IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 178 documents. Displaying 25 entries per page.


Assessment of decay risk of airborne wood-decay fungi
2012 - IRG/WP 12-10787
The decay risk of airborne wood-decay fungi was investigated by using an air sampler. Japanese cedar disks measuring about 8 cm in diameter and 3 mm in thickness with moisture content at about 100 % were placed in a “BIOSAMP” air sampler and exposed to 1000 liters of air. Air sampling was carried out from June to September at the same sampling site in Tsukuba, Japan. The exposed disks were the...
I Momohara, Y Ota, K Sotome, T Nishimura


Assessment of the marine borer resistance and abrasion resistance of lesser known hardwood timber species for use in marine construction
2010 - IRG/WP 10-10711
Naturally durable species of timber are used as an alternative to preservative treated timber for marine structures, but many species have not been evaluated for their potential for use in this environment. EN 275 specifies a 5-year test period - too long a period for screening tests to be economically viable. In this study, candidate timber species were selected for testing both in the laboratory...
J R Williams, G S Sawyer, G Malyon, S M Cragg, J D Icely, J Simm, M Meaden


Assessment of antagonism between lignicolous microorganisms: Research on possible use to preserve wood poles
2010 - IRG/WP 10-10718
Biological environments contain a certain number of microbial populations which, within a given ecological niche, display various relations ranging from symbiosis to parasitism. Researchers have been interested in these types of relations for around fifty years, especially in one very particular type of relationship: the antagonism exerted between individuals of the same microbial population. Toda...
J-F Labrecque, A Zaremski, L Gastonguay, Y Prin


Toward an assessment of copper bioavailability in treated wood
2010 - IRG/WP 10-20445
Many modern wood preservative systems rely on copper (Cu). Some oxalate-producing fungi detoxify Cu by immobilizing it in crystals, and this may decrease its physiological availability (bioavailability). Cu bioavailability may also decrease during wood treatment. Cu retention in wood, however, is typically measured as a weight-to-volume concentration without an estimate of its bioavailability and ...
J S Schilling, J J Inda


Onset of mould growth – the effect of climate variability and different geographic locations
2010 - IRG/WP 10-20446
This paper presents a study on how climate conditions at numerous locations in Sweden affect the risk of onset of mould on wood sheltered outdoors. The results indicate that the risk is clearly higher in the south compared to the north of Sweden. These differences are mainly explained by colder and dryer winter periods in the north which is unfavorable for development of mould. The results also sh...
M Häglund, T Isaksson, S Thelandersson


Assessment of Boracol 200RH (FrameSaver) as a remedial treatment to control decay in pre-decayed model timber frame units
2010 - IRG/WP 10-30529
Model timber frame units constructed from untreated radiata pine were pre-wetted to approximately 40% moisture content and inoculated with Coniophora puteana and Oligoporus placenta. Units were transferred to a controlled environment room maintained at 25°C and 95% RH for 7 and 10 weeks to allow two levels of decay to become established in units. Following pre-decay, units were disassembled, clea...
Mick Hedley, Dave Page, Jackie van der Waals


Life Cycle Assessment Comparison of Treated Wood to Alternate Materials – Overview, Results and Lessons
2011 - IRG/WP 11-50282
Life Cycle Assessment (LCA) has proven useful in documenting the “green” benefits of various treated products compared to the commonly used alternates. To date, six LCA comparisons have been done or are nearing completion using ISO14040 and 14044 principles and data from US EPA databases. In almost all cases, the impact indicators for treated wood products show considerably smaller adverse e...
T Stephen, P E Smith, C R McIntyre


The assessment of biological and mechanical properties of wood treated with ionic liquids – N,N-dimethylamine and 1-decylimidazole derivatives
2012 - IRG/WP 12-40582
This paper presents the results of tests of the effectiveness of action of new imidazolium and bis-ammonium ionic liquids against Basidiomycotina and Ascomycotina wood-destroying fungi. All the investigated ionic liquids showed high fungicidal action against Coniophora puteana. In order to characterize the influence of ionic liquids on mechanical wood properties, the compression strength along the...
W Przybylska


Guideline for Environmental Product Declaration for Thermally Modified Timber
2012 - IRG/WP 12-50287
Environmental Product Declarations (EPD) intend to enable the comparison of the environmental attributes of products that meet equivalent functional requirements. This guideline describes the proceedings of EPD for thermally modified timber (TMT). The main objective is the general survey on requirements on EPD which are based on European and international standards.Up to now only a few EPDs for na...
L Clauder


Development of a quality control assessment method to predict properties of heat treated wood
2012 - IRG/WP 12-40611
Heat treatment has been used to improve properties of non durable European species. Chemical modification of some of the wood components provides improved dimensional stability and biological performance against decay fungi while mechanical properties such as modulus of rupture are reduced. Quality control of commercially made thermally treated wood is one of the major challenges to allow its indu...
M Chaouch, K Candelier, S Dumarcay, A Pétrissans, M Pétrissans, P Gérardin


An assessment of soft rot in preservative-treated poles in two test sites and two network areas in New South Wales
2013 - IRG/WP 13-10801
This document presents an extended summary of recent investigations into soft rot attack of preservative treated power poles from the re-inspection of samples selected from two field sites and two in-service trials located in New South Wales, Australia. The in-ground sapwood of selected poles was assessed by probing and, after core sampling, by microscopy to determine the severity and extent of s...
W D Gardner, M A Powell, C Kirton


The assessment by visual grading, change of color and ergosterol content ratings, the resistance to mould fungi of treated with wood preservative Scots pine sapwood
2013 - IRG/WP 13-20514
The filamentous (mould) fungi belonging to Ascomycetes, Deuteromycetes group are an cosmopolitan organisms which attacks wooden elements disfiguring them, dropping their value and causing environmental and health hazard. The fungi in a short time cause mainly disfigurement of wood does not effect on strength properties of wood, but with strong prolongation of duration of conditions favourable for ...
A Fojutowski, A Koziróg, A Kropacz


The Effect of Water Repellent on Semi-Field Leaching of Active Substances from Metal Free Wood Preservative Formulation
2013 - IRG/WP 13-30615
The risk assessments for the use of wood preservatives proposed by the OECD and used under the Biocidal Products Directive (BPD) (98/8/EC) require the derivation of leaching rates for active substances. These rates are to be used as input data in to agreed exposure scenarios. A comparison of the leaching of active substances from wood treated with a metal free preservative formulation with and wit...
D G Cantrell


Application of a model for the prediction of fungal degradation of thermally modified beech timber by Trametes versicolor
2013 - IRG/WP 13-40622
Colour measurement technology is found to be feasible for characterization of the property changes of thermally modified timber (TMT). In opposite to time-consuming and expensive laboratory tests a non-destructive test represents an improvement for the manufacturer of TMT. Therefore the aim of this study was to develop a method which allows sorting the different treatment intensities after the man...
Clauder, L., Richter S., Unger, W., Pfriem, A


Conclusions and Summary Report on an Environmental Life Cycle Assessment of ACQ-Treated Lumber Decking with Comparisons to Wood Plastic Composite Decking
2013 - IRG/WP 13-50295
The Treated Wood Council has completed a quantitative evaluation of the environmental impacts associated with the national production, use, and disposition of ACQ (alkaline copper quaternary)-treated lumber decking and wood plastic composite decking using life cycle assessment (LCA) methodologies and following ISO 14044 standards. The results for treated wood decking are significant. • Less En...
AquAeTer, Inc.


Conclusions and Summary Report on an Environmental Life Cycle Assessment of Borate-Treated Lumber Structural Framing with Comparisons to Galvanized Steel Framing
2013 - IRG/WP 13-50296
The Treated Wood Council has completed a quantitative evaluation of the environmental impacts associated with the national production, use, and disposition of borate (disodium octaborate tetrahydrate)-treated lumber structural framing and galvanized steel framing using life cycle assessment (LCA) methodologies and following ISO 14044 standards. The results for treated wood framing are significant....
AquAeTer, Inc.


Conclusions and Summary Report Environmental Life Cycle Assessment of Highway Guard Rail Posts
2013 - IRG/WP 13-50297
The Treated Wood Council has completed a quantitative evaluation of the environmental impacts associated with the national production, use, and disposition of treated wood and galvanized steel highway guard rail posts using life cycle assessment (LCA) methodologies and following ISO 14044 standards. The results for treated wood guard rail posts are significant. • Less Energy & Resource Use: ...
AquAeTer, Inc.


Conclusions and Summary Report Environmental Life Cycle Assessment of Marine Pilings
2013 - IRG/WP 13-50298
The Treated Wood Council has completed a quantitative evaluation of the environmental impacts associated with the national production, use, and disposition of treated wood, concrete, galvanized steel, and plastic marine piles using life cycle assessment (LCA) methodologies and following ISO 14044 standards. The results for treated wood piles are significant. • Less Energy & Resource Use: Tre...
AquAeTer, Inc.


Conclusions and Summary Report on an Environmental Life Cycle Assessment of Utility Poles
2013 - IRG/WP 13-50299
The Treated Wood Council has completed a quantitative evaluation of the environmental impacts associated with the national production, use, and disposition of pentachlorophenol-treated wood, concrete, galvanized steel, and fiber-reinforced composite utility poles using life cycle assessment (LCA) methodologies and following ISO 14044 standards. The results for treated wood poles are significant. ...
AquAeTer, Inc.


Assessment of Scots pine sapwood susceptibility to moulds by determination of fungi growth and ergosterol content in infested wood
2014 - IRG/WP 14-20540
The susceptibility of wood to filamentous fungi (mould) attack is determine mainly by laboratory methods with descriptive grading of fungal growth on the surface of the wood specimens. It is a lot of different grading scale of fungi growth, but determination of the size of fungi growth is many times not easy, not clear and often difficult. Although the filamentous fungi are not included to microor...
A Fojutowski, A Koziróg, A Kropacz


In-ground durability of wood-based products – Comparative assessment of graveyard field tests and terrestrial microcosms
2014 - IRG/WP 14-20538
Traditionally wood durability and the effectiveness of wood preservatives are determined in so-called graveyard tests (according to EN 252 or AWPA E7). For laboratory testing, terrestrial microcosms (TMC) can serve as an alternative. Both tests have been applied for different types of wood-based materials, preservative treated, modified and unmodified wood. However, the usability of laboratory res...
A Soetbeer, L Meyer, C Brischke, P Larsson-Brelid, J Jermer


Indentation and pendulum hardness tests: two convenient assessment methods of the performance of exterior wood coatings
2015 - IRG/WP 15-40689
Developing formulations of exterior wood coatings with long service life is a big challenge. For many years in Europe the performances have been mainly evaluated through weathering tests (within the EN 927 series) followed by visual assessment (blistering, flaking, mould growth, chalking and cracking), colour and gloss measurements, and adhesion tests. Very recently the importance of the mechanica...
L Malassenet, L Podgorski, M Truskaller, G Grüll


A review of the analytical methods used in determining the decay resistance of heat treated wood
2015 - IRG/WP 15-40690
Heat treatment as a wood process is increasingly used because of its non-biocide behaviour and its low environmental impact. This sort of treatment is based on biopolymer chemical degradation by heat transfer. This process improves mainly the dimensional stability and the decay resistance of wood. Wood becomes darker after this type of treatment and thus gives it an aesthetic appearance. These i...
K Candelier, M-F Thévenon, A Pétrissans, S Dumarçay, P Gérardin, M Pétrissans


Environmental Fate of Micronized Copper
2015 - IRG/WP 15-50310
The environmental fate of wood preservatives is an important aspect to estimate the health and environmental impact. Although biocides from treated wood may be released into the soil, water or air, the latter pathway is frequently neglected in favour of leaching studies. Nonetheless, wood dust is well known to cause a variety of adverse health effects, in particular diseases to the respiratory tra...
C Civardi, L Schlagenhauf, J Benz, C Hirsch, J Van den Bulcke, M Schubert, J Van Acker, P Wick,


Transfer of microorganisms from wooden crates to foodstuffs: assessment of a transfer threshold
2016 - IRG/WP 16-20574
Wood is commonly used in contact with foodstuffs, for example for packaging fruits or vegetables. Most common species used are beech, pine, spruce and poplar. Wood is often considered as being less safe than plastic because it is less easy to clean whereas several studies have demonstrated that microorganisms cannot survive easily on wood (Milling et al., 2005; Revol-Junelles et al., 2005). Nation...
M Montibus, R Ismail, I Le Bayon, A Jasick, M Gabille, F Aviat, V Michel, M Federighi, M Kutnik


Previous Page | Next Page