Ten year field test with a copper-borate ground line treatment for poles
1993 - IRG/WP 93-30017
A wood preservative paste consisting of borax and copper naphthenate has been tested to determine its efficiency in protecting wood from decay fungi and insects. The paste was applied to polyethylene-backed wraps that were fastened to the below-ground portions of unseasoned southern pine pole stubs. After 4 years of exposure in Mississippi, the untreated control stubs were completely deteriorated....
T L Amburgey, M H Freeman


The attack of naturally durable and creosote treated timbers by Limnoria tripunctata Menzies
1995 - IRG/WP 95-10132
Limnoria tripunctata was found tunnelling in creosote treated Douglas fir (Pseudotsuga menziesii) pilings and naturally durable greenheart (Ocotea rodiaei) gate seals at two sites on the south coast of the United Kingdom. Examination of thc creosote-treated wood showed that Limnoria tunnels were concentrated at a depth of 2-3 cm from the timber surface, where creosote loading was lower. Fewer tunn...
A J Pitman, G S Sawyer, G F Daniel


Chemical analyses of IRG/COIPM INTERNATIONAL MARINE TEST (to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water) samples
1987 - IRG/WP 4114
Chemical analysis of CCA and CCB treated timber was carried out after exposure at tropical and temperate marine sites. Results indicated that losses of all elements had occurred. In particular, losses of boron were severe. Arsenic and copper were also lost. The chromium components in both formulations was the most dominant metal remaining. The results suggest that chromium modification was importa...
L E Leightley


Iron in stone wool - one reason for the increased growth and decay capacity of Serpula lacrymans
1992 - IRG/WP 92-1537
The chemical compositions of stone wool and glass wool were analysed. There was more iron in the stone wool than in the glass wool. It was found that iron present in stone wool was easily dissolved by oxalic acid that Serpula lacrymans is able to produce. The stone wool promoted the decay of pine wood by Serpula lacrymans. The glass wool had no effect on the decay capacity of Serpula Iacrymans. Th...
L Paajanen, A-C Ritschkoff


Durability of wood in the area of wood-inhabiting termites in Slovenia
1981 - IRG/WP 1139
This report describes a research dealing with resistance and durability of five different species of wood. The experiment was made in natural conditions in the Slovene area of wood-inhabiting termites. The results of our experimental field, which correspond to the results of the former laboratory experiments, show a very weak resistance of spruce-wood, fir-wood, and beech-wood. They also show thei...
L Kervina


An engineering model for the decay of timber in ground contact
2003 - IRG/WP 03-20260
To predict the residual strength of an engineered structure, it is first necessary to predict the effect of decay. A model was developed in which the effective area of structural decay in large section timbers was defined as that area that could be picked out with a pen-knife. Some limited studies indicated that for practical purposes the remaining wood could be assumed to have its full residual s...
R H Leicester, C-H Wang, M N Nguyen, J D Thornton, G Johnson, D Gardner, G C Foliente, C MacKenzie


Laboratory determination of the natural decay resistance of some lesser-utilized timbers from Tanzania against wood decay fungi
2004 - IRG/WP 04-10517
Four lesser known/utilized timber species (sap and heartwoods) from Tanzania, namely Albizia lebbeck, Zanthoxylum gilletii, Faurea saligna and Parinari curatellifolia were exposed to the brown rot fungi (Gloeophyllum trabeum and Coniophora puteana) and the white rot fungus (Coriolus versicolor) to determine their natural decay resistance according to the EN 113 standard procedure. The timbers were...
P R Gillah, R C Ishengoma, E Julias, S A Amartey, D H Kitojo


Fluoride woodpill
1987 - IRG/WP 3431
Decay problems of spruce joinery in the Netherlands in the 1960's and 1970's led to the introduction of preservative treatment. Because of the known penetration difficulties with Spruce, the results of the treatments were not always successful. The fact that the decay was found only in the joints led to development of the philosophy of "local preservation" of the joints in remedi...
J W P T Van der Drift, K J M Bonsen


Evaluating the potential of modified wood for use in marine environments using a short-term laboratory bioassay
2004 - IRG/WP 04-10525
Chemically modified wood may be an alternative to preservative treated timber for marine structures. In this study a screening laboratory test using the wood-boring isopod crustacean Limnoria quadripunctata was used to assess the durability of chemically modified Pinus sylvestris, Pinus radiata and Picea sp. Most of the treatments used a combination of one of two of types of the resin dimethyloldi...
L M S Borges, S M Cragg, M van der Zee


Information from the COIPM Wood Group
1986 - IRG/WP 4130
The Chairman outlined the progress of the co-operative work "testing the resistance to marine borers of heat shrinkable polyolefin sheathings and of wood treated by vacuum/pressure with polymers (polystyrene)". The first part of the work has been started: the samples of wood wrapped with shrinkable polyolefin sheathings have been prepared and sent to the stations participating. The second part of ...
A Gambetta


Decay types observed in small stakes of pine and Alstonia scholaris inserted in different types of unsterile soil
1990 - IRG/WP 1443
The attack of various wood-degrading microorganisms occurring in mini-stakes of pine and Alstonia scholaris buried in various types of unsterile soil was studied. Attacks by white rot, brown rot, soft rot, erosion bacteria, tunnelling bacteria and actinomycetes were found. Soft rot occurred in all soils, whereas attack by white rot and especially brown rot and erosion bacteria was rare. The type o...
T Nilsson, G F Daniel


A summary of work carried out to compare natural and artificial weathering for preconditioning test specimens in testing anti-stain chemicals for wood in service
1976 - IRG/WP 266
Since 1972 work has been in progress within CEN to establish a European standard for the testing of wood preservatives designed to prevent blue-staining of wood in service. The method is based on the Butin test and involves pre-weathering of the samples prior to biological testing. The weathering regime employed is 6 months outside exposure from March to October. This imposes severe limitations on...
D J Dickinson, A F Bravery


Soft rot decay of Eucalyptus maculata Hook. in different soils from Queensland, Australia
1980 - IRG/WP 1113
In the present work, different Queensland soils were chosen and their gross effects on the decay of treated and untreated Eucalyptus maculata examined. The soils were also amended with various levels of phosphate to study the response of the wood decay mycota to an increasing supply of this nutrient. Phosphate amendment was chosen because of the wide-scale use of superphosphate on Queensland soils...
L E Leightley, I W Russell


Effects of boron treatments on partially decayed oak and pitch pine heartwood
1996 - IRG/WP 96-30106
This paper reports results of borate based preservative treatment and leaching experiments on partially decayed oak and pitch pine heartwood. Previous experiments have shown little damage is caused to sound timber of these types when treated with Polybor and Boracol 20 preservatives. This experiment was carried out to assess the suitability of selected borate based preservatives for use in histori...
S McCutcheon, G M Smith, J W Palfreyman, P Durrant


Blue stain resistance of exterior wood coatings as a function of their typology
1998 - IRG/WP 98-20145
Paints and wood stains were evaluated on their blue stain resistance using both EN 152 method and the reverse method. The typology of these exterior coatings was varied including standard and high solid solvent-borne coatings as well as different types of waterborne coatings. For the water-borne acrylic, alkyd based and hybrid coatings both applied as opaque primer paints and as decorative wood st...
J Van Acker, M Stevens, C Brauwers, V Rijckaert, E Mol


Natural durability of European wood species for exterior use above ground
2003 - IRG/WP 03-10499
The main interest in using more timber for exterior constructions is to protect the environment, where wood is considered an environmentally friendly material. However, chemicals for wood protection are getting more and more restricted, consequently, the focus on the natural durability of wood is increased. Good, well-documented data on the durability of wood species in ground contact exist, which...
B Lindegaard, N Morsing


Role of cell wall structure in soft rot decay of bamboo
1995 - IRG/WP 95-10133
Models of soft rot hyphal penetration of bamboo cell walls are proposed. Soft rot hyphae show an interesting capability of penetrating the bamboo cell wall in different forms; typical longitudinal penetrating hyphae and tangentially orientated penetrating hyphae. The second form of penetration was found to be different from that normally associated with wood cell walls. The differences can be attr...
O Sulaiman, R J Murphy


Effect of light and ventilation condition on the rate of wood decay by the brown rot basidiomycete, Tyromyces palustris
1991 - IRG/WP 1517
Effect of light and the ventilation conditions of incubation jars on the wood decay by Tyromyces palustris (Berk. et Curt.) Murr. FFPRI 0507 was investigated. Under no irradiation of light, the ventilation conditions gave extensive effect on mass loss of the test pieces when the culturing was performed with culture medium designated in Japanese Industrial Standard (JIS) A 9302 (Medium A; glucose 4...
T Suzuki, M Higaki


Modelling the control of decay in freshly felled pine poles
1997 - IRG/WP 97-10206
In a recent study investigating control of decay in freshly felled pine utility poles, it became apparent that the efficacy of different treatment methods was strongly related to the size of the material being treated. A topical application of 5% w/v disodium octaborate tetrahydrate (DOT), brush applied to the cut surfaces of logs with otherwise intact bark was just as effective at excluding white...
M W Schoeman, W Van der Werf, J F Webber, D J Dickinson


Investigation of microwave as a means of eradicating dry rot attack in buildings
1992 - IRG/WP 92-1545
A microwave-apparatus developed for treatment of building-structures infested by dry rot was tested in the laboratory. The test-conditions simulated treatment of either infested timber or infested brickwork. Sawdust samples, both wet and dry, infested by viable mycelium of Serpula lacrymans were packed in glass-tubes. The tubes were then placed in the middle of either 20 cm thick wooden beams or 3...
C Kjerulf-Jensen, A P Koch


An evaluation of CCA, CCB and CCP preservatives using a "sandwich test"
1991 - IRG/WP 2370
The last two years has seen some important changes in standards and preservative types used in Scandinavia, which have led to a wider choice for specifiers. In order to identify those treatments suitable for replacement or reinforcement of decayed constructional timbers, it was felt necessary to modify the standard EN 113 test. Impregnated blocks were sandwiched between two untreated blocks, previ...
A P Koch, L B Sheard


Methyl bromide eradication of the oak wilt fungus in logs. Laboratory and field fumigation
1981 - IRG/WP 3168
Concern over accidental introduction of the oak wilt fungus (Ceratocystis fagacearum) into oak-importing nations has prompted a study supported by the U.S. National Lumber Exporter's Assn. to assess the efficacy of methyl bromide fumigation to eradicate the fungus from logs and lumber. Laboratory and field fumigation trials to develop a reliable and realistic treatment were performed on r...
E L Schmidt, M M Ruetze, D W French


The performance of CCA treatment in bamboo against decay fungi
1993 - IRG/WP 93-30027
Samples of culm wall material from young (< 6 month age) and mature (> 3 years age) culms of the bamboo, Phyllostachys virideglaucescens were treated to equivalent% w/w retentions of a CCA preservative. After fixation and leaching the treated samples were exposed to decay by Chaetomium globosum FPRL S70K, Coriolus versicolor FPRL 28A and Coniophora puteana FPRL 11E. Thin section samples of u...
O Sulaiman, R J Murphy


Movement and persistence of Dazomet and pellected methylisothiocyanate in wrapped Douglas fir and southern pine timbers
1991 - IRG/WP 1496
The movement and persistence of Dazomet (tetrahydro-3,5-dimethyl-2 H-1,3,5 thiadiazine-6-thione) and pelleted methylisothiocyanate (MIT) was evaluated in wrapped Douglas-fir and Southern Pine timbers. MIT pellets did not impart a fungistatic effect to any of the timbers. Failure of MIT was probably due to loss of MIT from pellets prior to application. Fungistatic effect of Dazomet was consistently...
T L Highley


Work programme of CEN/TC 38 (April 1999) and European publications
1999 - IRG/WP 99-20165
Scope of the CEN/TC38: Standardization of the characteristics of natural or conferred durability of wood and its derived materials against biological agents, including the characteristics of protection products and associated processes to obtain this durability. This applies in particular to: - the identification of hazard classes-, - the test methods (wood preservatives and treated wood and wood ...
R Hüe