Biological Performance of micronized copper wood preservative formulations in field and laboratory tests
2008 - IRG/WP 08-30488
Micronized Copper wood preservative formulations with different co-biocides were exposed to brown rot fungi in an 8-week AWPA E10 soil block decay test and two AWPA E7 ground-contact decay tests in Hawaii. The micronized copper formulations performed well against decay at or above the AWPA UC3 and UC4 retentions stipulated by the ICC-ES. Micronized copper preservatives performed comparably to a ...
G M Larkin, J Zhang, D L Richter, R J Ziobro, P E Laks


Performance of dip and pressure treated wood in termite ground proximity exposures in Hilo, HI, and Colombia
2008 - IRG/WP 08-30491
A number of preservative systems were evaluated for their ability to control termite attack when applied as both dip and pressure treatments. With dip treatments, better performance was observed with southern pine than spruce-pine-fir using the same solution strength treatment, probably as a result of the about 50% greater uptake with southern pine and associated deeper preservative penetration. B...
P Walcheski, A Zahora


Alkaline copper treated wood for use in residential decking
2008 - IRG/WP 08-30490
Alkaline copper quaternary ammonium compound (ACQ) treated decking was exposed in a field experiment and the mobile copper assessed based on that collected in the leachate. The amount of copper which leached was modeled after 4 years. The results showed that boards which leached most chemical initially provided the greatest loss over four years. The reduction in the mobility of copper with time wa...
J N R Ruddick


Field Stake Performance of Parallel Strand Lumber Treated with Waterborne Copper Naphthenate
2008 - IRG/WP 08-40435
Wood and wood products have been considered a premium building material for residential and industrial structures for many centuries. More recently, structural composite lumber (SCL) products have played an increasing role in satisfying the needs of the building industry. However, both wood and wood composites are naturally biodegradable materials which require enhanced durability when used in ce...
G P Merrick, M H Freeman, J A Brient


Detection and Assessment Healthy Situation of Poulus Euphratica Oliv. with Stress Wave
2009 - IRG/WP 09-20415
The defects of tree trunk of Poulus euphratica Oliv were inspected by stress wave method and diagnosed with transmission time and velocity. The reference values of transmission time of unit length and velocity from stress wave were used to assess the healthy situation of tree trunk. The goal is provide fast inspecting technology and assessment method for the historic trees in China. The results sh...
Shanqing Liang, Nana Hu, Lanying Lin, Feng Fu


Assessment of mould growth on coated wood - methods and application
2009 - IRG/WP 09-20423
Discolouring fungi reduce the service life of coated wooden claddings in façades and increase the total cost of ownership due to shorter maintenance intervals. The project “Enhanced service life on coated wooden facades” has as its main objective to develop new methods for early prediction of durability and longer aesthetic service life of coated wooden cladding related to consumer needs and ...
L Ross Gobakken, C M Whist, O Høibø, P J Hovde, E Larnøy


Leaching performance, decay and termite resistance of wood treated with boron compounds incorporated with phenol-formaldehyde resin
2009 - IRG/WP 09-30503
A resol-type phenol-formaldehyde (PF) resin was synthesized and designed to penetrate wood incorporated with boron compounds in order to immobilize boron in wood. The leaching performance, decay and termite resistance of treated wood was investigated. Three kinds of boron compounds, that is, boric acid (BA), borax (BX) and disodium octaborate tetrahydrate (DOT), were selected to mix with PF and tw...
Liping Yu, Jinzhen Cao


Micronized Copper Preservative Systems: Observations on the Release of Cupric ion (Cu2+) from Treated Wood and Performance against Wood Decay Fungi
2009 - IRG/WP 09-30519
In an attempt to address the mechanism of action of micronized copper preservatives, a 20-week continuous water leaching study was conducted. The leaching results indicated that, once impregnated in wood, micronized copper preservatives continuously release cupric ion, and the levels of cupric ion released from micronized copper treated wood are higher than those released from CCA treated wood, a...
J Zhang, R Ziobro


Environmental Emission of Wood Preservatives: Interpretation of Data Relevant to BPD Risk Assessments
2009 - IRG/WP 09-50259
The risk assessments for the use of wood preservatives proposed by the OECD and used under the Biocidal Products Directive (BPD) (98/8/EC) require the derivation of leaching rates for active substances. These rates are to be used as input data in to agreed exposure scenarios. The leaching rates can be derived from laboratory testing and from field testing. The relationship between laboratory and f...
D G Cantrell


Life Cycle Assessment of treated timber: methodological aspects and first results
2009 - IRG/WP 09-50264
Environmental information on products is more and more required as a key to the market, and the building sector in Europe is certainly advanced in that direction. In France, Environmental Product Declarations are becoming very common for construction products. Therefore, the CTB P+ and CTB B+ certification comity as commissioned FCBA to perform the Life Cycle Analysis of treated timber in order to...
E Vial, M Bertrand, C Cornillier, G Deroubaix


Assessment of decay risk of airborne wood-decay fungi
2012 - IRG/WP 12-10787
The decay risk of airborne wood-decay fungi was investigated by using an air sampler. Japanese cedar disks measuring about 8 cm in diameter and 3 mm in thickness with moisture content at about 100 % were placed in a “BIOSAMP” air sampler and exposed to 1000 liters of air. Air sampling was carried out from June to September at the same sampling site in Tsukuba, Japan. The exposed disks were the...
I Momohara, Y Ota, K Sotome, T Nishimura


Biological Performance of Boron-based Chemicals Treated Wood Composites
2009 - IRG/WP 09-40464
In this study, the biological performance of wood-based composites panels treated with boron containing chemicals against to a fungus was determined. Boric acid, borax, zinc borate and agricultural borate (Tarım-bor™), developed and patented by National Boron Research Institute, were mixed with wood chips or fibers and then particleboard, medium strand board and middle density fiberboar...
Ü C Yıldız, H Kalaycıoğlu, S Yıldız, A Temiz, E Tomak Dizman, A Çavdar Dönmez


Performance of Fasteners in Treated Wood: A Comparative Study
2009 - IRG/WP 09-40465
Fastener performance is an important property for treated wood. Published data on screw and nail performance for different preservative systems currently on the market are, however, limited. In this study, screw and nail withdrawal strength for southern pine wood treated with ACQ (above ground and ground contact), MCQ (above ground and ground contact), borate (disodium octaborate tetrahydrate – ...
Q Wu, T Shupe, J Curole, K Ragon, M Voitier, M Freeman, D Ring


Weathering of Wood Modified with the N-Methylol Compound 1,3‑dimethylol-4,5-dihydroxyethyleneurea (DMDHEU)
2009 - IRG/WP 09-40467
Scots pine (Pinus sylvestris L.) sapwood boards were treated with a methylated 1,3‑dimethylol-4,5-dihydroxyethyleneurea (mDMDHEU) causing weight gains of approx. 25% and exposed to weathering for 18 months. Compared to untreated boards, treatment with mDMDHEU reduced surface discoloration mainly caused by staining fungi. Boards treated with mDMDHEU exhibited clearly lower moisture content th...
C Mai, Yanjun Xie, A Krause, K Urban, P D Evans, K Richter, H Militz


Which are the best painting methods for the beech wood products protection?
2009 - IRG/WP 09-40477
Beech wood (Fagus Sylvatica L.) is one of the most important species of the wood in Kosovo. About 33% of the trees in our country are beech wood. The wood products in Kosovo are from the beech wood. The color difference between red heart wood and white wood of the beech is significant. The main problem for the wood companies in our country is that they haven’t adequate protection against weather...
A Bajraktari


Assessment of the marine borer resistance and abrasion resistance of lesser known hardwood timber species for use in marine construction
2010 - IRG/WP 10-10711
Naturally durable species of timber are used as an alternative to preservative treated timber for marine structures, but many species have not been evaluated for their potential for use in this environment. EN 275 specifies a 5-year test period - too long a period for screening tests to be economically viable. In this study, candidate timber species were selected for testing both in the laboratory...
J R Williams, G S Sawyer, G Malyon, S M Cragg, J D Icely, J Simm, M Meaden


Assessment of antagonism between lignicolous microorganisms: Research on possible use to preserve wood poles
2010 - IRG/WP 10-10718
Biological environments contain a certain number of microbial populations which, within a given ecological niche, display various relations ranging from symbiosis to parasitism. Researchers have been interested in these types of relations for around fifty years, especially in one very particular type of relationship: the antagonism exerted between individuals of the same microbial population. Toda...
J-F Labrecque, A Zaremski, L Gastonguay, Y Prin


Grading the Performance of 18 Common Bamboo Species
2010 - IRG/WP 10-10723
A grading method for assessing the performance of 18 common bamboo species was introduced in this article. The method was based on 4 grade levels with corresponding scores of 4 reference indexes of bamboos including culm diameter, culm-wall thickness, natural durabiliy and preservative treatability. In comparison with the traditional utlilization of bamboo, the grading results showed that this gra...
Chen Lifang, Su Haitao, Zhang Yanjun, Wang Yuxia, He Xuexiang, Ma Hongxia, Xie Guijun


The Relative Performance of an Organic Preservative System under UC3A and UC3B Conditions using Two Test Methods
2010 - IRG/WP 10-20429
Coated L-joints have been used for decades to evaluate the performance of wood preservatives in protected environments. This study was conducted using matched coated and uncoated L-joints to simulate above ground protected and unprotect exposures. When exposed to constant moisture in a greenhouse environment, coated and uncoated L-joints give very similar performance results. In contrast, exposi...
C F Schauwecker, A Zahora, A F Preston


Profiling fungal community in wood decay ecosystem by Denaturing High-Performance Liquid Chromatography
2010 - IRG/WP 10-20443
A DNA-based fingerprinting technique, Denaturing High Performance Liquid Chromatography (DHPLC) was developed to profile fungal communities colonizing indoor timber. Molecular fungal diversity was assessed using amplification based on the Internal Transcribed Spacer (ITS1) rDNA of 74 wood samples collected from infected buildings in France. Due to its high sensitivity, the PCR-DHPLC technique was ...
S Maurice, G Le Floch, M Le Bras-Quéré, J P Rioult, G Barbier


Toward an assessment of copper bioavailability in treated wood
2010 - IRG/WP 10-20445
Many modern wood preservative systems rely on copper (Cu). Some oxalate-producing fungi detoxify Cu by immobilizing it in crystals, and this may decrease its physiological availability (bioavailability). Cu bioavailability may also decrease during wood treatment. Cu retention in wood, however, is typically measured as a weight-to-volume concentration without an estimate of its bioavailability and ...
J S Schilling, J J Inda


Onset of mould growth – the effect of climate variability and different geographic locations
2010 - IRG/WP 10-20446
This paper presents a study on how climate conditions at numerous locations in Sweden affect the risk of onset of mould on wood sheltered outdoors. The results indicate that the risk is clearly higher in the south compared to the north of Sweden. These differences are mainly explained by colder and dryer winter periods in the north which is unfavorable for development of mould. The results also sh...
M Häglund, T Isaksson, S Thelandersson


The biological durability approach for wood product performance and service life prediction
2010 - IRG/WP 10-20457
The performance of wood-based products under conditions that enable biodegradation are of concern to all who envisage sustainable use of forest based products. This concern is also the basis of classification of wood species on the basis of their biological durability. Engineers are looking for options to transfer such classification into practical service life values for constructions and related...
J Van Acker, J Van den Bulcke, L De Boever


Biological performance of wood treated with tar-oil recovered during slow pyrolysis of macadamia nut shells
2010 - IRG/WP 10-30523
This study evaluated decay and termite resistance of wood treated with tar oil obtained from a commercial pyrolysis process of macadamia nut shells. Vacuum-treated pine wood specimens were subjected to various brown and white rot fungi based on the soil-block test method specified by the American Wood Protection Association (AWPA) after leaching process. Treated specimens were also subjected to th...
S Nami Kartal, E Terzi, C Kose, J Hofmeyr, Y Imamura


Assessment of Boracol 200RH (FrameSaver) as a remedial treatment to control decay in pre-decayed model timber frame units
2010 - IRG/WP 10-30529
Model timber frame units constructed from untreated radiata pine were pre-wetted to approximately 40% moisture content and inoculated with Coniophora puteana and Oligoporus placenta. Units were transferred to a controlled environment room maintained at 25°C and 95% RH for 7 and 10 weeks to allow two levels of decay to become established in units. Following pre-decay, units were disassembled, clea...
Mick Hedley, Dave Page, Jackie van der Waals


Previous Page | Next Page