IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 554 documents. Displaying 25 entries per page.


The EWPMG proposal for the environmental risk assessment of wood preservatives
2001 - IRG/WP 01-50166-09
This paper reviews the protocol prepared by the European Wood Preservative Manufacturer's Group, which could be used by an applicant for product approval under the Biocidal Products Directive 98/8/EC, to produce a risk assessment for an active substance or product in the Product Type 8 Wood Preservatives, in support of the application. The background and scope of the protocol are reviewed...
E F Baines


Field performance of novel antisapstain formulations
1997 - IRG/WP 97-30125
The effectiveness as antisapstain formulations of combinations of oxine copper (Cu-8), carbendazim, hexaconazole, cyproconazole, flusilazole, didecyldimethyl ammonium chloride (DDAC), an alkanolamine borate (SB), benzalkonium chloride (BAC), 2-n-octylisothiazolin -3-one (isothiazoline) and p-chlorophenyl-3-iodopropagilformal (CPIPF) was determined for freshly sawn, block-stacked radiata pine in th...
D R Eden, R N Wakeling, C M Chittenden, J G Van der Waals


L-joint trials: Part 1: Observations on the process of colonisation and decay
2002 - IRG/WP 02-20250
The first trials using the small L-joint, later adopted for use in BS EN 330 and AWPA Standard E9-97 were exposed at BRE in 1975 but all were assessed destructively during the early stages of exposure. The longest running trial which included replicates for long-term exposure will have been exposed for 20 years in July 2002. This paper provides an overview of the results of testing during that p...
J K Carey


A technique for the rapid assessment of wood surface degradation during weathering
1987 - IRG/WP 2281
Radiate pine (Pinus radiata D. Don) sapwood samples taken from four trees were converted into thin strips 100 x 10 x 0.085 (85 µm) mm³, (longitudinal x radial x tangential) in size and exposed in preweighed hatches to the weather inclined at 45° facing equatorially for 10, 20, 40, 60, 80 and 100 days. Significant (P < 0.001) weight losses occurred with time over the exposure period. Differen...
P D Evans, D Abbott, S Thein


Ecotoxicological behaviour of leachates from superficially treated timber as an approach for a test strategy of environmental risk assessment in wood preservation
1998 - IRG/WP 98-50101-09
At present for wood preservatives, which in Germany are subject to the quality mark of the RAL-Gütegemeinschaft Holzschutzmittel, health and safety as well as environmental aspects are evaluated by official authorities, as BgVV (Federal Institute for Consumer Health Protection and Veterinary Medicine) and the UBA (Federal Environmental Agency). From the environmental point of view to day there a...
H W Wegen, U J Lucks


IUFRO rating system compares favourably to weight loss for soil-bed testing
1990 - IRG/WP 2343
The soil-bed/small stake test is commonly used for rapidly evaluating the performance of new, more environmentally acceptable, preservatives. In a 1.5 year experiment with three copper-based waterborne preservatives, visual evaluation and probing using the IUFRO performance rating scale (0-4) gave very similar toxic thresholds to those derived from measurement of weight loss at the end of the expe...
P I Morris


A novel solvent penetration assessment technique for wood preservativation treatments using waterborne systems
1990 - IRG/WP 2346
Solvent and hence solute (a.i.) penetration during any wood preservation treatment cycle and the flow pathways taken by the solvent in the wood are crucial elements in determining the adequacy of any treatment. Inadequate solvent penetration into specimens or an inappropriate tissue throughflow pattern during impregnation will markedly affect the distribution pattern achieved by many non-diffusibl...
A J Pendlebury, J Coetzee, E Sorfa, A Botha


Effect of kerfing on performance of Douglas-fir utility poles in the Pacific Northwest
1990 - IRG/WP 3604
Preservative treatment produces an external layer of protection in Douglas-fir poles, but the development of deep checks as the wood dries after treatment can permit entry by fungi and insects. A variety of remedial treatments can arrest this decay; however, it is far more efficient to prevent checking. Kerfing represents one potential method for limiting the development of deep checks. In previou...
J J Morrell


Performance trials of treated hardwood fences
2002 - IRG/WP 02-30281
This paper examines the performance of the traditional hardwood paling fence used in Australia, after preservative treatment. Unseasoned rails, palings and plinths of the low natural durability species Eucalyptus regnans (mountain ash) and E. obliqua (messmate) were treated with PEC (pigment emulsified creosote) or PROCCA (an oil emulsion of CCA). Treated posts of these species were also compared ...
L J Cookson D Scown, B Iskra


Performance of preservative-treated timber against biodeterioration in Indian waters
1984 - IRG/WP 4106
Results on the investigation on the durability of panels of 32 timber species, pressure-treated with various preservatives and exposed along the Indian coast for varying periods upto a maximum of 15 years, are summarised. Panels of even non-durable timber gave excellent results against biodeterioration after treatment. Their life was comparable to that of treated durable timber. The preservative t...
L N Santhakumaran, J C Jain, M C Tewari


Performance of borate-treated sill plates (dodai) in a protected, above-ground field test in Japan
2002 - IRG/WP 02-30278
This document is supplemental to the previous IRG document (IRG/WP 2000-30239). An experiment to simulate the dodai (sill plate) of the Japanese houses was conducted at the termite field test site of the Wood Research Institute in Kagoshima, Japan where two economically important subterranean termite species [Coptotermes formosanus Shiraki and Reticulitermes speratus (Kolbe)] are established. DOT...
K Tsunoda, A Adachi, A Byrne, P I Morris, J K Grace


Non-destructive stress wave measurement of decay and termite attack in experimental wood units
1986 - IRG/WP 2256
The purpose of this study was to determine if stress wave analysis could be used to monitor the degradation of wood specimens exposed to the brown-rot decay fungi (Gloeophyllum trabeum) and of wood specimens subjected to attack by subterranean termites. One hundred fifty 3/4 by 3/4 by 12 in. Southern pine specimens were used for exposure to brown-rot decay fungi and two hundred twenty-five 3/4 by ...
R F Pellerin, R C De Groot, G R Esenther


Future Directions Regarding Research on the Environmental Impacts of Preservative-Treated Wood: Environmental Impacts of Preservative-Treated Wood. February 8-11, 2004, FL, USA Workshop – Research Needs
2004 - IRG/WP 04-50222
This paper presents a series of documents that focus on research needs for potential future work focusing on the environmental impacts of preservative-treated wood. These documents were developed through a conference sponsored by the Florida Center for Environmental Solutions (FCES), located in Gainesville, Florida. The conference was held in Orlando, Florida, February 8 – 11, 2004 and the tit...
H M Solo-Gabriele, J D Schert, T G Townsend


Treatment application method and CCA efficacy in Corsican pine - Assessment by serial exposure and soil burial tests
1993 - IRG/WP 93-40006
A previous report on this research (Newman and Murphy, 1992) identified possible variation in the efficacy of a CCA preservative applied to Corsican pine (Pinus nigra var. maritima) dependant upon the treatment application method (Bethel, Lowry or Steam/Bethel). This paper presents further data from biological testing of CCA treated Corsican pine using serial exposure and unsterile soil techniques...
P R Newman, R J Murphy


Timber deterioration and its prevention in marine environment
2005 - IRG/WP 05-10559
Wood-borer activity is an established fact in Mumbai harbour that leads to severe deterioration of timber. In order to prevent the deterioration caused by wood borers three resin preservatives containing Zinc borate, Organo-copper polymer (4 wt% Cu) and Organo-Tin polymer &#61531;Copoly(TBTM-MMA)&#61533; were used for timber treatment. Test panels were treated using standard method and the...
B S Swami, M Udhayakumar, P Kumar, A B Samui


Assessment of the Inhibition of wood decay fungi by volatile organic compounds identified from Trichoderma spp.
1999 - IRG/WP 99-10302
Previous research identified five volatile organic compounds produced by Trichoderma spp. that may be inhibitory to wood decay fungi. The effects of four of these volatile organic compounds, 2-propanone, 2-methyl-1-butanol, heptanal and octanal were tested over a range of concentrations against four selected wood decay fungi. The fungi were incubated in malt extract broth under appropriate conditi...
S N Humphris, R E Wheatley, A Bruce, C Payne


Assessment of untreated Papua New Guinea timbers against subterranean termites. Final report
1993 - IRG/WP 93-10041
Four years after the exposure of eight timber species of varying density against subterranean termites in a field trial, Kwila was still generally sound while Taun, Malas and PNG Walnut were beginning to be attacked slightly to moderately. Calophyllum, Kamarere, PNG Beech and White Cheesewood were severely attacked and failed. Results after the period of exposure shows that Kwila rates highly as t...
H C Konabe, M Rokova


Assessment of residual retentions in creosote treated Scots pine (Pinus sylvestris) poles after 45 years ground contact service in the Lemstervaart in the Dutch polder
1994 - IRG/WP 94-50022
In a project funded by the Water State Authorities (RWS) and the Noordoostpolder Water Board, the residual retentions in ten creosote treated Scots pine (Pinus sylvestris) poles were examined after 45 years ground contact service along a canal (Lemstervaart) in the Dutch Noordoostpolder. The Lemstervaart location was selected due to the fact that the poles involved had been originally treated and ...
P Esser, W L D Suitela, A J Pendlebury, H Visscher


A preliminary assessment of the costs of termite activity in Australia: A discussion paper
1983 - IRG/WP 1207
A preliminary assessment has been made of the economic importance of termite activity in Australia and this paper is intended to serve as a starting point in discussing this topic. Damage to timber in service represents their greatest area of economic importance in urban and rural environments. Costs resulting from termite activity include timber replacements in buildings, railway sleepers, transm...
J R J French


The performance of metal-chromium-arsenic formulations after 32 to 38 years' in-ground exposure in Australia
2000 - IRG/WP 00-30240
Two trials of metal-chromium-arsenic preservatives were exposed in-ground in Australia. In Trial 1, Pinus radiata stakes treated with Boliden K.33, Boliden S.25, Celcure A, Tanalith C and Tanalith CA were installed at Sydney and Narrandera in 1961/1962. In Trial 2, P. radiata and Eucalyptus regnans sapwood were treated with Celcure A, Celcure A21-N, Celcure A 21-O and Tanalith CA (new) and install...
G C Johnson, J D Thornton, J Beesley


Development of a model system to assess the efficacy and environmental impact of a chromated fluoride remedial treatment for creosoted distribution poles
1992 - IRG/WP 92-2395
A closed model system was designed to facilitate a controlled study of the leachability and environmental fate of a remedial preservative under laboratory conditions. The elements of the model include a precipitation apparatus above a treated pole section which is positioned in a representative soil profile supporting a sward of perennial ryegrass. The model will allow detailed examination of the ...
D C R Sinclair, G M Smith, A Bruce, B King


Assessment of treated wood leachates genotoxicity with a bacterial test
1997 - IRG/WP 97-50089
Genotoxicity is known as the damage caused by environmental stressors (biological, chemical and physical) on the genetic material of an organism. This toxicological effect can be assessed by a lot of biological assays and especially by bacterial tests. These tests are frequently performed on environmental samples or on pures substances and are in that case, strongly correlated to the carcinogenic ...
P Marchal, C Martin


A methodology for the life-cycle assessment of treated timber products
1993 - IRG/WP 93-50001-01
Using case studies of CCA-treated motorway fenceposts and creosote-treated electricity transmission poles, the paper suggests an approach to evaluation of the overall environmental impact of treated timber products, utilising the emerging systems analysis method of life-cycle assessment (LCA). The development and application of LCA methodologies to date is reviewed and the key features identified....
S R Smith, R J Murphy, D J Dickinson


Performance of different treatments and finishes on wood out of ground contact. Preliminary results
1984 - IRG/WP 2221
Pinus and Eucalyptus L-joints treated with CCA, a water dispersable PCP and untreated ones were painted according to seven different finish&apos;s schedules and exposed at two sites in State of Sao Paulo. After ten months of exposure, it was possible to verify that preservative treatment improve the performance of both wood and finish. It was also possible to observe that wood substrate, prese...
S Milano


Performance of Paraserianthus falcataria treated with ACZA, ACQ, CC or CCA and exposed in Krishnapatnam harbour, India
2005 - IRG/WP 05-30382
Paraserianthus falcataria (=Albizia falcataria) treated to two retentions with ammoniacal copper zinc arsenate (ACZA), ammoniacal copper quaternary (ACQ), ammoniacal copper citrate (CC) and chromated copper arsenate (CCA) was assessed over 34 months in a tropical marine waters at Krishnapatnam harbour on the east coast of India. ACZA treatment showed comparatively better resistance than CCA, ACQ a...
B Tarakanadha, K S Rao, J J Morrell


Previous Page | Next Page