IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 889 documents. Displaying 25 entries per page.


Natural resistance of different species of timber to marine borer attack in the Trondheimsfjord (Western Norway)
1978 - IRG/WP 435
Natural resistance of 34 timber species to marine wood-borers has been discussed, based on data collected from panels immersed in selected localities in the Trondheimsfjord during 1977-78. The wood-borers encountered on the panels were Psiloteredo megotara, Xylophaga dorsalis, Xylophaga praestans and Limnoria lignorum. The number of borers present and their growth were taken as the criterion for a...
L N Santhakumaran, J A Sneli


Waste management of wood products in life cycle assessment
2000 - IRG/WP 00-50154
Within the framework of the European project LIFE SYS WOOD (contractnr. FAIR CT95-7026) TNO has performed a study on the waste management of wood demolition waste for inclusion in Life Cycle Assessment. In LIFE SYS WOOD one of the main aims was to develop a consistent LCA methodology for wood products. LCA case studies have been performed by partners on wood as raw material, glulam contructions, O...
P Esser, P Eggels, A Voss


Ten year field test with a copper-borate ground line treatment for poles
1993 - IRG/WP 93-30017
A wood preservative paste consisting of borax and copper naphthenate has been tested to determine its efficiency in protecting wood from decay fungi and insects. The paste was applied to polyethylene-backed wraps that were fastened to the below-ground portions of unseasoned southern pine pole stubs. After 4 years of exposure in Mississippi, the untreated control stubs were completely deteriorated....
T L Amburgey, M H Freeman


Chemical analyses of IRG/COIPM INTERNATIONAL MARINE TEST (to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water) samples
1987 - IRG/WP 4114
Chemical analysis of CCA and CCB treated timber was carried out after exposure at tropical and temperate marine sites. Results indicated that losses of all elements had occurred. In particular, losses of boron were severe. Arsenic and copper were also lost. The chromium components in both formulations was the most dominant metal remaining. The results suggest that chromium modification was importa...
L E Leightley


Durability of wood in the area of wood-inhabiting termites in Slovenia
1981 - IRG/WP 1139
This report describes a research dealing with resistance and durability of five different species of wood. The experiment was made in natural conditions in the Slovene area of wood-inhabiting termites. The results of our experimental field, which correspond to the results of the former laboratory experiments, show a very weak resistance of spruce-wood, fir-wood, and beech-wood. They also show thei...
L Kervina


Development of an Australasian protocol for assessment of wood preservatives
1994 - IRG/WP 94-20043
The Australasian Wood Preservation Committee (AWPC) is currently developing a suite of assessment procedures (protocols) for the biocidal efficacy of wood preservatives for approval in Australasia (Australia, New Zealand, Papua New Guinea, Fiji). Protocols are being prepared for the six hazard levels recognised in the relevant standards of member countries and represent the minimum procedures requ...
W D Gardner, H Greaves, M E Hedley, K J McCarthy, J Norton


Second international symposium on wood preservation "The challenge safety-environment" 8-9 February 1993, Cannes-Mandelieu, France
1993 - IRG/WP 93-50001
Contains the following 34 Documents (IRG/WP 93-50001/1 - IRG/WP 93-50001/34) and 4 abstracts: A methodology for the life-cycle assessment of treated timber products (IRG/WP 93-50001/1) Initial results and observations of a model system to assess the efficacy and environmetal impact of preservative treated wood (IRG/WP 93-50001/2) Borates as wood preservatives - an environmental, health and safe...
Anonymous


Evaluating the potential of modified wood for use in marine environments using a short-term laboratory bioassay
2004 - IRG/WP 04-10525
Chemically modified wood may be an alternative to preservative treated timber for marine structures. In this study a screening laboratory test using the wood-boring isopod crustacean Limnoria quadripunctata was used to assess the durability of chemically modified Pinus sylvestris, Pinus radiata and Picea sp. Most of the treatments used a combination of one of two of types of the resin dimethyloldi...
L M S Borges, S M Cragg, M van der Zee


Information from the COIPM Wood Group
1986 - IRG/WP 4130
The Chairman outlined the progress of the co-operative work "testing the resistance to marine borers of heat shrinkable polyolefin sheathings and of wood treated by vacuum/pressure with polymers (polystyrene)". The first part of the work has been started: the samples of wood wrapped with shrinkable polyolefin sheathings have been prepared and sent to the stations participating. The second part of ...
A Gambetta


A summary of work carried out to compare natural and artificial weathering for preconditioning test specimens in testing anti-stain chemicals for wood in service
1976 - IRG/WP 266
Since 1972 work has been in progress within CEN to establish a European standard for the testing of wood preservatives designed to prevent blue-staining of wood in service. The method is based on the Butin test and involves pre-weathering of the samples prior to biological testing. The weathering regime employed is 6 months outside exposure from March to October. This imposes severe limitations on...
D J Dickinson, A F Bravery


Comparison of decay rates of preservative-treated stakes in field and fungus cellar tests. Results after 40 months fungal cellar exposure
1983 - IRG/WP 2200
Decay rates of preservative-treated Pinus radiata stakes during 40 months exposure in the FRI fungus cellar were compared with those of similarly treated material in a field test. Decay rates in the fungus cellar were from 4 to 100 times higher than in the field, although for the majority of preservatives the rate was between 7 and 12 times higher. The lag phase before onset of decay, noticeable w...
M E Hedley


Examination of the Pilodyn as a non-destructive test method for detecting decay in CCA treated eucalypt poles
1982 - IRG/WP 2177
Below groundline condition of 274 CCA treated eucalypt poles comprising 13 different species was examined using 6 and 12 Joule Pilodyn units with 2 and 2.5 mm diameter pins. The data obtained was used to calculate regressions of density on pin penetration. A decrease in density was accompanied by an increase in pin penetration. The best correlation was found using the 6 Joule, 60 x 2.5 mm² diamet...
L E Leightley


Blue stain resistance of exterior wood coatings as a function of their typology
1998 - IRG/WP 98-20145
Paints and wood stains were evaluated on their blue stain resistance using both EN 152 method and the reverse method. The typology of these exterior coatings was varied including standard and high solid solvent-borne coatings as well as different types of waterborne coatings. For the water-borne acrylic, alkyd based and hybrid coatings both applied as opaque primer paints and as decorative wood st...
J Van Acker, M Stevens, C Brauwers, V Rijckaert, E Mol


Natural durability of European wood species for exterior use above ground
2003 - IRG/WP 03-10499
The main interest in using more timber for exterior constructions is to protect the environment, where wood is considered an environmentally friendly material. However, chemicals for wood protection are getting more and more restricted, consequently, the focus on the natural durability of wood is increased. Good, well-documented data on the durability of wood species in ground contact exist, which...
B Lindegaard, N Morsing


Bioassays for rapid assessment of heavy metal toxicity in seawater
1998 - IRG/WP 98-50112
In evaluating the effect of CCA leachate on the establishment of fouling communities on wood exposed in the sea, three organisms were assessed as biological indicators of heavy metal toxicity. These were two macroalgae, Fucus serratus and Undaria pinnatifida. and the motile protist thraustochytrid, Schizochytrium aggregatum. The choice of these organisms for the tests carried out was based on the ...
C J Brown, R L Fletcher, R A Eaton


Investigation of microwave as a means of eradicating dry rot attack in buildings
1992 - IRG/WP 92-1545
A microwave-apparatus developed for treatment of building-structures infested by dry rot was tested in the laboratory. The test-conditions simulated treatment of either infested timber or infested brickwork. Sawdust samples, both wet and dry, infested by viable mycelium of Serpula lacrymans were packed in glass-tubes. The tubes were then placed in the middle of either 20 cm thick wooden beams or 3...
C Kjerulf-Jensen, A P Koch


An evaluation of CCA, CCB and CCP preservatives using a "sandwich test"
1991 - IRG/WP 2370
The last two years has seen some important changes in standards and preservative types used in Scandinavia, which have led to a wider choice for specifiers. In order to identify those treatments suitable for replacement or reinforcement of decayed constructional timbers, it was felt necessary to modify the standard EN 113 test. Impregnated blocks were sandwiched between two untreated blocks, previ...
A P Koch, L B Sheard


Methyl bromide eradication of the oak wilt fungus in logs. Laboratory and field fumigation
1981 - IRG/WP 3168
Concern over accidental introduction of the oak wilt fungus (Ceratocystis fagacearum) into oak-importing nations has prompted a study supported by the U.S. National Lumber Exporter's Assn. to assess the efficacy of methyl bromide fumigation to eradicate the fungus from logs and lumber. Laboratory and field fumigation trials to develop a reliable and realistic treatment were performed on r...
E L Schmidt, M M Ruetze, D W French


Work programme of CEN/TC 38 (April 1999) and European publications
1999 - IRG/WP 99-20165
Scope of the CEN/TC38: Standardization of the characteristics of natural or conferred durability of wood and its derived materials against biological agents, including the characteristics of protection products and associated processes to obtain this durability. This applies in particular to: - the identification of hazard classes-, - the test methods (wood preservatives and treated wood and wood ...
R Hüe


A Soil Bed Test of the Effect of CCA Penetration on the Performance of Hem-fir Plywood
2004 - IRG/WP 04-30332
An accelerated decay test was set up to compare the performance of CCA-treated Western hemlock/amabilis fir plywood treated to meet the preserved wood foundation (PWF) retention standard with various patterns of preservative penetration. Short lengths of treated plywood and comparable untreated material were installed in a soil bed. After eleven years of exposure, the CCA treatments were all sou...
P I Morris, J K Ingram


Long-term protection of stored lumber against mould, stain, and specifically decay: A comparative field test of fungicidal formulations
1984 - IRG/WP 3281
The problem of decay in packaged, unseasoned lumber stored for many months has become of major importance in recent years. Large financial claims have resulted from decay in Canadian lumber stored at length in seaports and storage yards of distributors. For decades acceptable protection from moulds and sapstain was readily achieved with chlorinated phenols applied at appropriate treating levels. H...
A J Cserjesi, A Byrne, E L Johnson


Bending creep test of plywoods under long term exposure to fungal attack
1981 - IRG/WP 2163
Bending creep test and decay test were coupled in order to evaluate the durability of structural plywoods and preservative efficacy. Experimental blocks, 5.0 x 1.2 cm² section x 35.0 cm length, were impregnated with distilled water and inoculated with mycelial fragments of test fungus. Polyethylene bags stretched with metal frame were used as decay chambers. The chambers containing inoculated blo...
M Takahashi


Termites in Eastern Canada: A brief review and assessment
1987 - IRG/WP 1333
The distribution of termites in Canada is reviewed, with particular emphasis on the eastern subterranean termite Reticulitermes flavipes (Kollar) in Ontario province. Municipal and provincial termite control programs are discussed and current treatment practices are described. Previous research on Reticulitermes flavipes in Ontario is briefly reviewed, with reference to a number of unpublished rep...
J K Grace


The shower test method. A leaching test for assessing preservative losses from treated timber under simulated open storage conditions
1993 - IRG/WP 93-50001-04
In the late 1980's against the background of increasing environmental concern a laboratory based accelerated leaching test method for assessing preservative losses-from stored, treated timber was developed by the Dutch organisation for applied Scientific Research (TNO). This test method quantifies the amount of specific preservative components which leach from treated timber under simulat...
J B G A Havermans, W J Homan, M J Boonstra


Premature decay of CCA-treated pine posts in horticultural soils - An overview
1984 - IRG/WP 1241
The recent discovery in New Zealand of early decay in CCA-treated pine posts set in horticultural soils led to the establishment of a comprehensive research programme. The objectives and outline of this programme are presented together with an overview of research progress to date. Results suggest that premature decay of CCA-treated timber is restricted to material placed in highly cultivated soil...
J A Butcher


Previous Page | Next Page