Your search resulted in 430 documents. Displaying 25 entries per page.
Antagonistic effects of a range of fungi to Serpula lacrymans
1996 - IRG/WP 96-10156
Certain fungi have been demonstrated to exhibit antagonism towards Serpula lacrymans in culture. Species from the genera Trichoderma, Gliocladium, Penicillium and Hypomyces were among those exhibiting the strongest antagonism. Certain species showed antagonism in a range of media of varying nutritional status. The possible role of antagonistic fungi as biocontrol agents for Serpula lacrymans is di...
P Rattray, G McGill, D D Clarke
Possibility of use of wood species per class of biological risks. Attempt to determine criteria based on Pr EN 350-1/2/3
1992 - IRG/WP 92-2409
M Rayzal
Japanese wood preserving industry
1990 - IRG/WP 3596
Although a great amount of wood is in use in Japan, a little attention has been paid to the significance and importance of wood preservation. The fact reflects that only less than 0.5% of the total wood consumption is treated with wood preservatives today in the country. Over the 20 years before 1970, the annual volume of preservative treated (pressure treatment) wood was relatively at a stable le...
K Tsunoda
Decay resistance of wood removed from poles treated with Trichoderma
1989 - IRG/WP 1386
Wood blocks removed from a distribution pole previously treated with a biological control product (Binab FYT pellets) were exposed in soil block tests to selected basidiomycetes. The blocks were removed from regions of poles where Trichoderma colonization had been confirmed by extensive sampling and computer mapping of microbial inhabitants. The results indicate that material from pole interiors c...
A Bruce, B King, T L Highley
Biological Durability of Laminated Veneer Lumber from Durable and Non-Durable Wood Species
2005 - IRG/WP 05-10567
Laminated Veneer Lumber (LVL) was laboratory manufactured using veneers from decay and non decay resistant species in order to evaluate changes in the durability as a result of the LVL manufacturing process, and to test if the mixing of decay resistant species and non decay resistant species can improve durability. Laboratory soil block test and field test were conducted. The durability of solid w...
P Nzokou, J Zyskowski, S Boury, D P Kamdem
Assessment of losses of wood preservatives from treated wood by leaching into the environment
1993 - IRG/WP 93-50001-13
Wood preservative chemicals may be lost from treated timber by leaching into water or soil. The degree to which this might occur and its effect on the environment is difficult to assess quantitatively due to the absence of appropriate test methods. This paper describes work to assess test methodology capable of allowing the rates of loss of wood preservative from treated timber to be quantified. T...
R J Orsler, G E Holland
Biological performance of gypsum products containing borates
2000 - IRG/WP 00-30237
At suitable retentions borates have biostatic properties enabling them to be used for biodeterioration control in wood. They provide protection against decay fungi, mould, and termites, which are known to also attack gypsum products. Currently, many gypsum products contain added borates, which are used to improve physical and processing characteristics. Work examining the effect of borates at cont...
J L Fogel, J D Lloyd
Surveillance médicale des personnels exposés aux produits de préservation du bois
1990 - IRG/WP 3588
J-C Aubrun
Protocols for assessment and approval of wood preservatives in the Nordic countries
1994 - IRG/WP 94-20046
This paper reviews the protocols presently in use in the Nordic countries (Denmark, Finland, Iceland, Norway and Sweden) for assessment and approval of wood preservatives with respect to their biocidal efficacy....
J Jermer, B Henningsson
Biological control of Serpula lacrymans using Trichoderma spp
1994 - IRG/WP 94-10069
The effectiveness, or otherwise, in killing Serpula lacrymans, of a range of Trichoderma spp. in a variety of media and using two different incubation systems has been tested. In agar based systems with normal nutrients or minimal nutrients with high or low nitrogen contents and high or low iron content Trichoderma harzianum 25 proved to be the most efficient and killing Serpula lacrymans. Other s...
A J Score, J W Palfreyman
Reliability-based service life prediction methodology for assessment of water protection efficiency for coatings on wood
2003 - IRG/WP 03-20268
Assessment of water protection efficiency according to EN 927-5 has been shown to give significant differences in water absorption values for different types of coatings on wood. It is shown that the combination of EN 927-5 and an artificial weathering procedure gives more information regarding expected durability and long-term performance than a single measurement of water absorption on fresh, un...
J Ekstedt
The collaborative developement of soil acceptance criteria for timber treatment chemicals in New Zealand
1995 - IRG/WP 95-50040-34
In New Zealand, the issue of potential contamination on timber treatment sites arose in the late 80's due to the long history of use of PCP by the industry. One of the recommendations from the task group set up to investigate the issue was the development of a set of acceptance criteria to define trigger levels for remediation. A technical group from the government, industry and regional ...
H C Boyd
How best to specify retentions of preservative treatments: kg/m3 or % (m/m)
1998 - IRG/WP 98-20151
When specifying treatments according to the European Standard EN 351-1, retentions in the analytical zone are based on the amount of product found to be effective in biological tests; this is expressed in terms of the retention of the product per unit volume (kg/m3) for penetrating treatments and per unit area (g/m2) for superficial treatments. However, to check whether the retentions have been ac...
J K Carey
European standardization for wood preservation
1990 - IRG/WP 2359
G Castan
Programme section 4, Processes
1996 - IRG/WP 96-40066
IRG Secretariat
Biological control of decay in standing creosote-treated poles
1976 - IRG/WP 156
Internal decay caused by basidiomycetes in standing creosoted poles can be controlled biologically, it seems, by artificial inoculation near the ground line. For such inoculation IC-type facultative mycoparasites, Scytalidium sp FY strain or Trichoderma spp for example, may be used. Apparent residual action can be explained by the release of non water soluble chemically stable antibiotics from the...
J Ricard
Biological agents of timber degradation in Portugal. Marine borers
1991 - IRG/WP 4171
A brief report of the studies carried out in Portugal on marine borers is presented. The marine borers found in the portuguese coast are refered as well as the wood species where those organisms were identified. Emphasis is given to a study carried out from 1960 to 1975 at the Tagus estuary in Lisbon with the purpose, among others, of establishing the natural durability of different timbers....
J S Machado, L Nunes
About the water and biological resistance of some new chemically modified wood composites
1997 - IRG/WP 97-40077
As well known, wood represents a valuable natural composite material with a very large utilisation as solid wood or in wood based composite materials. Its qualities but also its defects as the dimensional instability, the susceptibility to biological attack, the anisotropy, are due to its complex structure. Research has demonstrated that the chemical modification of wood, meaning the involving of ...
M C Timar, M D Mihai, G Baciu
The leachability, biological resistance, and mechanical properties of wood (Pinus sylvestris L.) treated with CCA and CCB preservatives
1999 - IRG/WP 99-30207
Scots pine (Pinus sylvestris L.) specimens treated with CCA and CCB preservative solutions (1.0%) were subjected to several fixation processes and leached elements from the specimens were determined. In addition, the specimens exposed to different fixation temperatures were subjected to soil-block test using two brown-rot fungi and one white-rot fungus in order to investigate the effects of fixati...
S N Kartal
Effects of pretreatments for the amelioration of preservative impregnability using the Oscillating pressure method (OPM)
1995 - IRG/WP 95-40044
For the purpose of an amelioration of preservative impregnability, three types of pretreatment: the steaming, the explosion and the boiling, were tested. The specimens were prepared by the domestic four species: Itajii, Ryukyumatsu, Sugi and Hinoki, and 1 refractry imported species: Douglas-fir. The dimension of specimens was 20 x 20 x 300 mm³ and were treated with CCA in a laboratory OPM machine...
K Suzuki, I Asaoka, S Tani, K Okada, T Hidaka
Quantitative assessment of field specimens. A proposal for discussion
1980 - IRG/WP 2143
H Friis-Hansen
Some biological observations on the management of preservativion experiments with submerged timber in the marine environment
1976 - IRG/WP 421 E
P Deschamps
Programme section 2, Test methodology and assessment
1996 - IRG/WP 96-20094
IRG Secretariat
Antagonistic effect of some mycorrhiza fungi as biological control of blue-stain
1987 - IRG/WP 1314
This report discussed the possibility of using some mycorrhiza fungi as biological control of blue-stain. The results show that new bio-technological possibilities are opening, because, by cultivating antibiosis fungi in fermentor, it is possible to prepare extracts which can then be used as the natural preservative to control the blue-stain in wood....
R Benko
Durability of different heat treated materials from industrial processes in ground contact
2005 - IRG/WP 05-40312
In this study the durability of heat treated wood originating from four different European industrial heat treatment processes in ground contact was examined. The manufacturers of heat treated material were: PLATO Hout B.V./Netherlands, Thermo Wood/Finland, New Option Wood/France and Menz Holz/Germany where Oil-Heat treated Wood (OHT) is produced.
All heat treated materials showed significantly i...
C R Welzbacher, A O Rapp