and on the plasmalemma. Infiltration of wood specimen with culture filtrates, concentrated 300-fold, gave clear information on the penetration of the enzyme into the wood cell wall. Penetration was restricted to...
E Srebotnik, K Messner


Detection of trace organics by ion mobility spectrometry
1990 - IRG/WP 3635
Ion Mobility Spectrometry (IMS) is a time of flight analytical technique that is suited to detect chemicals in the low parts per billion range. Some of the advantages of IMS are: operation at atmospheric pressure, fast response time (0.1-10 sec), and the ability to characterize individual chemical species in complex matrices without any prior sample preparation. In this paper, the utility of IMS i...
A H Lawrence


Co-operative research project on L-joint testing. Progress report to May 1989
1989 - IRG/WP 2338
Further sets of data received from STU (Sweden) after 36 months exposure and Sipad-IRC (Yugoslavia) after 45 months exposure are presented and discussed in conjunction with data reported previously. The new data are generally in agreement with those presented previously and the major difference between institutes continues to be one of rate of colonisation rather than any relative difference in pe...
J K Carey, A F Bravery


Inspection of tropical hardwood window frames in Nigeria for decay presence
1987 - IRG/WP 2294
A method of in situ inspection of hardwood window frames for expression of decay is discussed in this paper. The results show that about 6% of the frames inspected or 23% of the volume of wood in all the frames sampled in buildings erected between 1920 and 1984, exhibited evidence of advanced decay. Protection by the length of the eaves, species of the framing timber used, length of exposure to se...
M A Odeyinde, M A Amakiri, E B Lucas, J O Eyenike, S Akanni


The performance of glue laminated railway ties after 40 years of service in the main line track
1989 - IRG/WP 2325
Two series of horizontally glue laminated ties made of a softwood body and topped with a hardwood lamination were creosoted and installed in 1947 in a tangent and a curved main line track. The tests are now 40 years old and the excellent condition of the ties of these two series suggest that a service life of 50-60 years can be expected....
J P Hösli, E E Doyle, C P Bird, T Lee


Results of collaborative work on laboratory soft rot testing
1989 - IRG/WP 2341
S M Gray, D J Dickinson


Phytotoxic effects of preservative treated props for agricultural use
1989 - IRG/WP 3550
The phytotoxic effect due to the use of wood treated with organic preservatives for agricultural purposes was studied. The assays were carried out on plants tutored with props of Pinus sylvestris treated with three different organic wood preservatives. Pre-assays were carried out to observe the reaction on the plants, spreading directly the preservative on different parts of the plant and to the s...
D Franco, M V Baonza Merino


The preliminary evaluation of selected sulfonium salts for use in wood preservation
1984 - IRG/WP 3278
Five sulfonium compounds, including two sulfonium methosulfates, one sulfonium bromide and two amphoteric sulfonium propanesulfonates, were prepared in crude form and subjected to various biocidal screening tests. A rapid screening test in which treated Pinus radiata pulp pellets were exposed to one of three wood-decaying fungi growing on malt agar revealed that dodecyl dimethyl sulfonium methosul...
D V Plackett


A laboratory evaluation of the susceptibility to biological attack of glued laminated pine timber
1991 - IRG/WP 2387
In the scope of a research programme concerning the use of maritime pine (Pinus pinaster) to produce glued laminated timber structures in Portugal, the natural durability of this material was checked by using laboratory test methods. An European standard, EN 113, was used to test durability against basidiomycetes and a test method developed at LNEC for termites was adapted for this purpose. From t...
L Nunes, H Cruz


Performance of chromated copper arsenate-treated aspen fence posts installed in Forintek's Eastern test plot from 1951 to 1963
1984 - IRG/WP 3272
Aspen poplar fence posts were pressure treated by the full cell process using three formulations of copper chrome arsenate wood preservative. A total of one hundred and fifty nine of the posts were installed in service in Forintek's Chalk River post plot from 1951 to 1962. During the 1982 general inspection of the post plot all 159 posts were still in service. A groundline inspection was ...
C D Ralph


A baiting technique to monitor the development and control of decay in transmission poles
1981 - IRG/WP 2149
P I Morris, D J Dickinson


Micromorphology of the decay caused by Chondrostereum purpureum (Pers.:Fr.) Pouzar and Flammulina velutipes (Curt.:Fr.) Singer
1988 - IRG/WP 1358
Two basidiomycetes, Chondrostereum purpureum and Flammulina velutipes, form typical soft rot cavities in hardwoods and softwoods. Cavity formation is prececed by T-branching or bending of hyphae penetrating the wood cell walls. The two fungi also cause erosion of the wood cell walls....
T Nilsson, G F Daniel


Determination of toxic limits of wood preservatives towards wood-destroying Basidiomycetes. Investigation on the effect of the use of two impregnated wood blocks and of one impregnated and an untreated block respectively in Kolle jars on the toxic limits of wood preservatives
1973 - IRG/WP 225
O Wälchli


Previous Page | Next Page